{"id":4322,"date":"2016-03-22T08:00:58","date_gmt":"2016-03-22T00:00:58","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=4322"},"modified":"2016-03-22T14:23:56","modified_gmt":"2016-03-22T06:23:56","slug":"%e4%b8%80%e7%a7%8d%e6%96%b0%e5%9e%8b%e7%9a%84%e6%97%a0%e6%87%88%e5%8f%af%e5%87%bb%e7%9a%84%e6%b0%94%e6%80%81%e6%b6%82%e5%b1%82%e5%88%87%e5%89%b2%e5%88%80%e5%85%b7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=4322","title":{"rendered":"\u201c\u786c\u786c\u7ed3\u5408\u201d\u201c\u65e0\u61c8\u53ef\u51fb\u201d\u7684\u6d82\u5c42\u5207\u5272\u5200\u5177"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-4384 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/03\/2014052822183223033620.jpg\" alt=\"2014052822183223033620\" width=\"778\" height=\"370\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/03\/2014052822183223033620.jpg 778w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/03\/2014052822183223033620-300x143.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/03\/2014052822183223033620-768x365.jpg 768w\" sizes=\"(max-width: 778px) 100vw, 778px\" \/><\/p>\n<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u6765\u81ea\u6258\u6728\u65af\u514b\u7406\u5de5\u5927\u5b66(TPU)\u7684\u79d1\u5b66\u5bb6\u4eec\u521b\u9020\u4e86\u65b0\u4e00\u4ee3\u6d82\u5c42\u5200\u5177\uff1a\u65b0\u5200\u5177\u4e0d\u4ec5\u8010\u7528\uff0c\u5e76\u4e14\u80fd\u591f\u5207\u5272\u5927\u591a\u6570\u7684\u6750\u6599\u3002\u8be5\u6d82\u5c42\u662f\u901a\u8fc7\u6c14\u4f53\u6df7\u5408\u7269\u751f\u4ea7\u91d1\u521a\u77f3\u548c\u7acb\u65b9\u6c2e\u5316\u787c\u8584\u819c\u5236\u5f97\u7684\u3002<\/p>\n<p>\u9ad8\u786c\u5ea6\u7684\u91d1\u521a\u77f3\u6d82\u6599\u5df2\u7ecf\u5e7f\u6cdb\u5e94\u7528\u4e8e\u5207\u524a\u5de5\u5177\u7684\u5236\u9020\u3002\u4ed6\u4eec\u53ef\u4ee5\u5207\u524a\u4e00\u90e8\u5206\u91d1\u5c5e\u5408\u91d1\u3001\u9676\u74f7\u3001\u78b3\u590d\u5408\u6750\u6599\uff0c\u4f46\u65e0\u6cd5\u5207\u524a\u94a2\u94c1\u6750\u6599\uff1a\u78b3\u5728\u9ad8\u6e29\u4e0b\u4e0e\u94c1\u53cd\u5e94\u5e76\u4e14\u9010\u6e10\u5d29\u6e83\u3002<\/p>\n<p>\u8981\u89e3\u51b3\u8fd9\u4e2a\u95ee\u9898\uff0cTPU\u79d1\u5b66\u5bb6\u63d0\u51fa\u5f00\u53d1\u4e00\u79cd\u76ee\u524d\u6700\u786c\u7684\u91d1\u521a\u77f3\u4e0e\u7acb\u65b9\u6c2e\u5316\u787c\u590d\u5408\u6d82\u5c42\u3002<\/p>\n<p>\u7acb\u65b9\u6c2e\u5316\u787c\u5728\u5207\u5272\u94a2\u94c1\u65f6\u4e0d\u4f1a\u53d7\u5230\u635f\u4f24\uff0c\u8fd9\u4f7f\u5f97\u7531\u5b83\u5236\u4f5c\u7684\u5200\u5177\u51e0\u4e4e\u201c\u65e0\u61c8\u53ef\u51fb\u201d\u3002<\/p>\n<p>\u201c\u76ee\u524d\u8fd8\u672a\u6709\u4eba\u5408\u6210\u8fc7\u591a\u6676\u78b3\u5f62\u5f0f\u7684\u7acb\u65b9\u6c2e\u5316\u787c\u6d82\u6599\u3002\u6211\u4eec\u60f3\u5229\u7528\u7acb\u65b9\u6c2e\u5316\u787c\u548c\u91d1\u521a\u77f3\u7684\u6676\u683c\u8ddd\u79bb\u7684\u76f8\u4f3c\u6027\uff0c\u4f7f\u7acb\u65b9\u6c2e\u5316\u787c\u6676\u4f53\u80fd\u591f\u751f\u957f\u5728\u91d1\u521a\u77f3\u6676\u7c92\u4e0a\u3002<\/p>\n<p>\u201c\u6211\u4eec\u7684\u6d82\u5c42\uff0c\u96c6\u6210\u4e86\u91d1\u521a\u77f3\u548c\u6c2e\u5316\u7845\u6d82\u5c42\u7684\u6027\u8d28\uff0c\u5c06\u9002\u7528\u4e8e\u5927\u591a\u6570\u91d1\u5c5e\uff0c\u201d Stepan Linnik\u89e3\u91ca\u9053\uff08Stepan Linnik\u662f\u6765\u81eaTPU\u9ad8\u6280\u672f\u7269\u7406\u7814\u7a76\u6240\u7684\u4e00\u540d\u5b9e\u9a8c\u5ba4\u7814\u7a76\u5de5\u7a0b\u5e08\uff09\u3002<\/p>\n<p>\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u6c14\u76f8\u7b49\u79bb\u5b50\u4f53\u6c89\u79ef\u83b7\u5f97\u6d82\u5c42\u3002\u4ed6\u4eec\u5728\u7532\u70f7\u548c\u6c22\u6c14\u7684\u6df7\u5408\u6c14\u6c1b\u4e2d\uff0c\u91c7\u7528\u6e85\u5c04\u6280\u672f\u5f00\u5236\u5907\u91d1\u521a\u77f3\u3002\u7acb\u65b9\u6c2e\u5316\u787c\u5219\u662f\u5728\u4e59\u787c\u70f7\u6c14\u6c1b\u4e0b\u5236\u5f97\u7684\u3002\u5236\u5f97\u7684\u6d82\u5c42\u6d82\u8986\u5728\u786c\u8d28\u5408\u91d1\u5de5\u5177\u8868\u9762\u4f1a\u663e\u8457\u589e\u52a0\u5176\u5f3a\u5ea6\u3002<\/p>\n<p>2015\u5e74, Stepan Linnik\u7684\u7814\u7a76\u5f97\u5230\u4e86\u4fc4\u7f57\u65af\u57fa\u7840\u7814\u7a76\u57fa\u91d1\u4f1a(RFBR)\uff1a\u7406\u5de5\u5927\u5b66\u8d62\u5f97\u4e86\u672a\u6765\u4e09\u5e74\u62e8\u6b3e510\u4e07\u5362\u5e03\u7684\u8d44\u52a9\u3002\u65e9\u4e9b\u65f6\u5019\uff0c\u79d1\u5b66\u5bb6\u53c2\u4e0e\u4e86 \u201cTPU\u535a\u58eb\u540e\u201d\u9879\u76ee\u3002\u6b64\u9879\u76ee\u4e2d\u7684\u5e74\u8f7b\u7684\u535a\u58eb\u4ece\u4e8b\u4e8e\u4e00\u9879\u7531\u4e00\u4f4d\u6709\u7ecf\u9a8c\u7684\u9886\u5bfc\u4eba\u7275\u5934\u7684\u524d\u6cbf\u9879\u76ee\u3002\u6839\u636eStepan Linnik\u6240\u8a00\uff0c\u8fd9\u4e9b\u9879\u76ee\u4e3a\u4ed6\u7684\u5bfc\u5e08Remnev\u6559\u6388\u548c\u9879\u76ee\u63d0\u4f9b\u4e86\u4e00\u4e2a\u673a\u4f1a\u6765\u5f00\u5c55\u81ea\u5df1\u7684\u7814\u7a76\uff0c\u5bfb\u627e\u65b9\u6cd5\uff0c\u5e76\u4e3a\u4ed6\u7684\u9879\u76ee\u5438\u5f15\u8d44\u91d1\u3002<\/p>\n<p>2016\u5e74\u521d Stepan Linnik\u4e5f\u6536\u5230\u4e00\u4efd\u6765\u81ea\u4fc4\u7f57\u65af\u8054\u90a6\u603b\u7edf\u5bf9\u5e74\u8f7b\u79d1\u5b66\u5bb6\u91d1\u521a\u77f3\u6d82\u5c42\u6c89\u79ef\u6280\u672f\u53d1\u5c55\u7684\u8d44\u52a9\u3002<\/p>\n<p>\u539f\u6587\u5730\u5740\uff1a<a href=\"http:\/\/www.eurekalert.org\/pub_releases\/2016-03\/tpu-cf031616.php\" target=\"_blank\">&#8216;Invulnerable&#8217; coatings for cutting tools from gas<\/a><\/p>\n<p>\u611f\u8c22\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u675c\u5f81\u94ee\u63d0\u4f9b\u7d20\u6750\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u6765\u81ea\u6258\u6728\u65af\u514b\u7406\u5de5\u5927\u5b66(TPU)\u7684\u79d1\u5b66\u5bb6\u4eec\u521b\u9020\u4e86\u65b0\u4e00\u4ee3\u6d82\u5c42\u5200\u5177\uff1a\u65b0\u5200\u5177\u4e0d\u4ec5\u8010\u7528\uff0c\u5e76\u4e14\u80fd\u591f\u5207\u5272\u5927\u591a\u6570\u7684\u6750\u6599\u3002\u8be5\u6d82\u5c42\u662f\u901a\u8fc7\u6c14\u4f53\u6df7\u5408\u7269\u751f\u4ea7\u91d1\u521a\u77f3\u548c\u7acb\u65b9\u6c2e\u5316\u787c\u8584&#8230;<\/p>\n","protected":false},"author":50,"featured_media":4384,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[54],"class_list":["post-4322","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-making"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/4322"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/50"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=4322"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/4322\/revisions"}],"predecessor-version":[{"id":4405,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/4322\/revisions\/4405"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/4384"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=4322"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=4322"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=4322"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}