{"id":33935,"date":"2016-08-16T17:00:22","date_gmt":"2016-08-16T09:00:22","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=33935"},"modified":"2016-08-16T18:50:11","modified_gmt":"2016-08-16T10:50:11","slug":"%e7%a9%ba%e6%b0%94%e5%90%88%e9%87%91-%e6%96%b0%e5%9e%8b%e6%b0%94%e5%87%9d%e8%83%b6%ef%bc%8c%e7%a5%9e%e4%b8%80%e6%a0%b7%e7%9a%84%e6%9d%90%e6%96%99%ef%bc%81","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=33935","title":{"rendered":"\u7a7a\u6c14\u5408\u91d1\u2014\u2014\u65b0\u578b\u6c14\u51dd\u80f6\uff0c\u795e\u4e00\u6837\u7684\u6750\u6599\uff01"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u6c14\u51dd\u80f6\uff0c\u4f5c\u4e3a\u4e16\u754c\u4e0a\u6700\u8f7b\u7684\u56fa\u4f53\uff0c\u8fd1\u5e74\u6765\u53d7\u5230\u4f17\u591a\u79d1\u5b66\u5bb6\u7684\u9752\u7750\uff0c\u800c\u8fd1\u65e5\uff0c\u79d1\u5b66\u5bb6\u4eec\u7814\u53d1\u51fa\u4e86\u4e00\u79cd\u65b0\u7684\u6c14\u51dd\u80f6\u2014\u2014\u7a7a\u6c14\u5408\u91d1\uff0c\u8fd9\u79cd\u6750\u6599\u5177\u6709\u9ad8\u5f3a\u5ea6\u3001\u8010\u4e45\u6027\u3001\u91cd\u91cf\u8d85\u8f7b\u3001\u53ef\u8bbe\u8ba1\u6027\u7b49\u7279\u70b9\uff0c\u6700\u91cd\u8981\u7684\u662f\u8fd9\u79cd\u6750\u6599\u5177\u6709\u8d85\u7edd\u7f18\u6027\u80fd\uff0c\u8fd9\u5bf9\u7edd\u70ed\u6750\u6599\u7684\u7814\u53d1\u4ee5\u53ca\u822a\u7a7a\u5b87\u822a\u9886\u57df\u5177\u6709\u975e\u51e1\u7684\u610f\u4e49\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-33936\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/2-25.jpg\" alt=\"2\" width=\"700\" height=\"524\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/2-25.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/2-25-300x225.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><br \/>\n\u4e16\u754c\u4e0a\u7528\u9014\u6700\u591a\u7684\u6750\u6599\u53ef\u80fd\u5c31\u5728\u8fd9\u4e86\uff0c\u5b83\u5c06\u6539\u53d8\u4e00\u5207\u3002\u6c14\u51dd\u80f6\u5df2\u7ecf\u51fa\u73b0\u6709\u4e00\u6bb5\u65f6\u95f4\u4e86\uff0c\u4f46\u521b\u65b0\u5df2\u7ecf\u4f7f\u6c14\u51dd\u80f6\u6280\u672f\u66f4\u52a0\u5b8c\u5584\u3001\u66f4\u52a0\u6709\u7528\u3002\u6c14\u51dd\u80f6\u662f\u4e00\u79cd\u4f4e\u5bc6\u5ea6\u7684\u56fa\u4f53\u6750\u6599\uff0c\u901a\u8fc7\u8d85\u4e34\u754c\u5e72\u71e5\u5de5\u827a\uff0c\u4ece\u80f6\u4f53\u4e2d\u63d0\u53d6\u51fa\u6db2\u4f53\u5373\u53ef\u5f97\u5230\u6c14\u51dd\u80f6\u3002\u4e00\u822c\u5e38\u89c1\u7684\u6c14\u51dd\u80f6\u4e3a\u7845\u6c14\u51dd\u80f6\uff0c\u4f46\u662f\u8fd9\u79cd\u6750\u6599\u8106\u6027\u975e\u5e38\u5927\u3002\u7ecf\u8fc7\u591a\u5e74\u7684\u7814\u7a76\uff0c\u7f8e\u56fd\u56fd\u5bb6\u822a\u7a7a\u822a\u5929\u5c40(NASA)\u7684\u79d1\u5b66\u5bb6\u4e0e\u4e00\u4e9b\u516c\u53f8\u5df2\u7ecf\u7814\u53d1\u51fa\u4e86\u65b0\u7684\u4ea7\u54c1\u2014\u2014\u7a7a\u6c14\u5408\u91d1\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-33937\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/1-35.jpg\" alt=\"1\" width=\"750\" height=\"443\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/1-35.jpg 750w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/1-35-300x177.jpg 300w\" sizes=\"(max-width: 750px) 100vw, 750px\" \/><br \/>\n\u8fd9\u79cd\u7a7a\u6c14\u5408\u91d1\u65e2\u5177\u6709\u4f20\u7edf\u5851\u6599\u7684\u9ad8\u5f3a\u5ea6\u548c\u8010\u4e45\u6027\uff0c\u53c8\u5177\u6709\u91cd\u91cf\u8f7b\u7684\u7279\u70b9\uff0c\u800c\u5728\u6c14\u51dd\u80f6\u4e2d\u53ef\u4ee5\u53d1\u73b0\u7684\u8d85\u7edd\u7f18\u6027\u80fd\u662f\u8fd9\u4e00\u4ea7\u54c1\u7684\u6700\u5927\u4f18\u52bf\u3002\u8fd9\u79cd\u6750\u6599\u5982\u6b64\u6709\u524d\u9014\u7684\u90e8\u5206\u539f\u56e0\u662f\u5b83\u7684\u53ef\u8bbe\u8ba1\u6027\u8d85\u5f3a\u3002\u7a7a\u6c14\u5408\u91d1\u5177\u6709\u6781\u5176\u4f4e\u7684\u5bc6\u5ea6\uff080.01~0.9g\/c2\uff09\uff0c\u8fd9\u4f7f\u5f97\u5b83\u4eec\u6210\u4e3a\u5730\u7403\u4e0a\u6700\u8f7b\u7684\u56fa\u4f53\u6750\u6599\u3002\u9664\u4e86\u8fd9\u79cd\u4f4e\u5bc6\u5ea6\u7279\u6027\uff0c\u8fd9\u79cd\u6750\u6599\u8fd8\u5177\u6709\u8d85\u7edd\u7f18\u6027\u80fd\u548c\u6781\u7aef\u7684\u6750\u6599\u5f3a\u5ea6\u3002\u57fa\u4e8e\u8fd9\u79cd\u7a7a\u6c14\u5408\u91d1\u7684\u9ad8\u5206\u5b50\u6750\u6599\u53ef\u4ee5\u627f\u62c5\u8d85\u8fc7\u5b83\u4eec\u81ea\u8eab20000\u500d\u7684\u91cd\u91cf\u3002<\/p>\n<p>\u8fd9\u79cd\u6750\u6599\u5177\u6709\u7684\u8d85\u7edd\u7f18\u6027\u4f7f\u79d1\u5b66\u5bb6\u4eec\u6781\u4e3a\u9707\u60ca\uff0c\u8fd9\u9010\u6e10\u4f7f\u5f97\u65e2\u8584\u53c8\u8f7b\u7684\u7edd\u7f18\u6750\u6599\u6210\u4e3a\u53ef\u80fd\u3002\u8be5\u6750\u6599\u4e0d\u4ec5\u53ef\u4ee5\u9694\u7edd\u6e29\u5ea6\uff0c\u800c\u4e14\u9694\u7edd\u58f0\u97f3\u7684\u6548\u679c\u4e5f\u5f88\u597d\u3002\u4e8b\u5b9e\u4e0a\uff0c\u4f5c\u4e3a\u4e00\u79cd\u58f0\u97f3\u7edd\u7f18\u4f53\uff0c\u8fd9\u79cd\u6750\u6599\u6bd4\u5e02\u573a\u4e0a\u7684\u5176\u4ed6\u4ea7\u54c1\u8981\u597d100\u52301000\u500d\u3002\u8fd1\u65e5\uff0c\u7f8e\u56fd\u56fd\u5bb6\u822a\u7a7a\u822a\u5929\u5c40(NASA)\u5df2\u7ecf\u7814\u53d1\u51fa\u4e86\u4e00\u79cd\u8d85\u8584\u6613\u5f2f\u66f2\u7684\u7a7a\u6c14\u5408\u91d1\uff08\u5982\u4e0b\u56fe\uff09\uff0c\u5728\u592a\u7a7a\u670d\u548c\u706b\u7bad\u6280\u672f\u4e0a\u5f97\u5230\u5145\u5206\u5e94\u7528\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-33938\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/3-23.jpg\" alt=\"3\" width=\"750\" height=\"422\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/3-23.jpg 750w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/3-23-300x169.jpg 300w\" sizes=\"(max-width: 750px) 100vw, 750px\" \/><br \/>\n\u8fd9\u79cd\u6750\u6599\u7684\u673a\u68b0\u548c\u7ed3\u6784\u6027\u80fd\u6b63\u9010\u6e10\u5411\u524d\u53d1\u5c55\uff0c\u5b83\u751a\u81f3\u53ef\u4ee5\u88ab\u5236\u6210\u900f\u660e\u7684\u4ece\u800c\u53ef\u4ee5\u8ba9\u65e5\u5149\u8fdb\u5165\uff0c\u4f46\u7edd\u5bf9\u4e0d\u4f1a\u5f71\u54cd\u9694\u70ed\u6027\u80fd\u3002\u8be5\u6750\u6599\u7684\u672a\u6765\u7531\u90a3\u4e9b\u4e0d\u505c\u5de5\u4f5c\u4e3a\u4e86\u53d1\u73b0\u6750\u6599\u7684\u66f4\u591a\u7528\u5904\u7684\u5de5\u7a0b\u5e08\u548c\u8bbe\u8ba1\u4eba\u5458\u6240\u638c\u63e1\u3002\u8bb8\u591a\u6c14\u51dd\u80f6\u5546\u4e1a\u516c\u53f8\u4e5f\u5df2\u7ecf\u6210\u7acb\uff0c\u751a\u81f3\u4f1a\u6709\u4e00\u5bb6\u516c\u53f8\u7528\u6539\u826f\u7248\u7684\u6c14\u51dd\u80f6\u5236\u6210\u9ad8\u8d28\u91cf\u7684\u5939\u514b\u5462\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/interestingengineering.com\/airloy-the-new-super-material\/\" target=\"_blank\">Airloy: The New Super Material<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u5f20\u83b9\u63d0\u4f9b\u7d20\u6750\uff0c\u6a0a\u8d85\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u6c14\u51dd\u80f6\uff0c\u4f5c\u4e3a\u4e16\u754c\u4e0a\u6700\u8f7b\u7684\u56fa\u4f53\uff0c\u8fd1\u5e74\u6765\u53d7\u5230\u4f17\u591a\u79d1\u5b66\u5bb6\u7684\u9752\u7750\uff0c\u800c\u8fd1\u65e5\uff0c\u79d1\u5b66\u5bb6\u4eec\u7814\u53d1\u51fa\u4e86\u4e00\u79cd\u65b0\u7684\u6c14\u51dd\u80f6\u2014\u2014\u7a7a\u6c14\u5408\u91d1\uff0c\u8fd9\u79cd\u6750\u6599\u5177\u6709\u9ad8\u5f3a\u5ea6\u3001\u8010\u4e45\u6027\u3001\u91cd\u91cf\u8d85\u8f7b\u3001\u53ef&#8230;<\/p>\n","protected":false},"author":842,"featured_media":33936,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[4],"tags":[14],"class_list":["post-33935","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-ganhuo","tag-lightweight"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/33935"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/842"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=33935"}],"version-history":[{"count":7,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/33935\/revisions"}],"predecessor-version":[{"id":34155,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/33935\/revisions\/34155"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/33936"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=33935"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=33935"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=33935"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}