{"id":38517,"date":"2016-09-07T14:00:15","date_gmt":"2016-09-07T06:00:15","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=38517"},"modified":"2016-09-06T22:37:56","modified_gmt":"2016-09-06T14:37:56","slug":"macromolecules-%e8%81%9a%e5%90%88%e7%89%a9%e7%bd%91%e7%bb%9c%e7%bb%93%e6%9e%84%ef%bc%9a%e6%8b%93%e6%89%91%e8%bf%9e%e6%8e%a5%e7%82%b9%e7%b1%bb%e5%9e%8b%e5%af%b9%e4%ba%a4%e8%81%94%e5%af%86%e5%ba%a6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=38517","title":{"rendered":"Macromolecules \u805a\u5408\u7269\u7f51\u7edc\u7ed3\u6784\uff1a\u62d3\u6251\u8fde\u63a5\u70b9\u7c7b\u578b\u5bf9\u4ea4\u8054\u5bc6\u5ea6\u548c\u5b8f\u89c2\u51dd\u80f6\u6027\u80fd\u7684\u5f71\u54cd"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u6c34\u51dd\u80f6\u7684\u5fae\u89c2\u7ed3\u6784\u548c\u52a8\u529b\u5b66\u5728\u5f88\u5927\u7a0b\u5ea6\u4e0a\u51b3\u5b9a\u5176\u6027\u80fd\uff0c\u5982\u6c34\u6e17\u900f\u6027\uff0c\u5f39\u6027\uff0c\u5f3a\u5ea6\u548c\u4f7f\u7528\u5bff\u547d\u3002\u7ed3\u5408\u9002\u5f53\u7684\u6a61\u80f6\u5f39\u6027\u7406\u8bba\u6a21\u578b\uff0c\u901a\u8fc7\u673a\u68b0\u5206\u6790\u548c\u5e73\u8861\u6eb6\u80c0\u6d4b\u8bd5\u662f\u8868\u5f81\u7f51\u7edc\u7ed3\u6784\u6700\u5e38\u7528\u7684\u65b9\u6cd5\u3002\u4e0d\u540c\u6a21\u578b\u7684\u533a\u522b\u5728\u4e8e\u5bf9\u65bd\u52a0\u5b8f\u89c2\u5e94\u529b\u540e\u7f51\u7edc\u7ed3\u70b9\u54cd\u5e94\u7684\u63cf\u8ff0\u4e0d\u540c\u3002\u5728\u8fd1\u5341\u5e74\u95f4\uff0c\u79d1\u5b66\u5bb6\u4eec\u81f4\u529b\u4e8e\u6539\u5584\u6b64\u7c7b\u6a21\u578b\uff0c\u671f\u671b\u5f97\u5230\u5fae\u89c2\u5c3a\u5bf8\u805a\u5408\u7269\u52a8\u529b\u5b66\u666e\u9002\u6a21\u578b\uff0c\u4f46\u5e76\u672a\u53d6\u5f97\u8f83\u597d\u7684\u6210\u679c\u3002\u5f88\u591a\u60c5\u51b5\u4e0b\uff0c\u8fd9\u4e9b\u6a21\u578b\u53ea\u9002\u7528\u4e8e\u6700\u7b80\u5355\u7684\u5747\u76f8\u7f51\u7edc\uff0c\u5bf9\u4e8e\u591a\u76f8\u548c\u6709\u7f3a\u9677\u7f51\u7edc\u4e0d\u518d\u9002\u7528\u3002\u7531\u4e8e\u5bf9\u805a\u5408\u7269\u7cfb\u7edf\u5fae\u89c2\u7ed3\u6784\u5982\u4f55\u51b3\u5b9a\u6574\u4f53\u6027\u8d28\u7684\u539f\u56e0\u4ecd\u4e0d\u5341\u5206\u6e05\u695a\uff0c\u4ece\u800c\u963b\u788d\u4e86\u65b0\u4e00\u4ee3\u6c34\u51dd\u80f6\u7684\u8bbe\u8ba1\u4e0e\u5e94\u7528\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u6700\u8fd1\uff0c\u7231\u5c14\u5170\u90fd\u67cf\u6797\u5927\u5b66\u7684Dermot F. Brougham(\u901a\u8baf\u4f5c\u8005)\u548c\u8377\u5170\u5185\u6885\u4ea8\u5927\u5b66\u7684Victor M. Litvinov(\u901a\u8baf\u4f5c\u8005)\u7b49\u4eba\u4f7f\u7528\u5355\u4f53\u805a\u4e59\u4e8c\u9187\u4e8c\u4e19\u70ef\u9178\u916f(PEGDA)\uff0c\u4e19\u70ef\u9178\u5df1\u916f(HA)\u548c\u5b63\u620a\u56db\u9187\u56db(3-\u5def\u57fa\u4e19\u9178\u916f)(PETM)\u901a\u8fc7\u5149\u5f15\u53d1\u81ea\u7531\u57fa\u805a\u5408\u5236\u5907\u5f97\u5230\u5177\u6709\u4e24\u4e2a\u4e0d\u540c\u62d3\u6251\u7ed3\u6784\u7684\u805a\u4e59\u4e8c\u9187(PEG)\u57fa\u805a\u4e19\u70ef\u9178\u916f\u7f51\u7edc\u3002\u9996\u6b21\u5c06\u5316\u5b66\u4f4d\u79fb\u7279\u5f02\u6027\u53cc\u91cf\u5b50NMR\u5206\u6790\u7528\u4e8eUV\u56fa\u5316\u7684PEGDA\u7cfb\u7edf\u7684\u7814\u7a76\u3002\u8fd9\u79cd\u65b9\u6cd5\u53ef\u4ee5\u68c0\u6d4b\u5355\u5b98\u80fd\u56e2\u4e19\u70ef\u9178\u916f\u5728PEGDA\u7f51\u7edc\u52a8\u529b\u5b66\u4e2d\u7684\u5f71\u54cd\u3002<\/p>\n<p>\u901a\u8fc7\u62c9\u94fe\u72b6\u8fde\u63a5\u70b9\u7f51\u7edc\u548c\u70b9\u72b6\u8fde\u63a5\u70b9\u7f51\u7edc\u7684\u6bd4\u8f83\uff0c\u8868\u660e\u7f51\u7edc\u62d3\u6251\u7ed3\u6784\u662f\u805a\u5408\u7269\u52a8\u529b\u5b66\u4e2d\u4ea7\u751f\u6240\u8c13\u201c\u77ed\u94fe\u5f02\u5e38\u201d\u7684\u5173\u952e\u3002\u7279\u522b\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u62c9\u94fe\u72b6\u7f51\u7edc\u7684\u53cc\u91cf\u5b50(DQ)NMR\u5206\u6790\u8868\u660e\uff0c\u62d3\u6251\u7ed3\u6784\u5bf9\u7f51\u7edc\u94fe\u6bb5\u5404\u5411\u540c\u6027\u8fd0\u52a8\u7684\u8f83\u5f3a\u7ea6\u675f\u76f4\u63a5\u5bfc\u81f4\u7cfb\u7edf\u6709\u6548\u529f\u80fd\u7684\u589e\u52a0\u3002\u7531\u4e8e\u62d3\u6251\u7ea6\u675f\u4f7f\u5f97\u7f51\u7edc\u4e2d\u94fe\u6bb5\u8fd0\u52a8\u51fa\u73b0\u975e\u9ad8\u65af\u884c\u4e3a\uff0c\u4f7f\u5f97\u7ecf\u5178\u7684\u6a61\u80f6\u5f39\u6027\u7406\u8bba\u4e0d\u9002\u7528\u4e8e\u5177\u6709\u62c9\u94fe\u72b6\u8fde\u63a5\u70b9\u7684\u7f51\u7edc\u3002\u800c\u5728\u5177\u6709\u70b9\u72b6\u7ed3\u70b9\u7684PEGDA-PETM\u7f51\u7edc\u4e2d\uff0c\u7c7b\u4f3c\u5178\u578b\u7684\u5e7b\u8c61\u6a21\u578b\u652f\u914d\u7f51\u7edc\u7684\u52a8\u6001\u884c\u4e3a\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u7b80\u4ecb\u3011<\/strong><\/p>\n<p><strong>\u56fe1\uff1a\u7f51\u7edc\u7ed3\u6784\u793a\u610f\u56fe<\/strong><\/p>\n<p style=\"text-align: center;\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-38789\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c1.jpeg\" alt=\"\u037c1\" width=\"700\" height=\"241\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c1.jpeg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c1-300x103.jpeg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>(a)\u62c9\u94fe\u72b6\u8fde\u63a5\u7f51\u7edc(PEGDA-HA)\uff1b(b)\u70b9\u72b6\u8fde\u63a5\u7f51\u7edc(PEGDA-PETM)<\/p>\n<p><strong>\u56fe2\uff1aPEG\u94fe\u7684\u5f52\u4e00\u5316DQ\u7d2f\u79ef\u66f2\u7ebf\u548c\u76f8\u5e94\u7684\u8026\u5408\u5e38\u6570\u5206\u5e03<\/strong><\/p>\n<p style=\"text-align: center;\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-38790\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c2.jpeg\" alt=\"\u037c2\" width=\"700\" height=\"987\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c2.jpeg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c2-213x300.jpeg 213w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>(a)PEG\u94fe\u7684\u5f52\u4e00\u5316DQ \u7d2f\u79ef\u5f3a\u5ea6\u4e0eDQ\u6f14\u5316\u65f6\u95f4\u7684\u5173\u7cfb\u66f2\u7ebf(3.56 ppm)\uff1b<\/p>\n<p>(b)\u76f8\u5e94\u7684\u8026\u5408\u5e38\u6570\u5206\u5e03\uff0c\u5782\u76f4\u865a\u7ebf\u8868\u793a\u5e73\u5747\u503c\u8026\u5408\u5e38\u6570D<sub>avg<\/sub>\u3002\u63d2\u56fe\u662fD<sub>avg<\/sub>\u4e0eHA\u5171\u805a\u5355\u4f53\u7684\u91cd\u91cf\u5206\u6570\u7684\u51fd\u6570\u4ee5\u53caPEGDA-PETM\u7f51\u7edc\u4e2d\u7684D<sub>avg<\/sub>\u3002<\/p>\n<p><strong>\u56fe3\uff1a\u4e0d\u540cHA\u8d28\u91cf\u5206\u6570\u7684\u7f51\u7edc\u52a8\u529b\u5b66\u793a\u610f\u56fe\u548c\u6027\u80fd\u6bd4\u8f83<\/strong><\/p>\n<p style=\"text-align: center;\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-38791\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c3.jpeg\" alt=\"\u037c3\" width=\"700\" height=\"614\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c3.jpeg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u037c3-300x263.jpeg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>(a)HA\u542b\u91cf\u7684\u589e\u52a0\u4f7f\u5f97\u4e19\u70ef\u9178\u94fe\u7684\u7075\u6d3b\u6027\u589e\u52a0\uff0c\u5bfc\u81f4\u6240\u6709\u94fe\u5355\u5143\u7684\u6b8b\u7559\u5076\u6781\u8026\u5408(RDC)\u964d\u4f4e\uff1b<\/p>\n<p>(b) HA\u4fa7\u94fe\u4e0d\u540c\u94fe\u5355\u5143\u7684D<sub>avg<\/sub>\u503c\uff1b(c)PEG\u94fe\u7684\u5f39\u6027\u50a8\u80fd\u6a21\u91cfE&#8217;\u548c\u5e73\u5747RDC D<sub>avg<\/sub>\u7684\u6bd4\u8f83\u3002<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u901a\u8fc7\u4e0d\u540c\u7684\u65b9\u6cd5\u5bf9\u4e24\u79cd\u7c7b\u578b\u7684\u805a\u4e19\u70ef\u9178\u916f\u7f51\u7edc\u8fdb\u884c\u7814\u7a76\uff0c\u5bf9\u7ecf\u5178\u6a61\u80f6\u5f39\u6027\u7406\u8bba\u8fdb\u884c\u4e00\u5b9a\u7a0b\u5ea6\u7684\u6821\u6b63\u3002\u4e0d\u540c\u4e8e\u5176\u4ed6\u7814\u7a76\u8005\uff0c\u8be5\u7814\u7a76\u7ed3\u679c\u7a81\u51fa\u4e86\u57fa\u4e8e\u5b9e\u9645\u7f51\u7edc\u7ed3\u6784\u7684\u7269\u7406\u9700\u6c42\u800c\u4f7f\u7528NMR\u6280\u672f\u8fdb\u884c\u6821\u6b63\uff0c\u53ef\u88ab\u5e94\u7528\u4e8e\u66f4\u5927\u8303\u56f4\u7684\u5f02\u6784\u7f51\u7edc\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acs.macromol.6b01070\">Network Structure in Acrylate Systems: Effect of Junction Topology<\/a>\u00a0<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acs.macromol.6b01070\" target=\"_blank\">on Cross-Link Density and Macroscopic Gel Properties <\/a>(Macromolecules\uff0c2016\uff0cDOI\uff1a10.1021\/acs.macromol.6b01070)<\/p>\n<p>\u611f\u8c22\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u9ad8\u5206\u5b50\u7ec4watermelon\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c <a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u4eba\u7f51\u5c0a\u91cd\u6240\u6709\u8fdb\u884c\u77e5\u8bc6\u4f20\u64ad\u7684\u5a92\u4f53\uff0c\u8f6c\u8f7d\u8bf7\u8054\u7cfbtougao@cailiaoren.com\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u6c34\u51dd\u80f6\u7684\u5fae\u89c2\u7ed3\u6784\u548c\u52a8\u529b\u5b66\u5728\u5f88\u5927\u7a0b\u5ea6\u4e0a\u51b3\u5b9a\u5176\u6027\u80fd\uff0c\u5982\u6c34\u6e17\u900f\u6027\uff0c\u5f39\u6027\uff0c\u5f3a\u5ea6\u548c\u4f7f\u7528\u5bff\u547d\u3002\u7ed3\u5408\u9002\u5f53\u7684\u6a61\u80f6\u5f39\u6027\u7406\u8bba\u6a21\u578b\uff0c\u901a\u8fc7\u673a\u68b0\u5206\u6790\u548c\u5e73\u8861\u6eb6\u80c0\u6d4b\u8bd5\u662f\u8868\u5f81\u7f51\u7edc\u7ed3\u6784&#8230;<\/p>\n","protected":false},"author":393,"featured_media":38789,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[42],"class_list":["post-38517","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-gaofenzi"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/38517"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/393"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=38517"}],"version-history":[{"count":7,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/38517\/revisions"}],"predecessor-version":[{"id":39051,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/38517\/revisions\/39051"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/38789"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=38517"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=38517"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=38517"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}