{"id":31873,"date":"2016-08-09T08:00:58","date_gmt":"2016-08-09T00:00:58","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=31873"},"modified":"2016-08-08T23:36:22","modified_gmt":"2016-08-08T15:36:22","slug":"%e7%94%a8%e7%a2%b3%e7%ba%b3%e7%b1%b3%e7%ae%a1%e7%bc%9d%e5%88%b6%e5%87%ba%e8%bd%bb%e8%b4%a8%e9%ab%98%e5%bc%ba%e7%9a%84%e5%a4%8d%e5%90%88%e6%9d%90%e6%96%99%ef%bc%81","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=31873","title":{"rendered":"\u7528\u78b3\u7eb3\u7c73\u7ba1\u201c\u7f1d\u5236\u51fa\u201d\u8f7b\u8d28\u9ad8\u5f3a\u7684\u590d\u5408\u6750\u6599\uff01"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-31878\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/160803111753_1_540x360.jpg\" alt=\"160803111753_1_540x360\" width=\"540\" height=\"360\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/160803111753_1_540x360.jpg 540w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/160803111753_1_540x360-300x200.jpg 300w\" sizes=\"(max-width: 540px) 100vw, 540px\" \/><\/p>\n<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u9ebb\u7701\u7406\u5de5\u5b66\u9662\u822a\u5929\u5de5\u7a0b\u5e08\u8bbe\u8ba1\u4e86\u78b3\u7eb3\u7c73\u7ba1\u201c\u9488\u201d\uff0c\u5b83\u53ef\u4ee5\u201c\u7a7f\u9488\u5f15\u7ebf\u201d\u4f7f\u590d\u5408\u6750\u6599\u5c42\u95f4\u5b9e\u73b0\u826f\u597d\u7ed3\u5408\uff0c\u4ece\u800c\u6709\u52a9\u4e8e\u5236\u9020\u51fa\u8d28\u91cf\u66f4\u8f7b\u3001\u6297\u635f\u4f24\u6027\u80fd\u66f4\u5f3a\u7684\u822a\u5929\u98de\u673a\u3002<\/p>\n<p>\u76ee\u524d\uff0c\u7a7a\u5ba2\u548c\u6ce2\u97f3\u516c\u53f8\u6700\u65b0\u7684\u8f7d\u4eba\u822a\u5929\u98de\u673a\u673a\u8eab\u4e3b\u8981\u662f\u7531\u5148\u8fdb\u7684\u590d\u5408\u6750\u6599\u6784\u6210\u7684\uff0c\u8b6c\u5982\u7528\u8d28\u91cf\u6781\u8f7b\u4e14\u4f7f\u7528\u6027\u80fd\u4f18\u5f02\u7684\u78b3\u7ea4\u7ef4\u589e\u5f3a\u5851\u6599\u4ee3\u66ff\u98de\u673a\u7684\u94dd\u57fa\u6750\u6599\uff0c\u53ef\u4ee5\u4f7f\u5176\u91cd\u91cf\u51cf\u8f7b\u7ea620%\u3002\u590d\u5408\u6750\u6599\u5728\u98de\u673a\u4e0a\u7684\u4e3b\u8981\u5e94\u7528\u4f18\u52bf\u5c31\u5728\u4e8e\u901a\u8fc7\u51cf\u8f7b\u91cd\u91cf\u4ee5\u8282\u7701\u71c3\u6cb9\u6d88\u8017\u3002<\/p>\n<p>\u4f46\u662f\u590d\u5408\u6750\u6599\u6297\u635f\u4f24\u6027\u80fd\u8f83\u5dee\uff1a\u4e0e\u94dd\u57fa\u6750\u6599\u5728\u65ad\u88c2\u524d\u53ef\u4ee5\u627f\u53d7\u8f83\u5927\u7684\u51b2\u51fb\u76f8\u6bd4\uff0c\u590d\u5408\u6750\u6599\u7684\u591a\u5c42\u7ed3\u6784\u5728\u8f83\u5c0f\u51b2\u51fb\u4e0b\u5c31\u5f88\u5bb9\u6613\u53d1\u751f\u65ad\u88c2\u3002\u4f4e\u6297\u635f\u4f24\u6027\u80fd\u5df2\u7ecf\u6210\u4e3a\u590d\u5408\u6750\u6599\u7684\u963f\u5580\u7409\u65af\u4e4b\u8e35\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u9ebb\u7701\u7406\u5de5\u5b66\u9662\uff08MIT\uff09\u7684\u822a\u7a7a\u5de5\u7a0b\u5e08\u63a2\u7d22\u51fa\u4e00\u79cd\u7c98\u7ed3\u590d\u5408\u6750\u6599\u5c42\u7684\u65b0\u65b9\u6cd5\uff0c\u4ece\u800c\u4f7f\u5176\u5f3a\u5ea6\u66f4\u9ad8\uff0c\u8010\u635f\u4f24\u6027\u80fd\u66f4\u597d\u3002<\/p>\n<p>\u7814\u7a76\u4eba\u5458\u4f7f\u7528\u78b3\u7eb3\u7c73\u7ba1\u5c06\u6bcf\u4e00\u5c42\u590d\u5408\u6750\u6599\u201c\u6813\u201d\u5728\u4e00\u8d77\u3002\u78b3\u7eb3\u7c73\u7ba1\u4e2d\u7684\u8584\u5377\u72b6\u78b3\u539f\u5b50\u867d\u7136\u201c\u8eab\u5f62\u201d\u5fae\u5c0f\uff0c\u4f46\u662f\u5f3a\u5ea6\u6781\u9ad8\u3002\u4ed6\u4eec\u5728\u7c7b\u80f6\u72b6\u805a\u5408\u7269\u57fa\u4f53\u4e2d\u5d4c\u5165\u78b3\u7eb3\u7c73\u7ba1 \u201c\u68ee\u6797\u201d\uff0c\u7136\u540e\u201c\u538b\u7d27\u201d\u78b3\u7ea4\u7ef4\u590d\u5408\u6750\u6599\u5c42\u95f4\u7684\u805a\u5408\u7269\u57fa\u4f53\u3002\u7eb3\u7c73\u7ba1\u5c31\u50cf\u662f\u7ec6\u5c0f\u7684\u7ad6\u76f4\u6392\u5217\u7684\u201c\u9488\u201d\uff0c\u5145\u5f53\u591a\u5c42\u7ed3\u6784\u7684\u652f\u67b6\uff0c\u5728\u5c42\u95f4\u90e8\u4f4d\u8fdb\u884c\u201c\u7f1d\u5408\u201d\u3002<\/p>\n<p>\u6d4b\u8bd5\u7ed3\u679c\u8868\u660e\uff0c\u4e0e\u73b0\u6709\u590d\u5408\u6750\u6599\u76f8\u6bd4\uff0c\u7ecf\u78b3\u7eb3\u7c73\u7ba1\u201c\u7f1d\u5408\u201d\u7684\u590d\u5408\u6750\u6599\u5f3a\u5ea6\u53ef\u63d0\u534730%\uff0c\u5728\u65ad\u88c2\u524d\u80fd\u627f\u53d7\u66f4\u5927\u7684\u4f5c\u7528\u529b\u3002<\/p>\n<p>\u6b64\u9879\u7814\u7a76\u7684\u9996\u5e2d\u7814\u7a76\u5458\uff0cMIT\u822a\u7a7a\u822a\u5929\u7cfb\u535a\u58eb\u540eRoberto Guzman\u8ba4\u4e3a\uff0c\u6027\u80fd\u63d0\u5347\u7684\u590d\u5408\u6750\u6599\u53ef\u4ee5\u7528\u4e8e\u5236\u9020\u5f3a\u5ea6\u66f4\u9ad8\u3001\u8d28\u91cf\u66f4\u8f7b\u7684\u98de\u673a\u96f6\u90e8\u4ef6\uff0c\u5c24\u5176\u662f\u90a3\u4e9b\u4f7f\u7528\u4f20\u7edf\u590d\u5408\u6750\u6599\u5236\u9020\u7684\u56e0\u5305\u542b\u87ba\u9489\u6216\u87ba\u6813\u800c\u5bb9\u6613\u65ad\u88c2\u7684\u96f6\u90e8\u4ef6\u3002<\/p>\n<p><strong>\u201c\u5c3a\u5bf8\u662f\u5173\u952e\u201d<\/strong><\/p>\n<p>\u5f53\u524d\uff0c\u590d\u5408\u6750\u6599\u7531\u5c42\u72b6\u7684\u6a2a\u5411\u78b3\u7ea4\u7ef4\u7ec4\u6210\uff0c\u901a\u8fc7\u805a\u5408\u7269\u80f6\u7c98\u63a5\u3002\u6b64\u9879\u7814\u7a76\u53c2\u4e0e\u8005\uff0cMIT\u822a\u7a7a\u822a\u5929\u7cfb\u6559\u6388Wardle\u6307\u51fa\uff0c\u201c\u5c42\u95f4\u7ed3\u5408\u5904\u662f\u975e\u5e38\u8584\u5f31\u3001\u5b58\u5728\u95ee\u9898\u7684\u533a\u57df\u201d\u3002\u8bb8\u591a\u5b66\u8005\u5c1d\u8bd5\u91c7\u7528\u201cZ\u9489\u624e\u201d\u65b9\u6cd5\u56fa\u5b9a\u6216\u901a\u8fc7\u201c\u4e09\u7ef4\u7f16\u5236\u201d\u590d\u5408\u6750\u6599\u5c42\u7684\u78b3\u7ea4\u7ef4\u675f\u4ee5\u589e\u5f3a\u7ed3\u5408\u6027\u80fd\uff0c\u7c7b\u4f3c\u4e8e\u9489\u5b50\u548c\u9488\u7ebf\u6240\u8d77\u7684\u4f5c\u7528\u3002<\/p>\n<p>Wardle \u8868\u793a\uff0c\u201c\u9489\u5b50\u6216\u9488\u7684\u5c3a\u5bf8\u662f\u78b3\u7ea4\u7ef4\u7684\u51e0\u5343\u500d\uff0c\u6240\u4ee5\u5982\u679c\u5728\u78b3\u7ea4\u7ef4\u4e2d\u52a0\u5165\u8fd9\u4e9b\u7269\u8d28\uff0c\u5c06\u4f1a\u7834\u574f\u6210\u5343\u4e0a\u4e07\u7684\u78b3\u7ea4\u7ef4\uff0c\u5bf9\u590d\u5408\u6750\u6599\u672c\u8eab\u7684\u635f\u4f24\u4e0d\u8a00\u800c\u55bb\u3002\u201d\u800c\u78b3\u7eb3\u7c73\u7ba1\u76f4\u5f84\u7ea610\u7eb3\u7c73\uff0c\u53ea\u6709\u78b3\u7ea4\u7ef4\u5c3a\u5bf8\u7684\u767e\u4e07\u5206\u4e4b\u4e00\u3002<\/p>\n<p>\u201c\u5c3a\u5bf8\u7684\u95ee\u9898\u5f88\u91cd\u8981\uff0c\u6b63\u56e0\u4e3a\u7eb3\u7c73\u7ba1\u8fdb\u5165\u590d\u5408\u6750\u6599\u5185\u90e8\u800c\u4e0d\u4f1a\u5f71\u54cd\u5927\u5c3a\u5bf8\u7684\u78b3\u7ea4\u7ef4\uff0c\u624d\u4f7f\u590d\u5408\u6750\u6599\u7684\u6027\u80fd\u5f97\u4ee5\u4fdd\u6301\uff0c\u201d Wardle\u89e3\u91ca\u8bf4\uff0c\u201c\u78b3\u7eb3\u7c73\u7ba1\u62e5\u6709\u7684\u8868\u9762\u79ef\u8fbe\u5230\u78b3\u7ea4\u7ef4\u76841000\u500d\uff0c\u8fd9\u4f7f\u5b83\u4eec\u4e0e\u805a\u5408\u7269\u57fa\u4f53\u7ed3\u5408\u826f\u597d\u3002\u201d<\/p>\n<p>Guzman\u548cWardle\u91c7\u7528\u7684\u65b0\u6280\u672f\u5373\u53ef\u4f7f\u78b3\u7eb3\u7c73\u7ba1\u5d4c\u5165\u805a\u5408\u7269\u80f6\u5185\u90e8\u3002\u9996\u5148\uff0c\u4ed6\u4eec\u83b7\u5f97\u7ad6\u76f4\u6392\u5217\u7684\u78b3\u7eb3\u7c73\u7ba1\u68ee\u6797\uff0c\u7136\u540e\u5c06\u7eb3\u7c73\u68ee\u6797\u7f6e\u4e8e\u7c98\u7a20\u7684\u3001\u672a\u56fa\u5316\u7684\u590d\u5408\u5c42\u4e4b\u95f4\uff0c\u91cd\u590d\u6b64\u8fc7\u7a0b\u4e00\u76f4\u523016\u5c42\uff08\u5178\u578b\u7684\u590d\u5408\u6750\u6599\u53e0\u5c42\u7ed3\u6784\uff09\uff0c\u5b9e\u73b0\u78b3\u7eb3\u7c73\u7ba1\u5728\u5c42\u4e0e\u5c42\u4e4b\u95f4\u7c98\u7ed3\u3002<\/p>\n<p>Wardle\u8ba4\u4e3a\uff0c\u201c\u968f\u7740\u5927\u591a\u6570\u65b0\u578b\u98de\u673a\u7684\u91cd\u91cf\u8d85\u8fc7\u4e00\u534a\u6765\u81ea\u4e8e\u590d\u5408\u6750\u6599\uff0c\u63d0\u5347\u5f53\u524d\u590d\u5408\u6750\u6599\u7684\u7efc\u5408\u6027\u80fd\u5bf9\u62d3\u5bbd\u5176\u5728\u822a\u7a7a\u7ed3\u6784\u4e2d\u7684\u5e94\u7528\u5c06\u8d77\u5230\u5f88\u5927\u7684\u63a8\u52a8\u4f5c\u7528\u3002\u201d<\/p>\n<p>\u53c2\u8003\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/www.sciencedaily.com\/releases\/2016\/08\/160803111753.htm\" target=\"_blank\">Carbon nanotube &#8216;stitches&#8217; make stronger, lighter composites<\/a>.<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.sciencedirect.com\/science\/article\/pii\/S026635381630687X\" target=\"_blank\">In-plane strength enhancement of laminated composites via aligned carbon nanotube interlaminar reinforcement<\/a>.<\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u66fe\u5e86\u8f89\u63d0\u4f9b\u7d20\u6750\uff0c\u674e\u7389\u98de\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u4eba\u7f51\u5c0a\u91cd\u6240\u6709\u8fdb\u884c\u77e5\u8bc6\u4f20\u64ad\u7684\u5a92\u4f53\uff0c\u8f6c\u8f7d\u8bf7\u8054\u7cfbtougao@cailiaoren.com<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u9ebb\u7701\u7406\u5de5\u5b66\u9662\u822a\u5929\u5de5\u7a0b\u5e08\u8bbe\u8ba1\u4e86\u78b3\u7eb3\u7c73\u7ba1\u201c\u9488\u201d\uff0c\u5b83\u53ef\u4ee5\u201c\u7a7f\u9488\u5f15\u7ebf\u201d\u4f7f\u590d\u5408\u6750\u6599\u5c42\u95f4\u5b9e\u73b0\u826f\u597d\u7ed3\u5408\uff0c\u4ece\u800c\u6709\u52a9\u4e8e\u5236\u9020\u51fa\u8d28\u91cf\u66f4\u8f7b\u3001\u6297\u635f\u4f24\u6027\u80fd\u66f4\u5f3a\u7684\u822a\u5929\u98de\u673a\u3002 \u76ee\u524d\uff0c&#8230;<\/p>\n","protected":false},"author":213,"featured_media":31878,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[43,33,63],"class_list":["post-31873","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-composite","tag-nano","tag-aircraft"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/31873"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/213"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=31873"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/31873\/revisions"}],"predecessor-version":[{"id":32481,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/31873\/revisions\/32481"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/31878"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=31873"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=31873"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=31873"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}