{"id":31900,"date":"2016-08-08T14:00:24","date_gmt":"2016-08-08T06:00:24","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=31900"},"modified":"2016-08-08T14:15:59","modified_gmt":"2016-08-08T06:15:59","slug":"%e7%a9%b6%e7%ab%9f%e6%98%af%e6%80%8e%e6%a0%b7%e7%9a%84%e5%a4%a7%e5%b8%88%e6%89%8d%e9%85%8d%e5%be%97%e4%b8%8a%e7%84%8a%e6%8e%a5%e7%bb%88%e8%ba%ab%e6%88%90%e5%b0%b1%e5%a5%96%ef%bc%9f","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=31900","title":{"rendered":"\u7a76\u7adf\u662f\u600e\u6837\u7684\u5927\u5e08\u624d\u914d\u5f97\u4e0a\u710a\u63a5\u7ec8\u8eab\u6210\u5c31\u5956\uff1f"},"content":{"rendered":"<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/welder-pic.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-32265\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/welder-pic.jpg\" alt=\"091114-N-5549O-135 NEWPORT NEWS, Va. (Nov. 14, 2009) Robert Bowker welds the initials of Susan Ford Bales into the keel of the aircraft carrier Gerald R. Ford (CVN 78) during a keel laying and authentication ceremony at Northrop Grumman Shipbuilding in Newport News. Gerald R. Ford is the newest class of aircraft carrier. (U.S. Navy photo by Mass Communication Specialist 2nd Class Kevin S. O'Brien\/Released)\" width=\"740\" height=\"491\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/welder-pic.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/welder-pic-300x199.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/a><\/p>\n<p>\u4ece\u710a\u63a5\u7ec8\u8eab\u6210\u5c31\u5956\u8bbe\u7acb\u4ee5\u6765\uff0c\u4e00\u5171\u670911\u4f4d\u83b7\u5f97\u4e86\u8be5\u8363\u8a89\uff0c\u4ed6\u4eec\u5206\u522b\u662f\u710a\u63a5\u754c\u56db\u4f4d\u9662\u58eb\uff1a\u6f58\u9645\u92ae\u9662\u58eb\u3001\u5173\u6865\u9662\u58eb\u3001\u5f90\u6ee8\u58eb\u9662\u58eb\u3001\u6797\u5c1a\u626c\u9662\u58eb\u4ee5\u53ca7\u4f4d\u5728\u710a\u63a5\u9886\u57df\u505a\u51fa\u5353\u8d8a\u8d21\u732e\u7684\u5b8b\u5929\u864e\u7814\u7a76\u5458\uff0c\u5434\u6797\u6559\u6388\uff0c\u9648\u5251\u8679\u6559\u6388\uff0c\u9648\u4e19\u68ee\u6559\u6388\uff0c\u4faf\u7acb\u5c0a\u8463\u4e8b\u957f\uff0c\u53f2\u8000\u6b66\u6559\u6388\uff0c\u5434\u7956\u4e7e\u535a\u58eb\u3002<\/p>\n<table width=\"100%\">\n<tbody>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u59d3\u540d<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u5355\u4f4d<\/td>\n<td style=\"text-align: center;\" width=\"90\">\u83b7\u5956\u65f6\u95f4<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u6f58\u9645\u92ae<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u6e05\u534e\u5927\u5b66<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2001<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u5173\u6865<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u4e2d\u822a\u5de5\u4e1a\uff08625\u6240\uff09<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2005<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u5f90\u6ee8\u58eb<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u88c5\u7532\u5175\u5de5\u7a0b\u5b66\u9662<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2005<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u6797\u5c1a\u626c<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u54c8\u5c14\u6ee8\u710a\u63a5\u7814\u7a76\u6240<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2005<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u5b8b\u5929\u864e<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u4e2d\u56fd\u5de5\u7a0b\u673a\u68b0\u5b66\u4f1a<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2007<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u5434\u6797<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u54c8\u5c14\u6ee8\u5de5\u4e1a\u5927\u5b66<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2007<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u9648\u5251\u8679<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u5170\u5dde\u7406\u5de5\u5927\u5b66<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2008<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u9648\u4e19\u68ee<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u6e05\u534e\u5927\u5b66<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2009<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u4faf\u7acb\u5c0a<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u91d1\u6865\u710a\u6750\u96c6\u56e2\u6709\u9650\u516c\u53f8<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2009<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td width=\"114\">\n<p style=\"text-align: center;\">\u53f2\u8000\u6b66<\/p>\n<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u5317\u4eac\u5de5\u4e1a\u5927\u5b66<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2010<\/p>\n<\/td>\n<\/tr>\n<tr>\n<td style=\"text-align: center;\" width=\"114\">\u5434\u7956\u4e7e<\/td>\n<td style=\"text-align: center;\" width=\"188\">\u4e0a\u6d77\u53d1\u7535\u8bbe\u5907\u6210\u5957\u8bbe\u8ba1\u7814\u7a76\u9662<\/td>\n<td width=\"90\">\n<p style=\"text-align: center;\">2011<\/p>\n<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>\u8ba9\u6211\u4eec\u6765\u770b\u770b\u4ed6\u4eec\u90fd\u6709\u54ea\u4e9b\u4e3b\u8981\u6210\u5c31\u4e0e\u8363\u8a89\u5427\uff01<\/p>\n<p><strong>\u6f58\u9645\u92ae<\/strong>\uff1a60\u5e74\u4ee3\u521d\u8bd5\u9a8c\u6210\u529f\u6c29\u5f27\u710a\u5e76\u5efa\u8bbe\u6210\u529f\u6211\u56fd\u7b2c\u4e00\u5ea7\u6838\u53cd\u5e94\u5806\u5de5\u7a0b\uff0c\u7ee7\u4e4b\u7814\u7a76\u6210\u529f\u6211\u56fd\u7b2c\u4e00\u53f0\u7535\u5b50\u675f\u710a\u673a; 1965\u5e74\uff0c&#8221;ZD-30\u7535\u5b50\u675f\u710a\u673a&#8221;\u83b7\u56fd\u5bb6\u79d1\u59d4\u3001\u56fd\u5bb6\u7ecf\u59d4\u3001\u56fd\u5bb6\u8ba1\u59d4\u7b49\u8054\u5408\u6388\u4e88\u7684\u65b0\u4ea7\u54c1\u521b\u9020\u4e8c\u7b49\u5956\uff1b<\/p>\n<p>70\u5e74\u4ee3\u672b\u7814\u7a76\u7535\u5f27\u4f20\u611f\u5668\uff0c\u9996\u6b21\u5efa\u7acb\u7535\u5f27\u4f20\u611f\u5668\u7684\u52a8\u3001\u9759\u6001\u7269\u7406\u6570\u5b66\u6a21\u578b\uff0c\u5e76\u7814\u5236\u6210\u5177\u6709\u7279\u8272\u7684\u7535\u5f27\u4f20\u611f\u5668\u53ca\u81ea\u52a8\u8ddf\u8e2a\u7cfb\u7edf;<\/p>\n<p>80\u5e74\u4ee3\u7814\u7a76\u6210\u529f\u65b0\u578bMIG\u710a\u63a5\u7535\u5f27\u63a7\u5236\u6cd5&#8221;QH-ARC\u6cd5&#8221;\uff0c\u9996\u6b21\u63d0\u51fa\u7528\u7535\u6e90\u7684\u591a\u6298\u7ebf\u5916\u7279\u6027\u3001\u9661\u5347\u5916\u7279\u6027\u53ca\u626b\u63cf\u5916\u7279\u6027\u63a7\u5236\u7535\u5f27\u7684\u6982\u5ff5\uff0c\u4e3a\u710a\u63a5\u7535\u5f27\u7684\u63a7\u5236\u5f00\u8f9f\u4e86\u65b0\u7684\u9014\u5f84\u3002<\/p>\n<p>1984\u5e74\uff0c&#8221;QH-ARC\u6cd5&#8221;\u83b7\u56fd\u5bb6\u521b\u9020\u53d1\u660e\u4e00\u7b49\u5956\u3001&#8221;\u710a\u63a5\u7528\u53cc\u5411\u6fc0\u5149\u81ea\u52a8\u8ddf\u8e2a\u7cfb\u7edf&#8221;\u83b7\u5317\u4eac\u5e02\u79d1\u5b66\u6280\u672f\u6210\u679c\u4e8c\u7b49\u5956\uff1b1987-1991\u5e74\u5728\u6211\u56fd\u81ea\u884c\u5efa\u8bbe\u7b2c\u4e00\u5ea7\u6838\u7535\u7ad9(\u79e6\u5c71\u6838\u7535\u7ad9)\u65f6\u62c5\u4efb\u710a\u63a5\u987e\u95ee\uff0c\u4e3a\u8be5\u5de5\u7a0b\u4f5c\u51fa\u91cd\u8981\u8d21\u732e\uff1b2000\u5e74\u4f55\u6881\u4f55\u5229\u79d1\u5b66\u4e0e\u6280\u672f\u8fdb\u6b65\u5956\uff1b2003\u5e74\u7814\u5236\u6210\u529f\u722c\u884c\u5f0f\u5f27\u710a\u673a\u5668\u4eba\uff0c\u5c5e\u56fd\u9645\u9886\u5148\u6c34\u5e73\u3002<\/p>\n<p><strong>\u5173\u6865<\/strong>\uff1a1992\u5e74\u83b7\u822a\u7a7a\u5de5\u4e1a\u6700\u9ad8\u5956&#8211;\u822a\u7a7a\u91d1\u5956\uff0c1996\u5e74\u83b7\u5149\u534e\u79d1\u6280\u57fa\u91d1\u4e00\u7b49\u5956\uff0c1998\u5e74\u83b7\u4f55\u6881\u4f55\u5229\u79d1\u6280\u5956\uff0c\u5148\u540e5\u6b21\u83b7\u90e8\u7ea7\u79d1\u6280\u8fdb\u6b65\u4e00\u3001\u4e8c\u7b49\u5956\u30021995\u5e74\u83b7\u56fd\u5bb6\u53d1\u660e\u4e8c\u7b49\u5956\u30021978\u5e74\uff0c&#8221;\u94a8\u6781\u8109\u51b2\u6c29\u5f27\u710a\u4e0e\u60ac\u7a7a\u710a\u5de5\u827a\u7814\u7a76&#8221;\u83b7\u5168\u56fd\u79d1\u5b66\u5927\u4f1a\u5956\u3002<\/p>\n<p>\u6298\u53e0&#8221;\u4f4e\u5e94\u529b\u65e0\u53d8\u5f62\u710a\u63a5&#8221;\u7406\u8bba\u7684\u521b\u59cb\u4eba\u3002\u4ed6\u53d1\u660e\u7684&#8221;\u8584\u58c1\u7ed3\u6784\u4f4e\u5e94\u529b\u65e0\u53d8\u5f62\u710a\u63a5\u65b9\u6cd5\u53ca\u88c5\u7f6e&#8221;\u662f\u710a\u63a5\u53d8\u5f62\u63a7\u5236\u9886\u57df\u4e2d\u7684\u91cd\u5927\u7a81\u7834\u3002\u4ed6\u53c8\u662f\u822a\u7a7a\u710a\u63a5\u4e13\u4e1a\u7684\u5b66\u79d1\u5e26\u5934\u4eba\u548c\u4e2d\u56fd\u98de\u884c\u5668\u5236\u9020\u5de5\u7a0b\u4e2d\u591a\u9879\u7279\u79cd\u710a\u63a5\u6280\u672f\u7684\u5f00\u62d3\u8005\u3002\u5728\u710a\u63a5\u529b\u5b66\u4e0e\u710a\u63a5\u7ed3\u6784\u5b8c\u6574\u6027\u7814\u7a76\u65b9\u9762\uff0c\u4e5f\u6709\u91cd\u8981\u5efa\u6811\u3002\u4ed6\u9886\u5bfc\u7684&#8221;\u710a\u63a5\u77ac\u6001\u70ed\u5e94\u53d8\u4e91\u7eb9\u6d4b\u8bd5\u6280\u672f&#8221;\u7814\u7a76\u6210\u679c\uff0c\u5bf9\u63a8\u52a8\u710a\u63a5\u529b\u5b66\u5b66\u79d1\u53d1\u5c55\u3001\u4e30\u5bcc\u5b66\u79d1\u5185\u5bb9\u5177\u6709\u91cd\u8981\u5b66\u672f\u4ef7\u503c\u3002<\/p>\n<p><strong>\u5f90\u6ee8\u58eb\uff1a<\/strong>(1)\u7cfb\u7edf\u7684\u5f00\u53d1\u4e86\u7535\u5237\u9540\u8bbe\u5907\u3001\u9540\u6db2\u548c\u5de5\u827a\uff0c\u7a81\u7834\u4e86\u73b0\u573a\u4fee\u590d\u5927\u578b\u8bbe\u5907\u7684\u91cd\u5927\u5de5\u7a0b\u6280\u672f\u96be\u5173\u30021985\u5e74\u83b7\u5f97\u56fd\u5bb6\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\u3002\u5f00\u53d1\u51fa\u7eb3\u7c73\u9897\u7c92\u590d\u5408\u7535\u5237\u9540\u6280\u672f\uff0c\u5236\u5907\u7684\u7eb3\u7c73\u590d\u5408\u6d82\u5c42\u53ef\u663e\u8457\u63d0\u9ad8\u6750\u6599\u7684\u8010\u9ad8\u6e29\u78e8\u635f\u53ca\u6297\u63a5\u89e6\u75b2\u52b3\u6027\u80fd\uff0c\u4e8e2004\u5e74\u83b7\u5f97\u519b\u961f\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\u3002<\/p>\n<p>(2)\u5728\u56fd\u5185\u9996\u6b21\u7528\u7b49\u79bb\u5b50\u55b7\u6d82\u6280\u672f\u89e3\u51b3\u4e86\u5766\u514b\u7b49\u91cd\u8f7d\u8f66\u8f86\u8584\u58c1\u78e8\u635f\u96f6\u4ef6\u4e0d\u80fd\u4fee\u590d\u7684\u91cd\u5927\u96be\u9898\uff0c\u8be5\u6280\u672f\u4e8e1985\u5e74\u83b7\u5f97\u56fd\u5bb6\u6280\u672f\u8fdb\u6b65\u4e8c\u7b49\u5956\u300290\u5e74\u4ee3\u672b\u5728\u4f20\u7edf\u7b49\u79bb\u5b50\u55b7\u6d82\u6280\u672f\u7684\u57fa\u7840\u4e0a\u7814\u7a76\u5f00\u53d1\u51fa\u9ad8\u6548\u80fd\u8d85\u97f3\u901f\u7b49\u79bb\u5b50\u55b7\u6d82\u6280\u672f\uff0c\u8be5\u6280\u672f\u4e8e2003\u5e74\u83b7\u5f97\u56fd\u5bb6\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\u3002(3)\u53d1\u660e\u4e86\u65b0\u578b\u5766\u514b\u5c65\u5e26\u677f\u6750\u6599ZGMn8CrMo\uff0c\u8be5\u6280\u672f\u83b7\u5f972003\u5e74\u56fd\u5bb6\u6280\u672f\u53d1\u660e\u4e8c\u7b49\u5956\u3002<\/p>\n<p>(4)\u9996\u6b21\u5728\u56fd\u5185\u5c06\u7535\u5f27\u55b7\u6d82\u6280\u672f\u7528\u4e8e\u5927\u578b\u8230\u8239\u94a2\u7ed3\u6784\u7684\u8868\u9762\u9632\u8150\u7814\u7a76\uff0c1997\u5e74\u83b7\u519b\u961f\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\u3002<\/p>\n<p>1996\u5e747\u6708\u83b7\u4e2d\u56fd\u673a\u68b0\u5de5\u7a0b\u5b66\u4f1a&#8221;\u79d1\u6280\u6210\u5c31\u5956&#8221;\uff1b2004\u5e746\u6708\u83b7\u00a0\u4e2d\u56fd\u5de5\u7a0b\u9662&#8221;\u5149\u534e\u79d1\u6280\u5de5\u7a0b\u5956&#8221;\uff1b2004\u5e7410\u6708\u83b7\u56fd\u9645\u70ed\u5904\u7406\u4e0e\u8868\u9762\u5de5\u7a0b\u8054\u5408\u4f1a&#8221;\u6700\u9ad8\u5b66\u672f\u6210\u5c31\u5956&#8221;\uff1b2005\u5e7410\u6708\u83b7\u4f55\u6881\u4f55\u5229\u57fa\u91d1\u79d1\u5b66\u4e0e\u6280\u672f\u8fdb\u6b65\u5956&#8221;\u6280\u672f\u79d1\u5b66\u5956&#8221;\uff1b2009\u5e7410\u6708\u83b7\u4e2d\u56fd\u673a\u68b0\u5de5\u7a0b\u5b66\u4f1a\u6469\u64e6\u5b66\u5206\u4f1a&#8221;\u6469\u64e6\u5b66\u6700\u9ad8\u6210\u5c31\u5956&#8221;\uff1b2010\u5e744\u6708\u83b7\u4e2d\u56fd\u673a\u68b0\u5de5\u7a0b\u5b66\u4f1a\u8868\u9762\u5de5\u7a0b\u5206\u4f1a&#8221;\u4e2d\u56fd\u8868\u9762\u5de5\u7a0b\u6700\u9ad8\u6210\u5c31\u5956\u3002<\/p>\n<p><strong>\u6797\u5c1a\u626c<\/strong>\uff1a20\u4e16\u7eaa70\u5e74\u4ee3\uff0c\u89e3\u51b3\u4e86\u9ad8\u94dd\u710a\u6761\u5de5\u827a\u6027\u7684\u6280\u672f\u96be\u70b9\u3002\u540c\u65f6\uff0c\u8fd8\u7814\u7a76\u6210\u529f\u8010\u6d77\u6c34\u8150\u8680\u94a2\u7528\u7ed3507CrNiCu\u710a\u6761\uff0c\u7528\u4e8e\u6c34\u4e0b\u7ba1\u7ebf\u548c\u8db8\u8239\u7801\u5934\u7684\u710a\u63a5\u300270\u5e74\u4ee3\u4e2d\u671f\u4ee5\u6765\uff0c\u4e3b\u6301\u5f00\u5c55\u4e86\u6c34\u4e0b\u710a\u63a5\u6280\u672f\u7684\u7814\u7a76\uff0c\u4f7f\u4e2d\u56fd\u7684\u6c34\u4e0b\u710a\u63a5\u6280\u672f\u8dc3\u8fdb20\u5e74\uff0c\u5e76\u8de8\u5165\u56fd\u9645\u5148\u8fdb\u6c34\u5e73\u7684\u884c\u5217\u300220\u5e74\u6765\u5148\u540e\u53c2\u52a0\u5341\u591a\u9879\u91cd\u8981\u6c34\u4e0b\u710a\u63a5\u65bd\u5de5\uff0c\u8fd9\u9879\u6210\u679c\u66fe\u83b7\u673a\u68b0\u90e8\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\u548c\u56fd\u5bb6\u53d1\u660e\u521b\u9020\u4e09\u7b49\u5956. \u5728\u7814\u7a76200m\u6c34\u6df1\u6c34\u4e0b\u5e72\u6cd5\u710a\u63a5\u6280\u672f\u65f6\uff0c\u5f00\u53d1\u4e00\u79cd\u65b0\u578b\u7684\u65cb\u6d41\u5f0f\u53cc\u5c42\u6c14\u6d41\u4fdd\u62a4\u710a\u710a\u67aa\uff0c\u83b7\u4e2d\u56fd\u4e13\u5229\u5c40\u9881\u53d1\u7684\u53d1\u660e\u4e13\u5229\u3002<\/p>\n<p>20\u4e16\u7eaa80\u5e74\u4ee3\uff0c\u53d1\u660e\u4e86\u53cc\u4e1d\u7a84\u95f4\u9699\u57cb\u5f27\u710a\u65b9\u6cd5\uff0c\u6210\u529f\u5730\u89e3\u51b3\u4e86\u7279\u539a\u94a2\u7ed3\u6784\u710a\u63a5\u7684\u6548\u7387\u548c\u8d28\u91cf\u7684\u77db\u76fe\u4ee5\u53ca\u710a\u63a5\u81ea\u52a8\u5316\u95ee\u9898\uff0c\u672c\u6210\u679c\u66fe\u83b7\u673a\u68b0\u90e8\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\uff0c\u56fd\u5bb6\u53d1\u660e\u521b\u9020\u4e09\u7b49\u5956\u548c\u5168\u56fd\u4f18\u79c0\u4e13\u5229\u9879\u76ee\u5956\u3002\u540c\u671f\u8fd8\u4e3b\u6301\u7814\u5236\u4e86\u81ea\u884c\u9f99\u95e8\u5f0f\u53cc\u5934\u4e24\u7ef4\u8ddf\u8e2a\u81ea\u52a8\u710a\u63a5\u673a\uff0c\u710a\u63a5\u4e86\u4e3a\u5b9d\u94a2\u4e8c\u671f\u5de5\u7a0b\u5236\u9020\u7684\u5927\u578b\u51b6\u91d1\u8d77\u91cd\u673a\u4e3b\u6881\u53ca\u706b\u7bad\u53d1\u5c04\u5854\u7684\u6746\u4ef6\u7b49\u4ea7\u54c1\uff0c\u66fe\u83b7\u673a\u68b0\u90e8\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\u3002\u4e3b\u6301\u4e3a\u5de5\u5382\u7814\u523680\u578b\u6469\u6258\u8f66\u81ea\u52a8\u710a\u63a5\u673a\u7fa4\uff0c\u5171\u670914\u53f0\u710a\u63a5\u4e13\u673a\uff0c\u8fd9\u9879\u6210\u679c\u66fe\u83b7\u673a\u68b0\u90e8\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\u548c\u56fd\u5bb6\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\u3002<\/p>\n<p>20\u4e16\u7eaa90\u5e74\u4ee3\uff0c\u7ec4\u5efa\u4e86\u710a\u63a5\u673a\u5668\u4eba\u5de5\u7a0b\u5e94\u7528\u7814\u7a76\u5ba4\uff0c\u4e3b\u6301\u7814\u5236\u6210\u529f\u4e2d\u56fd\u81ea\u884c\u5f00\u53d1\u6210\u5957\u7684\u5f53\u65f6\u5168\u56fd\u6700\u5927\u3001\u6700\u590d\u6742\u7684\u63a8\u571f\u673a\u53f0\u8f66\u67b6\u5f27\u710a\u673a\u5668\u4eba\u5de5\u4f5c\u7ad9\uff0c\u66fe\u83b7\u673a\u68b0\u90e8\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\u548c\u56fd\u5bb6\u79d1\u6280\u8fdb\u6b65\u4e09\u7b49\u5956\u3002<\/p>\n<p><strong>\u5b8b\u5929\u864e<\/strong>\uff1a\u5728\u710a\u63a5\u751f\u4ea7\u8fc7\u7a0b\u673a\u68b0\u5316\u4e0e\u81ea\u52a8\u5316\u548c\u6c34\u4e0b\u710a\u63a5\u7b49\u65b9\u9762\u6709\u7cbe\u6df1\u7684\u7814\u7a76\u3002 \u53c2\u4e0e\u7684\u7814\u7a76\u9879\u76ee\u66fe\u83b7\u5f97\u673a\u68b0\u90e8\u79d1\u6280\u8fdb\u6b65\u4e00\u7b49\u5956\uff0c\u56fd\u5bb6\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\uff0c\u56fd\u5bb6\u7ecf\u59d4\u77f3\u6cb9\u8bbe\u5907\u4f18\u79c0\u79d1\u6280\u6210\u679c\u4e8c\u7b49\u5956\uff0c\u5168\u56fd\u79d1\u5b66\u5927\u4f1a\u5956\u7b49\u5956\u9879\u3002\u66fe\u4efb\u54c8\u5c14\u6ee8\u710a\u63a5\u7814\u7a76\u6240\u6240\u957f\u3001\u673a\u68b0\u79d1\u5b66\u7814\u7a76\u9662\u9662\u957f\u3001\u673a\u68b0\u5de5\u4e1a\u90e8\u79d1\u6280\u4e0e\u8d28\u91cf\u53f8\u53f8\u957f\uff0c\u73b0\u4efb\u4e2d\u56fd\u673a\u68b0\u5de5\u4e1a\u8054\u5408\u4f1a\u526f\u4f1a\u957f\u3001\u4e2d\u56fd\u673a\u68b0\u5de5\u7a0b\u5b66\u4f1a\u526f\u7406\u4e8b\u957f\u517c\u79d8\u4e66\u957f\u3001\u4e2d\u56fd\u710a\u63a5\u534f\u4f1a\u526f\u7406\u4e8b\u957f\u3001\u6559\u6388\u7ea7\u9ad8\u7ea7\u5de5\u7a0b\u5e08\u3001\u300a\u673a\u68b0\u5de5\u7a0b\u5b66\u62a5\u300b\u4e3b\u7f16\u3001\u56fd\u5bb6\u6709\u7a81\u51fa\u8d21\u732e\u7684\u4e2d\u9752\u5e74\u4e13\u5bb6\u5e76\u4eab\u53d7\u56fd\u52a1\u9662\u653f\u5e9c\u6d25\u8d34\u3002<\/p>\n<p><strong>\u5434\u6797<\/strong>\uff1a\u66fe\u5148\u540e\u4efb\u56fd\u52a1\u9662\u5b66\u4f4d\u59d4\u5458\u4f1a\u5b66\u79d1\u8bc4\u8bae\u7ec4\u6210\u5458\uff0c \u56fd\u52a1\u9662\u5b66\u4f4d\u59d4\u5458\u4f1a\u59d4\u5458\uff0c\u4e2d\u56fd\u710a\u63a5\u5b66\u4f1a\u524d\u4efb\u7406\u4e8b \u957f\uff0c\u73b0\u4efb\u6267\u59d4\uff0c\u56fd\u9645\u710a\u63a5\u5b66\u4f1a\u526f\u4e3b\u5e2d\uff0c\u6267\u59d4\u3002\u4e3b\u8981\u7814\u7a76\u65b9\u5411\uff1a\u673a\u5668\u4eba\u4e0e\u710a\u63a5\u667a\u80fd\u5316\u3001\u81ea\u52a8\u5316\u3002\u4e3b\u8981\u7814\u7a76\u5177\u6709\u4e00\u5b9a\u667a\u80fd\u7684\u710a\u63a5\u673a\u5668\u4eba\uff0c\u710a\u63a5\u8fc7\u7a0b\u4f20\u611f\uff0c\u710a\u63a5\u673a\u5668\u4eba\u667a\u80fd\u7cfb\u7edf\uff0c\u7279\u79cd\u73af\u5883\u4e0b\u7684\u710a\u63a5\u81ea\u52a8\u5316\u3001\u667a\u80fd\u5316\u7cfb\u7edf\uff0c\u710a\u63a5\u81ea\u52a8\u63a7\u5236\u548c\u667a\u80fd\u63a7\u5236\u5e94\u7528\u57fa\u7840\u7406\u8bba\u53ca\u65b0\u6280\u672f\uff0c\u5305\u62ec\u7a7a\u95f4\u710a\u63a5\u53ca\u9065\u63a7\u710a\u63a5\u3002<\/p>\n<p><strong>\u9648\u5251\u8679<\/strong>\uff1a1982\u5e74\u4ee5\u524d\u4e3b\u8981\u4ece\u4e8b\u710a\u63a5\u51b6\u91d1\u7684\u7814\u7a76\uff0c\u5206\u522b\u83b7\u56fd\u5bb6\u79d1\u5b66\u5927\u4f1a\u6210\u679c\u5956\u548c\u673a\u68b0\u90e8\u4e09\u7b49\u5956\uff0c\u7518\u8083\u7701\u4e8c\u7b49\u5956\uff0c\u83b7\u4e24\u9879\u4e13\u5229\uff0c\u7814\u7a76\u5de5\u4f5c\u5728\u56fd\u5185\u6709\u8f83\u5927\u5f71\u54cd\uff0c\u5171\u6709\u5341\u7bc7\u76f8\u5173\u8bba\u6587\u53d1\u8868\u5728WeldingJournal\uff0cMaterialsScience\u4e0a\u3002\u6750\u6599\u710a\u63a5\u8ba1\u7b97\u4e2d\u6a21\u62df\u53ca\u5de5\u827a\u4f18\u5316\u7684\u5b50\u8bfe\u9898\u83b7\u56fd\u5bb6\u201c\u4e03\u4e94\u201d\u653b\u5173\u91cd\u5927\u6210\u679c\u5956\u30021994\u5e74\u7ec4\u7ec7\u56fd\u9645\u4f1a\u8bae\u51fa\u7248\u8bba\u6587\u96c6\u3002<\/p>\n<p>1982\u5e74\u4ee5\u540e\u5728\u7814\u4fee\u5de5\u4f5c\u4e00\u5e74\u7684\u57fa\u7840\u4e0a\u4ece\u4e8b\u91d1\u5c5e\u8106\u6027\u65ad\u88c2\u673a\u7406\u7684\u7814\u7a76\uff0c1992\u5e74\u20141994\u5e74\u63d0\u51fa\u89e3\u7406\u65ad\u88c2\u65b0\u7684\u6a21\u578b\uff0c1996\u5e74\u5e94\u7f8e\u56fd\u54c8\u4f5b\u5927\u5b66\u6559\u6388\uff0c\u56fd\u9645\u529b\u5b66\u6743\u5a01\uff0c\u7f8e\u56fd\u4e24\u9662\u9662\u58ebJamesRice\u9080\u8bf7\u5728\u8be5\u6821\u4e3e\u884c\u8bb2\u5ea7\uff0c1997\u5e74\u56fd\u9645\u89e3\u7406\u65ad\u88c2\u4e13\u9898\u4f1a\u4e2d\u7f8e\u56fdRosenfield\u628a\u5b8c\u6210\u7684\u7269\u7406\u6a21\u578b\u79f0\u4e3a\u9648\u4e00\u738b\u56fe\u8c61\u3002<\/p>\n<p>2002\u5e74\u8fdb\u4e00\u6b65\u5b8c\u5584\u4e86\u6a21\u578b\uff0c\u5b8c\u6574\u5730\u9610\u8ff0\u4e86\u89e3\u7406\u65ad\u88c2\u7684\u7269\u7406\u8fc7\u7a0b\uff0c\u4fee\u6b63\u4e8673\u5e74\u56fd\u9645\u4e0a\u63d0\u51fa\u7684RKR\u6a21\u578b\uff0c\u89e3\u51b3\u4e86\u4e09\u5341\u5e74\u6765\u672a\u5f7b\u5e95\u89e3\u51b3\u7684\u4e00\u4e2a\u79d1\u5b66\u76f2\u70b9\uff0c\u5728\u6b64\u4e13\u9898\u4e0a\u5171\u670943\u7bc7\u8bba\u6587\u53d1\u8868\u5728\u77e5\u540d\u56fd\u9645\u6742\u5fd7\uff08Transactians\u00a0of\u00a0Metallugy\u00a0and\u00a0Materials\u548cActa\u00a0Materialia\u00a0\u7b49\uff09\u4e0a\uff0c\u5de5\u4f5c\u8fbe\u5230\u4e16\u754c\u524d\u6cbf\uff0c\u5728\u56fd\u9645\u4e0a\u4ea7\u751f\u8f83\u5927\u5f71\u54cd\u3002\u5148\u540e\u5728\u56fd\u5185\u5916\u6742\u5fd7\u548c\u5b66\u672f\u4f1a\u8bae\u4e0a\u5171\u53d1\u8868\u8bba\u6587\u8fd1\u767e\u7bc7\u3002\u4e0a\u8ff0\u7814\u7a76\u6210\u679c\u4e3a\u5b66\u68211998\u5e74\u83b7\u5f97\u535a\u58eb\u6388\u6743\u70b9\uff0c\u5960\u5b9a\u4e86\u5b66\u672f\u57fa\u7840\u3002<\/p>\n<p><strong>\u9648\u4e19\u68ee<\/strong>\uff1a50\uff5e60\u5e74\u4ee3\u9648\u4e19\u68ee\u53c2\u4e0e\u7ec4\u7ec7\u4e86\u5927\u578b\u8f67\u673a\u673a\u67b6\u7535\u6e23\u710a\u3001\u5927\u578b\u953b\u6a21\u5806\u710a\u3001\u5927\u578b\u8f67\u8f8a\u5806\u710a\u3001\u706b\u8f66\u8f6e\u7b8d\u5806\u710a\u3001\u6838\u53cd\u5e94\u5806\u94dd\u6c60\u58f3\u6c29\u5f27\u710a\u3001\u7535\u5b50\u675f\u710a\u673a\u7814\u5236\u3001\u591a\u5c42\u5305\u624e\u5f0f\u6c34\u538b\u673a\u9ad8\u538b\u84c4\u52bf\u5668\u5236\u9020\u7b49\u9879\u76ee\uff1b\u572870\u5e74\u4ee3\u53c2\u52a0\u8fdb\u884c\u7684&#8221;\u5927\u76f4\u5f84\u539a\u58c1\u7ba1\u5168\u4f4d\u7f6e\u81ea\u52a8\u710a\u673a&#8221;\u9879\u76ee\uff0c\u57281978\u5e74\u83b7\u5f97\u5168\u56fd\u79d1\u5b66\u5927\u4f1a\u7684\u5956\u52b1\u3002<\/p>\n<p>80\u5e74\u4ee3\u4ee5\u6765\uff0c\u4e3b\u6301\u4e86&#8221;9%Ni\u94a2\u5927\u578b\u7403\u7f50\u5e94\u529b\u5206\u6790\u4e0e\u8bc4\u5b9a&#8221;\u3001&#8221;\u710a\u63a5\u63a5\u5934\u5f39\u5851\u6027\u6761\u4ef6\u4e0b\u65ad\u88c2\u53c2\u91cf\u7684\u7814\u7a76&#8221;\u3001&#8221;\u710a\u63a5\u63a5\u5934\u65ad\u88c2\u884c\u4e3a\u7684\u5206\u5f62\u5206\u6790&#8221;\u3001&#8221;\u710a\u63a5\u63a5\u5934\u5931\u6548\u65ad\u53e3\u8ba1\u7b97\u673a\u8f85\u52a9\u4f53\u89c6\u5b66\u7814\u7a76&#8221;\u7b49\u9879\u76ee\uff1b\u4ed6\u7814\u5236\u7684&#8221;\u5f27\u710a\u5de5\u827a\u4e13\u5bb6\u7cfb\u7edf&#8221;\u83b7\u5f97\u4e86\u4e2d\u56fd\u77f3\u5316\u603b\u516c\u53f8\u79d1\u6280\u8fdb\u6b65\u4e8c\u7b49\u5956\u548c\u5317\u4eac\u5e02\u79d1\u6280\u8fdb\u6b65\u4e09\u7b49\u5956\u3002\u8fd9\u4e00\u7cfb\u7edf\u73b0\u5df2\u5728\u56fd\u518520\u4f59\u5bb6\u4f01\u4e1a\u5e94\u7528\u3002<\/p>\n<p>\u4ed6\u9886\u5bfc\u7684\u5c0f\u7ec4\u8fd8\u5f00\u53d1\u4e86&#8221;\u710a\u63a5CCT\u56fe\u5e94\u7528\u7cfb\u7edf&#8221;\u3001&#8221;\u710a\u5de5\u6280\u672f\u6863\u6848\u7ba1\u7406\u7cfb\u7edf&#8221;\u3001&#8221;\u710a\u6750\u7528\u91cf\u3001\u5de5\u65f6\u53ca\u6210\u672c\u4f30\u7b97\u7cfb\u7edf&#8221;\u3001&#8221;\u6709\u7f3a\u9677\u710a\u63a5\u7ed3\u6784\u5b89\u5168\u8bc4\u5b9a\u7cfb\u7edf&#8221;\u7b49\u710a\u63a5\u5de5\u7a0b\u5e94\u7528\u8f6f\u4ef6\u4ee5\u53ca\u5de5\u7a0b\u673a\u68b0\u710a\u63a5\u7ed3\u6784\u88c5\u914d\u710a\u63a5\u5de5\u827a\u8ba1\u7b97\u673a\u8f85\u52a9\u8bbe\u8ba1\u7cfb\u7edf(CAPP)\u3002<\/p>\n<p><strong>\u4faf\u7acb\u5c0a<\/strong>\uff1a\u65e9\u5728\u4e0a\u4e16\u7eaa50\u5e74\u4ee3\u5c31\u7814\u5236\u51fa\u5168\u9762\u66ff\u4ee3\u624b\u5de5\u751f\u4ea7\u7684\u201c\u87ba\u65cb\u538b\u6d82\u673a\u201d\u3001\u201c\u96a7\u9053\u7a91\u70d8\u5e72\u7089\u201d\u3001\u201c\u81ea\u52a8\u94fe\u6761\u70d8\u5e72\u7089\u201d\u7b49\u6210\u5957\u8bbe\u5907\uff0c\u4f7f\u710a\u6761\u751f\u4ea7\u6b65\u5165\u673a\u68b0\u5316\u65f6\u4ee3\u300250\u5e74\u4ee3\u672b\u7814\u5236\u6210\u529f\u949b\u9499\u6e23\u7cfb\u7535\u710a\u6761\u914d\u65b9T-50\uff08J422\uff09\uff0c\u81f3\u4eca\u4e3a\u5168\u56fd\u5404\u7535\u710a\u6761\u751f\u4ea7\u5382\u5bb6\u666e\u904d\u91c7\u7528\u300260\u5e74\u4ee3\u4e3a\u6253\u7834\u897f\u65b9\u56fd\u5bb6\u5bf9\u6211\u56fd\u710a\u6761\u4e3b\u539f\u6750\u6599\u201c\u91d1\u7ea2\u77f3\u201d\u7684\u7981\u8fd0\uff0c\u6210\u529f\u7814\u5236\u51fa\u201c\u8fd8\u539f\u949b\u94c1\u77ff\u201d\u66ff\u4ee3\u201c\u91d1\u7ea2\u77f3\u201d\uff0c\u751f\u4ea7\u78b3\u94a2\u710a\u6761\uff0c\u914d\u65b9\uff0c\u7ed3\u675f\u4e86\u6211\u56fd\u4f9d\u8d56\u8fdb\u53e3\u7684\u5386\u53f2\u30021983\u5e74\uff0c\u4ed6\u6210\u529f\u8bbe\u8ba1\u5236\u9020\u4e86\u56fd\u5185\u9996\u53f0\u201c\u9ad8\u6e29\u94fe\u6761\u5f0f\u710a\u6761\u70d8\u70e4\u7089\u201d\u3002\u51ed\u501f\u8fd9\u4e00\u8fbe\u5230\u56fd\u9645\u5148\u8fdb\u6c34\u5e73\u7684\u88c5\u5907\uff0c\u4e2d\u56fd\u7535\u710a\u6761\u751f\u4ea7\u5411\u81ea\u52a8\u5316\u8fc8\u51fa\u4e86\u5173\u952e\u7684\u4e00\u6b65\u3002<\/p>\n<p>1986\u5e74\uff0c62\u5c81\u7684\u4faf\u7acb\u5c0a\u6210\u7acb\u4e86\u5929\u6d25\u91d1\u6865\u710a\u6750\u96c6\u56e2\u6709\u9650\u516c\u53f8\u3002<\/p>\n<p><strong>\u53f2\u8000\u6b66<\/strong>\uff1a1991\u5e74\u7531\u56fd\u5bb6\u6559\u59d4\u548c\u52b3\u52a8\u4eba\u4e8b\u90e8\u6388\u4e88\u6709\u7a81\u51fa\u8d21\u732e\u56de\u56fd\u7559\u5b66\u4eba\u5458\u8363\u8a89\u8bc1\u4e66\uff0c 1992\u5e74\u8d77\u4eab\u53d7\u56fd\u52a1\u9662\u9881\u53d1\u7684\u653f\u5e9c\u7279\u6b8a\u6d25\u8d34\u3002\u517c\u4efb\u4e2d\u56fd\u673a\u68b0\u5de5\u7a0b\u5b66\u4f1a\u710a\u63a5\u5b66\u4f1a\u526f\u7406\u4e8b\u957f\u517c\u5b66\u672f\u5de5\u4f5c\u59d4\u5458\u4f1a\u4e3b\u4efb\uff0c \u4e2d\u56fd\u7535\u5de5\u6280\u672f\u5b66\u4f1a\u7535\u710a\u4e13\u4e1a\u59d4\u5458\u4f1a\u526f\u4e3b\u4efb\u3002\u591a\u79cd\u5b66\u672f\u671f\u520a\u53ca\u4e1b\u4e66\u7f16\u59d4\u3002<\/p>\n<p>\u957f\u671f\u4ece\u4e8b\u6750\u6599\u8fde\u63a5\u53ca\u5176\u5148\u8fdb\u5236\u9020\u6280\u672f\u7684\u7814\u7a76\u4e0e\u5f00\u53d1\u5de5\u4f5c\u3002\u5176\u4e2d\u5305\u62ec\u6750\u6599\u4e0e\u5de5\u7a0b\u7ed3\u6784\u7684\u65ad\u88c2\u4e0e\u75b2\u52b3\u3001\u6750\u6599\u5de5\u7a0b\u95ee\u9898\u7684\u5efa\u6a21\u4e0e\u6a21\u62df\u3001\u6750\u6599\u8fde\u63a5\u79d1\u5b66\u4e0e\u6280\u672f\u3001\u7535\u5b50\u7ec4\u88c5\u6750\u6599\u4e0e\u6280\u672f\u3001\u6750\u6599\u8d85\u58f0\u7279\u6027\u4e0e\u4fe1\u53f7\u5904\u7406\u7b49\u3002<\/p>\n<p>\u8d1f\u8d23\u6216\u627f\u62c5\u4e86\u5fb7\u56fd\u5927\u4f17\u6c7d\u8f66\u57fa\u91d1\u4f1a\u7b49\u5355\u4f4d\u8d44\u52a9\u7684\u56fd\u9645\u5408\u4f5c\u9879\u76ee3\u9879\uff0c \u56fd\u5bb6&#8221;\u4e03\u4e94&#8221;\u548c&#8221;\u516b\u4e94&#8221;\u91cd\u70b9\u79d1\u6280\u653b\u51735\u9879\uff0c 973\u91cd\u5927\u57fa\u7840\u7814\u7a761\u9879\uff0c863\u9879\u76ee1\u9879\uff0c\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u8bfe\u98986\u9879\uff0c \u5317\u4eac\u5e02\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u53ca\u653f\u5e9c\u9879\u76ee7\u9879\uff0c \u56fd\u5bb6\u6559\u59d4\u535a\u58eb\u70b9\u57fa\u91d1\u8bfe\u98982\u9879\u548c\u591a\u9879\u4f01\u4e1a\u59d4\u6258\u7684\u6280\u672f\u5f00\u53d1\u9879\u76ee\u3002\u83b7\u5f97\u90e8\u7ea7\u79d1\u6280\u8fdb\u6b65\u59565\u9879\u3002<\/p>\n<p><strong>\u5434\u7956\u4e7e<\/strong>\uff1a\u53c2\u4e0e\u4e86\u79e6\u5c71300MW\u548c600MW\u6838\u7535\u5de5\u7a0b\u4e00\u56de\u8def\u4e3b\u8bbe\u5907\u6750\u6599\u4e0e\u710a\u63a5\u6280\u672f\u7814\u7a76\uff0c\u4efb\u7814\u5236\u653b\u5173\u7ec4\u8d1f\u8d23\u4eba\u4e4b\u4e00\uff0c\u83b7\u5f97\u591a\u9879\u6838\u7535\u79d1\u6280\u6210\u679c\u5956\uff0c\u83b7\u4e0a\u6d77\u5e02\u6838\u7535\u529e\u5609\u5956\u4e3a\u6211\u56fd\u7b2c\u4e00\u53f0300MW\u6838\u7535\u5de5\u7a0b\u7684\u79d1\u6280\u529f\u81e3\u3002\u4ed6\u53c2\u4e0e\u7814\u5236\u6210\u529f\u7684\u96c6\u7bb1\u5185\u5b54\u6c29\u5f27\u5c01\u5e95\u710a\u88c5\u7f6e\u83b7\u673a\u68b0\u90e8\u79d1\u7814\u6210\u679c\u4e09\u7b49\u5956;\u9505\u7089\u78e8\u7164\u673a\u78e8\u8f8a\u5806\u710a\u4e13\u7528\u710a\u5242\u83b7\u4e0a\u6d77\u5e02\u79d1\u6280\u632f\u5174\u4e8c\u7b49\u5956\u7b49\u7b49\u3002\u81ea1992\u5e74\u8d77\u83b7\u56fd\u52a1\u9662\u7279\u6b8a\u6d25\u8d34\u8363\u8a89\u3002<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u725b\u65b0\u9510\u4f5c\u8005\u6768\u6811\u7f16\u8f91\u6574\u7406\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4ece\u710a\u63a5\u7ec8\u8eab\u6210\u5c31\u5956\u8bbe\u7acb\u4ee5\u6765\uff0c\u4e00\u5171\u670911\u4f4d\u83b7\u5f97\u4e86\u8be5\u8363\u8a89\uff0c\u4ed6\u4eec\u5206\u522b\u662f\u710a\u63a5\u754c\u56db\u4f4d\u9662\u58eb\uff1a\u6f58\u9645\u92ae\u9662\u58eb\u3001\u5173\u6865\u9662\u58eb\u3001\u5f90\u6ee8\u58eb\u9662\u58eb\u3001\u6797\u5c1a\u626c\u9662\u58eb\u4ee5\u53ca7\u4f4d\u5728\u710a\u63a5\u9886\u57df\u505a\u51fa\u5353\u8d8a\u8d21\u732e\u7684\u5b8b\u5929\u864e&#8230;<\/p>\n","protected":false},"author":129,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[3],"tags":[173],"class_list":["post-31900","post","type-post","status-publish","format-standard","hentry","category-yejie","tag-renwu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/31900"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/129"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=31900"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/31900\/revisions"}],"predecessor-version":[{"id":32266,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/31900\/revisions\/32266"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=31900"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=31900"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=31900"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}