{"id":35719,"date":"2016-08-23T08:00:52","date_gmt":"2016-08-23T00:00:52","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=35719"},"modified":"2016-08-23T17:13:46","modified_gmt":"2016-08-23T09:13:46","slug":"%e7%bb%86%e8%8f%8c%e5%bc%95%e5%8f%91%e7%9a%84%e7%9f%b3%e5%a2%a8%e7%83%af%e5%a4%aa%e9%98%b3%e7%94%b5%e6%b1%a0%e7%9a%84%e6%94%b9%e9%9d%a9","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=35719","title":{"rendered":"\u7ec6\u83cc\u5f15\u53d1\u7684\u77f3\u58a8\u70ef\u592a\u9633\u7535\u6c60\u7684\u6539\u9769"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b<\/strong>:\u7ec6\u83cc\u7684\u53c2\u4e0e\u4f7f\u65b0\u4e00\u4ee3\u7684\u592a\u9633\u80fd\u7535\u6c60\u548c\u5176\u5b83\u7535\u5b50\u8bbe\u5907\u53d8\u5f97\u66f4\u5c0f\u3001\u66f4\u8f7b\u3001\u66f4\u4fbf\u5b9c\u6210\u4e3a\u53ef\u80fd\u3002\u4e00\u79cd\u5236\u9020\u5177\u6709\u65b0\u7535\u5b50\u5c5e\u6027\u7684\u77f3\u58a8\u70ef\u7684\u65b9\u6cd5\u904d\u53ca\u4e86\u7f51\u7edc\u7684\u5404\u4e2a\u89d2\u843d\u3002\u8fd9\u9879\u7814\u7a76\u5bf9\u751f\u4ea7\u66f4\u5c0f\u3001\u66f4\u8f7b\u3001\u66f4\u4fbf\u5b9c\u7684\u592a\u9633\u80fd\u7535\u6c60\u548c\u5176\u5b83\u7535\u5b50\u8bbe\u5907\u6709\u5de8\u5927\u7684\u5f71\u54cd\uff0c\u4f46\u8fd9\u4e0d\u662f\u552f\u4e00\u4ee4\u4eba\u5174\u594b\u7684\u539f\u56e0\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-35722\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/bacteria-graphene-solar-1.jpg\" alt=\"bacteria-graphene-solar-1\" width=\"600\" height=\"502\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/bacteria-graphene-solar-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/bacteria-graphene-solar-1-300x251.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u67af\u8349\u82bd\u80de\u6746\u83cc\u843d<\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u7ec6\u83cc\u77f3\u58a8\u70ef\u592a\u9633\u80fd\uff1a\u5728\u7ec6\u83cc\u7684\u5e2e\u52a9\u4e0b\u4ea7\u751f\u7684\u65b0\u4e00\u4ee3\u592a\u9633\u80fd\u7535\u6c60<\/strong><\/span><\/p>\n<p>\u65b0\u7684\u77f3\u58a8\u70ef\u7814\u7a76\u4e2d\u4e00\u4e2a\u76f8\u5f53\u597d\u7684\u90e8\u5206\u662f\u5176\u4e0e\u4f17\u4e0d\u540c\u7684\u5236\u9020\u65b9\u6cd5\u3002\u8fd9\u79cd\u77f3\u58a8\u70ef\u56e0\u4e3a\u5177\u6709\u7eb3\u7c73\u7ea7\u7684\u8936\u76b1\u800c\u5177\u6709\u72ec\u7279\u7684\u7535\u5b50\u6027\u8d28\u3002\u8fd9\u4e9b\u8936\u76b1\u7684\u4ea7\u751f\u662f\u7531\u4e8e\u7814\u7a76\u4eba\u5458\u5728\u5236\u9020\u8fc7\u7a0b\u4e2d\u52a0\u5165\u7ec6\u83cc\u7684\u7f18\u6545\u3002<\/p>\n<p>\u662f\u7684\uff0c\u7ec6\u83cc\u2014\u2014\u5730\u7403\u4e0a\u6700\u53e4\u8001\u7684\u751f\u7269\u4e4b\u4e00\u2014\u2014\u5df2\u7ecf\u5e94\u7528\u5230\u526a\u88c1\u6700\u65b0\u7684\u7eb3\u7c73\u6750\u6599\u4e2d(\u77f3\u58a8\u70ef\u57282004\u5e74\u88ab\u53d1\u73b0)\u3002\u5728\u77f3\u58a8\u70ef\u8868\u9762\u751f\u6210\u8936\u76b1\u5e76\u4e0d\u662f\u4e00\u79cd\u65b0\u9896\u7684\u505a\u6cd5\u3002\u4f46\u4f20\u7edf\u7684\u65b9\u6cd5\uff08\u6bd4\u5982\u62c9\u4f38\u7247\u5c42\u5e76\u8ba9\u5176\u7a81\u7136\u6298\u56de\uff09\u662f\u6709\u6548\u7684\uff0c\u5374\u4e0d\u80fd\u5f97\u5230\u7279\u522b\u7cbe\u786e\u7684\u8936\u76b1\u3002<\/p>\n<p>\u8fd9\u65b0\u9879\u76ee\u7684\u56e2\u961f\u662f\u7531\u829d\u52a0\u54e5\u7684\u4f0a\u5229\u8bfa\u4f0a\u5927\u5b66\u5927\u5b66\u521b\u5efa\u7684\u3002\u4ed6\u4eec\u7684\u60f3\u6cd5\u662f\u901a\u8fc7\u6392\u5217\u7ec6\u83cc\u9635\u5217\u76f4\u63a5\u8fdb\u5165\u77f3\u58a8\u70ef\u7684\u6765\u6784\u5efa\u7cbe\u786e\u7684\u8936\u76b1\u3002<\/p>\n<p>\u5728\u8fd9\u4e2a\u9879\u76ee\u4e2d\uff0c\u4ed6\u4eec\u4f7f\u7528\u4e86\u67af\u8349\u82bd\u5b62\u6746\u83cc\uff08\u4e00\u79cd\u5df2\u7ecf\u88ab\u5145\u5206\u7814\u7a76\u5e76\u80fd\u7528\u4e8e\u5236\u9020\u6297\u751f\u7d20\u7684\u571f\u6816\u7684\u7ec6\u83cc\uff09\u3002\u5b83\u662f\u975e\u5e38\u5c0f\u4e14\u5177\u6709\u51e0\u4e4e\u6c38\u8fdc\u6c89\u7761\u80fd\u529b\u7684\u7ec6\u83cc\uff0c\u6240\u4ee5\u5c06\u5176\u7528\u4e8e\u5236\u9020\u4ea7\u54c1\u5177\u6709\u5f88\u597d\u7684\u524d\u666f\u3002<\/p>\n<p>\u5728\u663e\u5fae\u955c\u4e0b, \u67af\u8349\u82bd\u5b62\u6746\u83cc\u770b\u8d77\u6765\u50cf\u8ff7\u4f60\u9999\u80a0\u3002\u7814\u7a76\u56e2\u961f\u8ba9\u5b83\u4eec\u50cf\u9999\u80a0\u4e32\u4e00\u6837\u8fdb\u884c\u6392\u5217\uff0c\u5e76\u5c06\u5176\u653e\u5165\u5177\u6709\u7535\u573a\u7684\u5355\u5c42\u77f3\u58a8\u70ef\u4e2d\u3002\u63a5\u4e0b\u6765\uff0c\u4ed6\u4eec\u5c06\u77f3\u58a8\u70ef\/\u7ec6\u83cc\u7ec4\u5408\u653e\u5165\u771f\u7a7a\u4e2d\u3002\u5728\u771f\u7a7a\u6761\u4ef6\u4e0b\u4ece\u7ec6\u83cc\u4e2d\u5438\u53d6\u6c34\u5206\uff0c\u4ece\u800c\u8feb\u4f7f\u5b83\u4eec\u840e\u7f29\u3002\u7531\u4e8e\u77f3\u58a8\u70ef\u7684\u67d4\u97e7\u6027\u975e\u5e38\u597d\uff0c\u5b83\u968f\u7740\u6210\u6392\u7684\u7ec6\u83cc\u7684\u840e\u7f29\u800c\u91cd\u65b0\u914d\u7f6e,\u8fd9\u6837\u5c31\u5f97\u5230\u4e86\u7cbe\u786e\u5bf9\u9f50\u7684\u7eb3\u7c73\u8936\u76b1\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-35723 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/bacteria-graphene-solar-2.jpg\" alt=\"bacteria-graphene-solar-2\" width=\"600\" height=\"400\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/bacteria-graphene-solar-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/08\/bacteria-graphene-solar-2-300x200.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u539f\u5b50\u529b\u663e\u5fae\u955c\u663e\u793a\u7ec6\u83cc\u8986\u76d6\u5728\u77f3\u58a8\u70ef\u7247\u7684\u5f62\u8c8c(\u5de6\u56fe),\u548c\u771f\u7a7a\u5904\u7406\u540e\u77f3\u58a8\u70ef\u8936\u76b1\u7684\u5f62\u8c8c(\u53f3\u56fe,2\u500d\u653e\u5927):<\/p>\n<p>\u7814\u7a76\u56e2\u961f\u7684\u7ec4\u957fVikas Berry\u8868\u793a\uff1a\u201c\u7531\u4e8e\u771f\u7a7a\u8fc7\u7a0b\u4e2d\u521b\u5efa\u4e86\u78b3\u7eb3\u7c73\u7ba1\uff0c\u90a3\u4e48\u7531\u6b64\u4ea7\u751f\u7684\u6df7\u5408\u6750\u6599\u5176\u6027\u8d28\u4e0d\u540c\u4e8e\u5355\u7eaf\u7684\u77f3\u58a8\u70ef\u3002\u8936\u76b1\u5728\u78b3\u539f\u5b50\u5468\u56f4\u7684\u7535\u5b50\u4e91\u5f00\u8f9f\u4e86\u4e00\u4e2a\u201cV\u201d\u2026\u201d\u8fd9\u53ef\u4ee5\u62d3\u5c55\u7535\u5b50\u5e26\u9699\u7684\u5076\u6781\u77e9\uff0c\u7136\u800c\u5e73\u9762\u77f3\u58a8\u70ef\u5e76\u4e0d\u5177\u5907\u8fd9\u79cd\u6027\u8d28\u3002\u201d<\/p>\n<p>\u6839\u636eBerry\u7684\u63cf\u8ff0\uff0c\u8fd9\u79cd\u7edf\u4e00\u7684\u6392\u5217\u5728\u7535\u573a\u4e2d\u521b\u5efa\u4e00\u4e2a\u5dee\u5f02\uff0c\u4f7f\u5f97\u6a2a\u5411\u7535\u6d41\u5c0f\u4e8e\u7eb5\u5411\u7535\u6d41\u3002\u7814\u7a76\u56e2\u961f\u7684\u4e0b\u4e00\u4e2a\u76ee\u6807\u662f\u66f4\u51c6\u786e\u7684\u6539\u5584\u548c\u88c1\u526a\u7684\u8936\u76b1\uff0c\u5373\u5b8c\u6210\u4e24\u4e2a\u8936\u76b1\u76f8\u8ddd\u5927\u7ea6\u4e24\u4e2a\u7eb3\u7c73(\u4e16\u754c\u4e0a\u6700\u5c0f\u7684)\u7684\u76ee\u6807\u3002<\/p>\n<p>\u4f60\u53ef\u4ee5\u5728Nano\u6742\u5fd7\u4e2d\u7684\u201cConfined, Oriented, and Electrically Anisotropic Graphene Wrinkles on Bacteria.\u201d\u5f97\u5230\u66f4\u591a\u7684\u7ec6\u8282\u3002\u8fd9\u91cc\u6709\u4e00\u5c0f\u6bb5\u662f\u5173\u4e8e\u8fd9\u7bc7\u6587\u7ae0\u7684\u6458\u8981(\u5404\u5411\u5f02\u6027\u6307\u6750\u6599\u5728\u4e0d\u540c\u7684\u65b9\u5411\u6d4b\u91cf\u8868\u73b0\u51fa\u4e0d\u540c\u7684\u6027\u8d28):\u2026\u2026\u7ed3\u679c\u663e\u793a\u7531\u751f\u7269\u8bf1\u5bfc\u4ea7\u751f\u7684\u5177\u6709\u53ef\u63a7\u7684\u3001\u5b9a\u5411\u7684\u4ee5\u53ca\u7535\u5b50\u5404\u5411\u5f02\u6027\u7684\u77f3\u58a8\u70ef\u8936\u76b1\u53ef\u5e94\u7528\u4e8e\u7535\u5b50\u3001\u751f\u7269\u7535\u673a\u68b0\u5b66\u548c\u5e94\u53d8\u6a21\u5f0f\u3002<\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u7ec6\u83cc\u4f7f\u7f8e\u56fd\u8d70\u5411\u590d\u5174<\/strong><\/span><\/p>\n<p>\u5728\u5176\u4ed6\u65b9\u9762\uff0c\u7ec6\u83cc\u5df2\u7ecf\u6162\u6162\u8fdb\u5165\u6e05\u6d01\u6280\u672f\u9886\u57df\u3002\u7ebd\u7ea6\u5dde\u5bbe\u5384\u59c6\u987f\u5dde\u7acb\u5927\u5b66\u6700\u8fd1\u5229\u7528\u84dd\u85fb\u7ec6\u83cc\u521b\u5efa\u4e86\u4e00\u4e2a\u57fa\u4e8e\u751f\u7269\u7684\u592a\u9633\u80fd\u7535\u6c60\u3002<\/p>\n<p>\u5728\u582a\u8428\u65af\u5dde\u7acb\u5927\u5b66\uff0c\u7814\u7a76\u4eba\u5458\u4e5f\u4e00\u76f4\u81f4\u529b\u4e8e\u7528\u7ec6\u83cc\u4ea7\u751f\u7684\u67d3\u6599\u4ee3\u66ff\u67d3\u8272\u654f\u5316\u592a\u9633\u80fd\u7535\u6c60\u4e2d\u7684\u6709\u6bd2\u5316\u5b66\u7269\u8d28\u3002\u7ec6\u83cc\u5728\u50a8\u80fd\u9886\u57df\u4e5f\u5d2d\u9732\u5934\u89d2\u3002<\/p>\n<p>\u5728\u5148\u8fdb\u5236\u9020\u4e1a\u65b9\u9762\uff0c\u7814\u7a76\u4eba\u5458\u6b63\u5728\u5229\u7528\u7ec6\u83cc\u6765\u63a2\u7d22\u795e\u79d8\u7684\u751f\u7269\u81ea\u7ec4\u88c5\u3002\u5982\u679c\u628a\u4e09\u7ef4\u6253\u5370\u3001\u6a21\u5757\u81ea\u7ec4\u88c5\u4ee5\u53ca\u673a\u5668\u4eba\u8fdb\u884c\u7ec4\u5408\uff0c\u90a3\u4e48\u672a\u6765\u4f60\u5c06\u770b\u5230\u4e0e\u4f20\u7edf\u65b9\u5f0f\u622a\u7136\u4e0d\u540c\u7684\u5236\u9020\u4ea7\u4e1a\u7684\u751f\u4ea7\u7ebf\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/cleantechnica.com\/2016\/08\/11\/common-bug-opens-door-to-next-gen-graphene-solar-cells\/\" target=\"_blank\">Common Bug Opens Door To Next-Gen Graphene Solar Cells<\/a><\/p>\n<p>\u76f8\u5173\u6587\u732e\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b03214\" target=\"_blank\"><span class=\"hlFld-Title\">Confined, Oriented, and Electrically Anisotropic Graphene Wrinkles on Bacteria<\/span><\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u5f20\u83b9\u63d0\u4f9b\u7d20\u6750\uff1b\u725b\u6548\u83b9\u7f16\u8bd1\uff1b\u9ec4\u8d85\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b:\u7ec6\u83cc\u7684\u53c2\u4e0e\u4f7f\u65b0\u4e00\u4ee3\u7684\u592a\u9633\u80fd\u7535\u6c60\u548c\u5176\u5b83\u7535\u5b50\u8bbe\u5907\u53d8\u5f97\u66f4\u5c0f\u3001\u66f4\u8f7b\u3001\u66f4\u4fbf\u5b9c\u6210\u4e3a\u53ef\u80fd\u3002\u4e00\u79cd\u5236\u9020\u5177\u6709\u65b0\u7535\u5b50\u5c5e\u6027\u7684\u77f3\u58a8\u70ef\u7684\u65b9\u6cd5\u904d\u53ca\u4e86\u7f51\u7edc\u7684\u5404\u4e2a\u89d2\u843d\u3002\u8fd9\u9879\u7814\u7a76\u5bf9\u751f\u4ea7\u66f4\u5c0f&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[78,18],"class_list":["post-35719","post","type-post","status-publish","format-standard","hentry","category-keji","tag-photovoltaic","tag-xinnengyuan"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/35719"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=35719"}],"version-history":[{"count":7,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/35719\/revisions"}],"predecessor-version":[{"id":36088,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/35719\/revisions\/36088"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=35719"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=35719"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=35719"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}