{"id":38123,"date":"2016-09-04T14:00:21","date_gmt":"2016-09-04T06:00:21","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=38123"},"modified":"2016-09-15T22:12:37","modified_gmt":"2016-09-15T14:12:37","slug":"%e4%b8%80%e8%a8%80%e4%b8%8d%e5%90%88%e5%b0%b1%e9%9a%90%e8%ba%ab%ef%bc%81%e7%8e%a9%e5%bc%84%e5%85%89%e7%ba%bf%e7%9a%84%e5%85%89%e5%ad%90%e6%99%b6%e4%bd%93%e6%98%af%e6%80%8e%e6%a0%b7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=38123","title":{"rendered":"\u4e00\u8a00\u4e0d\u5408\u5c31\u9690\u8eab\uff01\u201c\u73a9\u5f04\u201d\u5149\u7ebf\u7684\u5149\u5b50\u6676\u4f53\u662f\u600e\u6837\u7684\u5b58\u5728\uff1f"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u9690\u8eab\u6597\u7bf7\u6700\u8fd1\u4e5f\u4e0d\u662f\u4ec0\u4e48\u65b0\u9c9c\u4e8b\u4e86\uff0c\u53ef\u662f\u771f\u6b63\u4fbf\u6377\u5b9e\u7528\u597d\u7528\u7684\u8fd8\u771f\u6ca1\u6709\uff0c\u95ee\u9898\u5c31\u51fa\u5728\u8fd9\u4e2a\u6750\u6599\u4e0a\uff01\u8fd1\u65e5\uff0c\u5bc6\u897f\u6839\u7406\u5de5\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u5c31\u5236\u5907\u51fa\u4e86\u4e00\u79cd\u5947\u7279\u7684\u5149\u5b50\u6676\u4f53\uff0c\u80fd\u591f\u201c\u73a9\u5f04\u201d\u5149\u7ebf\u4e8e\u80a1\u638c\u4e4b\u95f4\uff0c\u4e0d\u4ec5\u80fd\u4f7f\u5149\u62d0\u5f2f\uff0c\u8fd8\u80fd\u518d\u52a0\u901f\uff0c\u4ece\u800c\u8fbe\u5230\u4f7f\u7269\u4f53\u9690\u8eab\u7684\u6548\u679c\uff01<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-38278 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/11111-1.jpg\" alt=\"11111\" width=\"740\" height=\"327\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/11111-1.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/11111-1-300x133.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/p>\n<p>\u73b0\u5728\uff0c\u91c7\u7528\u91d1\u5c5e\u5143\u7d20\u5236\u9020\u9690\u8eab\u6597\u7bf7\u7684\u8d85\u6750\u6599\uff0c\u6709\u4e00\u4e9b\u96be\u9898\u8fd8\u662f\u65e0\u6cd5\u5f97\u5230\u89e3\u51b3\u3002<\/p>\n<p>\u4e3b\u8981\u6709\u4e09\u70b9\uff1a\u4e00\u662f\u63a7\u5236\u5404\u5411\u5f02\u6027\uff0c\u5373\u5fc5\u987b\u5408\u7406\u63a7\u5236\u6597\u7bf7\u5728\u4e0d\u540c\u65b9\u5411\u5bf9\u5149\u6ce2\u7684\u4f20\u5bfc\u5b58\u5728\u7684\u5dee\u5f02\uff1b\u4e8c\u662f\u5fc5\u987b\u4fdd\u8bc1\u6597\u7bf7\u6750\u6599\u80fd\u5bf9\u5fae\u6ce2\u548c\u53ef\u89c1\u5149\u6ce2\u8d77\u4f5c\u7528\uff0c\u8fd9\u4e00\u70b9\u5f88\u91cd\u8981\uff1b\u4e09\u662f\u79d1\u5b66\u5bb6\u9700\u8981\u5c3d\u91cf\u964d\u4f4e\u635f\u8017\uff0c\u56e0\u4e3a\u8fd9\u4f1a\u9650\u5236\u9690\u8eab\u7269\u4f53\u7684\u5c3a\u5bf8\u3002<\/p>\n<p>\u7535\u6c14\u5de5\u7a0b\u526f\u6559\u6388Elena Semouchkina\u548c\u5979\u7684\u7814\u7a76\u751f\u4eec\u5df2\u7ecf\u7814\u53d1\u51fa\u4e00\u4e9b\u65b0\u6280\u672f\uff0c\u4f7f\u9690\u8eab\u6597\u7bf7\u66f4\u52a0\u5b9e\u7528\u3002\u4ed6\u4eec\u6700\u65b0\u7684\u6210\u679c\u53d1\u8868\u5728Journal of Optics\u6742\u5fd7\u7684\u4e00\u671f\u5173\u4e8e\u53d8\u6362\u5149\u5b66\u7684\u4e13\u520a\u4e0a\uff0c\u4e3b\u8981\u4ecb\u7ecd\u4e86\u4e00\u79cd\u5f88\u6709\u524d\u666f\u7684\u65b0\u65b9\u6cd5\uff0c\u80fd\u591f\u63a7\u5236\u7535\u78c1\u6ce2\u4f7f\u7269\u4f53\u9690\u8eab\u3002\u4ed6\u4eec\u91c7\u7528\u4e86\u4e00\u79cd\u5149\u5b50\u6676\u4f53\u6765\u5b9e\u73b0\u8fd9\u4e00\u6548\u679c\u3002<\/p>\n<p><strong>\u9690\u8eab\u7684\u79d1\u5b66<\/strong><\/p>\n<p>\u9690\u8eab\u5e76\u4e0d\u662f\u9b54\u672f\u5e08\u7684\u5c0f\u628a\u620f\uff0c\u5176\u771f\u6b63\u7684\u79d1\u5b66\u539f\u7406\u662f\u6539\u53d8\u7535\u78c1\u6ce2\u7684\u4f20\u64ad\u65b9\u5411\u3002\u9690\u8eab\u88c5\u7f6e\u5728\u4e00\u5b9a\u7684\u7a7a\u95f4\u5185\u4f7f\u7535\u78c1\u6ce2\u7684\u4f20\u64ad\u8def\u5f84\u53d1\u751f\u626d\u66f2\uff0c\u4ece\u800c\u9690\u85cf\u67d0\u4e00\u7269\u4f53\uff0c\u7136\u540e\u4f7f\u7535\u78c1\u6ce2\u6cbf\u7740\u5f2f\u66f2\u7684\u8f68\u8ff9\u52a0\u901f\u79fb\u52a8\u3002\u6839\u636e\u53d8\u6362\u5149\u5b66\u7684\u57fa\u672c\u539f\u7406\uff0c\u53ef\u4ee5\u901a\u8fc7\u516c\u5f0f\u8ba1\u7b97\uff0c\u9884\u6d4b\u51fa\u80fd\u591f\u4ee5\u7279\u5b9a\u65b9\u5f0f\u626d\u66f2\u7535\u78c1\u6ce2\u7684\u6750\u6599\u7684\u6027\u80fd\u5728\u7a7a\u95f4\u4e0a\u7684\u5206\u5e03\u7279\u70b9\u3002<\/p>\n<p>\u4e3a\u4e86\u7814\u5236\u51fa\u8fd9\u79cd\u6750\u6599\uff0cSemouchkina\u548c\u5979\u7684\u56e2\u961f\u5f00\u59cb\u4f7f\u7528\u4ecb\u7535\u8c10\u632f\u5668\u5236\u5907\u7684\u8d85\u6750\u6599\uff0c\u800c\u4e0d\u662f\u91d1\u5c5e\u8d85\u6750\u6599\u3002\u56e0\u4e3a\u4ecb\u7535\u6750\u6599\u5177\u6709\u6781\u4f4e\u7684\u7535\u5bfc\u7387\u548c\u635f\u8017\uff0c\u5e76\u4e14\u4ecb\u7535\u8c10\u632f\u5668\u80fd\u4f7f\u7535\u78c1\u6ce2\u5728\u5176\u4e2d\u6765\u56de\u53cd\u5f39\uff0c\u5c31\u50cf\u4f5c\u4e3a\u58f0\u6ce2\u5171\u9e23\u5668\u7684\u97f3\u53c9\u4e00\u6837\uff0c\u8fd9\u6837\u5c31\u80fd\u63a7\u5236\u7535\u78c1\u6ce2\u5728\u9690\u8eab\u88c5\u7f6e\u4e2d\u7684\u4f20\u64ad\u4e86\u3002<\/p>\n<p>\u76ee\u524d\uff0cSemouchkina\u7814\u5236\u51fa\u6765\u7684\u9690\u8eab\u6750\u6599\u5177\u6709\u5468\u671f\u7ed3\u6784\uff0c\u53eb\u505a\u5149\u5b50\u6676\u4f53\u3002\u8fd9\u79cd\u5149\u5b50\u6676\u4f53\u662f\u542b\u6709\u4ecb\u7535\u6746\u7684\u7279\u5b9a\u6676\u4f53\u7ed3\u6784\u3002\u4e0e\u4e00\u822c\u7684\u8d85\u6750\u6599\u4e0d\u540c\uff0c\u8fd9\u4e9b\u6676\u4f53\u539f\u5b50\u7684\u5171\u632f\u5e76\u4e0d\u4f1a\u4ee5\u6ce2\u7684\u5f62\u5f0f\u4f20\u64ad\u3002\u62e5\u6709\u5947\u7279\u6027\u80fd\u7684\u5149\u5b50\u6676\u4f53\u8ba9\u9690\u8eab\u6597\u7bf7\u7684\u4e0d\u518d\u9065\u8fdc\uff01<\/p>\n<p><strong>\u8d85\u5149\u901f\u6750\u6599<\/strong><\/p>\n<p>Semouchkina\u56e2\u961f\u7528\u6765\u5236\u5907\u9690\u8eab\u6750\u6599\u7684\u5149\u5b50\u6676\u4f53\u80fd\u4f7f\u4f20\u64ad\u7684\u7535\u78c1\u6ce2\u8fbe\u5230\u8d85\u5149\u901f\u7684\u76f8\u4f4d\u901f\u5ea6\uff0c\u7b80\u5355\u7684\u8bf4\uff0c\u5c31\u662f\u5b83\u80fd\u4f7f\u7535\u78c1\u6ce2\u8d85\u5149\u901f\u3002<\/p>\n<p>\u8fd9\u6837\u7684\u9ad8\u901f\u5c31\u80fd\u4f7f\u7535\u78c1\u6ce2\u524d\u6cbf\u5feb\u901f\u5730\u201c\u7ed5\u201d\u8fc7\u7269\u4f53\u7ee7\u7eed\u5411\u524d\u4f20\u64ad\u3002\u5c31\u50cf\u94bb\u77f3\u80fd\u5c06\u5149\u6298\u5c04\u6210\u4e94\u989c\u516d\u8272\uff0c\u8fd9\u79cd\u5149\u5b50\u6676\u4f53\u4e5f\u62e5\u6709\u8fd9\u79cd\u7279\u5b9a\u7684\u6298\u5c04\u6307\u6570\u5404\u5411\u5f02\u6027\uff0c\u4e5f\u5c31\u662f\u8bf4\u6cbf\u7740\u4e0d\u540c\u6676\u9762\u4f20\u64ad\u7684\u7535\u78c1\u6ce2\u7684\u76f8\u4f4d\u901f\u5ea6\u4e5f\u662f\u4e0d\u4e00\u6837\u7684\u3002\u6b63\u662f\u7531\u4e8e\u8fd9\u79cd\u76f8\u4f4d\u901f\u5ea6\u7684\u76f8\u4e92\u62b5\u6d88\uff0c\u624d\u4ea7\u751f\u4e86\u9690\u8eab\u7684\u5947\u7279\u6548\u679c\u3002<\/p>\n<p>Semouchkina\u8868\u793a\uff1a\u201c\u89e3\u51b3\u5404\u5411\u5f02\u6027\u96be\u9898\u7684\u5173\u952e\u7684\u4e00\u70b9\u662f\uff0c\u8c03\u6574\u6676\u4f53\u5728\u7279\u5b9a\u65b9\u5411\u4e0a\u7684\u6676\u683c\u53c2\u6570\u3002\u201d<\/p>\n<p>\u9690\u8eab\u6280\u672f\u7684\u5e94\u7528\u6781\u5176\u7684\u5e7f\u6cdb\uff0c\u4ece\u56fd\u9632\u5230\u5de5\u4e1a\uff0c\u5b83\u80fd\u53d1\u6325\u7684\u4f5c\u7528\u8d85\u51fa\u4f60\u6211\u7684\u60f3\u8c61\u3002\u867d\u7136\u9690\u8eab\u6597\u7bf7\u8fd8\u662f\u90a3\u4e48\u795e\u79d8\u83ab\u6d4b\uff0c\u4f46\u662f\u79d1\u5b66\u7684\u9053\u7406\u5176\u5b9e\u5f88\u7b80\u5355\uff0c\u5c31\u662f\u63a7\u5236\u5149\u7ebf\u800c\u5df2\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/www.sciencedaily.com\/releases\/2016\/08\/160831111000.htm\" target=\"_blank\">Invisibility cloak with photonic crystals<\/a>\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/iopscience.iop.org\/article\/10.1088\/2040-8978\/18\/4\/044007\/meta;jsessionid=EFBDB39DF64B45BD8F8D94EAD197F5E5.c2.iopscience.cld.iop.org\" target=\"_blank\">Superluminal media formed by photonic crystals for transformation optics-based invisibility cloaks<\/a>\u3002<\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u5218\u4e07\u6625\u63d0\u4f9b\u7d20\u6750\uff0cwilliamyen\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u9690\u8eab\u6597\u7bf7\u6700\u8fd1\u4e5f\u4e0d\u662f\u4ec0\u4e48\u65b0\u9c9c\u4e8b\u4e86\uff0c\u53ef\u662f\u771f\u6b63\u4fbf\u6377\u5b9e\u7528\u597d\u7528\u7684\u8fd8\u771f\u6ca1\u6709\uff0c\u95ee\u9898\u5c31\u51fa\u5728\u8fd9\u4e2a\u6750\u6599\u4e0a\uff01\u8fd1\u65e5\uff0c\u5bc6\u897f\u6839\u7406\u5de5\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u5c31\u5236\u5907\u51fa\u4e86\u4e00\u79cd\u5947\u7279\u7684\u5149\u5b50\u6676\u4f53\uff0c\u80fd\u591f&#8230;<\/p>\n","protected":false},"author":579,"featured_media":38126,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[70],"class_list":["post-38123","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-chaocailiao"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/38123"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/579"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=38123"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/38123\/revisions"}],"predecessor-version":[{"id":41262,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/38123\/revisions\/41262"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/38126"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=38123"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=38123"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=38123"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}