{"id":29191,"date":"2016-07-27T08:00:39","date_gmt":"2016-07-27T00:00:39","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=29191"},"modified":"2016-07-27T08:58:19","modified_gmt":"2016-07-27T00:58:19","slug":"%e6%97%a5%e6%9c%ac%e6%8f%90%e5%8d%87%e8%88%aa%e7%a9%ba%e6%9d%90%e6%96%99%e5%87%ba%e5%8f%a3%e9%87%8f","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=29191","title":{"rendered":"\u65e5\u672c\u63d0\u5347\u822a\u7a7a\u6750\u6599\u51fa\u53e3\u91cf"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u65e5\u672c\u8bf8\u5bb6\u516c\u53f8\u7eb7\u7eb7\u6295\u8d44\u98de\u673a\u5236\u9020\u4e1a\u76f8\u5173\u4ea7\u4e1a\uff0c\u8fd9\u4f7f\u5f97\u822a\u7a7a\u6750\u6599\u51fa\u53e3\u91cf\u6c34\u6da8\u8239\u9ad8\uff0c\u4f5c\u4e3a\u56fd\u5bb6\u57fa\u7840\u5de5\u4e1a\u7684\u98de\u673a\u5236\u9020\u4e1a\u4e5f\u5f02\u519b\u7a81\u8d77\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-29193 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/0720N-Sumitomo-Chemical_article_main_image.jpg\" alt=\"0720N-Sumitomo-Chemical_article_main_image\" width=\"580\" height=\"365\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/0720N-Sumitomo-Chemical_article_main_image.jpg 580w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/07\/0720N-Sumitomo-Chemical_article_main_image-300x189.jpg 300w\" sizes=\"(max-width: 580px) 100vw, 580px\" \/><\/p>\n<p>\u4e1c\u4eac-\u65e5\u672c\u6750\u6599\u516c\u53f8\u5728\u56fd\u5185\u751f\u4ea7\u8bbe\u65bd\u65b9\u9762\u8fdb\u884c\u4e86\u79ef\u6781\u7684\u6295\u8d44\u4ee5\u4fc3\u8fdb\u98de\u673a\u76f8\u5173\u4ea7\u54c1\u7684\u751f\u4ea7\uff0c\u98de\u673a\u5236\u9020\u4e1a\u4f5c\u4e3a\u56fd\u5bb6\u57fa\u7840\u5de5\u4e1a\u5728\u65e5\u672c\u5f02\u519b\u7a81\u8d77\u3002<\/p>\n<p>\u4f4f\u53cb\u5316\u5b66\u5c06\u6295\u8d4450\u4ebf\u65e5\u5143($4.69\u5343\u4e07)\u5f00\u8bbe\u5de5\u5382\uff0c\u7528\u4e8e\u751f\u4ea7\u5de5\u7a0b\u7528\u6811\u8102-\u805a\u82ef\u919a\u781c\u3002\u76f8\u5173\u8bbe\u65bd\u5c06\u4e8e2018\u5e74\u5728\u5343\u53f6\u5e02\u3001\u5e02\u539f\u5e02\u521d\u6b65\u4eae\u76f8\u3002\u4ea7\u51fa\u7684\u805a\u82ef\u919a\u781c\u5c06\u7528\u4e8e\u5236\u9020\u8f7b\u8d28\u78b3\u7ea4\u7ef4\u589e\u5f3a\u5851\u6599\u6216CFRP\u3002\u805a\u82ef\u919a\u781c\u53ef\u589e\u5f3a\u5851\u6599\u7684\u7c98\u6027\uff0c\u4f7f\u5176\u66f4\u8010\u51b2\u51fb\u3002\u5728\u8fd9\u79cd\u5e94\u7528\u4e8e\u98de\u673a\u4e0a\u7684\u6811\u8102\u9886\u57df\uff0c\u4f4f\u53cb\u5316\u5b66\u516c\u53f8\u51e0\u4e4e\u62e5\u6709\u8d85\u8fc750%\u7684\u5168\u7403\u5e02\u573a\u5360\u6709\u7387\u3002<\/p>\n<p>\u98de\u673a\u5236\u9020\u5546\u8d8a\u6765\u8d8a\u591a\u5730\u4f7f\u7528CFRP\u6765\u964d\u4f4e\u71c3\u6599\u6210\u672c\uff0c\u540c\u65f6\uff0c\u5bf9\u805a\u82ef\u919a\u781c\u7684\u9700\u6c42\u4e5f\u4ee5\u6bcf\u5e7410%\u7684\u901f\u5ea6\u9010\u5e74\u4e0a\u6da8\u3002\u5e02\u539f\u5e02\u7684\u5de5\u5382\u4ee5\u6bcf\u5e743000\u5428\u7684\u4ea7\u91cf\u5927\u91cf\u751f\u4ea7\u805a\u82ef\u919a\u781c\uff0c\u4f7f\u4f4f\u53cb\u5316\u5b66\u6709\u80fd\u529b\u5c06\u805a\u82ef\u919a\u781c\u7684\u4ea7\u91cf\u7ffb\u500d\uff0c\u8fbe\u52306150\u5428\/\u5e74\u3002<\/p>\n<p>\u65e5\u672c\u78b3\u9ed1\u516c\u53f8\u6295\u8d4460\u4ebf\u65e5\u5143\u4e0e\u7f8e\u56fd\u98de\u673a\u5f15\u64ce\u5236\u9020\u5546\u901a\u7528\u7535\u6c14\u7b49\u5408\u4f5c\uff0c\u5728\u5bcc\u5c71\u53bf\u5efa\u7acb\u5de5\u5382\uff0c\u7528\u4e8e\u751f\u4ea7\u78b3\u5316\u7845\u7ea4\u7ef4\u3002\u78b3\u5316\u7845\u7ea4\u7ef4\u4e0e\u9676\u74f7\u70ed\u538b\u800c\u6210\u7684\u590d\u5408\u6750\u6599\u53ef\u80101900\u2103\u7684\u9ad8\u6e29\uff0c\u4e14\u5176\u8d28\u91cf\u53ea\u6709\u666e\u901a\u954d\u5408\u91d1\u7684\u4e09\u5206\u4e4b\u4e00\uff0c\u5f3a\u5ea6\u5374\u662f\u5176\u4e24\u500d\u3002\u901a\u7528\u7535\u6c14\u516c\u53f8\u5df2\u51b3\u5b9a\u5728\u6700\u65b0\u7684\u5f15\u64ce\u751f\u4ea7\u4e2d\u4f7f\u7528\u8fd9\u79cd\u590d\u5408\u6750\u6599\u3002<\/p>\n<p>\u65e5\u672c\u78b3\u9ed1\u516c\u53f8\u8ba1\u5212\u5728\u4eca\u5e74\u5e95\u542f\u52a8\u5927\u89c4\u6a21\u751f\u4ea7\uff0c\u4ea7\u91cf\u5c06\u4f1a\u4e0a\u5347\u81f3\u76ee\u524d\u4ea7\u91cf\u768410\u500d\uff0c\u8fbe\u523010\u5428\/\u5e74\u3002<\/p>\n<p>\u5b87\u90e8\u5de5\u4e1a\u81f4\u529b\u4e8e\u57282025\u5e74\u65f6\u5c06\u78b3\u5316\u7845\u7ea4\u7ef4\u7684\u5e74\u9500\u552e\u989d\u63d0\u9ad8\u81f350\u4ebf\u65e5\u5143\u3002\u516c\u53f8\u5c06\u5728\u5b87\u90e8\u5e02\u5c71\u53e3\u53bf\u9010\u6b65\u6269\u5c55\u5de5\u5382\uff0c\u4ee5\u589e\u52a0\u4ea7\u54c1\u751f\u4ea7\u91cf\u3002<\/p>\n<p>\u4e1c\u4e3d\u5de5\u4e1a\u6295\u8d4430\u4ebf\u65e5\u5143\u5347\u7ea7\u4f4d\u4e8e\u77f3\u5ddd\u53bf\u7528\u4e8e\u751f\u4ea7\u78b3\u7ea4\u7ef4\u7247\u6750\u7684\u5de5\u5382\uff0c\u622a\u6b62\u81f32014\u5e74\u5e95\u4ea7\u91cf\u5df2\u7ecf\u7ffb\u756a\u3002\u957f\u671f\u4ee5\u6765\uff0c\u8be5\u516c\u53f8\u4ea7\u54c1\u4e3b\u8981\u4f9b\u5e94\u7ed9\u6ce2\u97f3\u516c\u53f8\u3002\u4e0d\u8fc7\uff0c\u4ece6\u6708\u4efd\u5f00\u59cb\uff0c\u5176\u4ea7\u54c1\u4e5f\u9010\u6b65\u51fa\u552e\u7ed9\u201c\u6b27\u6d32\u7a7a\u4e2d\u5df4\u58eb\u201d\u516c\u53f8\u7528\u4e8e\u98de\u673a\u7684\u4e00\u7ea7\u7ed3\u6784\u5236\u9020\u3002\u8be5\u516c\u53f8\u56e0\u6b64\u5927\u5927\u6269\u5c55\u4e86\u5ba2\u6237\u7fa4\u3002<\/p>\n<p>\u65e5\u672c\u516c\u53f8\u6b63\u5728\u6210\u4e3a\u673a\u7ffc\u3001\u673a\u8eab\u53ca\u5176\u4ed6\u98de\u673a\u6750\u6599\u7684\u4f9b\u5e94\u5546\u3002\u6750\u6599\u751f\u4ea7\u5546\u4eec\u7eb7\u7eb7\u52a0\u5165\uff0c\u4ee5\u671f\u5728\u5de5\u4e1a\u589e\u957f\u7684\u5927\u6f6e\u4e2d\u83b7\u53d6\u6536\u76ca\u3002<\/p>\n<p>\u53c2\u8003\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/asia.nikkei.com\/Business\/Trends\/Japanese-companies-lift-domestic-output-of-aircraft-materials\" target=\"_blank\">Japanese companies lift domestic output of aircraft materials<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u5c09\u8c37\u96e8\u63d0\u4f9b\u7d20\u6750\uff0c\u4faf\u5029\u7f16\u8bd1\uff0c<a href=\"http:\/\/cailiaoren.mikecrm.com\/6qSdMU\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u65e5\u672c\u8bf8\u5bb6\u516c\u53f8\u7eb7\u7eb7\u6295\u8d44\u98de\u673a\u5236\u9020\u4e1a\u76f8\u5173\u4ea7\u4e1a\uff0c\u8fd9\u4f7f\u5f97\u822a\u7a7a\u6750\u6599\u51fa\u53e3\u91cf\u6c34\u6da8\u8239\u9ad8\uff0c\u4f5c\u4e3a\u56fd\u5bb6\u57fa\u7840\u5de5\u4e1a\u7684\u98de\u673a\u5236\u9020\u4e1a\u4e5f\u5f02\u519b\u7a81\u8d77\u3002 \u4e1c\u4eac-\u65e5\u672c\u6750\u6599\u516c\u53f8\u5728\u56fd\u5185\u751f\u4ea7\u8bbe\u65bd\u65b9\u9762\u8fdb&#8230;<\/p>\n","protected":false},"author":713,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[3],"tags":[],"class_list":["post-29191","post","type-post","status-publish","format-standard","hentry","category-yejie"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/29191"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/713"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=29191"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/29191\/revisions"}],"predecessor-version":[{"id":29399,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/29191\/revisions\/29399"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=29191"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=29191"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=29191"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}