{"id":42497,"date":"2016-09-23T14:00:02","date_gmt":"2016-09-23T06:00:02","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=42497"},"modified":"2016-09-23T00:12:03","modified_gmt":"2016-09-22T16:12:03","slug":"%e5%8e%9f%e6%b2%b9%e6%b3%84%e6%bc%8f%e6%80%8e%e4%b9%88%e5%8a%9e%ef%bc%9f%e7%ba%b3%e7%b1%b3%e6%8a%80%e6%9c%af%e6%9d%a5%e6%94%af%e6%8b%9b","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=42497","title":{"rendered":"\u539f\u6cb9\u6cc4\u6f0f\u600e\u4e48\u529e\uff1f\u7eb3\u7c73\u6280\u672f\u6765\u652f\u62db"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8<\/strong>\uff1a\u8fd1\u5e74\u6765\uff0c\u9891\u7e41\u7684\u6d77\u4e0a\u77f3\u6cb9\u4e8b\u6545\u5bf9\u4eba\u7c7b\u6240\u5904\u7684\u751f\u6001\u73af\u5883\u9020\u6210\u4e86\u4e25\u91cd\u6c61\u67d3\uff0c\u6c61\u67d3\u7269\u5728\u77ed\u65f6\u95f4\u5185\u96be\u4ee5\u6d88\u9664\u3002\u52a0\u62ff\u5927Alberta Ingenuity\u5b9e\u9a8c\u5ba4\u81ea\u58a8\u897f\u54e5\u6e7e\u6f0f\u6cb9\u4e8b\u4ef6\u4ee5\u6765\u4e00\u76f4\u4e13\u6ce8\u4e8e\u89e3\u51b3\u8fd9\u4e00\u96be\u9898\uff0c\u76ee\u524d\uff0c\u7814\u7a76\u4eba\u5458\u91c7\u7528\u5404\u79cd\u523a\u6fc0-\u54cd\u5e94\u7684\u7eb3\u7c73\u6750\u6599\u6210\u529f\u5b9e\u73b0\u4ece\u6c34\u4e2d\u5206\u79bb\u6cb9\u8fd9\u4e00\u8fc7\u7a0b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-42675 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-15-1.jpg\" alt=\"\u56fe\u72471-15\" width=\"591\" height=\"509\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-15-1.jpg 591w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-15-1-300x258.jpg 300w\" sizes=\"(max-width: 591px) 100vw, 591px\" \/><\/p>\n<p>\u81ea2010\u5e74\u82f1\u56fd\u77f3\u6cb9\u516c\u53f8\u7684\u6d77\u4e0a\u94bb\u4e95\u5e73\u53f0\u201c\u6df1\u6c34\u5730\u5e73\u7ebf\u201d\u5728\u58a8\u897f\u54e5\u6e7e\u53d1\u751f\u6f0f\u6cb9\u7684\u60b2\u60e8\u4e8b\u4ef6\u4ee5\u6765\uff0c\u77f3\u6cb9\u5b89\u5168\u5df2\u7ecf\u8d70\u5728\u4e86\u73af\u5883\u8fa9\u8bba\u548c\u5a92\u4f53\u5173\u6ce8\u7126\u70b9\u7684\u6700\u524d\u6cbf\u3002\u7531\u4e8e\u5bf9\u8fd9\u4e00\u516c\u5171\u95ee\u9898\u7684\u5927\u91cf\u5173\u6ce8\uff0c\u8fd9\u6708\u5e95\uff0c\u597d\u83b1\u575e\u5c06\u63a8\u51fa\u5173\u4e8e\u8fd9\u4e00\u4e8b\u4ef6\u7684\u7eaa\u5f55\u7247\u3002\u53ef\u4ee5\u9884\u6599\u7684\u662f\uff0c\u968f\u4e4b\u800c\u6765\u7684\u5c06\u4f1a\u6709\u5173\u4e8e\u4e8b\u4ef6\u7a76\u7adf\u662f\u5982\u4f55\u53d1\u751f\u7684\u8fd9\u4e00\u95ee\u9898\uff0c\u8fd8\u6709\u5c31\u662f\u5bf9\u6574\u4e2a\u884c\u4e1a\u7684\u6279\u5224\u3002<\/p>\n<p>\u5f88\u6709\u53ef\u80fd\u51fa\u73b0\u7684\u4e00\u4e2a\u95ee\u9898\u5c31\u662f\u6211\u4eec\u5982\u4f55\u907f\u514d\u518d\u6b21\u53d1\u751f\u8fd9\u6837\u7684\u707e\u96be\uff1f\u5e78\u8fd0\u7684\u662f\uff0c\u4e00\u4e9b\u79d1\u5b66\u5bb6\u4eec\u65e9\u5df2\u6709\u6240\u51c6\u5907\u3002<\/p>\n<p>\u4e00\u76f4\u4e13\u6ce8\u4e8e\u8fd9\u4e00\u96be\u9898\u7684\u662f\u52a0\u62ff\u5927Alberta Ingenuity\u5b9e\u9a8c\u5ba4\u7684\u4e00\u4e2a\u56e2\u961f\u3002\u8be5\u673a\u6784\u521a\u521a\u83b7\u5f97\u4e861700\u4e07\u7f8e\u5143\u7684\u9879\u76ee\u8d44\u91d1\u7528\u4e8e\u5f00\u53d1\u4ece\u6f0f\u6cb9\u4e2d\u56de\u6536\u6cb9\u7684\u5148\u8fdb\u7684\u7cfb\u7edf\u3002\u8fd9\u79cd\u8d44\u672c\u6ce8\u5165\u5c06\u4f7fIngenuity\u5b9e\u9a8c\u5ba4\u80fd\u591f\u5f00\u5c55\u65b0\u7684\u7814\u7a76\uff0c\u5f00\u53d1\u5728\u6d77\u6d0b\u73af\u5883\u4e2d\u4fee\u590d\u91cd\u6cb9\u6cc4\u6f0f\u7684\u5546\u4e1a\u751f\u4ea7\u6d41\u7a0b\u3002\u8be5\u6280\u672f\u7684\u6838\u5fc3\u5728\u4e8e\u5176\u80fd\u591f\u56de\u6536\u6cb9\u7684\u57fa\u4e8e\u7eb3\u7c73\u7ebf\u7684\u523a\u6fc0-\u54cd\u5e94\u7684\u819c\u548c\u88c5\u7f6e\u3002<\/p>\n<p>\u77f3\u6cb9\u662f\u6d77\u6d0b\u4e2d\u6bd4\u8f83\u5e38\u89c1\u7684\u4e00\u79cd\u6c61\u67d3\u7269\uff0c\u6bcf\u5e74\u6709\u8d85\u8fc7300\u4e07\u516c\u5428\u6c61\u67d3\u6d77\u6d0b\u3002\u5f53\u539f\u6cb9\u4e0d\u614e\u4ece\u4e00\u8258\u6cb9\u8f6e\u3001\u70bc\u6cb9\u5382\u3001\u4ed3\u50a8\u8bbe\u65bd\u3001\u6c34\u4e0b\u7ba1\u9053\u6216\u6d77\u4e0a\u77f3\u6cb9\u94bb\u673a\u8fdb\u5165\u6c34\u4f53\u65f6\uff0c\u662f\u6700\u7d27\u8feb\u7684\u73af\u5883\u7d27\u6025\u95ee\u9898\u3002<\/p>\n<p>\u6839\u636e\u5176\u4f4d\u7f6e\uff0c\u539f\u6cb9\u6cc4\u6f0f\u53ef\u80fd\u662f\u9ad8\u5ea6\u5371\u9669\u7684\uff0c\u4ee5\u53ca\u73af\u5883\u7834\u574f\u6027\u7684\u3002\u76f8\u5e94\u7684\uff0c\u53ca\u65f6\u6e05\u7406\u5bf9\u4fdd\u62a4\u6c34\u4f53\u7684\u5b8c\u6574\u6027\u3001\u6d77\u5cb8\u7ebf\u548c\u4f17\u591a\u751f\u7269\u8d56\u4ee5\u751f\u5b58\u7684\u6816\u606f\u5730\u662f\u6781\u4e3a\u91cd\u8981\u7684\u3002<\/p>\n<p>\u7531\u4e8e\u5bf9\u77f3\u6cb9\u5de5\u4e1a\u7684\u73af\u5883\u8bb0\u5f55\u65e5\u76ca\u4e25\u683c\u7684\u5ba1\u67e5\uff0c\u5fc5\u987b\u5c06\u7cbe\u529b\u96c6\u4e2d\u5728\u80fd\u53bb\u9664\u6c34\u4e2d\u7684\u6709\u673a\u7269\u7684\u65b0\u6750\u6599\u3001\u65b0\u6280\u672f\u7684\u5f00\u53d1\u4e0a\u3002\u7b80\u5355\u6765\u8bf4\uff0c\u5c31\u662f\u73b0\u6709\u7684\u65b9\u6cd5\u8fd8\u4e0d\u5b8c\u5584\u3002<\/p>\n<p>\u7136\u800c\uff0c\u5e78\u8fd0\u7684\u662f\uff0c\u7eb3\u7c73\u6280\u672f\u4e3a\u5206\u79bb\u5de5\u5177\u7684\u53d1\u5c55\u6253\u5f00\u4e86\u4e00\u6247\u65b0\u5927\u95e8\uff0c\u901a\u8fc7\u7eb3\u7c73\u6280\u672f\u53ef\u4ee5\u8bbe\u8ba1\u6750\u6599\u7684\u7279\u6027\uff0c\u4f7f\u5176\u9002\u7528\u4e8e\u590d\u6742\u7684\u5206\u79bb\u8fc7\u7a0b\uff0c\u5176\u4e2d\u4e5f\u5305\u62ec\u4ece\u6c34\u4e2d\u5206\u79bb\u539f\u6cb9\u3002<\/p>\n<p>Ingenuity\u5b9e\u9a8c\u5ba4\u7684\u9879\u76ee\u91cd\u70b9\u5728\u4e8e\u901a\u8fc7\u5404\u79cd\u523a\u6fc0-\u54cd\u5e94\u7684\u7eb3\u7c73\u6750\u6599\u8fd9\u4e00\u65b0\u6280\u672f\u6765\u6709\u6548\u5730\u56de\u6536\u539f\u6cb9\u3002\u5f53\u8fd9\u4e00\u6280\u672f\u80fd\u591f\u5927\u89c4\u6a21\u5e94\u7528\u65f6\uff0c\u8be5\u5b9e\u9a8c\u5ba4\u5c06\u4f1a\u4e0e\u4e1a\u754cTortech Nanofiber\u516c\u53f8\u8fdb\u884c\u5bc6\u5207\u5730\u5408\u4f5c\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.nanowerk.com\/nanotechnology-news\/newsid=44573.php\" target=\"_blank\">Scientists use nanotechnology to prevent oil spill disaster<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u8d75\u4e39\u63d0\u4f9b\u7d20\u6750\uff0c\u9ec4\u654f\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u8fd1\u5e74\u6765\uff0c\u9891\u7e41\u7684\u6d77\u4e0a\u77f3\u6cb9\u4e8b\u6545\u5bf9\u4eba\u7c7b\u6240\u5904\u7684\u751f\u6001\u73af\u5883\u9020\u6210\u4e86\u4e25\u91cd\u6c61\u67d3\uff0c\u6c61\u67d3\u7269\u5728\u77ed\u65f6\u95f4\u5185\u96be\u4ee5\u6d88\u9664\u3002\u52a0\u62ff\u5927Alberta Ingenuity\u5b9e\u9a8c\u5ba4\u81ea\u58a8\u897f\u54e5\u6e7e\u6f0f\u6cb9\u4e8b&#8230;<\/p>\n","protected":false},"author":660,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[33],"class_list":["post-42497","post","type-post","status-publish","format-standard","hentry","category-keji","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/42497"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/660"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=42497"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/42497\/revisions"}],"predecessor-version":[{"id":42676,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/42497\/revisions\/42676"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=42497"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=42497"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=42497"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}