{"id":3903,"date":"2016-03-20T17:00:15","date_gmt":"2016-03-20T09:00:15","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=3903"},"modified":"2016-03-20T15:36:02","modified_gmt":"2016-03-20T07:36:02","slug":"%e8%96%84%e8%86%9c%e6%9d%90%e6%96%99%e4%b8%8e%e8%a1%a8%e9%9d%a2%e5%b7%a5%e7%a8%8b%e5%8d%8a%e6%9c%88%e5%88%8a-nasa%ef%bc%88%e7%be%8e%ef%bc%89%e5%bc%80%e5%8f%91%e5%87%ba%e8%b6%85%e6%bb%91%e9%a3%9e","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=3903","title":{"rendered":"#\u8584\u819c\u6750\u6599\u4e0e\u8868\u9762\u5de5\u7a0b\u534a\u6708\u520a# NASA\uff08\u7f8e\uff09\u5f00\u53d1\u51fa\u8d85\u6ed1\u98de\u673a\u6d82\u5c42"},"content":{"rendered":"<p>Hello\uff0c\u5927\u5bb6\u597d\uff0c\u6539\u7248\u540e\u7684\u201c\u8584\u819c\u6750\u6599\u4e0e\u8868\u9762\u5de5\u7a0b\u201d\u534a\u6708\u520a\u4e0e\u5927\u5bb6\u89c1\u9762\u54af\uff0c\u6211\u4eec\u5c06\u6bcf\u6708\u4e24\u671f\u4e3a\u5927\u5bb6\u62a5\u9053\u8584\u819c\uff0c\u6d82\u5c42\u4ee5\u53ca\u8868\u9762\u5de5\u7a0b\u9886\u57df\u7684\u90a3\u4e9b\u4e8b\uff0c\u90a3\u4e9b\u4eba\u548c\u90a3\u4e9b\u6750\u6599\u3002\u5e0c\u671b\u5927\u5bb6\u591a\u591a\u652f\u6301\u3002<\/p>\n<p><strong>1\u3001\u5bc6\u6b47\u6839\u5927\u5b66\uff08\u7f8e\uff09\u5f00\u53d1\u51fa\u9632\u96ea\u6d82\u5c42<\/strong><br \/>\n<strong><a href=\"http:\/\/www.cnet.com\/roadshow\/news\/university-of-michigan-anti-ice-coating-perfect-for-cars\/\" target=\"_blank\">University of Michigan&#8217;s anti-ice coating would be perfect for cars<\/a><\/strong><\/p>\n<p>\u5bc6\u6b47\u6839\u5927\u5b66\uff08University of Michigan\uff09\u7814\u7a76\u4eba\u5458\u4eca\u65e5\u5f00\u53d1\u51fa\u4e00\u79cd\u9632\u96ea\u6d82\u5c42\uff0c\u5c06\u8be5\u6d82\u5c42\u6d82\u6577\u5728\u673a\u52a8\u8f66\u73bb\u7483\u4e0a\u6216\u662f\u5efa\u7b51\u7269\u5916\u5899\u4e0a\uff0c\u53ef\u4ee5\u6709\u6548\u9632\u6b62\u971c\u96ea\u5728\u5176\u8868\u9762\u7684\u6c89\u79ef\u3002\u636e\u62a5\u9053\uff0c\u8be5\u6d82\u5c42\u4e3b\u8981\u7531\u5f39\u6027\u7ec4\u7ec7\u6784\u6210\uff0c\u8be5\u7ec4\u7ec7\u53ef\u5728\u6781\u5c0f\u7684\u5916\u529b\u4f5c\u7528\u4e0b\u53d1\u751f\u8f83\u5927\u7684\u53d8\u5f62\uff0c\u8fd9\u4fbf\u4f7f\u5f97\u971c\u96ea\u5728\u6c89\u79ef\u65f6\u4e27\u5931\u56fa\u5b9a\u7684\u652f\u6491\uff0c\u56e0\u800c\u53d1\u751f\u8131\u843d\u3002<\/p>\n<p><strong>2\u3001\u4f2f\u514b\u5229\u52b3\u4f26\u65af\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\uff08\u7f8e\uff09\u5f00\u53d1\u51fa\u70ed\u53cd\u5c04\u8584\u819c<\/strong><br \/>\n<strong><a href=\"http:\/\/www.usglassmag.com\/2016\/03\/doe-develops-paint-on-coating-to-tackle-energy-leakage\/\" target=\"_blank\">DOE Develops Paint-On Coating to Tackle Energy Leakage<\/a><\/strong><\/p>\n<p>\u636e\u7edf\u8ba1\uff0c\u7f8e\u56fd\u6bcf\u5e74\u4ece\u7a97\u6237\u6563\u5931\u7684\u80fd\u91cf\u5c06\u9020\u6210500\u4ebf\u7f8e\u5143\u7684\u7ecf\u6d4e\u635f\u5931\uff0c\u4e3a\u4e86\u6539\u5584\u8fd9\u4e00\u95ee\u9898\uff0c\u4f2f\u514b\u5229\u52b3\u4f26\u65af\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u5f00\u53d1\u4e86\u4e00\u79cd\u9009\u62e9\u6027\u53cd\u5c04\u73bb\u7483\u8584\u819c\uff0c\u8be5\u8584\u819c\u5bf9\u53ef\u89c1\u5149\u7684\u5177\u6709\u900f\u5c04\u6027\uff0c\u800c\u5bf9\u7ea2\u5916\u7ebf\u5177\u6709\u53cd\u5c04\u6027\uff0c\u8fd9\u610f\u5473\u7740\u5728\u590f\u5929\u5916\u9762\u7684\u5149\u7ebf\u4e0d\u80fd\u4f7f\u5ba4\u5185\u5347\u6e29\uff0c\u800c\u51ac\u5929\u5ba4\u5185\u4ea7\u751f\u7684\u70ed\u91cf\u4e5f\u4e0d\u4f1a\u6563\u5931\u5230\u5c4b\u5916\u3002<\/p>\n<p><strong>3\u3001NASA\uff08\u7f8e\uff09\u5f00\u53d1\u51fa\u8d85\u6ed1\u98de\u673a\u6d82\u5c42<\/strong><br \/>\n<strong><a href=\"http:\/\/www.telegraph.co.uk\/news\/science\/science-news\/12190393\/Nasas-super-slippery-anti-insect-coating-could-slash-cost-of-flying.html\" target=\"_blank\">Nasa&#8217;s super-slippery anti-insect coating could slash cost of flying<\/a><\/strong><\/p>\n<p>\u98de\u673a\u5728\u5927\u6c14\u4e2d\u98de\u884c\u65f6\uff0c\u5373\u4f7f\u6781\u5c0f\u7684\u9897\u7c92\u5305\u62ec\u6606\u866b\u7b49\u90fd\u4f1a\u4f7f\u5176\u98de\u884c\u963b\u529b\u589e\u5927\uff0c\u9488\u5bf9\u4e8e\u6b64\uff0cNASA\u7814\u5236\u51fa\u4e86\u4e00\u79cd\u8d85\u6ed1\u8584\u819c\uff0c\u5176\u8868\u9762\u5177\u6709\u7c7b\u4f3c\u83b2\u82b1\u7684\u5f62\u8c8c\uff0c\u8fd9\u53ef\u4ee5\u4f7f\u9897\u7c92\u7269\u8fc5\u901f\u5212\u8fc7\u3002NASA\u9884\u6d4b\uff0c\u91c7\u7528\u8fd9\u79cd\u8bbe\u8ba1\u7684\u98de\u8d77\u71c3\u6599\u6548\u7387\u5c06\u4f1a\u81f3\u5c11\u63d0\u9ad8\u4e00\u4e2a\u767e\u5206\u70b9\uff0c\u8fd9\u5c06\u4f7f\u7c7b\u4f3c\u82f1\u56fd\u822a\u7a7a\u516c\u53f8\u7b49\u5927\u578b\u822a\u7a7a\u516c\u53f8\u6bcf\u5e74\u8282\u77013500\u4e07\u7f8e\u5143\u3002<\/p>\n<p><strong>4\u3001\u9ebb\u7701\u7406\u5de5\u5927\u5b66\uff08\u7f8e\uff09\u5f00\u53d1\u51fa\u6291\u83cc\u8584\u819c<\/strong><br \/>\n<strong><a href=\"http:\/\/cen.acs.org\/articles\/94\/web\/2016\/03\/Designer-coatings-fight-infections-help.html\" target=\"_blank\">Designer coatings fight infections and help bones heal<\/a><\/strong><\/p>\n<p>\u9ebb\u7701\u7406\u5de5\u5927\u5b66\u7814\u7a76\u4eba\u5458\u5229\u7528\u9010\u5c42\u6c89\u79ef\u7684\u65b9\u6cd5\u5236\u5907\u4e86\u4e00\u79cd\u80fd\u6291\u5236\u7ec6\u83cc\u7684\u8584\u819c\uff0c\u8be5\u8584\u819c\u4e3b\u8981\u7528\u4e8e\u5e2e\u52a9\u9aa8\u635f\u4f24\u60a3\u8005\u5eb7\u590d\u3002\u8584\u819c\u7684\u603b\u539a\u5ea6\u4e3a0.5-2\u03bcm\uff0c\u4e0a\u5c42\u542b\u6709\u6297\u751f\u7d20\uff0c\u4e0b\u5c42\u5219\u542b\u6709\u4fc3\u8fdb\u9aa8\u9abc\u75ca\u6108\u7684\u836f\u7269\uff0c\u8fd9\u4f7f\u5f97\u8be5\u8584\u819c\u5177\u6709\u6291\u83cc\u548c\u4fc3\u8fdb\u9aa8\u9abc\u6062\u590d\u53cc\u91cd\u529f\u6548\uff0c\u8fd9\u5c06\u6709\u52a9\u4e8e\u60a3\u8005\u7684\u5eb7\u590d\u6cbb\u7597\u3002<\/p>\n<p><strong>5\u3001Carbodeon\uff08\u82ac\u5170\uff09\u7eb3\u7c73\u91d1\u521a\u77f3\u9897\u7c92\u53ef\u4f7f\u6c1f\u5316\u7269\u6d82\u5c42\u8010\u78e8\u6027\u63d0\u9ad8\u4e00\u500d\u4ee5\u4e0a<\/strong><br \/>\n<strong><a href=\"http:\/\/www.jeccomposites.com\/news\/composites-news\/carbodeon-nanodiamond-additive-doubles-wear-resistance-standard-fluoropolymer-c\" target=\"_blank\">Carbodeon nanoDiamond additive doubles the wear resistance of standard fluoropolymer coatings<\/a><\/strong><\/p>\n<p>Carbodeon\u516c\u53f8\u4eca\u65e5\u5f00\u53d1\u51fa\u4e00\u79cd\u9002\u4e8e\u6dfb\u52a0\u5230\u6c1f\u5316\u7269\u4e2d\u7684\u7eb3\u7c73\u7ea7\u91d1\u521a\u77f3\u9897\u7c92\uff0c\u7814\u7a76\u4eba\u5458\u6539\u53d8\u4e86\u91d1\u521a\u77f3\u9897\u7c92\u7684\u8868\u9762\u72b6\u51b5\uff0c\u4f7f\u5f97\u9897\u7c92\u6613\u4e8e\u5f25\u6563\u5230\u6c1f\u5316\u7269\u4e2d\uff0c\u800c\u4e0d\u662f\u805a\u96c6\u8d77\u6765\u3002\u8be5\u7eb3\u7c73\u9897\u7c92\u76f4\u5f84\u53ea\u6709\u7ea610 nm\uff0c\u4e0d\u8fc7\u5176\u5374\u53ef\u663e\u8457\u63d0\u9ad8\u6c1f\u5316\u7269\u7684\u8010\u78e8\u6027\u3002<\/p>\n<p><strong>6\u3001A*STAR\uff08\u65b0\u52a0\u5761\uff09\u7814\u5236\u51fa\u73af\u5883\u53cb\u597d\u578b\u6291\u83cc\u6d82\u5c42<\/strong><br \/>\n<strong><a href=\"http:\/\/phys.org\/news\/2016-03-environmentally-friendly-polymer-coatings-inhibit.html\" target=\"_blank\">Environmentally friendly polymer coatings inhibit the surface buildup of bacterial and marine organisms<\/a><\/strong><\/p>\n<p>\u8239\u8236\u7b49\u822a\u6d77\u8bbe\u5907\u7684\u5916\u8868\u9762\u5e38\u5e38\u4f1a\u8986\u76d6\u4e00\u5c42\u6709\u673a\u7269\u6d82\u5c42\uff0c\u5176\u4f5c\u7528\u662f\u9632\u6b62\u7ec6\u83cc\u4ee5\u53ca\u6d77\u6c34\u6709\u673a\u7269\u5728\u8239\u8236\u8868\u9762\u6ecb\u751f\u3002\u8fd9\u5c42\u6d82\u5c42\u4ee5\u5f80\u5e38\u7531\u6709\u6bd2\u6750\u6599\u6784\u6210\uff0c\u800c\u8fd9\u4f1a\u5bf9\u73af\u5883\u4ea7\u751f\u5f71\u54cd\u3002\u9488\u5bf9\u4e8e\u6b64\uff0c\u6765\u81eaA*STAR\u7684\u7814\u7a76\u4eba\u5458\u91c7\u7528poly(methyl oxazoline) (PMOx)\u5236\u5907\u4e86\u65b0\u578b\u6d82\u5c42\uff0c\u8be5\u6d82\u5c42\u5177\u6709\u67d4\u6027\uff0c\u8010\u6c27\u5316\u7b49\u7279\u6027\uff0c\u800c\u6700\u6700\u91cd\u8981\u7684\u662f\u8be5\u6d82\u5c42\u4e3a\u73af\u5883\u53cb\u597d\u578b\u3002<\/p>\n<p><strong>7\u3001MoS2\u8584\u819c\u52a9\u529b\u79d1\u5b66\u5bb6\u5236\u5907\u4e16\u754c\u6700\u8584\u955c\u5934<\/strong><br \/>\n<strong><a href=\"http:\/\/www.dailymail.co.uk\/sciencetech\/article-3488312\/World-s-thinnest-lens-make-phone-credit-card-Lens-just-one-two-thousandth-thickness-human-hair.html\" target=\"_blank\">Camera lens one two-thousandth the thickness of human hair could make your phone thinner than a credit card<\/a><\/strong><\/p>\n<p>MoS2\u8584\u819c\u5177\u6709\u5de8\u5927\u7684\u5149\u7a0b\u957f\u5ea6\uff0c\u5176\u6570\u503c\u751a\u81f3\u6bd4\u5355\u5c42\u77f3\u58a8\u70ef\u819c\u5927\u4e00\u4e2a\u6570\u91cf\u7ea7\uff0c\u6b63\u662f\u5229\u7528\u5176\u8fd9\u4e00\u7279\u6027\uff0c\u6765\u81ea\u6fb3\u5927\u5229\u4e9a\u56fd\u7acb\u5927\u5b66\uff08Australian National University\uff09\u7684\u7814\u7a76\u4eba\u5458\u5236\u5907\u4e86\u76ee\u524d\u4e16\u754c\u4e0a\u6700\u8584\u7684\u900f\u955c\u955c\u5934\uff0c\u5176\u539a\u5ea6\u4ec5\u4ec5\u4e3a6.3 nm\u3002\u7814\u7a76\u4eba\u5458\u8ba4\u4e3a\u8fd9\u9879\u6280\u672f\u5c06\u4f1a\u6781\u5927\u5730\u6539\u53d8\u4eba\u7c7b\u7684\u751f\u6d3b\uff0c\u60f3\u60f3\u79d1\u5e7b\u7247\u4e2d\u7684\u90a3\u4e9b\u7eb8\u7247\u822c\u539a\u5ea6\u7684\u624b\u673a\uff0c\u6216\u8bb8\u5b83\u4eec\u79bb\u6211\u4eec\u771f\u7684\u4e0d\u8fdc\u4e86\u3002<\/p>\n<p><strong>8\u3001\u53ef\u5728\u5ba4\u6e29\u4e0b\u4ea7\u751f\u6fc0\u5b50\u7684\u8584\u819c\u6750\u6599<\/strong><br \/>\n<strong><a href=\"http:\/\/phys.org\/news\/2016-03-material-excitons-room-temperature.html\" target=\"_blank\">New material can control excitons at room temperature<\/a><\/strong><\/p>\n<p>\u5f53\u6fc0\u5149\u7167\u5c04\u5230\u534a\u5bfc\u4f53\u8868\u9762\u65f6\uff0c\u4f1a\u5728\u534a\u5bfc\u4f53\u8868\u9762\u4ea7\u751f\u6fc0\u5b50\uff0c\u6fc0\u5b50\u4f1a\u4e0e\u534a\u5bfc\u4f53\u8868\u9762\u7684\u7269\u8d28\u95f4\u53d1\u751f\u80fd\u91cf\u4f20\u9012\uff0c\u800c\u540e\u53c8\u91cd\u65b0\u53d8\u56de\u5149\u4fe1\u53f7\u4ece\u7269\u4f53\u8868\u9762\u5c04\u51fa\u3002\u8fd9\u79cd\u7279\u6027\u4f7f\u5f97\u6fc0\u5b50\u5728\u4f5c\u5149\u7535\u68c0\u6d4b\u6750\u6599\u65b9\u9762\u5b58\u5728\u4e00\u5b9a\u7684\u5e94\u7528\u524d\u666f\u3002\u4f46\u662f\uff0c\u8fd9\u79cd\u73b0\u8c61\u5148\u524d\u53ea\u6709\u5728\u4f4e\u6e29\u4e0b\u624d\u80fd\u591f\u5b9e\u73b0\u3002\u9488\u5bf9\u4e8e\u6b64\uff0c\u52a0\u5229\u798f\u5c3c\u4e9a\u5927\u5b66\u9009\u7528\u4e86\u4e00\u79cd\u8d85\u8584\u7684MoS2\u53cah-BN\u590d\u5408\u819c\uff0c\u6bcf\u5c42\u7684\u539a\u5ea6\u4e0d\u8fc7\u4e3a\u4e00\u539f\u5b50\u539a\u5ea6\uff0c\u8fd9\u79cd\u6750\u6599\u53ef\u5728\u5ba4\u6e29\u4e0b\u4ea7\u751f\u6fc0\u5b50\u3002<\/p>\n<p>\u672c\u6587\u7531thunder17 \u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Hello\uff0c\u5927\u5bb6\u597d\uff0c\u6539\u7248\u540e\u7684\u201c\u8584\u819c\u6750\u6599\u4e0e\u8868\u9762\u5de5\u7a0b\u201d\u534a\u6708\u520a\u4e0e\u5927\u5bb6\u89c1\u9762\u54af\uff0c\u6211\u4eec\u5c06\u6bcf\u6708\u4e24\u671f\u4e3a\u5927\u5bb6\u62a5\u9053\u8584\u819c\uff0c\u6d82\u5c42\u4ee5\u53ca\u8868\u9762\u5de5\u7a0b\u9886\u57df\u7684\u90a3\u4e9b\u4e8b\uff0c\u90a3\u4e9b\u4eba\u548c\u90a3\u4e9b\u6750\u6599\u3002\u5e0c\u671b\u5927\u5bb6\u591a\u591a&#8230;<\/p>\n","protected":false},"author":96,"featured_media":4182,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[67],"tags":[33,32],"class_list":["post-3903","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhoubao","tag-nano","tag-film"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/3903"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/96"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=3903"}],"version-history":[{"count":7,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/3903\/revisions"}],"predecessor-version":[{"id":4181,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/3903\/revisions\/4181"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/4182"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=3903"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=3903"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=3903"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}