{"id":39224,"date":"2016-09-13T06:30:01","date_gmt":"2016-09-12T22:30:01","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=39224"},"modified":"2016-09-11T21:48:47","modified_gmt":"2016-09-11T13:48:47","slug":"%e9%a1%b6%e5%88%8a%e5%8a%a8%e6%80%81%e4%b8%a8nature%e5%ad%90%e5%88%8aadv-mater-%e7%ad%89%e6%9c%9f%e5%88%8a%e7%94%b5%e5%ad%90%e6%9d%90%e6%96%99%e5%89%8d%e6%b2%bf%e6%9c%80%e6%96%b0%e7%a7%91%e7%a0%94","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=39224","title":{"rendered":"\u9876\u520a\u52a8\u6001\u4e28Nature\u5b50\u520a\/Adv. Mater.\u7b49\u671f\u520a\u7535\u5b50\u6750\u6599\u524d\u6cbf\u6700\u65b0\u79d1\u7814\u6210\u679c\u7cbe\u9009\u3010\u7b2c22\u671f\u3011"},"content":{"rendered":"<p><strong>\u672c\u671f\u7cbe\u9009\u9884\u89c8\uff1a<\/strong>ACS Nano MoS2\u8026\u5408\u7eb3\u7c73\u7ed3\u6784\u886c\u5e95\u5b9e\u73b0\u5149\u5b66\u589e\u76ca\uff1aFabry\u2013Perot\u5e72\u6d89\u548c\u7b49\u79bb\u6fc0\u5143\u7684\u6fc0\u53d1\uff1bJACS Terazulene \u5f02\u6784\u4f53\uff1a\u901a\u8fc7\u5206\u5b50\u8f68\u9053\u5206\u5e03\u5dee\u5f02\u5b9e\u73b0OFETs\u6781\u6027\u53d8\u5316\uff1bJACS \u901a\u8fc7\u6c27\u5316\u7ed3\u5408Bi-2\u65b9\u5f62\u7f51\u4e0e\u5c42\u72b6Y2O2Bi\u5f62\u6210\u4e8c\u7ef4\u8d85\u5bfc\u6750\u6599\uff1bNat. Commun. \u7194\u878d\u534a\u5bfc\u4f53\u7535\u89e3\uff1bAdv. Mater. \u80f6\u4f53\u5408\u6210\u5c3a\u5bf8\u5747\u4e00\u4e8c\u786b\u5316\u94bc\u7eb3\u7c73\u7247\u5236\u5907\u6676\u7247\u89c4\u6a21\u67d4\u6027\u975e\u6613\u5931\u6027\u5b58\u50a8\u5668\uff1bAdv. Mater. \u8d85\u7075\u654f\u591a\u4f4d\u4e8c\u786b\u5316\u94bc\u5149\u7535\u5b58\u50a8\u5668\uff1bAdv. Mater. \u65e0\u5b9a\u578bBPIII\u805a\u5408\u7269\u57fa\u7eb3\u7c73\u5668\u4ef6\u7684\u5149\u7535\u8bb0\u5fc6\u6548\u5e94\uff1bAdv. Mater. Co\u66ff\u4f4dBiFeO3\u5916\u5ef6\u8584\u819c\u7684\u504f\u632f\u65cb\u8f6c\u63d0\u9ad8\u538b\u7535\u54cd\u5e94\u3002<\/p>\n<p><strong>1\u3001ACS Nano MoS2\u8026\u5408\u7eb3\u7c73\u7ed3\u6784\u886c\u5e95\u5b9e\u73b0\u5149\u5b66\u589e\u76ca\uff1aFabry\u2013Perot\u5e72\u6d89\u548c\u7b49\u79bb\u6fc0\u5143\u7684\u6fc0\u53d1<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39225\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-2.jpg\" alt=\"\u56fe\u72471\" width=\"468\" height=\"401\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-2.jpg 468w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-2-300x257.jpg 300w\" sizes=\"(max-width: 468px) 100vw, 468px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe1<\/strong> \u5668\u4ef6\u7ed3\u6784\u793a\u610f\u56fe<\/p>\n<p>\u5c3d\u7ba1\u5355\u5c42\u8fc7\u6e21\u91d1\u5c5e\u786b\u5316\u7269\uff08TMDs\uff09\u5177\u6709\u76f4\u63a5\u5e26\u9699\uff0c\u7531\u4e8e\u5728\u539f\u5b50\u8584\u7684\u5c42\u72b6\u6750\u6599\u4e2d\u7cdf\u7cd5\u7684\u5149\u5438\u6536\u7387\u5149\u5b66\u589e\u76ca\u4e00\u76f4\u53d7\u5230\u9650\u5236\u3002\u5927\u591a\u6570\u63d0\u9ad8TMDs\u7684\u5149\u5b66\u589e\u76ca\u7684\u65b9\u6cd5\u4e3b\u8981\u901a\u8fc7\u5bf9\u6d3b\u6027\u6750\u6599\u8fdb\u884c\u8c03\u5236\u6216\u591a\u5c42\u53e0\u52a0\u3002<\/p>\n<p>\u97e9\u56fd\u57fa\u7840\u79d1\u5b66\u7814\u7a76\u6240\u7684Young Hee Lee\uff08\u901a\u8baf\u4f5c\u8005\uff09\u4ee5\u53ca\u4e09\u661f\u5148\u8fdb\u6280\u672f\u7814\u7a76\u9662\u7684Yeonsang Park \uff08\u901a\u8baf\u4f5c\u8005\uff09\u548cUn Jeong Kim\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u62a5\u9053\u4e86\u4e00\u4e2a\u7b80\u5355\u5730\u901a\u8fc7\u8bbe\u8ba1\u7eb3\u7c73\u886c\u5e95\u7684\u65b9\u6cd5\u63d0\u9ad8MoS2\u7684\u5149\u5b66\u5438\u6536\u548c\u6fc0\u53d1\u3002\u886c\u5e95\u5305\u62ec\u4ecb\u7535\u8584\u819c\u9694\u5c42\uff08TiO2\uff09\u548c\u91d1\u5c5e\u819c\u3002\u7eb3\u7c73\u886c\u5e95\u4e0a\u5355\u5c42MoS2\u6574\u4f53\u7684\u5149\u81f4\u53d1\u5149\uff08PL\uff09\u5f3a\u5ea6\u57fa\u4e8eTiO2\u539a\u5ea6\u5e76\u53d7\u5230Fabry\u2013Perot \u5e72\u6d89\u653e\u5927\u3002\u6b64\u5916\uff0c\u4e2d\u6027\u6fc0\u5b50\u901a\u8fc7\u5c40\u57df\u573a\u4ea7\u751f\u7684\u7b49\u79bb\u6fc0\u5143\u88ab\u53d1\u5c04\u9009\u62e9\u6027\u5730\u653e\u5927\uff0c\u800c\u5c40\u57df\u573a\u6e90\u4e8e\u95f4\u9694\u539a\u5ea6\u5c0f\u4e8e10\u7eb3\u7c73\u7684\u91d1\u5c5e\u819c\u8868\u9762\u7c97\u7cd9\u3002\u8fdb\u4e00\u6b65\u7814\u7a76\u8868\u660e\uff0c\u8be5\u5668\u4ef6\u7684\u8d28\u91cf\u56e0\u5b50\u4e5f\u53ef\u4ee5\u901a\u8fc7\u9009\u62e9\u4e0d\u540c\u6298\u5c04\u7387\u7684\u95f4\u9694\u6750\u6599\u800c\u8fdb\u884c\u8bbe\u8ba1\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b03237\" target=\"_blank\">Optical Gain in MoS2 via Coupling with Nanostructured Substrate: Fabry\u2013Perot Interference and Plasmonic Excitation<\/a> \uff08ACS Nano, 2016, DOI: 10.1021\/acsnano.6b03237\uff09<\/p>\n<p><strong>2\u3001JACS Terazulene\u5f02\u6784\u4f53\uff1a\u901a\u8fc7\u5206\u5b50\u8f68\u9053\u5206\u5e03\u5dee\u5f02\u5b9e\u73b0OFETs\u6781\u6027\u53d8\u5316<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39226\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72472-1.jpg\" alt=\"\u56fe\u72472\" width=\"600\" height=\"340\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72472-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72472-1-300x170.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe2<\/strong> terazulene\u5f02\u6784\u4f53\u5316\u5b66\u7ed3\u6784\u3001OFET\u5668\u4ef6\u7ed3\u6784\u548c\u8f93\u8fd0<\/p>\n<p>Azulene\uff08C10H8\uff09\u662f\u975e\u82ef\u82b3\u9999\u70c3\u5316\u5408\u7269\u4e2d\u5907\u53d7\u5173\u6ce8\u7684\u5206\u5b50\uff0c\u8fd9\u6e90\u81ea\u4e8e\u5176\u72ec\u7279\u7684\u6027\u80fd\uff0c\u4e00\u4e2a\u5927\u7684\u5076\u6781\u77e9\u548c\u957f\u6ce2\u957f\u7684\u5438\u6536\u3002\u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u57fa\u4e8eazulene\u7684\u5171\u8f6d\u5316\u5408\u7269\u5df2\u88ab\u7814\u7a76\u7528\u5728\u5404\u79cd\u5e94\u7528\u4e2d\uff0c\u5305\u62ec\u8fd1\u7ea2\u5916\u5438\u6536\u6750\u6599\u3001\u5bfc\u7535\u9ad8\u5206\u5b50\u6750\u6599\u3001\u975e\u7ebf\u6027\u5149\u5b66\u3001\u8367\u5149\u5f00\u5173\u3001\u7535\u81f4\u53d8\u8272\u6750\u6599\u548c\u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u6750\u6599\u3002<\/p>\n<p>\u6700\u8fd1\uff0c\u65e5\u672c\u5c71\u5f62\u5927\u5b66\u7684Hiroshi Katagiri\uff08\u901a\u8baf\u4f5c\u8005\uff09\u62a5\u9053\u4e86\u901a\u8fc7\u5bf9\u5206\u5b50\u8f68\u9053\u5206\u5e03\u7684\u63a7\u5236\uff0c2,6\u2032:2\u2032,6\u2033-terazulene (TAz1)\u8868\u73b0\u51fa\u4f5c\u4e3an\u578b\u6676\u4f53\u7ba1\uff08OFET\uff09\u7684\u4f18\u5f02\u6027\u80fd\u3002\u4e3a\u4e86\u9a8c\u8bc1\u548c\u53d1\u5c55\u4e86\u8fd9\u4e00\u6982\u5ff5\uff0c\u8bba\u6587\u63d0\u51fa\u4e09\u79cd\u5f02\u6784\u4f53\u7684terazulene\uff0c\u8fd9\u4e09\u7c7b\u5206\u5b50\u6709\u6cbf\u7740azulene \u957f\u8f74\u76842-\u62166-\u4f4d\u7f6e\u7684\u4e09\u4e2aazulene \u57fa\u56e2\uff0c\u4ece\u800c\u6784\u5efa\u4e00\u4e2a\u7ebf\u6027\u6269\u5c55\u03c0\u5171\u8f6d\u4f53\u7cfb\uff1a2,2\u2032:6\u2032,2\u2033-terazulene (TAz2)\u30012,2\u2032:6\u2032,6\u2033-terazulene (TAz3)\u548c 6,2\u2032:6\u2032,6\u2033-terazulene (TAz4)\u3002TAz2\u548cTAz3\u8868\u73b0\u51fa\u53cc\u6781\u7279\u6027\uff1bTAz4\u4f5c\u4e3a\u4e00\u4e2a\u6709\u673a\u573a\u6548\u5e94\u6676\u4f53\u7ba1\u5448\u73b0\u660e\u663e\u7684N\u578b\u6676\u4f53\u7ba1\u7279\u6027\u3002\u6240\u6709terazulenes\u7684\u6700\u4f4e\u672a\u5360\u636e\u5206\u5b50\u8f68\u9053\uff08LUMO\uff09\u662f\u5728\u6574\u4e2a\u5206\u5b50\u4e2d\u5b8c\u5168\u79bb\u57df\u7684\u3002\u76f8\u53cd\uff0cTAz2 \u548c TAz3 \u7684\u6700\u9ad8\u5360\u636e\u5206\u5b50\u8f68\u9053\uff08HOMO\uff09\u662f\u57282,2\u2032-biazulene\u5355\u5143\u79bb\u57df\u7684\uff1b\u800cTAz4\u7684HOMOs\u5728\u4f4d\u4e8eazulene\u7684\u4e00\u7aef\u662f\u5c40\u57df\u7684\u3002\u8fd9\u4e9b\u7814\u7a76\u7ed3\u679c\u8bc1\u5b9e\uff0c\u4f5c\u4e3a\u7b80\u5355\u78b3\u6c22\u5316\u5408\u7269\u7684terazulene\u5f02\u6784\u4f53\u6781\u6709\u53ef\u8c03\u6781\u6027\u7684FET\u7279\u6027\uff0c\u6781\u6027\u53d6\u51b3\u4e8eazulene\u5355\u5143\u7684\u53d6\u5411\u548c\u5728terazulene\u9aa8\u5e72\u4e2d\u5206\u5b50\u8f68\u9053\u5206\u5e03\u76f8\u5173\u7684\u5dee\u5f02\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/pubs.acs.org\/doi\/full\/10.1021\/jacs.6b06877\" target=\"_blank\">Terazulene Isomers: Polarity Change of OFETs through Molecular Orbital Distribution Contrast<\/a> \uff08JACS, 2016, DOI: 10.1021\/jacs.6b06877\uff09<\/p>\n<p><strong>3\u3001JACS \u901a\u8fc7\u6c27\u5316\u7ed3\u5408Bi-2\u65b9\u5f62\u7f51\u4e0e\u5c42\u72b6Y2O2Bi\u5f62\u6210\u4e8c\u7ef4\u8d85\u5bfc\u6750\u6599<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39227\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72473-1.jpg\" alt=\"\u56fe\u72473\" width=\"600\" height=\"228\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72473-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72473-1-300x114.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe3<\/strong> BaFe2As2\u00a0\u548c Y2O2Bi\u7684\u6676\u4f53\u7ed3\u6784<\/p>\n<p>\u5c42\u7ec4\u72b6\u8d85\u5bfc\u4f53\u662f\u8574\u542b\u9ad8\u8f6c\u53d8\u6e29\u5ea6\u3001\u975e\u4f20\u7edf\u914d\u5bf9\u6027\u8d85\u5bfc\u4f53\u7684\u4e00\u5ea7\u91d1\u5c71\uff0c\u4eba\u4eec\u57fa\u4e8e\u94dc\u9178\u76d0\u548c\u94c1\u57fa\u5316\u5408\u7269\u5c42\u72b6\u8d85\u5bfc\u4f53\u53d1\u73b0\u4e86\u65b0\u7684\u8d85\u5bfc\u5316\u5408\u7269\uff0c\u5176\u4e2d\u5305\u542b\u4e86\u8fc7\u6e21\u91d1\u5c5e\u9633\u79bb\u5b50\u7684\u4e8c\u7ef4\u5c42\u72b6\u6750\u6599\uff0c\u5176\u5728\u8d85\u5bfc\u6750\u6599\u4e2d\u5177\u6709\u91cd\u8981\u4f5c\u7528\u3002\u5728\u94dc\u4e2d\u63d2\u5165Bi2Se3\u548cBi\u2212Se\u5c42\uff0c\u5176\u5177\u6709\u5f88\u5f3a\u7684\u81ea\u65cb\u8f68\u9053\u8026\u5408\u5e76\u56e0\u6b64\u5177\u6709\u62d3\u6251\u8d85\u5bfc\u6027\u3002\u540c\u6837Bi\u65b9\u5f62\u7f51\u683c\u4e5f\u53ef\u4ee5\u63d0\u4f9b\u4e00\u4e2a\u65b0\u7684\u5e73\u53f0\u53bb\u63a2\u7d22\u5c42\u72b6\u8d85\u5bfc\u4f53\u7684\u62d3\u6251\u8d85\u5bfc\u6027\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u4e1c\u4eac\u5927\u5b66\u7684Tomoteru Fukumura\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u53d1\u73b0\u4e86\u57282K\u4e0bCr2Si2\u578b\u5c42\u72b6\u6c27\u5316\u7269Y2O2Bi\u542b\u6709Bi2\u2212\u65b9\u5f62\u7f51\u683c\u800c\u5177\u6709\u72ec\u7279\u7684\u8d85\u5bfc\u6027\u3002\u8fd9\u79cd\u8d85\u5bfc\u6027\u4ec5\u5728Y2O2Bi\u5f88\u5927\u7684\u6c27\u5316\u8ddd\u79bb\u4e0b\u624d\u51fa\u73b0\u3002\u8be5\u53d1\u73b0\u63ed\u793a\u7740\u5143\u7d20\u7ed3\u5408\u53ef\u4ee5\u586b\u5145\u95f4\u9699\u4e3a\u65b0\u7684\u8d85\u5bfc\u4f53\u63d0\u4f9b\u4e86\u53e6\u5916\u4e00\u79cd\u4f20\u7edf\u7684\u66ff\u6362\u548c\u8bbe\u7f6e\u65b9\u6cd5\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/jacs.6b05275\" target=\"_blank\">Two-Dimensional Superconductivity Emerged at Monatomic Bi2\u2013 Square Net in Layered Y2O2Bi via Oxygen Incorporation<\/a>\uff08JACS, 2016, DOI: 10.1021\/jacs.6b05275\uff09<\/p>\n<p><strong>4\u3001Nat. Commun. \u7194\u878d\u534a\u5bfc\u4f53\u7535\u89e3<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39228\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72474-1.jpg\" alt=\"\u56fe\u72474\" width=\"600\" height=\"558\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72474-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72474-1-300x279.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe4<\/strong> \u4e09\u5c42\u7535\u89e3\u69fd\u7684\u539f\u7406\u56fe<\/p>\n<p>\u76f4\u63a5\u4ee5\u7535\u5316\u5b66\u7684\u65b9\u5f0f\u8fd8\u539f\u91d1\u5c5e\u53ef\u4ee5\u7b80\u5316\u6d41\u7a0b\u3001\u51cf\u5c11\u80fd\u6e90\u6d88\u8017\u3001\u51cf\u8f7b\u751f\u4ea7\u548c\u6295\u5165\u7684\u8d39\u7528\uff0c\u6240\u4ee5\u5b83\u662f\u4e00\u79cd\u53ef\u6301\u7eed\u7684\u63d0\u53d6\u65b9\u6cd5\u3002\u4e00\u4e2a\u5178\u578b\u4f8b\u5b50\u5c31\u662f\u94dd\u7684\u51b6\u70bc\u4f7f\u5f97\u5176\u53ef\u4ee5\u53d6\u4ee3\u94f6\u7684\u5730\u4f4d\u800c\u5728\u65e5\u5e38\u751f\u6d3b\u4e2d\u5e7f\u6cdb\u4f7f\u7528\u3002<\/p>\n<p>\u9ebb\u7701\u7406\u5de5\u5b66\u9662\u7684Donald R. Sadoway\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u5f00\u53d1\u51fa\u4e86\u4e00\u79cd\u9ad8\u6548\u7684\u7535\u89e3\u8131\u786b\u5de5\u827a\u5176\u53ef\u4ee5\u76f4\u63a5\u5c06\u7194\u878d\u534a\u5bfc\u4f53\u8f89\u9511\u77ff\uff08Sb2S3\uff09\u8f6c\u6362\u4e3a\u7eaf\u5ea6\u4e3a99.9%\u7684\u9511\u6db2\u4f53\u548c\u786b\u84b8\u6c14\u3002\u5728\u6db2\u6001\u9511\u5e95\u90e8\u4e3a\u7194\u878d\u7684\u8f89\u9511\u77ff\u9634\u6781\uff0c\u9876\u90e8\u7684\u786b\u6765\u81ea\u4e8e\u6d78\u5165\u5728\u975e\u6df7\u76f8\u4e8c\u6b21\u7194\u76d0\u7535\u89e3\u6db2\u7684\u78b3\u68d2\u6b63\u6781\u3002\u4e0e\u4f20\u7edf\u7684\u63d0\u53d6\u65b9\u6cd5\u4e0d\u540c\uff0c\u786b\u5316\u7535\u89e3\u53ef\u4ee5\u907f\u514dCO2\u3001CO \u4ee5\u53ca SO2\u6c14\u4f53\u7684\u6392\u653e\u3002\u5176\u53ef\u4ee5\u5927\u89c4\u6a21\u5e94\u7528\u4e8e\u5bfc\u7535\u8fc7\u6e21\u91d1\u5c5e\u786b\u5c5e\u5316\u5408\u7269\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/www.nature.com\/ncomms\/2016\/160824\/ncomms12584\/full\/ncomms12584.html\" target=\"_blank\">Electrolysis of a molten semiconductor<\/a>\uff08Nat. Commun., 2016, DOI: 10.1038\/ncomms12584\uff09<\/p>\n<p><strong>5\u3001Adv. Mater. \u80f6\u4f53\u5408\u6210\u5c3a\u5bf8\u5747\u4e00\u4e8c\u786b\u5316\u94bc\u7eb3\u7c73\u7247\u5236\u5907\u6676\u7247\u89c4\u6a21\u67d4\u6027\u975e\u6613\u5931\u6027\u5b58\u50a8\u5668<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39229\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72475-1.jpg\" alt=\"\u56fe\u72475\" width=\"500\" height=\"234\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72475-1.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72475-1-300x140.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe5<\/strong> MoS2-MoOx\u5f02\u8d28\u7ed3\u6784\u7684\u6676\u7247\u89c4\u6a21\u5236\u5907<\/p>\n<p>\u57fa\u4e8e\u5265\u79bb\u4e8c\u786b\u5316\u94bc\u7684\u5668\u4ef6\u5177\u6709\u826f\u597d\u6027\u80fd\uff0c\u4f46\u5747\u4e3a\u5355\u4e2a\u5668\u4ef6\u800c\u975e\u5927\u89c4\u6a21\u5668\u4ef6\u9635\u5217\u3002\u5e78\u8fd0\u7684\u662f\uff0c\u901a\u8fc7\u5316\u5b66\u6c14\u76f8\u6c89\u79ef\u6cd5\uff08CVD\uff09\u5927\u89c4\u6a21\u5408\u6210\u4e8c\u786b\u5316\u94bc\u4f7f\u5f97\u6676\u7247\u89c4\u6a21\u5668\u4ef6\u9635\u5217\u7684\u5236\u5907\u53d8\u5f97\u53ef\u80fd\u3002\u7136\u800c\uff0c\u57fa\u4e8eCVD\u4e8c\u786b\u5316\u94bc\u7684\u5668\u4ef6\u5728\u6027\u80fd\u3001\u6210\u672c\u4e0a\u5747\u5dee\u4e8e\u8131\u843dMoS2\u5668\u4ef6\u3002\u8131\u843dMoS2\u7eb3\u7c73\u7247\u7684\u7ec4\u88c5\u6709\u53ef\u80fd\u662f\u89e3\u51b3\u4e0a\u8ff0\u95ee\u9898\u7684\u4e00\u4e2a\u53ef\u884c\u65b9\u6cd5\uff0c\u4f46\u8131\u843dMoS2\u7684\u5185\u5728\u5206\u6563\u6027\u4f1a\u9020\u6210\u5927\u89c4\u6a21\u5668\u4ef6\u9635\u5217\u7684\u975e\u5747\u5300\u6027\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u97e9\u56fd\u57fa\u7840\u79d1\u5b66\u7814\u7a76\u6240\u7684Taeghwan Hyeon\uff08\u901a\u8baf\u4f5c\u8005\uff09\u548cDae-Hyeong Kim\uff08\u901a\u8baf\u4f5c\u8005\uff09\u62a5\u9053\u4e86\u5c3a\u5bf8\u5747\u5300\u7684\u4e8c\u786b\u5316\u94bc\u7684\u5927\u89c4\u6a21\u80f6\u4f53\u5408\u6210\u4ee5\u53ca\u5176\u6676\u7247\u89c4\u6a21\u96c6\u6210\u4ee5\u5236\u9020\u67d4\u6027\u7535\u963b\u968f\u673a\u5b58\u53d6\u5b58\u50a8\u5668\uff08RRAM\uff09\u9635\u5217\u3002\u76f8\u8f83\u4e8e\u8131\u843dMoS2\uff0c\u5408\u6210MoS2\u7eb3\u7c73\u7247\u5728\u5176\u5927\u5c0f\u548c\u539a\u5ea6\u5206\u5e03\u4e0a\u5747\u5177\u6709\u826f\u597d\u7684\u5747\u5300\u6027\u3002\u7531\u5408\u6210MoS2\u7eb3\u7c73\u7247\u5236\u5907\u7684\u8bb0\u5fc6\u88c5\u7f6e\u4f18\u4e8e\u57fa\u4e8e\u8131\u843dMoS2\u7684\u63a7\u5236\u88c5\u7f6e\uff0c\u5982\u6781\u9ad8\u7684\u5f00\/\u5173\u6bd4\u7684RRAM \u3002\u6b64\u5916\uff0c\u7ec4\u88c5MoS2\u7eb3\u7c73\u7247\u7684\u8d85\u8584\u6027\u8d28\u5141\u8bb8\u53d8\u5f62\u5668\u4ef6\u7684\u5236\u5907\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5:<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201602391\/full\" target=\"_blank\"> Colloidal Synthesis of Uniform-Sized Molybdenum Disulfide Nanosheets for Wafer-Scale Flexible Nonvolatile Memory<\/a>\u00a0\uff08Adv. Mater., 2016, DOI: 10.1002\/adma.201602391\uff09<\/p>\n<p><strong>6\u3001Adv. Mater. \u8d85\u7075\u654f\u591a\u4f4d\u4e8c\u786b\u5316\u94bc\u5149\u7535\u5b58\u50a8\u5668<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39230\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72476-1.jpg\" alt=\"\u56fe\u72476\" width=\"448\" height=\"506\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72476-1.jpg 448w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72476-1-266x300.jpg 266w\" sizes=\"(max-width: 448px) 100vw, 448px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe6<\/strong> \u4e8c\u786b\u5316\u94bc\u5149\u7535\u5b58\u50a8\u5668\u7ed3\u6784\u793a\u610f\u56fe<\/p>\n<p>\u4f5c\u4e3a\u8fc7\u6e21\u91d1\u5c5e\u786b\u5c5e\u5316\u5408\u7269\uff08TMDs\uff09\uff0c\u5355\u5c42\u4e8c\u786b\u5316\u94bc\uff08MoS2\uff09\u7684\u72ec\u7279\u5e26\u9699\u5df2\u4f7f\u4e4b\u6210\u4e3a\u65e0\u5e26\u9699\u77f3\u58a8\u70ef\u7684\u4e00\u79cd\u53ef\u884c\u66ff\u4ee3\u901a\u9053\u6750\u6599\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u5305\u62ec\u6676\u4f53\u7ba1\u548c\u5b58\u50a8\u5668\u7684\u5404\u79cd\u7535\u5b50\u8bbe\u5907\u4e2d\u30021.8eV\u5927\u7684\u5e26\u9699\u6240\u5bfc\u81f4\u9ad8\u8fbe10^8 \u7684\u5f00\u5173\u6bd4\u4e3a\u5355\u4e2a\u5355\u5143\u63d0\u4f9b\u53ef\u533a\u5206\u7684\u5185\u5b58\u72b6\u6001\u53ca\u591a\u5c42\u6b21\u7684\u6570\u636e\u5b58\u50a8\u3002\u5c3d\u7ba1\u5177\u5907\u4f18\u5f02\u7684\u7535\u5b66\u3001\u5149\u5b66\u6027\u8d28\uff0c\u5177\u6709\u80fd\u591f\u6301\u7eed\u7d2f\u79ef\u7167\u5c04\u5230\u5668\u4ef6\u4e0a\u5149\u5b50\u91cf\u3001\u591a\u4f4d\u5149\u4fe1\u53f7\u53d1\u5c04\u7684\u80fd\u529b\uff0c\u6216\u6210\u4e3a\u5168\u5149\u903b\u8f91\u5904\u7406\u5668\u4ef6\uff0c\u4f9d\u7136\u662fMoS2\u5149\u7535\u5668\u4ef6\u7684\u8feb\u5207\u9700\u8981\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u97e9\u56fd\u6210\u5747\u9986\u5927\u5b66\u7684Jeong Ho Cho\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u5411\u6211\u4eec\u5c55\u793a\u4e86\u4e00\u79cd\u901a\u8fc7\u534f\u540c\u7ec4\u5408\u5408\u7406\u7684\u5668\u4ef6\u8bbe\u8ba1\u7684\u65b0\u578b\u975e\u6613\u5931\u6027\u591a\u4f4dMoS2\u5b58\u50a8\u5668\u7684\u5f00\u53d1\u53ca\u5927\u9762\u79ef\u7684MoS2\u7247\u6709\u6548\u4f20\u9012\u3002\u5728\u8be5\u5668\u4ef6\u4e2d\uff0c\u901a\u8fc7\u7c98\u6027\u53d7\u62c9\u7684\u91d1\u5c5e\u5c42\u8f6c\u79fb\u51c6\u5907\u597d\u7684\u5927\u9762\u79ef\u9ad8\u8d28\u91cf\u5355\u5c42MoS2\u88ab\u540c\u65f6\u7528\u4f5c\u901a\u9053\u6750\u6599\u548c\u5149\u5438\u6536\u5c42\uff0c\u91d1\u7eb3\u7c73\u7c92\u5b50\uff08AuNPs\uff09\u88ab\u5d4c\u5728\u963b\u6321\u548c\u96a7\u7a7f\u4ecb\u7535\u5c42\u4e4b\u95f4\u4f5c\u4e3a\u6d6e\u6805\u5b58\u50a8\u5149\u6fc0\u53d1\u7535\u8377\u3002\u8be5\u5149\u7535\u5b58\u50a8\u5668\u5728\u9ad8\u7f16\u7a0b\u6805\u6781\u7535\u538b\u65f6\u53ef\u4f5c\u4e3a\u5e38\u89c4\u7535\u5b50\u5b58\u50a8\u5668\u8fd0\u884c\uff0c\u6b64\u5916\uff0c\u8be5\u8bbe\u5907\u8fd8\u53ef\u4f5c\u4e3a\u7535\u5b50\u8bfb\u6570\u5668\u5728\u4f4e\uff08\u751a\u81f3\u4e3a\u96f6\uff09\u7f16\u7a0b\u6805\u6781\u7535\u538b\u5b58\u50a8\u5149\u4fe1\u606f\u3002\u9664\u4e0a\u8ff0\u53cc\u91cd\u529f\u80fd\u5916\uff0c\u8be5\u5b58\u50a8\u88c5\u7f6e\u7684\u5927\u7f16\u7a0b\/\u64e6\u9664\u7535\u6d41\u6bd4\u7ed9\u5b9e\u73b0\u591a\u4f4d\u6570\u636e\u5b58\u50a8\u63d0\u4f9b\u4e86\u4e00\u4e2a\u65b9\u5411\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201603571\/full\" target=\"_blank\">Multibit MoS2 Photoelectronic Memory with Ultrahigh Sensitivity<\/a>\uff08Adv. Mater., 2016, DOI: 10.1002\/adma.201603571\uff09<\/p>\n<p><strong>7\u3001Adv. Mater. \u65e0\u5b9a\u578bBPIII\u805a\u5408\u7269\u57fa\u7eb3\u7c73\u5668\u4ef6\u7684\u5149\u7535\u8bb0\u5fc6\u6548\u5e94<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39231\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72477-1.jpg\" alt=\"\u56fe\u72477\" width=\"600\" height=\"370\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72477-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72477-1-300x185.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe7<\/strong> \u80c6\u56fa\u9187\u7684BPs\u7ed3\u6784\u56fe<\/p>\n<p>\u8f6f\u6750\u6599\u9886\u57df\u7684\u8fdb\u6b65\u5e26\u52a8\u4e86\u7531\u6db2\u6676\u6216\u8005\u805a\u5408\u7269\u81ea\u7ec4\u88c5\u5236\u5907\u52a8\u6001\u529f\u80fd\u6750\u6599\u81ea\u4e0b\u800c\u4e0a\u6cd5\u7684\u53d1\u5c55\u3002\u5176\u4e2d\u5177\u6709\u7acb\u65b9\u5bf9\u79f0\uff08BPI\u548cBPII\uff09\u7684\u80c6\u56fa\u9187\u7684\u84dd\u76f8\uff08BP\uff09\u7531\u4e8e\u5176\u7535\u53ef\u5207\u6362\u76843D\u7eb3\u7c73\u7ed3\u6784\u53ca\u5728\u5149\u8c31\u8303\u56f4\u4e3a\u7684\u9009\u62e9\u6027\u5e03\u62c9\u683c\u53cd\u5c04\u800c\u53d7\u5230\u4e86\u5e7f\u6cdb\u5173\u6ce8\u3002BPLCs\u7684BPI\u548cBPII\u5206\u522b\u4e3a\u4f53\u5fc3\u7acb\u65b9\u548c\u7b80\u5355\u7acb\u65b9\uff0cLC\u5206\u5b50\u4e3a\u53cc\u87ba\u65cb\u7ed3\u6784\u3002\u53cc\u87ba\u65cb\u7ed3\u6784\u4e0d\u80fd\u6301\u7eed\u5360\u636e3D\u7a7a\u95f4\uff0c\u56e0\u6b64\u9700\u8981\u901a\u8fc7\u6676\u683c\u62d3\u6251\u7f3a\u9677\u6765\u7a33\u5b9a\u5176\u7ed3\u6784\uff0c\u5373\u88ab\u79f0\u4e3a\u5411\u9519\u3002BPIII\u7ed3\u6784\u88ab\u5e7f\u6cdb\u63a5\u53d7\u7684\u7406\u8bba\u6a21\u578b\u79f0\u4e3a\u201cblue fog\u201d\u548c \u201cfoggy phase\u201dBPIII\u4e3a\u65e0\u5b9a\u578b\u7f51\u7edc\u7ed3\u6784\uff0c\u5b83\u7531\u53cc\u87ba\u65cb\u5706\u67f1\u548c\u5411\u9519\u7ec4\u6210\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u7f8e\u56fd\u80af\u7279\u5dde\u7acb\u5927\u5b66\u7684Sahil Sandesh Gandhi\uff08\u901a\u8baf\u4f5c\u8005\uff09\u548cLiang-Chy Chien\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u4ecb\u7ecd\u4e86\u4e00\u79cd\u5177\u6709\u5149\u7535\u8bb0\u5fc6\u6548\u5e94\u7684\u5668\u4ef6\uff0c\u8be5\u5668\u4ef6\u5efa\u7acb\u5728\u80c6\u753e\u76f8\u6db2\u6676\u7684\u5177\u67093D\u7eb3\u7c73\u7ed3\u6784\u65e0\u5b9a\u578bBPIII\u805a\u5408\u7269\u9aa8\u67b6\u4e0a\uff0c\u8be5\u5668\u4ef6\u5177\u6709\u5149\u5b66\u5404\u5411\u540c\u6027\u3001\u65cb\u5149\u6027\u5e76\u4e14\u5177\u6709\u4e9a\u6beb\u79d2\u7ea7\u54cd\u5e94\u901f\u5ea6\u3002\u8fd9\u79cd\u529f\u80fd\u6027\u7ed3\u6784\u4f7f\u5f97\u957f\u4e45\u4ee5\u6765\u5907\u53d7\u4e89\u8bae\u7684BPIII\u7ed3\u6784\u7b2c\u4e00\u6b21\u5728\u5b9e\u9a8c\u4e2d\u88ab\u89c2\u5bdf\u5230\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201603226\/full\" target=\"_blank\">Electro-optical Memory of a Nanoengineered Amorphous Blue-Phase-III Polymer Scaffold<\/a>\uff08Adv. Mater., 2016, DOI: 10.1002\/adma.201603226\uff09<\/p>\n<p><strong>8\u3001Adv. Mater. Co\u66ff\u4f4dBiFeO3\u5916\u5ef6\u8584\u819c\u7684\u504f\u632f\u65cb\u8f6c\u63d0\u9ad8\u538b\u7535\u54cd\u5e94<\/strong><\/p>\n<p style=\"text-align: center;\"><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-39232\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72478-1.jpg\" alt=\"\u56fe\u72478\" width=\"600\" height=\"540\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72478-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72478-1-300x270.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe8<\/strong>\uff08a\uff09\u5012\u6613\u7a7a\u95f4\u56fe\uff0c\uff08b\uff09~\uff08d\uff09\u6676\u4f53\u7ed3\u6784\u56fe<\/p>\n<p>\u7531\u5916\u7535\u573a\u4e2d\u8bf1\u5bfc\u65cb\u8f6c\u6781\u5316\u7684\u538b\u7535\u6750\u6599\uff08\u4f8b\u5982PbZr1\u2212xTixO3 (PZT)\uff09\u88ab\u5e7f\u6cdb\u8ba4\u4e3a\u662f\u5927\u538b\u7535\u54cd\u5e94\u7684\u6e90\u5934\uff0c\u7136\u800c\u7531\u4e8e\u7f3a\u5c11\u5177\u6709\u65cb\u8f6c\u6781\u5316\u7684\u6a21\u578b\u6750\u6599\uff0c\u8fd9\u79cd\u5047\u8bbe\u4ece\u6765\u6ca1\u88ab\u5728\u5b9e\u9a8c\u4e2d\u88ab\u8bc1\u5b9e\u8fc7\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u6765\u81ea\u4e1c\u4eac\u5de5\u4e1a\u5927\u5b66\u7684Hajime Hojo\uff08\u901a\u8baf\u4f5c\u8005\uff09\u548cMasaki Azuma\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u5236\u5907\u4e86\u4e00\u79cd\u9ad8\u8d28\u91cf\u7684Co\u66ff\u4f4d\u5177\u6709\u5355\u659c\u7f3a\u9677\u7684BiFeO3\u5916\u5ef6\u8584\u819c\uff0c\u5e76\u4e14\u7cfb\u7edf\u6d4b\u8bd5\u4e86\u6781\u5316\u65b9\u5411\u548c\u538b\u7535\u54cd\u5e94\u95f4\u7684\u5173\u7cfb\u3002\u8be5\u56e2\u961f\u8bc1\u660e\u4e86\u6781\u5316\u65cb\u8f6c\u5728\u8be5\u6750\u6599\u5728\u6539\u8fdb\u538b\u7535\u54cd\u5e94\u65b9\u9762\u8d77\u5230\u4e86\u81f3\u5173\u91cd\u8981\u7684\u4f5c\u7528\u3002\u8be5\u5b9e\u9a8c\u7406\u8bba\u4e0d\u4ec5\u53ef\u4ee5\u88ab\u5e94\u7528\u5728BiFeO3\u4f53\u7cfb\uff0c\u4e5f\u53ef\u4ee5\u88ab\u5e94\u7528\u5728\u5e38\u89c4\u538b\u7535\u6750\u6599\u4e2d\uff0c\u5982PZT\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201602450\/full\" target=\"_blank\">Enhanced Piezoelectric Response due to Polarization Rotation in Cobalt-Substituted BiFeO3 Epitaxial Thin Films<\/a>\uff08Adv. Mater., 2016, DOI: 10.1002\/adma.201602450\uff09<\/p>\n<p>\u672c\u671f\u5185\u5bb9\u7531\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u5b66\u672f\u7ec4\u5929\u884c\u5065\uff0c\u6811\u82d7\uff0c\u674e\u5c0f\u4f9d\uff0c\u738b\u5c0f\u7626\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u5982\u679c\u4f60\u5bf9\u7535\u5b50\u6750\u6599\u611f\u5174\u8da3\uff0c\u613f\u610f\u4e0e\u7535\u5b50\u7535\u5de5\u9886\u57df\u4eba\u624d\u4ea4\u6d41\uff0c\u5e76\u4e14\u60f3\u53ca\u65f6\u638c\u63e1\u7535\u5b50\u6750\u6599\u7814\u7a76\u5b66\u672f\u52a8\u6001\u5e76\u6df1\u5165\u5256\u6790\u884c\u4e1a\u73b0\u72b6\uff0c\u8bf7\u52a0\u5165\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4(\u52a0\u5165\u65b9\u5f0f\uff1a<a href=\"http:\/\/cailiaoren.mikecrm.com\/6qSdMU\" target=\"_blank\">\u70b9\u51fb\u6b64\u5904\u62a5\u540d<\/a>\u6216\u8005\u7533\u8bf7\u52a0\u5165\u6211\u4eecQQ\u7fa4\uff1a482842474)<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u672c\u671f\u7cbe\u9009\u9884\u89c8\uff1aACS Nano MoS2\u8026\u5408\u7eb3\u7c73\u7ed3\u6784\u886c\u5e95\u5b9e\u73b0\u5149\u5b66\u589e\u76ca\uff1aFabry\u2013Perot\u5e72\u6d89\u548c\u7b49\u79bb\u6fc0\u5143\u7684\u6fc0\u53d1\uff1bJACS Terazulene \u5f02\u6784\u4f53\uff1a\u901a\u8fc7\u5206&#8230;<\/p>\n","protected":false},"author":99,"featured_media":39227,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[67],"tags":[113,31],"class_list":["post-39224","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhoubao","tag-semiconductor","tag-dianzi"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/39224"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/99"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=39224"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/39224\/revisions"}],"predecessor-version":[{"id":40087,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/39224\/revisions\/40087"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/39227"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=39224"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=39224"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=39224"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}