{"id":30836,"date":"2016-08-03T18:00:44","date_gmt":"2016-08-03T10:00:44","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=30836"},"modified":"2016-08-09T12:33:04","modified_gmt":"2016-08-09T04:33:04","slug":"adv-funct-mater-%e6%9c%80%e6%96%b0%e6%96%87%e7%8c%ae%e5%bf%ab%e8%ae%af%e4%b8%93%e9%a2%98-8-2%e5%8f%b7%e6%9b%b4%e6%96%b0","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=30836","title":{"rendered":"Adv. Funct. Mater. \u6700\u65b0\u6587\u732e\u5feb\u8baf\u4e13\u9898-8.2\u66f4\u65b0"},"content":{"rendered":"<p>\u672c\u671f\u4e13\u9898\u8ddf\u8e2a\u4e86Advanced Functional Materials\u4e8e2016\u5e748\u67082\u65e5\u89c1\u520a<strong>\uff08<\/strong><strong>Volume 26,\u00a0Issue 29<\/strong><strong>\uff09<\/strong>\u7684\u6240\u6709\u6587\u732e\uff0c\u5e76\u505a\u76f8\u5173\u5bfc\u8bfb\uff0c\u76f8\u5173\u6587\u732e\u8d44\u6e90\u7f51\u53cb\u5df2\u4e0a\u4f20\uff0c<a href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">\u70b9\u6211\u8df3\u8f6c\u5230\u6750\u6599\u4eba\u8bba\u575b\u4e0b\u8f7d<\/a>\uff08\u5fae\u4fe1\u8bfb\u8005\u8bf7\u70b9\u51fb\u9605\u8bfb\u539f\u6587\uff09\u3002<\/p>\n<p>\u672c\u671fAFM\u5171\u66f4\u65b0\u6587\u732e22\u7bc7\uff0c\u5176\u4e2d\u4e2d\u56fd\u4f5c\u8005\u6587\u7ae08\u7bc7<span style=\"color: #ff0000;\"><strong>\u3010\u534e\u4e1c\u7406\u5de5\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u4e0a\u6d77\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u6b66\u6c49\u7406\u5de5\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u5317\u4eac\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u5357\u4eac\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u82cf\u5dde\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u4e2d\u79d1\u9662\u5316\u5b66\u6240\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u6d59\u6c5f\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u90d1\u5dde\u5927\u5b66\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3001\u4e2d\u79d1\u9662\u56fd\u5bb6\u7eb3\u7c73\u79d1\u5b66\u4e2d\u5fc3\uff08<\/strong><strong>2<\/strong><strong>\uff09\u3001\u4e2d\u79d1\u9662\u6709\u673a\u56fa\u4f53\u91cd\u70b9\u5b9e\u9a8c\u5ba4\uff08<\/strong><strong>1<\/strong><strong>\uff09\u3011<\/strong><\/span>\uff0c\u6587\u7ae0\u5206\u522b\u6d89\u53ca\u4e09\u7ef4\u73af\u5f62\u7eb3\u7c73\u7ed3\u6784\u3001\u7eb3\u7c73\u53d1\u7535\u673a\u3001\u53ef\u4f38\u7f29\u7535\u5b50\u3001\u55b7\u58a8\u6253\u5370\u6750\u6599\u3001\u7535\u81f4\u53d8\u8272\u5668\u4ef6\u3001\u6709\u673a\u534a\u5bfc\u4f53\u6750\u6599\u7b49\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-30838 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762.png\" alt=\"\u5c01\u9762\" width=\"600\" height=\"799\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762-225x300.png 225w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u5c01\u9762\u6587\u7ae0\uff1a\u5229\u7528\u5149\u7684\u5e72\u6d89\u4e0e\u884d\u5c04\u5408\u7406\u6784\u5efa\u7684\u4e09\u7ef4\u73af\u5f62\u7eb3\u7c73\u7ed3\u6784<\/strong><\/span><\/p>\n<p>\u97e9\u56fd\u5927\u5b66\u7269\u7406\u7cfb\u7684Eun-Ah You\u7b49\u5229\u7528\u7d2b\u5916\u5149\u7684\u5e72\u6d89\u548c\u884d\u5c04\u53d1\u73b0\u4e00\u79cd\u7b80\u4fbf\u3001\u5408\u7406\u7684\u65b9\u6cd5\u6784\u5efa\u53ef\u8c03\u5c42\u6570\u7684\u4e09\u7ef4\u73af\u5f62\u7eb3\u7c73\u7ed3\u6784\u3002\u4ed6\u4eec\u901a\u8fc7\u79bb\u6563\u5316\u7684\u4eae\u70b9\u548c\u9a7b\u6ce2\u53ef\u4ee5\u91c7\u7528\u7b80\u5355\u4f20\u7edf\u7684\u5149\u523b\u6280\u672f\u5b9e\u73b0\u8fd9\u4e00\u7ed3\u6784\u3002\u8fd9\u4e00\u65b9\u6cd5\u4e5f\u5c06\u9002\u7528\u4e8e\u9700\u8981\u5236\u5907\u9ad8\u901a\u91cf\u5927\u9762\u79ef\u7684\u4e09\u7ef4\u7ed3\u6784\u7684\u4f17\u591a\u5e94\u7528\u4e2d\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31031\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762-1.png\" alt=\"\u5c01\u9762\" width=\"600\" height=\"261\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762-1-300x131.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u4e09\u7ef4\u73af\u72b6\u7eb3\u7c73\u7ed3\u6784\u793a\u610f\u56fe<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Rational and Facile Construction of 3D Annular Nanostructures with Tunable Layers by Exploiting the Diffraction and Interference of Light\uff08Adv. Funct. Mater., 2016, DOI: 10.1002\/adfm.201670183\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u5c01\u9762\u5185\u9875\uff1a\u81ea\u4f9b\u80fd\u7684\u53ef\u690d\u5165\u7535\u963b\u8bb0\u5fc6\u8bbe\u5907<\/strong><\/span><\/p>\n<p>\u97e9\u56fd\u5927\u5b66\u7684Sahn Nahm\u7b49\u5c06(Na<sub>0.5<\/sub>K<sub>0.5<\/sub>)NbO<sub>3<\/sub>\uff08NKN\uff09\u5206\u522b\u751f\u957f\u5728TiN\/SiO<sub>2<\/sub>\/Si\u57fa\u5e95\u4e0a\u4f5c\u4e3a\u963b\u53d8\u5b58\u50a8\u5668\u4ee5\u53ca\u67d4\u6027TiN\/PI\uff08\u805a\u9170\u4e9a\u80fa\uff09\u4e0a\u4f5c\u4e3a\u7eb3\u7c73\u53d1\u7535\u673a\u6784\u5efa\u53ef\u690d\u5165\u5f0f\u7684\u81ea\u4f9b\u80fd\u7684\u963b\u53d8\u5b58\u50a8\u5668\u3002\u8be5NKN\u81ea\u4f9b\u80fd\u5668\u4ef6\u5177\u6709\u53cc\u6781\u53d8\u5316\u7279\u6027\uff0c\u53ef\u4ee5\u83b7\u5f97\u7a33\u5b9a\u768410<sup>2<\/sup>\u7684\u5f00\/\u5173\u53d8\u5316\u7387\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31032\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875.png\" alt=\"\u5c01\u9762\u5185\u9875\" width=\"598\" height=\"543\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875.png 598w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875-300x272.png 300w\" sizes=\"(max-width: 598px) 100vw, 598px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u53ef\u690d\u5165\u7684\u81ea\u4f9b\u80fd\u963b\u53d8\u5b58\u50a8\u5668\u7684\u7ed3\u6784\u4e0e\u7b80\u5355\u673a\u7406\u56fe<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Resistive Switching Memory Integrated with Nanogenerator for Self-Powered Bioimplantable Devices \uff08Adv. Funct. Mater., 2016, DOI: 10.1002\/adfm.201505569\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u5168\u6587\uff1a<\/strong><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u00a01.<\/strong><strong>\u53ef\u770b\u900f\u7535\u81f4\u53d8\u8272\u5668\u4ef6\uff1a\u6700\u5148\u8fdb\u7684\u591a\u5f69\u805a\u5408\u7269\u7528\u4e8e\u9ad8\u5bf9\u6bd4\u5ea6\u7535\u81f4\u53d8\u8272\u5668\u4ef6\u3002<\/strong><\/span><\/p>\n<p>\u610f\u5927\u5229\u5e15\u591a\u74e6\u5927\u5b66\u7684Luca Beverina\u7b49\u63d0\u51fa\u4e24\u79cd\u65b0\u578b\u591a\u5f69\u8272\u7535\u81f4\u53d8\u8272\u805a\u5408\u7269\uff0c\u7531\u5171\u8f6d\u7684EDOT\/ProDOT\u4f5c\u4e3a\u5171\u805a\u7269\u4e3b\u94fe\u4ee5\u53caWeitz-\u578b\u7684\u6c27\u5316\u8fd8\u539f\u6d3b\u6027\u7535\u81f4\u53d8\u8272\u5c0f\u5206\u5b50\u8fde\u63a5\u7269\uff08WTE\uff09\u3002\u8fd9\u79cdWTE\u5b9e\u73b0\u4e86\u9ad8\u5ea6\u53ef\u9006\u7684\u6c27\u5316\u8fd8\u539f\u53cd\u5e94\uff0c\u4ee5\u65e0\u8272-\u7ea2\u8272\u53d8\u6362\u8865\u5145\u4e86\u4e3b\u94fe\u7684\u65e0\u8272-\u84dd\u8272\u7684\u53d8\u6362\uff0c\u8fd9\u8fdb\u4e00\u6b65\u7a81\u7834\u4e86\u6eb6\u6db2\u52a0\u5de5\u5b9e\u73b0\u7684\u805a\u5408\u7269\u5c42\u4ee5\u5b9e\u73b0\u53ef\u770b\u900f\u7535\u81f4\u53d8\u8272\u5668\u4ef6\u7684\u8bbe\u8ba1\u5c40\u9650\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/1-5.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31033\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/1-5.png\" alt=\"1\" width=\"600\" height=\"426\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/1-5.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/1-5-300x213.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u65b0\u578b\u591a\u5f69\u805a\u5408\u7269\u7535\u81f4\u53d8\u8272\u5668\u4ef6\u7684\u5149\u5b66\u6027\u80fd<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">State-of-the-Art Neutral Tint Multichromophoric Polymers for High-Contrast See-Through Electrochromic Devices\uff08Adv. Funct. Mater., 2016, DOI:\u00a010.1002\/adfm.201601819\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>2.\u6c22\u952e\u6709\u673a\u534a\u5bfc\u4f53\u6750\u6599\u4f5c\u4e3a\u9ad8\u6548\u7a33\u5b9a\u7684\u8fc7\u6c27\u5316\u6c22\u5149\u5408\u4f5c\u7528\u7684\u5149\u7535\u50ac\u5316\u5242<\/strong><\/span><\/p>\n<p>\u7ea6\u7ff0\u5f00\u666e\u52d2\u6797\u8328\u5927\u5b66\u7684Eric Daniel G\u0142owacki\u7b49\u9996\u6b21\u62a5\u9053\u4e86\u901a\u8fc7\u6c22\u952e\u6709\u673a\u534a\u5bfc\u4f53\u5728\u7535\u89e3\u8d28\u6c34\u6eb6\u6db2\u4e2d\u5149\u7535\u50ac\u5316\u6c27\u8fd8\u539f\u4e3a\u8fc7\u6c27\u5316\u7269\u3002\u7814\u7a76\u53d1\u73b0\u8fd9\u79cd\u6750\u6599\u80fd\u5728\u8fde\u7eed\u7167\u660e\u51e0\u5929\u7684\u60c5\u51b5\u4e0b\u4e8e\u5149\u7535\u5316\u5b66\u7535\u6c60\u4e2d\u7a33\u5b9a\u5de5\u4f5c\uff0c\u4e14\u5de5\u4f5c\u73af\u5883\u7684pH\u503c\u8303\u56f4\u4ece1\u523012\u3002\u5176\u5c31\u5355\u4f4d\uff08\u8fc7\u6c27\u5316\u6c22\u4ea7\u91cf\/\u50ac\u5316\u5242\u7528\u91cf\/\u65f6\u95f4\uff09\u50ac\u5316\u6027\u80fd\u800c\u8a00\u66f4\u662f\u8d85\u8fc7\u4e4b\u524d\u62a5\u9053\u7684\u4e00\u5230\u4e24\u4e2a\u6570\u91cf\u7ea7\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/2-6.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31034\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/2-6.png\" alt=\"2\" width=\"600\" height=\"547\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/2-6.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/2-6-300x274.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\">\u5177\u6709EPI\u534a\u5bfc\u4f53\u7535\u6781\u7684\u5149\u7535\u50ac\u5316\u6d4b\u8bd5\u7ed3\u6784\u56fe<\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Hydrogen-Bonded Organic Semiconductors as Stable Photoelectrocatalysts for Efficient Hydrogen Peroxide Photosynthesis\uff08Adv. Funct. Mater., 2016, DOI:\u00a010.1002\/adfm.201601946\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>3.\u5e73\u9762\u7eb3\u7c73\u7b5b\uff1a\u591a\u529f\u80fd\u7eb3\u7c73\u7b5b\u7528\u4e8e\u7eb3\u7c73\u5149\u5b66\u8bbe\u65bd<\/strong><\/span><\/p>\n<p>\u65b0\u52a0\u5761\u56fd\u7acb\u5927\u5b66\u7684Qiu Chengwei\u7b49\u4eba\u63d0\u51fa\u4e86\u4e00\u6761\u5341\u5206\u6709\u524d\u666f\u7684\u5173\u4e8e\u7eb3\u7c73\u7b5b\u57fa\u87ba\u65cb\u8bbe\u5907\u7684\u6280\u672f\u8def\u7ebf\uff0c\u5728\u5b9e\u9a8c\u4e0a\u5df2\u7ecf\u8bc1\u5b9e\u662f\u53ef\u884c\u7684\uff0c\u5b83\u53ef\u4ee5\u5b9e\u73b0\u5149\u6f29\u6da1\u7684\u5168\u64cd\u4f5c\u5305\u62ec\u5149\u6f29\u6da1\u7684\u4ea7\u751f\u3001\u6742\u5316\u3001\u591a\u8def\u590d\u7528\u3001\u805a\u7126\u4ee5\u53ca\u65e0\u884d\u5c04\u4f20\u64ad\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/3-5.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31036\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/3-5.png\" alt=\"3\" width=\"595\" height=\"359\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/3-5.png 595w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/3-5-300x181.png 300w\" sizes=\"(max-width: 595px) 100vw, 595px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u7eb3\u7c73\u7b5b\u7684\u591a\u529f\u80fd\u5e94\u7528<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Flat Helical Nanosieves (Adv. Funct. Mater. 2016, DOI: 10.1002\/adfm.201601345)<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>4.\u56fd\u5bb6\u7eb3\u7c73\u79d1\u5b66\u4e2d\u5fc3\uff1a\u6709\u673a<\/strong><strong>&#8211;<\/strong><strong>\u65e0\u673a\u9499\u949b\u77ff\u590d\u5408\u6750\u6599\u7528\u4e8e\u5149\u7535\u3001\u5149\u4f0f\u8bbe\u5907<\/strong><\/span><\/p>\n<p>\u56fd\u5bb6\u7eb3\u7c73\u79d1\u5b66\u4e2d\u5fc3\u7684Lin Niu\uff08\u7b2c\u4e00\u4f5c\u8005\uff09\u3001\u5218\u65b0\u98ce\u548c\u5357\u6d0b\u7406\u5de5\u5927\u5b66\u7684\u5218\u653f\uff08\u5171\u540c\u901a\u8baf\uff09\u7b49\u4eba\u7528\u4fbf\u6377\u7684\u4e24\u6b65\u6c14\u76f8\u8f93\u8fd0\u6dc0\u79ef\u6cd5\u5728SiO<sub>2<\/sub>\/Si\u57fa\u5e95\u4e0a\u63a7\u5236\u5408\u6210\u4e86\u6709\u673a\u5364\u5316\u94c5\u9499\u949b\u77ff\u7eb3\u7c73\u7247\uff0c\u5e76\u7814\u7a76\u4e86\u7eb3\u7c73\u7247\u539a\u5ea6\u4e0e\u5149\u7535\u6027\u80fd\u7684\u5173\u7cfb\uff0c\u53d1\u73b0\u7eb3\u7c73\u7247\u539a\u5ea6\u572830nm\u65f6\u5177\u6709\u6700\u597d\u7684\u5149\u7535\u54cd\u5e94\u6027\u80fd\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/4-4.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31038\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/4-4.png\" alt=\"4\" width=\"600\" height=\"258\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/4-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/4-4-300x129.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u9499\u949b\u77ff\u7eb3\u7c73\u7247\u5149\u7535\u6027\u80fd\u4e0e\u539a\u5ea6\u7684\u5173\u7cfb<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Controlled Growth and Reliable Thickness-Dependent Properties of Organic\u2013Inorganic Perovskite Platelet Crystal (Adv. Funct. Mater. 2016, DOI: 10.1002\/adfm.201601392)<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>5.\u4ece\u5757\u4f53\u5230\u7eb3\u7c73\u5c3a\u5ea6\u7684\u529b\u3001\u5149\u81f4\u53d8\u8272\uff1a\u5355\u6839\u81ea\u7ec4\u88c5\u4e1d\u5e26\u4e0a\u7684\u6570\u636e\u5b58\u50a8<\/strong><\/span><\/p>\n<p>\u5fb7\u56fd\u5361\u5c14\u65af\u9c81\u5384\u7406\u5de5\u5b66\u9662\u7684Damiano Genovese\u53caLuisa De Cola\u7b49\uff08\u5171\u540c\u901a\u8baf\uff09\u53d1\u73b0\u5229\u7528\u94c2\u7684\u590d\u5408\u7269\u80fd\u591f\u5728\u8d85\u957f\u5e26\u4e0a\u81ea\u7ec4\u88c5\uff0c\u4e14\u5728\u7eb3\u7c73\u5c3a\u5ea6\u7684\u529b\u6fc0\u52b1\u4e0b\u5c55\u73b0\u51fa\u529b\u81f4\u53d8\u8272\u73b0\u8c61\u3002\u539f\u5b50\u529b\u663e\u5fae\u955c\uff08AFM\uff09\u53d1\u73b0\uff0c\u529b\u81f4\u53d8\u8272\u4ec5\u5728\u539f\u4f4d\u523a\u6fc0\u7684\u77ed\u8ddd\u79bb\u5185\u80fd\u591f\u53d1\u751f\uff0c\u53ef\u4ee5\u636e\u6b64\u5728\u5355\u6839\u81ea\u7ec4\u88c5\u7684\u4e1d\u5e26\u4e0a\u8bbe\u8ba1\u5229\u7528AFM\u7eb3\u7c73\u5149\u523b\u9ad8\u5bc6\u5ea6\u4fe1\u606f\u3002\u53e6\u5916\uff0c\u6709\u673a\u53d1\u5149\u7684\u5149\u81f4\u53d8\u8272\u73b0\u8c61\u4e5f\u53ef\u7528\u4e8e\u5c01\u88c5\u548c\u64e6\u9664\u4fe1\u606f\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/5-4.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31040\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/5-4.png\" alt=\"5\" width=\"600\" height=\"194\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/5-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/5-4-300x97.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u529b\u81f4\u53d8\u8272\u54cd\u5e94\u56fe\u53ca\u7eb3\u7c73\u5149\u523b\u4e0e\u5149\u81f4\u53d8\u8272\u7684\u7ed3\u5408\u5e94\u7528<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Mechano- and Photochromism from Bulk to Nanoscale\uff1aData Storage on Individual Self-Assembled Ribbons\uff08Adv. Funct. Mater., 2016,DOI: 10.1002\/adfm.201601269\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>6.\u7eb3\u7c73\u590d\u5408\u6750\u6599\uff1a\u94bb\u77f3\u7eb3\u7c73\u7ebf<\/strong><strong>(DNT)<\/strong><strong>\u4f5c\u4e3a\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u589e\u5f3a\u4f53<\/strong><\/span><\/p>\n<p>\u65b0\u52a0\u5761\u9ad8\u6027\u80fd\u8ba1\u7b97\u7814\u7a76\u9662\u7684Zhang Gang\u4ee5\u53ca\u6606\u58eb\u5170\u79d1\u6280\u5927\u5b66\u7684Gu Yuantong\u7b49\uff08\u5171\u540c\u901a\u8baf\uff09\u4eba\u7814\u7a76\u4e86DNT\/PE(\u805a\u4e59\u70ef)\u4e4b\u95f4\u7684\u8f7d\u8377\u8f6c\u79fb\u4ee5\u53ca\u754c\u9762\u5207\u5e94\u529b\u5206\u6790\u7b49\uff0c\u8fd9\u9879\u7814\u7a76\u9996\u6b21\u89e3\u91ca\u4e86DNT\u4e0e\u805a\u5408\u7269\u4e4b\u95f4\u7684\u8f7d\u8377\u8f6c\u79fb\uff0c\u4e3a\u672a\u6765DNTs\u4f5c\u4e3a\u5404\u79cd\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u589e\u5f3a\u4f53\u63d0\u4f9b\u4e86\u57fa\u7840\u7406\u8bba\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/6-4.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31041\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/6-4.png\" alt=\"6\" width=\"600\" height=\"378\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/6-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/6-4-300x189.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>DNT\/PE\u62c9\u62d4\u6a21\u62df<\/strong><\/p>\n<p style=\"text-align: left;\"><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\">Diamond Nanothread as a New Reinforcement for Nanocomposites (Adv. Funct. Mater. 2016, DOI: 10.1002\/adfm.201600119)<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>7.\u4e2d\u79d1\u9662\u6709\u673a\u56fa\u4f53\u91cd\u70b9\u5b9e\u9a8c\u5ba4\uff1a\u9ad8\u6027\u80fd\u80f6\u4f53\u91cf\u5b50\u70b9\u7528\u4e8e\u592a\u9633\u80fd\u7535\u6c60\u7a7a\u7a74\u4f20\u8f93\u5c42<\/strong><\/span><\/p>\n<p>\u77f3\u58a8\u7094\uff0c\u4e00\u79cd\u65b0\u578b\u5927\u03c0\u5171\u8f6d\u78b3\u7a7a\u7a74\u4f20\u8f93\u6750\u6599\uff0c\u88ab\u7528\u4f5c\u80f6\u4f53\u91cf\u5b50\u70b9\u592a\u9633\u80fd\u7535\u6c60\u7684\u9633\u6781\u7f13\u51b2\u5c42\u3002\u4e0e\u5176\u76f8\u540c\u7684\u671f\u95f4\u7ed3\u6784\u76f8\u6bd4\uff0c\u529f\u7387\u8f6c\u6362\u6548\u7387\u4ece9.49%\u663e\u7740\u63d0\u5347\u523010.64%\u3002\u4ece\u91cf\u5b50\u70b9\u56fa\u4f53\u6d3b\u6027\u5c42\u5230\u9633\u6781\u7684\u7a7a\u7a74\u4f20\u8f93\u53ea\u80fd\u901a\u8fc7\u77f3\u58a8\u7094\u6765\u964d\u4f4e\u91cf\u5b50\u70b9\u56fa\u4f53\u7684\u529f\u51fd\u6570\u6765\u8fbe\u5230\u76ee\u7684\u3002\u4e2d\u79d1\u9662\u6709\u673a\u56fa\u4f53\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u7684\u674e\u7389\u826f\u3001Jizheng Wang\u4ee5\u53ca\u591a\u4f26\u591a\u5927\u5b66\u7684Edward H. Sargent\u7b49\uff08\u5171\u540c\u901a\u8baf\uff09\u7684\u7814\u7a76\u8868\u660e\u5168\u78b3\u7f13\u51b2\u5c42\u5ef6\u957f\u4e86\u8f7d\u6d41\u5b50\u5bff\u547d\uff0c\u964d\u4f4e\u4e86\u5148\u524d\u88ab\u5ffd\u89c6\u7684\u8868\u9762\u5149\u4f0f\u80cc\u9762\u7684\u91cd\u7ec4\u88c5\u7f6e\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u8be5\u88c5\u7f6e\u8fd8\u8868\u73b0\u51fa\u4e86\u8f83\u9ad8\u7684\u7a33\u5b9a\u6027\u3002\u7ed3\u679c\u8868\u660e\uff0c\u77f3\u58a8\u7094\u6709\u671b\u5e94\u7528\u5728\u5149\u7535\u6750\u6599\u7684\u5404\u79cd\u65b9\u9762\uff0c\u4ece\u800c\u589e\u5f3a\u6750\u6599\u6027\u80fd<strong>\u3002<\/strong><\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/7-3.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31042\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/7-3.png\" alt=\"7\" width=\"600\" height=\"325\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/7-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/7-3-300x163.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u4ee5\u77f3\u58a8\u7094\u4e3a\u9633\u6781\u7684PbS\u80f6\u4f53\u91cf\u5b50\u70b9\u592a\u9633\u80fd\u7535\u6c60\u539f\u7406\u56fe\u53ca\u5176\u5149\u7535\u6027\u80fd<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Graphdiyne: An Efficient Hole Transporter for Stable High-Performance Colloidal Quantum Dot Solar Cells\uff08Adv. Funct. Mater. 2016,DOI: 10.1002\/adfm.201601570\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>8.\u9ad8\u901f\u5ea6\u3001\u4f4e\u80fd\u91cf\u7684\u6c2e\u5316\u7269\u5fc6\u963b\u5668<\/strong><\/span><\/p>\n<p>\u7f8e\u56fd\u4f11\u5229\u7279\u5e15\u5361\u5fb7\u5b9e\u9a8c\u5ba4\u7684R. Stanley Williams\u53caJ. Joshua Yang\u7b49\uff08\u5171\u540c\u901a\u8baf\uff09\u91c7\u7528AlN\u8584\u819c\u4f5c\u4e3a\u9ad8\u6027\u80fd\u5fc6\u963b\u5668\uff0c\u5c55\u793a\u51fa\u8d85\u5feb\u7684\u5f00\u5173\u65f6\u95f4\uff08\u5728\u5149\u5bfc\u4e2d\u7684\u5fae\u5668\u4ef6\u4e3a85 ps\uff09\u4ee5\u53ca\u8f83\u4f4e\u7684\u5f00\u5173\u7535\u6d41\uff0850 nm\u5668\u4ef6\u4e2d\u7ea615 \u03bcA\uff09\uff0c\u5176\u5feb\u901f\u7684\u5f00\u5173\u7279\u6027\u53ef\u80fd\u4e0e\u5e26\u6b63\u7535\u7684\u6c2e\u7a7a\u4f4d\u7684\u8fd0\u52a8\u6709\u5173\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/8-4.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31043\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/8-4.png\" alt=\"8\" width=\"600\" height=\"867\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/8-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/8-4-208x300.png 208w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u5fc6\u963b\u5668\u7684\u5feb\u901f\u54cd\u5e94\u7279\u6027\u53ca\u673a\u7406\u7b80\u56fe<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">High-Speed and Low-Energy Nitride Memristors\uff08Adv. Funct. Mater., 2016, DOI: 10.1002\/adfm.201600680\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>9.\u6709\u673a<\/strong><strong>&#8211;<\/strong><strong>\u65e0\u673a\u6742\u5316\u7684\u9499\u949b\u77ff\u6750\u6599\u4e2d\u5404\u5411\u5f02\u6027\u7684\u8d85\u58f0\u5b50\u70ed\u8f93\u8fd0<\/strong><\/span><\/p>\n<p>\u4f5b\u7f57\u91cc\u8fbe\u5dde\u7acb\u5927\u5b66\u7684Shangchao Lin\u7b49\u91c7\u7528\u5e73\u8861\u5206\u5b50\u52a8\u529b\u5b66\u6a21\u62df\u53d1\u73b0\uff1a\u7532\u57fa\u7898\u5316\u94c5\uff08MAPbI<sub>3<\/sub>\uff09\u5728\u4e0d\u540c\u6676\u76f8\u4e2d\u7684\u70ed\u5bfc\u7387\u5c0f\u4e8e1 W m<sup>\u2212<\/sup><sup>1<\/sup> K<sup>\u2212<\/sup><sup>1<\/sup>\uff0c\u5728\u5ba4\u6e29\u4e0b\u4f4e\u81f30.31 W m<sup>\u22121<\/sup> K<sup>\u22121<\/sup>\u3002\u540c\u65f6\u63a2\u7a76\u4e86\u5bfc\u81f4\u8fd9\u79cd\u8d85\u4f4e\u5bfc\u70ed\u6027\u3001\u58f0\u5b50\u5bff\u547d\u548c\u5e73\u5747\u81ea\u7531\u7a0b\u77ed\u4ee5\u53ca\u5728\u4f4e\u6e29\u4e0b\u70ed\u5bfc\u7387\u7684\u5404\u5411\u5f02\u6027\u4ea7\u751f\u539f\u56e0\u7b49\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/9-4.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31046\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/9-4.png\" alt=\"9\" width=\"600\" height=\"236\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/9-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/9-4-300x118.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u4e0d\u540c\u6676\u76f8\u7684\u70ed\u5bfc\u6027\u80fd\u56fe<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\">Anisotropic and Ultralow Phonon Thermal Transport in Organic\u2013Inorganic Hybrid Perovskites: Atomistic Insights into Solar Cell Thermal Management and Thermoelectric Energy Conversion Efficiency\uff08Adv. Funct. Mater., 2016, DOI:\u00a010.1002\/adfm.201600284\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>10.\u90d1\u5dde\u5927\u5b66\uff1a\u7af9\u7ea4\u7ef4\u72b6\u6c2e\u5316\u9553\u7eb3\u7c73\u7ebf\u6784\u6210\u7684\u538b\u7535\u5f0f\u5fc6\u963b\u6750\u6599<\/strong><\/span><\/p>\n<p>\u90d1\u5dde\u5927\u5b66\u6750\u6599\u7269\u7406\u5b9e\u9a8c\u5ba4\u7684\u5218\u6d77\u6d9b\u7b49\u4eba\u901a\u8fc7\u5316\u5b66\u6c14\u76f8\u6c89\u79ef\u6cd5\u5408\u6210\u4e86\u7af9\u7ea4\u7ef4\u72b6\u6c2e\u5316\u9553\u7eb3\u7c73\u7ebf\u6765\u5236\u4f5c\u538b\u7535\u5f0f\u5fc6\u963b\u6750\u6599\u3002\u5b9e\u9a8c\u7ed3\u679c\u8868\u660e\u6240\u5236\u6210\u7684\u5668\u4ef6\u5728\u65ad\u5f00\u7535\u6e90\u65f6\u53ef\u4ee5\u8bb0\u5fc6\u8fd1\u671f\u6240\u6709\u7684\u7535\u963b\u72b6\u6001\uff0c\u800c\u4e14\u901a\u8fc7\u8f6c\u6362\u5ef6\u8fdf\u6548\u5e94\u8c03\u6574\u6ce2\u5f62\uff0c\u8be5\u5b9e\u9a8c\u8868\u660e\u53ef\u4ee5\u4f7f\u7528\u7eb3\u7c73\u7ed3\u6784\u538b\u7535\u6750\u6599\u7684\u538b\u7535\u6027\u8d28\u6765\u8bbe\u8ba1\u6216\u8005\u4fee\u6b63\u5fc6\u963b\u5668\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/10-4.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31047\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/10-4.png\" alt=\"10\" width=\"600\" height=\"433\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/10-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/10-4-300x217.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u5fc6\u963b\u5143\u4ef6\u7684\u8bb0\u5fc6\u6027\u80fd<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">A Bamboo-Like GaN Microwire-Based Piezotronic Memristor(Adv. Funct. Mater. 2016,DOI: 10.1002\/adfm.201600962\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>11.\u6d59\u6c5f\u5927\u5b66\uff1a\u666e\u9c81\u58eb\u84dd\uff08<\/strong><strong>PB<\/strong><strong>\uff09<\/strong><strong>@ C<\/strong><strong>\u590d\u5408\u6750\u6599\u4f5c\u4e3a\u9ad8\u500d\u7387\u548c\u957f\u5bff\u547d\u7684\u94a0\u79bb\u5b50\u7535\u6c60\u6b63\u6781\u6750\u6599<\/strong><\/span><\/p>\n<p>\u6d59\u6c5f\u5927\u5b66\u6750\u6599\u5b66\u9662\u59dc\u94f6\u73e0\u3001Yunhao Lu\u56e2\u961f\u548c\u6fb3\u5927\u5229\u4e9aWollongong\u5927\u5b66\u5b59\u6587\u5e73\u7814\u7a76\u5458\u7b49\uff08\u5171\u540c\u901a\u8baf\uff09\u4e3a\u4e86\u7814\u7a76\u7a7a\u4f4d\u5bf9\u94a0\u50a8\u5b58\u7684\u5f71\u54cd\u4ee5\u53ca\u5d4c\u94a0\u53cd\u5e94\u52a8\u529b\u5b66\uff0c\u63d0\u51fa\u4e86\u7528\u666e\u9c81\u58eb\u84dd@C\u4f5c\u4e3a\u94a0\u79bb\u5b50\u7535\u6c60\u6b63\u6781\u6750\u6599\u3002\u5f62\u72b6\u5b8c\u7f8e\u7684\u7eb3\u7c73PB\u7acb\u65b9\u4f53\u76f4\u63a5\u751f\u957f\u5728\u78b3\u94fe\u4e0a\uff0c\u4fdd\u8bc1\u4e86\u7535\u8377\u7684\u8f6c\u79fb\u548c\u94a0\u79bb\u5b50\u7684\u6269\u6563\u3002\u5728\u5f62\u72b6\u4e0e\u7ed3\u6784\u7684\u534f\u540c\u4f5c\u7528\u4e0b\uff0cPB@C\u590d\u5408\u6750\u6599\u8868\u73b0\u51fa\u524d\u6240\u672a\u6709\u7684\u500d\u7387\u6027\u80fd\u548c\u5faa\u73af\u7a33\u5b9a\u6027\u2014\u2014\u572890 C\u500d\u7387\u4e0b\uff0c\u5bb9\u91cf\u4e3a77.5 mAh g<sup>\u22121<\/sup>\uff1b\u572820 C\u500d\u7387\u4e0b\u5faa\u73af2000\u6b21\uff0c\u5bb9\u91cf\u4e3a90 mAh g<sup>\u22121<\/sup>\uff0c\u5bb9\u91cf\u4fdd\u6301\u7387\u8fbe\u523090%\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/11-3.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31048\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/11-3.png\" alt=\"11\" width=\"600\" height=\"357\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/11-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/11-3-300x179.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>PB@C\u7684\u5f62\u8c8c\u8868\u5f81<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Prussian Blue@C Composite as an Ultrahigh-Rate and Long-Life Sodium-Ion Battery Cathode \uff08Adv. Funct. Mater., 2016, DOI: 10.1002\/adfm.201600747\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>12.\u5149\u654f\u5149\u7ea4\u9635\u5217\uff1a\u7528\u4e8e\u7269\u4f53\u8f93\u8fd0<\/strong><\/span><\/p>\n<p>\u57c3\u56e0\u970d\u6e29\u79d1\u6280\u5927\u5b66\u7684Dirk J. Broer\u7b49\u4eba\u4eff\u7167\u547c\u5438\u7cfb\u7edf\u91cc\u7684\u7ea4\u6bdb\uff0c\u4f7f\u7528\u6db2\u6676\u805a\u5408\u7269\u4e0e\u5076\u6c2e\u82ef\u5236\u5907\u5f97\u5230\u5149\u654f\u7ea4\u7ef4\uff0c\u5e76\u4e14\u5728\u5236\u5907\u8fc7\u7a0b\u4e2d\u53ef\u4ee5\u63a7\u5236\u7ea4\u7ef4\u7684\u5c3a\u5bf8\u4ee5\u53ca\u6570\u91cf\uff0c\u7ea4\u7ef4\u4f1a\u5f2f\u5411\u7d2b\u5916\u5149\u4fa7\u4e14\u8be5\u8fc7\u7a0b\u53ef\u9006\u3002\u8fd9\u79cd\u6750\u6599\u9002\u7528\u4e8e\u9ad8\u6548\u5730\u8f93\u8fd0\u7269\u4f53\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/12-3.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31050\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/12-3.png\" alt=\"12\" width=\"600\" height=\"223\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/12-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/12-3-300x112.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u6a21\u4eff\u7ea4\u6bdb\u7684\u5149\u654f\u7ea4\u7ef4<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Photoresponsive Fiber Array: Toward Mimicking the Collective Motion of Cilia for Transport Applications (Adv. Funct. Mater. 2016, DOI: 10.1002\/adfm.201601221)<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong style=\"line-height: 1.5;\">13.Mxene<\/strong><strong style=\"line-height: 1.5;\">\u7535\u6781\u7528\u4e8e\u96c6\u6210<\/strong><strong style=\"line-height: 1.5;\">WSe<sub>2<\/sub><\/strong><strong style=\"line-height: 1.5;\">\u4ee5\u53ca<\/strong><strong style=\"line-height: 1.5;\">MoS<sub>2<\/sub><\/strong><strong style=\"line-height: 1.5;\">\u7684\u573a\u6548\u5e94\u7ba1<\/strong><\/span><\/p>\n<p>\u97e9\u56fd\u6210\u5747\u9986\u5927\u5b66\u7684Jin-Hong Park\u53caSungjoo Lee\u7b49\uff08\u5171\u540c\u901a\u8baf\uff09\u5c06Mxene\u5bb6\u65cf\u7684Ti<sub>2<\/sub>C(OH)<sub>x<\/sub>F<sub>y<\/sub>\u5e94\u7528\u4e8eWSe<sub>2<\/sub>\u53caMoS<sub>2<\/sub>\u573a\u6548\u5e94\u7ba1\u4e2d\uff0c\u529f\u51fd\u6570\u8fbe4.98 eV\u3002\u5c06Ti<sub>2<\/sub>C(OH)<sub>x<\/sub>F<sub>y<\/sub>\u548cWSe<sub>2<\/sub>\u53caMoS<sub>2<\/sub>\u7ec4\u6210\u91d1\u5c5e-\u6c27\u5316\u7269-\u534a\u5bfc\u4f53\u6362\u6d41\u5668\uff0c\u5728\u672a\u6765\u7eb3\u7c73\u7535\u5b50\u5668\u4ef6\u9886\u57df\u6709\u5e7f\u6cdb\u5e94\u7528\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/13-3.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31051\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/13-3.png\" alt=\"13\" width=\"600\" height=\"425\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/13-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/13-3-300x213.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\">Ti<sub>2<\/sub>C(OH)<em><sub>x<\/sub><\/em>F<em><sub>y<\/sub><\/em>\u7247\u7684\u5236\u5907\u6d41\u7a0b\u56fe\u548cTEM\u3001AFM\u56fe<\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">MXene Electrode for the Integration of WSe2 and MoS2 Field Effect Transistors\uff08Adv. Funct. Mater., 2016, DOI: 10.1002\/adfm.201600771\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>14.\u82cf\u5dde\u5927\u5b66<\/strong><strong>&amp;<\/strong><strong>\u4e2d\u79d1\u9662\u5316\u5b66\u6240\uff1a<\/strong><strong>Bi<sub>2<\/sub>S<sub>3<\/sub><\/strong><strong>\u7eb3\u7c73\u9897\u7c92\u7528\u4e8e\u80bf\u7624\u6210\u50cf\u53ca\u70ed\u7597<\/strong><\/span><\/p>\n<p>\u82cf\u5dde\u5927\u5b66\u7684Leshuai W. Zhang\u3001\u674e\u6862\u4ee5\u53ca\u4e2d\u79d1\u9662\u5316\u5b66\u6240\u7684\u9ad8\u660e\u8fdc\u7b49\uff08\u5171\u540c\u901a\u8baf\uff09\u901a\u8fc7\u4e00\u79cd\u725b\u8840\u6e05\u767d\u86cb\u767d\uff08BSA\uff09\u8c03\u8282\u7684\u751f\u7269\u5316\u4f5c\u7528\u5408\u6210\u4e8610 nm\u4ee5\u4e0b\u7684Bi<sub>2<\/sub>S<sub>3<\/sub>\u3002\u8be5\u7eb3\u7c73\u9897\u7c92\u53ef\u4ee5\u8fdb\u884c\u6709\u6548\u7684\u8840\u6db2\u5faa\u73af\u4ee5\u53ca\u80bf\u7624\u9776\u5411\u7684\u80fd\u529b\u3002\u53e6\u5916\uff0c\u5176\u5728\u5149\u70ed\u53ca\u653e\u5c04\u6cbb\u7597\u65b9\u9762\u7684\u5e94\u7528\u4e5f\u6709\u4ee4\u4eba\u60ca\u559c\u7684\u6548\u679c\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/14-2.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31052\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/14-2.png\" alt=\"14\" width=\"600\" height=\"714\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/14-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/14-2-252x300.png 252w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>Bi<sub>2<\/sub>S<sub>3<\/sub>\u7eb3\u7c73\u9897\u7c92\u5236\u5907\u6d41\u7a0b\u548c\u5728\u591a\u79cd\u80bf\u7624\u8bca\u65ad\u6cbb\u7597\u65b9\u9762\u7684\u5e94\u7528<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">BSA-Mediated Synthesis of Bismuth Sulfde Nanotheranostic Agents for Tumor Multimodal Imaging and Thermoradiotherapy\uff08Adv. Funct. Mater., 2016,DOI: 10.1002\/adfm.201601341\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>15.\u67d4\u6027\u53ef\u62c9\u4f38\u7535\u5b50\uff1a\u8bbe\u8ba1\u6781\u9650\u5e94\u53d8\u7684\u5f39\u6027\u57fa\u5e95<\/strong><\/span><\/p>\n<p>\u7f8e\u56fd\u897f\u5317\u5927\u5b66\u7684Yonggang Huang\u53ca\u4f0a\u5229\u8bfa\u4f0a\u5927\u5b66\u5384\u5df4\u7eb3-\u9999\u69df\u5206\u6821\u7684John A. Rogers\u7b49\u4eba\uff08\u5171\u540c\u901a\u8baf\uff09\u63d0\u51fa\u4e86\u4e00\u4e2a\u7b80\u5355\u7684\u8def\u7ebf\uff0c\u5c06\u8584\u819c\u6216\u7f51\u683c\u72b6\u7684\u9ad8\u6a21\u91cf\u6750\u6599\u8f6c\u79fb\u5230\u4e00\u4e2a\u9884\u62c9\u4f38\u67d4\u6027\u886c\u5e95\u4e0a\uff0c\u5f62\u6210\u8936\u76b1\u7684\u51e0\u4f55\u56fe\u5f62\u3002\u7531\u8fd9\u4e2a\u8fc7\u7a0b\u6240\u5f62\u6210\u7684\u7ed3\u6784\u8868\u73b0\u51fa\u4f4e\u7684\u5f39\u6027\u6a21\u91cf\uff0c\u5176\u662f\u7531\u4e8e\u5c0f\u7684\u6709\u6548\u521a\u5ea6\u7684\u8d77\u76b1\u819c\u6216\u7f51\u683c\u800c\u4ea7\u751f\u7684\uff0c\u5728\u5927\u5e94\u53d8\u4ea7\u751f\u65f6\uff0c\u5b83\u8868\u73b0\u51fa\u4e86\u9ad8\u7684\u5207\u7ebf\u6a21\u91cf\uff08\u4f8b\u5982&gt;1000\u500d\u7684\u5f39\u6027\u6a21\u91cf\uff09\u3002<\/p>\n<p style=\"text-align: center;\"><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/15-2.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31054\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/15-2.png\" alt=\"15\" width=\"600\" height=\"653\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/15-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/15-2-276x300.png 276w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><br \/>\n<strong>\u4e8c\u8f74\u62c9\u4f38\u7684\u539f\u7406\u56fe\u3001\u7535\u955c\u56fe\u4ee5\u53ca\u62c9\u4f38\u6027\u80fd<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Design of Strain-Limiting Substrate Materials for Stretchable and Flexible Electronics\uff08Adv. Funct. Mater. 2016,DOI: 10.1002\/adfm.201600713\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>16.\u5357\u4eac\u5927\u5b66<\/strong><strong>&amp;<\/strong><strong>\u5317\u4eac\u5927\u5b66\uff1a\u952f\u9f7f\u5f62\u7845\u7eb3\u7c73\u7ebf\u751f\u957f\u4e2d\u7684\u9762\u5185\u81ea\u6574\u5b9a\u548c\u5b6a\u751f\u52a8\u529b\u5b66\u8868\u73b0\u51fa\u7684\u5f3a\u4f38\u7f29\u6027<\/strong><\/span><\/p>\n<p>\u5357\u4eac\u5927\u5b66\u56fa\u4f53\u5fae\u7ed3\u6784\u7269\u7406\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u7684Linwei Yu\u53ca\u5317\u4eac\u5927\u5b66\u7684\u9648\u6e05\u7b49\u4eba\uff08\u5171\u540c\u901a\u8baf\uff09\u62a5\u9053\u4e86\u9521\u9762\u5185\u50ac\u5316\u7684\u6676\u4f53\u7845\u7eb3\u7c73\u7ebf\u5728\u4f4e\u80fd\u91cf\u4e0b\u5faa\u73af\u81ea\u6574\u5b9a\u7ed3\u6676\u548c\u5b6a\u751f\u52a8\u529b\u5b66\uff0c\u5176\u4e0d\u9700\u8981\u5916\u90e8\u53c2\u91cf\u8c03\u505c\u5c31\u53ef\u4ee5\u5468\u671f\u6027\u751f\u957f\u6210\u952f\u9f7f\u5f62\u6676\u4f53\u7845\u7eb3\u7c73\u7ebf\uff0c\u65b0\u65b9\u6cd5\u5408\u6210\u7684\u7c7b\u5355\u6676\u7845\u7eb3\u7c73\u7ebf\u4e3a\u8bbe\u8ba1\u9ad8\u6027\u80fd\u67d4\u6027\u7535\u5b50\u5143\u4ef6\u63d0\u4f9b\u4e86\u65b0\u601d\u8def\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/16-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31055\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/16-1.png\" alt=\"16\" width=\"600\" height=\"385\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/16-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/16-1-300x193.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\">SINWs\u751f\u957f\u793a\u610f\u56fe\u548c\u673a\u7406<\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">In-Plane Self-Turning and Twin Dynamics Renders Large Stretchability to Mono-Like Zigzag Silicon Nanowire Springs(Adv. Funct. Mater. 2016,DOI: 10.1002\/adfm.201600780\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>17.\u6b66\u6c49\u7406\u5de5\u5927\u5b66<\/strong><strong>&amp;<\/strong><strong>\u4e0a\u6d77\u5927\u5b66\uff1a\u94cb\u5806\u53e0\u7ed3\u6784\u62d3\u6251\u7edd\u7f18\u4f53\u8584\u7247\u7684\u6700\u5c0f\u70ed\u5bfc\u7387<\/strong><\/span><\/p>\n<p>\u6b66\u6c49\u7406\u5de5\u5927\u5b66\u7684\u5f20\u6e05\u6770\u3001\u4e0a\u6d77\u5927\u5b66\u7684\u5f20\u6587\u6e05\u4ee5\u53ca\u76db\u987f\u5927\u5b66Jihui Yang\u7b49\u4eba\uff08\u5171\u540c\u901a\u8baf\uff09\u62a5\u9053\u4e86\u4ea4\u66ff\u5806\u53e0\u65cb\u6d82\u62d3\u6251\u7edd\u7f18\u4f53\u548c\u666e\u901a\u7edd\u7f18\u4f53\u7684\u65b9\u6cd5\uff0c\u53ef\u4ee5\u83b7\u5f97\u5408\u9002\u7684\u70ed\u7535\u6027\u8d28\u3002\u5b83\u51ed\u501f\u81ea\u8eab\u7279\u70b9\u8f83\u597d\u7684\u8fbe\u5230\u4e86\u6240\u671f\u671b\u7684\u4f4e\u6676\u683c\u70ed\u5bfc\u7535\u6027\uff0c\u4e3a\u53d1\u5c55\u9ad8\u6027\u80fd\u62d3\u6251\u7edd\u7f18\u4f53\u70ed\u7535\u6750\u6599\u63d0\u4f9b\u4e86\u5e0c\u671b\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/17-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31057\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/17-1.png\" alt=\"17\" width=\"600\" height=\"519\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/17-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/17-1-300x260.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u62d3\u6251\u7edd\u7f18\u4f53\u7ed3\u6784\u8bbe\u8ba1\u56fe\u53ca\u70ed\u7535\u6027\u80fd<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Minimum Thermal Conductivity in Weak Topological Insulators with Bismuth-Based Stack Structure(Adv. Funct. Mater. 2016,DOI: 10.1002\/adfm.201600718\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>18.\u534e\u4e1c\u7406\u5de5\u5927\u5b66\uff1a\u5177\u6709\u4f18\u5f02\u7684\u6cb9\u5438\u9644\u548c\u5149<\/strong><strong>&#8211;<\/strong><strong>\u70ed\u84b8\u53d1\u6027\u80fd\u7684\u7a7a\u5fc3\u78b3\u7403<\/strong><\/span><\/p>\n<p>\u534e\u4e1c\u7406\u5de5\u5927\u5b66\u7684\u9f99\u4e1c\u8f89\u6559\u6388\u7b49\u63d0\u51fa\u4e86\u4e00\u79cd\u5236\u5907\u7edf\u4e00\u7a7a\u5fc3\u78b3\u7403\uff08HCSs\uff09\u7684\u65b9\u6cd5\u3002\u6240\u5236\u5907\u7684HCSs\u5177\u6709\u6beb\u7c73\u5c3a\u5ea6\u3001\u76f8\u4e92\u8d2f\u7a7f\u3001\u5f00\u5b54\u3001\u78b3\u58f3\u4ee5\u53ca\u5916\u90e8\u7684\u5de8\u5927\u7a7a\u6d1e\u7684\u5c42\u72b6\u7ed3\u6784\uff0c\u5141\u8bb8\u5206\u5b50\u4ece\u7a7a\u5fc3\u7ed3\u6784\u4e2d\u5feb\u901f\u5730\u8fd0\u8f93\u548c\u8d2f\u7a7f\u3002\u53e6\u5916\uff0c\u901a\u8fc7\u5c06\u78b3\u7eb3\u7c73\u7ba1\u5747\u5300\u5206\u6563\u5728\u524d\u9a71\u4f53\u6eb6\u6db2\u4e2d\u5f97\u5230\u78b3\u7eb3\u7c73\u7ba1\u52a0\u56fa\u7684 HCSs\uff0c\u6750\u6599\u7684\u673a\u68b0\u5f3a\u5ea6\u3001\u758f\u6c34\u6027\u4ee5\u53ca\u7535\u3001\u70ed\u6027\u8d28\u5f97\u5230\u663e\u8457\u63d0\u9ad8\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/18.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31058\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/18.png\" alt=\"18\" width=\"597\" height=\"187\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/18.png 597w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/18-300x94.png 300w\" sizes=\"(max-width: 597px) 100vw, 597px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>HCSs\u7684\u5149-\u70ed\u5438\u6536\u6027\u80fd<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Macroscopic and Mechanically Robust Hollow Carbon Spheres with Superior Oil Adsorption and Light-to-Heat Evaporation Properties\uff08Adv. Funct. Mater., 2016, DOI:\u00a010.1002\/adfm.201600564\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u5c01\u5e95\u5185\u9875\uff1a\u6539\u9020\u4e01\u57fa\u6a61\u80f6\u7528\u4e8e\u53ef\u4f38\u7f29\u7535\u5b50<\/strong><\/span><\/p>\n<p>\u52a0\u62ff\u5927\u6e29\u838e\u5927\u5b66\u7684Tricia Breen Carmichael\u7b49\u4eba\u5236\u5907\u51fa\u4ee5\u4e01\u57fa\u6a61\u80f6\u4e3a\u57fa\u5e95\u7684\u7535\u5b50\u6750\u6599\uff0c\u8fd9\u79cd\u7535\u5b50\u6750\u6599\u4e0d\u4ec5\u5149\u6ed1\u800c\u4e14\u5177\u6709\u9ad8\u7684\u5149\u5b66\u900f\u660e\u5ea6\u4ee5\u53ca\u4e01\u57fa\u6a61\u80f6\u7684\u4f4e\u900f\u6c14\u6027\uff0c\u5927\u5927\u4f18\u4e8e\u805a\u4e8c\u7532\u57fa\u7845\u6c27\u70f7\u7535\u5b50\u6750\u6599\uff0c\u6709\u671b\u6210\u4e3a\u53ef\u4f38\u7f29\u7535\u5b50\u6750\u6599\u7684\u4e00\u9897\u65b0\u661f\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31060\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875-1.png\" alt=\"\u5c01\u9762\u5185\u9875\" width=\"598\" height=\"543\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875-1.png 598w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u9762\u5185\u9875-1-300x272.png 300w\" sizes=\"(max-width: 598px) 100vw, 598px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u4e01\u57fa\u6a61\u80f6\u7684\u900f\u660e\u4e14\u4e0d\u900f\u6c34\u4e0d\u900f\u6c14<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Reinventing Butyl Rubber for Stretchable Electronics\uff08Adv. Funct. Mater., 2016, DOI: 10.1002\/adfm.201601283\uff09<\/a><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u5c01\u5e95\uff1a\u5168\u5f69\u8272\u5149\u54cd\u5e94\u7684\u55b7\u58a8\u6253\u5370\u6750\u6599\u7528\u4e8e\u53ef\u91cd\u590d\u5229\u7528\u7684\u7eb8\u5f20<\/strong><\/span><\/p>\n<p>\u5bf9\u4e8e\u7eb8\u5f20\u7684\u9700\u6c42\u4e0d\u51cf\u53cd\u589e\u8fd9\u4e00\u95ee\u9898\u53ef\u4ee5\u901a\u8fc7\u53d1\u660e\u53ef\u91cd\u65b0\u4e66\u5199\u7684\u7eb8\u5f20\u6216\u53ef\u64e6\u9664\u7684\u6cb9\u58a8\u5f97\u5230\u7f13\u89e3\u3002\u97e9\u56fd\u6c49\u9633\u5927\u5b66\u7684Jong-Man Kim\u7b49\u8bbe\u8ba1\u51fa\u4e00\u79cd\u5bf9\u7d2b\u5916-\u53ef\u89c1\u5149\u523a\u6fc0\u6709\u53d8\u8272\u54cd\u5e94\u4e14\u53ef\u9006\u7684\u4e8c\u82b3\u57fa\u4e59\u70ef\uff08DE\uff09\u884d\u751f\u7269\u6750\u6599\uff0c\u53ef\u4ee5\u5b9e\u73b0\u5168\u5f69\u8272\u55b7\u58a8\u5f0f\u6253\u5370\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u5e95-1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31061\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u5e95-1.png\" alt=\"\u5c01\u5e95-1\" width=\"600\" height=\"510\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u5e95-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/\u5c01\u5e95-1-300x255.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/a><\/p>\n<p style=\"text-align: center;\"><strong>\u5199-\u64e6-\u5199\u7684\u6253\u5370\u7eb8\u5f20\u5faa\u73af\u7cfb\u7edf<\/strong><\/p>\n<p><span style=\"color: #3366ff;\"><a style=\"color: #3366ff;\" href=\"http:\/\/www.cailiaoren.com\/thread-29211-1-1.html\" target=\"_blank\">Full Color Light Responsive Diarylethene Inks for Reusable Paper\uff08Adv. Funct. Mater., 2016, DOI: 10.1002\/adfm.201670190\uff09<\/a><\/span><\/p>\n<p>\u8be5\u4e13\u9898\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u5b66\u672f\u7ec4\u63d0\u4f9b\uff0c\u65e8\u5728\u53ca\u65f6\u8ddf\u8e2a\u6750\u6599\u7c7b\u9ad8\u8d28\u91cf\u671f\u520a\u524d\u6cbf\u70ed\u70b9\u5e76\u63d0\u4f9b\u6587\u732e\u5171\u4eab\u670d\u52a1\uff0c\u529b\u6c42\u5728\u6587\u7ae0\u89c1\u520a48\u5c0f\u65f6\u5185\uff0c\u5b8c\u6210\u52a8\u6001\u8ddf\u8e2a\u3001\u6587\u732e\u4e0b\u8f7d\u4ee5\u53ca\u56fe\u6587\u5bfc\u8bfb\u7b49\u5de5\u4f5c\uff0c\u6570\u5b57\u6765\u6e90\u4e3a\u5b66\u672f\u7ec4\u6210\u5458\u6240\u5728\u9ad8\u6821\u7684\u6570\u5b57\u8d44\u6e90\u3002<\/p>\n<p>\u6587\u4e2d\u51fa\u73b0\u7684\u4f5c\u8005\u548c\u5355\u4f4d\u7686\u4e3a\u901a\u8baf\u4f5c\u8005\u548c\u5176\u6240\u5728\u5355\u4f4d\uff0c\u82e5\u67d0\u4f5c\u8005\u540c\u5c5e\u4e24\u4e2a\u5355\u4f4d\u5219\u53ea\u5199\u7b2c\u4e00\u5355\u4f4d\uff0c\u67e5\u8be2\u4e0d\u5230\u4e2d\u6587\u540d\u7684\u4f5c\u8005\u7528\u82f1\u6587\u540d\u4ee3\u66ff\uff0c\u5982\u679c\u60a8\u5bf9\u5185\u5bb9\u8bbe\u7f6e\u7f16\u6392\u7b49\u6709\u597d\u7684\u610f\u89c1\u548c\u5efa\u8bae\uff0c\u6b22\u8fce\u4e0e\u6211\u4eec\u8054\u7cfb\u3002<\/p>\n<p>\u611f\u8c22\u535a\u5361\u5bf9\u52a8\u6001\u7684\u53ca\u65f6\u8ddf\u8e2a\uff0c\u6b66\u4fca\u751f\u63d0\u4f9b\u6570\u5b57\u8d44\u6e90\uff0c\u80fd\u6e90\u5c0f\u5c06\u3001\u5927\u5b8b\u3001\u8d8a\u5dde\u3001\u80cc\u9006\u65f6\u5149\u4ee5\u53ca\u4edd\u6c38\u6210\u7684\u8f9b\u52e4\u6574\u7406\uff0c\u652f\u6301\u6211\u4eec\uff0c<a href=\"http:\/\/cailiaoren.mikecrm.com\/6qSdMU\">\u52a0\u5165\u6211\u4eec<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u672c\u671f\u4e13\u9898\u8ddf\u8e2a\u4e86Advanced Functional Materials\u4e8e2016\u5e748\u67082\u65e5\u89c1\u520a\uff08Volume 26,\u00a0Issue 29\uff09\u7684\u6240\u6709\u6587\u732e\uff0c\u5e76\u505a\u76f8\u5173\u5bfc&#8230;<\/p>\n","protected":false},"author":90,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[67],"tags":[508],"class_list":["post-30836","post","type-post","status-publish","format-standard","hentry","category-zhoubao","tag-adv-funct-mater"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/30836"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/90"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=30836"}],"version-history":[{"count":19,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/30836\/revisions"}],"predecessor-version":[{"id":32569,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/30836\/revisions\/32569"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=30836"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=30836"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=30836"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}