{"id":3688,"date":"2016-03-15T17:00:09","date_gmt":"2016-03-15T09:00:09","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=3688"},"modified":"2016-03-15T16:00:15","modified_gmt":"2016-03-15T08:00:15","slug":"eth%e7%a0%94%e5%8f%91%e5%87%ba%e6%b6%82%e6%96%99%e4%b8%ad%e7%9a%84%e4%b8%87%e7%94%a8%e7%91%9e%e5%a3%ab%e5%86%9b%e5%88%80","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=3688","title":{"rendered":"ETH\u7814\u53d1\u51fa\u6d82\u6599\u4e2d\u7684\u4e07\u7528\u201c\u745e\u58eb\u519b\u5200\u201d"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-3689 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/03\/1-10.jpg\" alt=\"\" width=\"699\" height=\"429\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/03\/1-10.jpg 699w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/03\/1-10-300x184.jpg 300w\" sizes=\"(max-width: 699px) 100vw, 699px\" \/><\/p>\n<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u751f\u6d3b\u4e2d\u96be\u514d\u4f1a\u9047\u5230\u7269\u54c1\u8868\u9762\u6cbe\u6ee1\u6c61\u6e0d\u7684\u60c5\u5f62\uff0c\u4f60\u662f\u5426\u4e5f\u66fe\u7ecf\u4e3a\u4e4b\u53d1\u6101\uff1f\u90a3\u4e48ETH\u6700\u65b0\u7814\u53d1\u7684\u4e07\u7528\u578b\u6d82\u6599\u5c06\u4e3a\u4f60\u5e26\u6765\u798f\u97f3\uff0c\u5f7b\u5e95\u6446\u8131\u4f60\u7684\u70e6\u607c\u3002<\/p>\n<p>\u6d82\u6599\u5e38\u5e38\u7528\u4e8e\u8868\u9762\u9632\u62a4\uff0c\u53ef\u7528\u6765\u9632\u6b62\u85fb\u7c7b\u6c61\u67d3\u6c34\u8d28\uff0c\u86cb\u767d\u8d28\u548c\u7ec6\u83cc\u5371\u5bb3\u4eba\u4f53\u3002\u6d82\u5c42\u901a\u5e38\u53ef\u4ee5\u4f7f\u7269\u8d28\u8868\u9762\u66f4\u52a0\u5149\u6ed1\uff0c\u4ee5\u9632\u6b62\u8868\u9762\u88ab\u6d77\u85fb\u3001\u7ec6\u83cc\u3001\u86cb\u767d\u8d28\u8fd9\u7c7b\u7269\u8d28\u201c\u5f04\u810f\u201d\u3002\u4eb2\u6c34\u805a\u5408\u7269\u4e5f\u56e0\u6b64\u800c\u88ab\u5e7f\u6cdb\u4f7f\u7528\uff1a\u6c34\u5206\u5b50\u805a\u96c6\u5728\u4eb2\u6c34\u805a\u5408\u7269\u7684\u8868\u9762\uff0c\u80fd\u591f\u963b\u6b62\u5fae\u5c0f\u9897\u7c92\u548c\u5fae\u751f\u7269\u201c\u4fb5\u5165\u201d \u6750\u6599\u5185\u90e8\u3002<\/p>\n<p>\u7136\u800c\uff0c\u73b0\u5728\u6b63\u5728\u4f7f\u7528\u7684\u8bb8\u591a\u6d82\u5c42\u6bd4\u8f83\u8106\u5f31\uff0c\u56e0\u4e3a\u5b83\u4eec\u548c\u6750\u6599\u4ec5\u9760\u6bd4\u8f83\u5f31\u7684\u9759\u7535\u529b\u7ed3\u5408\u5728\u4e00\u8d77\u3002\u5927\u90e8\u5206\u6bd4\u8f83\u8010\u7528\u7684\u6d82\u5c42\u53c8\u901a\u5e38\u6bd4\u8f83\u6602\u8d35\uff0c\u751a\u81f3\u6709\u7684\u5e26\u6709\u6bd2\u6027\u3002<\/p>\n<p>\u4ee5\u745e\u58eb\u82cf\u9ece\u4e16\u8054\u90a6\u7406\u5de5\u5b66\u9662\u8868\u9762\u79d1\u5b66\u6280\u672f\u4e13\u5bb6Nicholas Spencer\u4e3a\u9996\u7684\u79d1\u7814\u5de5\u4f5c\u8005\u51b3\u5b9a\u5171\u540c\u5bfb\u627e\u4e00\u79cd\u7b80\u5355\u7684\u65b9\u6cd5\uff0c\u501f\u52a9\u5f3a\u6709\u529b\u7684\u5171\u4ef7\u952e\uff0c\u5c06\u6d82\u6599\u5206\u5b50\u56fa\u5b9a\u5728\u6750\u6599\u8868\u9762\u3002\u4ed6\u4eec\u4e5f\u5e0c\u671b\u80fd\u591f\u627e\u5230\u4e00\u79cd\u529e\u6cd5\uff0c\u53ef\u4ee5\u5c06\u6d82\u5c42\u9002\u7528\u4e8e\u51e0\u79cd\u4e0d\u540c\u6750\u6599\u7ec4\u6210\u7684\u8868\u9762\u6216\u8005\u8bbe\u5907\u4e0a\u3002\u201c\u6211\u4eec\u60f3\u5f97\u5230\u4e00\u79cd\u9ad8\u5206\u5b50\u6d82\u6599\uff0c\u53ef\u4ee5\u50cf\u745e\u58eb\u519b\u5200\u90a3\u6837\u4e07\u7528\u3002\u201dSpencer\u8bf4\u3002<\/p>\n<p>\u6700\u7ec8\u4ed6\u4eec\u6210\u529f\u4e86\uff01\u8fd9\u79cd\u51c0\u65e0\u6c61\u67d3\u7684\u9ad8\u5206\u5b50\u6750\u6599\u7531\u4e00\u6761\u4e3b\u94fe\u548c\u5e26\u6709\u4eb2\u6c34\u7aef\u7684\u652f\u94fe\u7ec4\u6210\uff0c\u540c\u65f6\u5177\u5907\u4e24\u79cd\u80fd\u591f\u5f62\u6210\u5171\u4ef7\u952e\u7684\u4fa7\u94fe\u2014\u2014\u4e00\u79cd\u80fd\u591f\u4e0e\u7845\u548c\u73bb\u7483\u5f62\u6210\u7ed3\u5408\u952e\uff0c\u53e6\u4e00\u79cd\u5219\u53ef\u4ee5\u548c\u8fc7\u6e21\u91d1\u5c5e\u6c27\u5316\u7269\uff08\u4f8b\u5982\u949b\u548c\u94c1\uff09\u6210\u952e\u3002<\/p>\n<p>\u201c\u4f7f\u7528\u6211\u4eec\u8fd9\u79cd\u65b0\u578b\u6750\u6599\u8fdb\u884c\u6d82\u8986\u5f88\u7b80\u5355\u2014\u2014\u6ce1\u8fdb\u53bb\uff0c\u7136\u540e\u62ff\u51fa\u6765\u51b2\u6d17\u4e00\u4e0b\uff01\u201dSpencer\u8bf4\uff0c\u201c\u5b83\u8fd8\u80fd\u6311\u6218\u5404\u79cd\u73af\u5883\uff0c\u65e0\u8bba\u9178\u6027\u3001\u78b1\u6027\u8fd8\u662f\u9ad8\u76d0\u6d53\u5ea6\u3002\u751a\u81f3\u53ef\u4ee5\u653e\u5728\u53bb\u57a2\u5242\u4e2d\u3002\u201d<\/p>\n<p>ETH\u7684\u5b50\u516c\u53f8Susos\u5df2\u7ecf\u63d0\u4ea4\u4e86\u8fd9\u79cd\u9ad8\u5206\u5b50\u7684\u4e13\u5229\u7533\u8bf7\u3002\u79d1\u5b66\u5bb6\u4eec\u8ba4\u4e3a\u8fd9\u79cd\u6d82\u6599\u53ef\u4ee5\u7528\u4e8e\u751f\u7269\u9886\u57df\uff0c\u963b\u6b62\u7ec6\u83cc\u5bf9\u4eba\u4f53\u7684\u5371\u5bb3\uff1b\u4e5f\u53ef\u4ee5\u7528\u4e8e\u963b\u9694\u751f\u7269\u9644\u7740\u7269\uff0c\u4ece\u800c\u5b9e\u73b0\u6c34\u8d28\u6cbb\u7406\uff0c\u4e3a\u8239\u8236\u7684\u822a\u884c\u4e0e\u6355\u9c7c\u63d0\u4f9b\u4fbf\u5229\uff1b\u8fd8\u80fd\u5e94\u7528\u5230\u98df\u54c1\u5de5\u4e1a\u65b9\u9762\uff0c\u4f8b\u5982\u5305\u88c5\u6750\u6599\u3002<\/p>\n<p>\u8fd9\u79cd\u6750\u6599\u5c31\u50cf\u6d82\u5c42\u754c\u7684\u745e\u58eb\u519b\u5200\uff0c\u800c\u4e14\u8fd8\u6709\u66f4\u5f00\u653e\u7684\u6539\u9020\u7a7a\u95f4\u3002\u5982\u679c\u6211\u4eec\u4e3a\u5176\u642d\u914d\u5176\u4ed6\u7c7b\u578b\u7684\u652f\u94fe\uff0c\u8fd8\u80fd\u5b9e\u73b0\u66f4\u5e7f\u6cdb\u7684\u5e94\u7528\u3002<\/p>\n<p>\u7814\u7a76\u7ed3\u679c\u53d1\u8868\u5728\u671f\u520a <a href=\"http:\/\/dx.doi.org\/10.1002\/marc.201500683\" target=\"_blank\"><em>Macromolecular Rapid\u00a0Communications<\/em><\/a>\u4e0a\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.materialstoday.com\/polymers-soft-materials\/news\/slippery-coating-sticks-fast-to-different-surfaces\/\" target=\"_blank\">Slippery Coating Sticks Fast to Different Surfaces<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u6768\u6d2a\u671f\u63d0\u4f9b\u7d20\u6750\uff0c\u738b\u65d7\u7f16\u8bd1\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u751f\u6d3b\u4e2d\u96be\u514d\u4f1a\u9047\u5230\u7269\u54c1\u8868\u9762\u6cbe\u6ee1\u6c61\u6e0d\u7684\u60c5\u5f62\uff0c\u4f60\u662f\u5426\u4e5f\u66fe\u7ecf\u4e3a\u4e4b\u53d1\u6101\uff1f\u90a3\u4e48ETH\u6700\u65b0\u7814\u53d1\u7684\u4e07\u7528\u578b\u6d82\u6599\u5c06\u4e3a\u4f60\u5e26\u6765\u798f\u97f3\uff0c\u5f7b\u5e95\u6446\u8131\u4f60\u7684\u70e6\u607c\u3002 \u6d82\u6599\u5e38\u5e38\u7528\u4e8e\u8868\u9762\u9632\u62a4\uff0c&#8230;<\/p>\n","protected":false},"author":230,"featured_media":3689,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[42],"class_list":["post-3688","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-gaofenzi"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/3688"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=3688"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/3688\/revisions"}],"predecessor-version":[{"id":3736,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/3688\/revisions\/3736"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/3689"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=3688"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=3688"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=3688"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}