{"id":41748,"date":"2016-09-24T06:30:41","date_gmt":"2016-09-23T22:30:41","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=41748"},"modified":"2017-03-18T21:37:31","modified_gmt":"2017-03-18T13:37:31","slug":"nat-commun-%e6%9e%97%e6%96%87%e6%96%8c%ef%bc%9amofs%e8%8a%82%e7%82%b9%e4%b8%8a%e7%9a%84%e5%85%b7%e6%9c%89%e5%8d%95%e4%bd%8d%e7%82%b9%e5%8c%96%e5%ad%a6%e9%80%89%e6%8b%a9%e6%80%a7%e4%b8%94%e5%82%a8","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=41748","title":{"rendered":"Nat. Commun. \u6797\u6587\u658c\uff1aMOFs\u8282\u70b9\u4e0a\u7684\u5177\u6709\u5355\u4f4d\u70b9\u5316\u5b66\u9009\u62e9\u6027\u4e14\u50a8\u91cf\u4e30\u5bcc\u7684\u91d1\u5c5e\u50ac\u5316\u5242"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>2016\u5e748\u670830\u65e5\uff0cNature Communications\u6742\u5fd7\u53d1\u8868\u4e86\u4e00\u7bc7\u5173\u4e8e\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u5316\u5408\u7269(MOFs)\u751f\u4ea7\u5730\u8868\u542b\u91cf\u4e30\u5bcc\u7684\u9ad8\u6548\u91d1\u5c5e\u50ac\u5316\u5242\u7684\u6587\u7ae0\uff0c\u9898\u4e3a\u201cChemoselective single-site Earth-abundant metal catalysts at metal\u2013organic framework nodes\u201d\uff0c\u8be5\u8bba\u6587\u901a\u8baf\u4f5c\u8005\u4e3a\u829d\u52a0\u54e5\u5927\u5b66\u5316\u5b66\u7cfb\u7684\u6797\u6587\u658c\u6559\u6388\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u5730\u8868\u542b\u91cf\u4e30\u5bcc\u7684\u91d1\u5c5e\u50ac\u5316\u5242\u5bf9\u4e8e\u53ef\u6301\u7eed\u5316\u5b66\u5408\u6210\u662f\u975e\u5e38\u9700\u8981\u7684\u3002\u56e0\u6b64\uff0c\u7814\u7a76\u8005\u4eec\u7814\u5236\u51fa\u4e86\u4e00\u79cd\u7b80\u5355\u3001\u4fbf\u5b9c\u3001\u9ad8\u6548\u7684\u65b9\u6cd5\uff0c\u7528\u6765\u751f\u4ea7\u5e94\u7528\u4e8e\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u5316\u5408\u7269(MOF)\u7684\u65b0\u578b\u5730\u8868\u542b\u91cf\u4e30\u5bcc\u7684\u91d1\u5c5e\u50ac\u5316\u5242\u3002\u542b\u6709\u94b4\u548c\u94c1\u76d0\u7684\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u5316\u5408\u7269(MOF)\u7ed3\u7684\u4e8c\u7ea7\u7ed3\u6784\u5355\u5143(SBUs)\u5177\u6709\u76f4\u63a5\u7684\u91d1\u5c5e\u5316\u4f5c\u7528\uff0c\u8fd9\u4e3a\u4e00\u7cfb\u5217\u6709\u673a\u53cd\u5e94\u63d0\u4f9b\u4e86\u9ad8\u6548\u3001\u53ef\u518d\u6b21\u5229\u7528\u7684\u5355\u70b9\u56fa\u4f53\u50ac\u5316\u5242\uff0c\u5305\u62ec\u82ef\u7532\u57faC-H\u952e\u7684\u787c\u70f7\u57fa\u5316\u3001\u7845\u70f7\u57fa\u5316\u548c\u6c28\u57fa\u5316\u6216\u8005\u70ef\u70c3\u3001\u916e\u7c7b\u7684\u6c22\u5316\u4f5c\u7528\u548c\u787c\u6c22\u5316\u4f5c\u7528\u3002<\/p>\n<p>\u7814\u7a76\u4eba\u5458\u5728\u7ed3\u6784\u3001\u5149\u8c31\u548c\u52a8\u529b\u5b66\u4e2d\u7684\u7814\u7a76\u7ed3\u679c\u8868\u660e\u7531\u4e8e\u50ac\u5316\u5242\u5468\u56f4\u7684\u7a7a\u95f4\u73af\u5883\uff0c\u5316\u5b66\u9009\u62e9\u7684\u6709\u673a\u8f6c\u53d8\u901a\u8fc7\u952e\u4ea4\u6362\u4f5c\u7528\u800c\u53d1\u751f\u5728\u4e8c\u7ea7\u7ed3\u6784\u5355\u5143(SBUs)\u4e2d\u7684\u4f4d\u7f6e\u5b64\u7acb\u7684\u3001\u5177\u6709\u7535\u5b50\u7f3a\u9677\u7684\u548c\u4e0d\u9971\u548c\u7684\u91d1\u5c5e\u4e2d\u5fc3\u3002\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u5316\u5408\u7269(MOF)\u56e0\u6b64\u4e3a\u7528\u4e8e\u7cbe\u7ec6\u5316\u5b66\u54c1\u53ef\u6301\u7eed\u5408\u6210\u7684\u9ad8\u6548\u78b1\u91d1\u5c5e\u50ac\u5316\u5242\u63d0\u4f9b\u4e86\u4e00\u79cd\u65b0\u578b\u7684\u5e73\u53f0\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe1\uff1a\u94b4\u548c\u94c1\u529f\u80fd\u5316\u7684UiO-68\u7684\u7279\u70b9<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-41749\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f1.jpg\" alt=\"ncomms12610-f1\" width=\"439\" height=\"700\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f1.jpg 439w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f1-188x300.jpg 188w\" sizes=\"(max-width: 439px) 100vw, 439px\" \/><\/p>\n<p>\u56fe(a)\uff1a\u56fe\u4e2d\u5c55\u793a\u4e86\u52a0\u5165CoCl2\u7684UiO-68\u7684\u4e8c\u7ea7\u7ed3\u6784\u5355\u5143\u7684\u9884\u5408\u6210\u91d1\u5c5e\u5316\u4f5c\u7528\uff1b<br \/>\n[\u6ce8]\uff1aUiO-68\u662f\u4ee5\u91d1\u5c5e\u9506\u4e3a\u4e2d\u5fc3\u5408\u6210\u51fa\u6765\u7684\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u6750\u6599Zr-MOF\u7684\u4e00\u79cd\u578b\u53f7\uff1b<\/p>\n<p>\u56fe(b)\uff1a\u4e94\u79cdUiO\u7c89\u672b\u7684XRD\u66f2\u7ebf\u76f8\u4f3c\u6027\u8868\u660e\uff0c\u5728\u9884\u5408\u6210\u91d1\u5c5e\u5316\u4f5c\u7528\u548c\u50ac\u5316\u4f5c\u7528\u540e\uff0cUiO-68\u4fdd\u7559\u4e86\u5176\u7ed3\u6676\u6027\u3002<br \/>\n\u56fe\u4e2d\u9ed1\u8272\u66f2\u7ebf\u4ee3\u8868UiO-68\uff0c\u7ea2\u8272\u66f2\u7ebf\u4ee3\u8868UiO-CoCl\uff0c\u84dd\u8272\u66f2\u7ebf\u4ee3\u8868UiO-Co\uff0c\u7eff\u8272\u66f2\u7ebf\u4ee3\u8868\u6b63\u8f9b\u70ef\u6c22\u5316\u4f5c\u7528\u540e\u7684UiO-Co\uff0c\u7c89\u8272\u66f2\u7ebf\u4ee3\u8868\u95f4\u4e8c\u7532\u82efC-H\u952e\u787c\u5316\u4f5c\u7528\u540e\u7684UiO-Co\uff1b<\/p>\n<p>\u56fe(c)\uff1a\u5728UiO-CoCl\u4e2dCo\u7684K\u8fb9\u754c\u5904\u7684\u5ef6\u4f38X\u5c04\u7ebf\u7cbe\u7ec6\u673a\u6784\u5149\u8c31\u548cR-\u7a7a\u95f4\u7ed3\u6784\u793a\u610f\u56fe\u3002\u56fe\u4e2d\u5b9e\u7ebf\u548c\u5b9e\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u91cf\u7ea7\uff0c\u865a\u7ebf\u548c\u7a7a\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u7ec4\u6210\uff0c\u7070\u8272\u5b9e\u7ebf\u8868\u793aR-\u7a7a\u95f4\u5408\u9002\u7684\u8303\u56f4\u4e3a1-5.0\u00c5\u3002<\/p>\n<p>\u56fe(d)\uff1aUiO-Co\u7684\u900f\u5c04\u7535\u955c-\u80fd\u8c31\u4eea\u56fe\u50cf\u3002\u5de6\u8fb9\u7684\u56fe\u5c55\u793a\u7684\u662f\u900f\u5c04\u7535\u955c\u7684\u56fe\u50cf\uff1b\u4e2d\u95f4\u56fe\u50cf\u5c55\u793a\u4e86Co\u7684\u5206\u5e03\uff0c\u7528\u84dd\u8272\u6807\u51fa\uff1b\u6700\u53f3\u8fb9\u7684\u56fe\u50cf\u5c55\u793a\u4e86Zr\u7684\u5206\u5e03\uff0c\u7528\u9ec4\u8272\u6807\u51fa\u3002UiO-Co\u7684\u900f\u5c04\u7535\u955c-\u80fd\u8c31\u4eea\u56fe\u50cf\u8868\u660eCo\u548cZr\u662f\u901a\u8fc7MOF\u7c92\u5b50\u6765\u5747\u5300\u5206\u5e03\u7684\u3002<br \/>\n\u56fe(e)\uff1a\u4e09\u79cdUiO\u7c89\u672b\u7684XRD\u66f2\u7ebf\u76f8\u4f3c\u6027\u8868\u660e\uff0c\u5728\u9884\u5408\u6210\u91d1\u5c5e\u5316\u4f5c\u7528\u548c\u50ac\u5316\u4f5c\u7528\u540e\uff0cUiO-68\u4fdd\u7559\u4e86\u5176\u7ed3\u6676\u6027\u3002\u56fe\u4e2d\u9ed1\u8272\u66f2\u7ebf\u4ee3\u8868UiO-68\uff0c\u7ea2\u8272\u66f2\u7ebf\u4ee3\u8868UiO-FeBr\uff0c\u84dd\u8272\u66f2\u7ebf\u4ee3\u8868\u5728\u56db\u6c22\u5316\u8418\u6c28\u57fa\u5316\u540e\u7684UiO-Fe\u3002<\/p>\n<p>\u56fe(f)\uff1a\u5728UiO-FeBr\u4e2dFe\u7684K\u8fb9\u754c\u5904\u7684\u5ef6\u4f38X\u5c04\u7ebf\u7cbe\u7ec6\u673a\u6784\u5149\u8c31\u548cR-\u7a7a\u95f4\u7ed3\u6784\u793a\u610f\u56fe\u3002\u56fe\u4e2d\u5b9e\u7ebf\u548c\u5b9e\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u91cf\u7ea7\uff0c\u865a\u7ebf\u548c\u7a7a\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u7ec4\u6210\uff0c\u7070\u8272\u5b9e\u7ebf\u8868\u793aR-\u7a7a\u95f4\u5408\u9002\u7684\u8303\u56f4\u4e3a1-5.1\u00c5\u3002<\/p>\n<p><strong>\u56fe2\uff1aCo@SBU\u50ac\u5316\u53cd\u5e94\u7684\u673a\u7406\u7814\u7a76<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-41750\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f2.jpg\" alt=\"ncomms12610-f2\" width=\"515\" height=\"700\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f2.jpg 515w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f2-221x300.jpg 221w\" sizes=\"(max-width: 515px) 100vw, 515px\" \/><br \/>\n\u56fe(a)\uff1a\u5728UiO68-CoBpin\u4e2dCo\u7684K\u8fb9\u754c\u5904\u7684\u5ef6\u4f38X\u5c04\u7ebf\u7cbe\u7ec6\u673a\u6784\u5149\u8c31\u548cR-\u7a7a\u95f4\u7ed3\u6784\u793a\u610f\u56fe\u3002\u56fe\u4e2d\u5b9e\u7ebf\u548c\u5b9e\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u91cf\u7ea7\uff0c\u865a\u7ebf\u548c\u7a7a\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u7ec4\u6210\uff0c\u7070\u8272\u5b9e\u7ebf\u8868\u793aR-\u7a7a\u95f4\u5408\u9002\u7684\u8303\u56f4\u4e3a1-5.3\u00c5\u3002<\/p>\n<p>\u56fe(b)\uff1aZr6O4(OCoCl)4(McO)12\u56e2\u805a\u4f53\u7684\u7ed3\u6784\u6a21\u578b\uff1b<\/p>\n<p>\u56fe(c)\uff1aZr6O4(OCoCl)4(McO)12\u56e2\u805a\u4f53\u4e2dCo\u7684K\u8fb9\u754c\u5904\u7684\u5ef6\u4f38X\u5c04\u7ebf\u7cbe\u7ec6\u673a\u6784\u5149\u8c31\u548cR-\u7a7a\u95f4\u7ed3\u6784\u793a\u610f\u56fe\u3002\u56fe\u4e2d\u5b9e\u7ebf\u548c\u5b9e\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u91cf\u7ea7\uff0c\u865a\u7ebf\u548c\u7a7a\u65b9\u5757\u8868\u793a\u5085\u91cc\u53f6\u53d8\u6362\u7684\u7ec4\u6210\uff0c\u7070\u8272\u5b9e\u7ebf\u8868\u793aR-\u7a7a\u95f4\u5408\u9002\u7684\u8303\u56f4\u4e3a1.18-4.98\u00c5\u3002<\/p>\n<p>\u56fe(d)\uff1ap-\u4e8c\u7532\u82ef\u7684\u82ef\u7532\u57faC-H\u952e\u787c\u5316\u4f5c\u7528\u7684\u521d\u59cb\u901f\u7387\u7684\u52a8\u529b\u5b66\u66f2\u7ebf\u548c\u52a0\u5165UiO-Co\u50ac\u5316\u5242\u7684\u5bf9\u6bd4\uff0c\u66f2\u7ebf\u8868\u660e\u4e86p-\u4e8c\u7532\u82ef\u7684C-H\u952e\u787c\u5316\u4f5c\u7528\u7684\u4e00\u7ea7\u52a8\u529b\u5b66\u53cd\u5e94\u4e0e\u50ac\u5316\u5242\u548cp-\u4e8c\u7532\u82ef\u7684\u6d53\u5ea6\u6709\u5173\u3002<\/p>\n<p>\u56fe(e)\uff1a\u6839\u636e\u52a8\u529b\u5b66\u548c\u5b9e\u9a8c\u7814\u7a76\uff0cUiO-Co\u50ac\u5316\u7684P-\u4e8c\u7532\u82ef\u7684\u82ef\u7532\u57faC-H\u952e\u787c\u5316\u4f5c\u7528\u662f\u901a\u8fc7Co-Bpin\u201d\u952e\u548c\u201cH-CH2ph\u201d\u952e\u7684[2+2]\u73af\u52a0\u6210\u53cd\u5e94\u8fdb\u884c\u7684\uff0c\u5e76\u4e14\u8fd9\u662f\u63a7\u5236\u901f\u7387\u7684\u4e00\u6b65\u53cd\u5e94\u3002<\/p>\n<p>\u56fe(f)\uff1a\u7ed3\u6784\u6a21\u578b\u5c55\u793a\u4e86\u5728\u63a7\u5236\u901f\u7387\u7684\u53cd\u5e94\u4e2dC-H\u787c\u5316\u53cd\u5e94\u7684\u5316\u5b66\u9009\u62e9\u6027\u7684\u539f\u56e0\u3002<\/p>\n<p><strong>\u56fe3\uff1a\u4e3aC-H\u952e\u7684sp3\u6742\u5316\u548c\u5176\u4ed6\u53cd\u5e94\u8bbe\u8ba1Co@SBU\u5355\u70b9\u56fa\u6001\u50ac\u5316\u5242\u7684\u7406\u8bba\u7814\u7a76<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-41751\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f3.jpg\" alt=\"ncomms12610-f3\" width=\"700\" height=\"226\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f3.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/ncomms12610-f3-300x97.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><br \/>\n\u56fe(a)\uff1a\u4f4d\u4e8eUiO-68\u7684\u4e8c\u7ea7\u7ed3\u6784\u5355\u5143\u7684\u7a7a\u95f4\u4fdd\u62a4\u73af\u5883\u4e2d\u7684\u7f3a\u5931\u7535\u5b50\u7684Co(\u2161)\u539f\u5b50\u4e2d\u5fc3\uff0c\u66f4\u504f\u5411\u4e8e\u8f83\u5c0f\u4f4d\u963b\u7684\u70f7\u57faC-H\u952e\u901a\u8fc7\u952e\u4ea4\u6362\u6765\u8fdb\u884c\u6fc0\u6d3b\u3002\uff081\uff09\u7a7a\u95f4\u4fdd\u62a4\u6765\u63a7\u5236\u4f4d\u7f6e\u7684\u9009\u62e9\uff082\uff09\u4f4d\u7f6e\u5206\u79bb\u907f\u514d\u5206\u5b50\u95f4\u5931\u6d3b\uff083\uff09\u4e0d\u7a33\u5b9a\u914d\u5408\u4fc3\u8fdb\u5e95\u7269\u7ed3\u5408\uff084\uff09\u6865\u6c27\u914d\u4f4d\u57fa\u521b\u9020\u7f3a\u7535\u5b50\u50ac\u5316\u4f4d\u7f6e\u3002<\/p>\n<p>\u56fe(b)\uff1aC-H\u952e\u7684sp3\u6742\u5316\u53cd\u5e94\u548cM@SBU\u50ac\u5316\u7684\u70ef\u70c3\u6c22\u5316\u53cd\u5e94\u3002<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<br \/>\n<\/strong><br \/>\n\u7814\u7a76\u8005\u4eec\u7814\u5236\u51fa\u4e86\u4e00\u79cd\u53ef\u4ee5\u7528\u6613\u5f97\u5ec9\u4ef7\u7684\u5730\u8868\u542b\u91cf\u4e30\u5bcc\u524d\u9a71\u4f53\u6765\u5904\u7406\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u6750\u6599\u8282\u70b9\uff0c\u4ece\u800c\u4e3a\u5927\u8303\u56f4\u7684\u6709\u673a\u8f6c\u53d8\u63d0\u4f9b\u9ad8\u6548\u3001\u53ef\u9009\u62e9\u7684\u5355\u70b9\u56fa\u4f53\u50ac\u5316\u5242\u3002\u6211\u4eec\u671f\u5f85\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u5316\u5408\u7269(MOFs)\u53ef\u4ee5\u4e3a\u53d1\u73b0\u65b0\u7684\u50ac\u5316\u8f6c\u53d8\u63d0\u4f9b\u4e00\u4e2a\u591a\u529f\u80fd\u7684\u5e73\u53f0\uff0c\u5e76\u4e14\u4fc3\u8fdb\u7528\u4e8e\u53ef\u6301\u7eed\u5316\u5b66\u5408\u6210\u7684\u91d1\u5c5e\u50ac\u5316\u5242\u7684\u53d1\u5c55\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/www.nature.com\/ncomms\/2016\/160830\/ncomms12610\/full\/ncomms12610.html#affil-auth\" target=\"_blank\">Chemoselective single-site Earth-abundant metal catalysts at metal\u2013organic framework nodes<\/a>\u00a0\uff08Nature Communications\uff0c2016\uff0cDOI:10.1038\/ncomms12610\uff09<\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8 \u6728\u6728\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 2016\u5e748\u670830\u65e5\uff0cNature Communications\u6742\u5fd7\u53d1\u8868\u4e86\u4e00\u7bc7\u5173\u4e8e\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u5316\u5408\u7269(MOFs)\u751f\u4ea7\u5730\u8868\u542b\u91cf\u4e30\u5bcc\u7684\u9ad8\u6548\u91d1\u5c5e\u50ac\u5316\u5242\u7684\u6587\u7ae0&#8230;<\/p>\n","protected":false},"author":842,"featured_media":41749,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[116,43,1405],"class_list":["post-41748","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-catalyst","tag-composite","tag-linwenbing"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/41748"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/842"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=41748"}],"version-history":[{"count":9,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/41748\/revisions"}],"predecessor-version":[{"id":42641,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/41748\/revisions\/42641"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/41749"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=41748"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=41748"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=41748"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}