{"id":49709,"date":"2016-11-01T06:30:21","date_gmt":"2016-10-31T22:30:21","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=49709"},"modified":"2016-10-31T22:38:23","modified_gmt":"2016-10-31T14:38:23","slug":"%e6%b4%bb%e4%b9%85%e8%a7%81%ef%bc%81%e4%ba%8c%e6%b0%a7%e5%8c%96%e7%a2%b3%e5%8f%98%e9%85%92%e7%b2%be%ef%bc%81","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=49709","title":{"rendered":"\u6d3b\u4e45\u89c1\uff01\u4e8c\u6c27\u5316\u78b3\u53d8\u9152\u7cbe\uff01"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u8fd0\u7528\u7eb3\u7c73\u6280\u672f\uff0c\u6a61\u6811\u5cad\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u7684\u7814\u7a76\u4eba\u5458\u6210\u529f\u5730\u5c06\u4e8c\u6c27\u5316\u78b3\u8f6c\u5316\u6210\u4e59\u9187\uff0c\u8be5\u5b9e\u9a8c\u5177\u6709\u975e\u5e38\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u770b\u8d77\u6765\u4f3c\u4e4e\u4e0d\u53ef\u601d\u8bae\uff0c\u8fd9\u662f\u5982\u4f55\u5b9e\u73b0\u7684\u5462\uff1f\u4e0b\u9762\u5c31\u968f\u5c0f\u7f16\u4e00\u63a2\u7a76\u7adf\u5427\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-49711 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/10\/\u56fe\u72471-19.jpg\" alt=\"\u56fe\u72471\" width=\"700\" height=\"467\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/10\/\u56fe\u72471-19.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/10\/\u56fe\u72471-19-300x200.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u6a61\u6811\u5cad\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u7684\u7814\u7a76\u4eba\u5458\u8fd0\u7528\u7eb3\u7c73\u6280\u672f\uff0c\u5c06\u4e8c\u6c27\u5316\u78b3\u8fd9\u79cd\u6e29\u5ba4\u6c14\u4f53\u6210\u529f\u5730\u8f6c\u5316\u6210\u4e59\u9187\u3002<\/p>\n<p>\u79d1\u5b66\u5bb6\u4eec\u8fd0\u7528\u7535\u5316\u5b66\u65b9\u6cd5\uff0c\u4f7f\u7528\u5fae\u91cf\u7684\u542b\u78b3\u548c\u94dc\u7684\u5c16\u72b6\u6df7\u5408\u7269\uff0c\u5c06\u4e8c\u6c27\u5316\u78b3\u8f6c\u5316\u4e3a\u4e59\u9187\u3002\u8be5\u8bba\u6587\u7684\u7b2c\u4e00\u4f5c\u8005Adam Rondinone\u8bf4\uff0c\u8fd9\u4e2a\u5b9e\u9a8c\u7684\u6700\u521d\u76ee\u7684\u662f\u751f\u4ea7\u7532\u9187\u800c\u5e76\u975e\u4e59\u9187\u3002\u201c\u6211\u4eec\u5076\u7136\u7684\u53d1\u73b0\u8fd9\u79cd\u6750\u6599\u4ea7\u751f\u7684\u6548\u679c\u201d \uff0cRondinone\u5728\u4e00\u4efd\u58f0\u660e\u4e2d\u8bf4\uff0c\u201c\u6211\u4eec\u610f\u8bc6\u5230\u50ac\u5316\u5242\u662f\u5728\u6574\u4e2a\u8fc7\u7a0b\u4e2d\u8d77\u4f5c\u7528\u65f6\uff0c\u4fbf\u5f00\u59cb\u8bd5\u56fe\u7814\u7a76\u8ba1\u5212\u4e2d\u53cd\u5e94\u7684\u7b2c\u4e00\u6b65\u3002\u201d<\/p>\n<p>\u8be5\u7814\u7a76\u56e2\u961f\u5c06\u7535\u538b\u65bd\u52a0\u5230\u7531\u78b3\u3001\u94dc\u548c\u6c2e\u5143\u7d20\u7ec4\u6210\u7684\u50ac\u5316\u5242\u4e0a\uff0c\u6765\u89e6\u53d1\u4e00\u79cd\u57fa\u672c\u4e0a\u9006\u8f6c\u71c3\u70e7\u8fc7\u7a0b\u7684\u5316\u5b66\u53cd\u5e94\u3002\u6240\u4f7f\u7528\u7684\u50ac\u5316\u5242\u662f\u5c06\u94dc\u7eb3\u7c73\u7c92\u5b50\u5d4c\u5165\u5728\u5c16\u72b6\u78b3\u5316\u7269\u4e2d\uff0c\u4ece\u800c\u907f\u514d\u4e86\u4f7f\u7528\u50cf\u94c2\u8fd9\u6837\u7f3a\u4e4f\u7ecf\u6d4e\u6027\u7684\u8d35\u91d1\u5c5e\u6216\u7a00\u6709\u91d1\u5c5e\u3002<\/p>\n<p>\u201c\u5c06\u7eb3\u7c73\u6280\u672f\u8fd0\u7528\u5230\u666e\u901a\u6750\u6599\u4e2d\uff0c\u6211\u4eec\u53d1\u73b0\u53ef\u4ee5\u5982\u4f55\u9650\u5236\u526f\u53cd\u5e94\uff0c\u6700\u7ec8\u5f97\u5230\u6211\u4eec\u60f3\u8981\u7684\u4e1c\u897f\u3002\u5b83\u4eec\u50cf50\u7eb3\u7c73\u7684\u907f\u96f7\u9488\uff0c\u5c06\u7535\u5316\u5b66\u53cd\u5e94\u96c6\u4e2d\u5728\u7ec6\u9488\u7684\u524d\u7aef\u3002\u201dRondinone\u8bf4\u3002\u5728\u542b\u6709\u591a\u4e2a\u53cd\u5e94\u70b9\u7684\u50ac\u5316\u5242\u7684\u5e2e\u52a9\u4e0b\uff0c\u4e8c\u6c27\u5316\u78b3\u6c34\u6eb6\u6db2\u8f6c\u5316\u4e3a\u4e59\u9187\u7684\u4ea7\u7387\u4e3a63%\u3002<\/p>\n<p>\u201c\u6211\u4eec\u5229\u7528\u4e86\u71c3\u70e7\u4e4b\u540e\u7684\u5e9f\u5f03\u4ea7\u7269\u4e8c\u6c27\u5316\u78b3\uff0c\u5e76\u4e14\u5c06\u71c3\u70e7\u53cd\u5e94\u53cd\u63a8\uff0c\u9ad8\u5ea6\u4e13\u4e00\u6027\u7684\u5f97\u5230\u4e86\u4e00\u79cd\u5f88\u6709\u7528\u7684\u71c3\u6599\uff0c\u201dRondinone\u8bf4\u3002\u201c\u4e59\u9187\u771f\u7684\u662f\u4e00\u4e2a\u60ca\u559c\u2014\u2014\u5229\u7528\u5355\u4e00\u7684\u50ac\u5316\u5242\u76f4\u63a5\u5c06\u4e8c\u6c27\u5316\u78b3\u8f6c\u53d8\u4e3a\u4e59\u9187\u662f\u975e\u5e38\u56f0\u96be\u7684\u3002\u201d\u8be5\u7535\u5316\u5b66\u53cd\u5e94\u540c\u6837\u53ef\u4ee5\u5728\u5ba4\u6e29\u4e0b\u7684\u6c34\u4e2d\u8fdb\u884c\uff0c\u4f7f\u7528\u7684\u6280\u672f\u76f8\u5bf9\u4fbf\u5b9c\uff0c\u8fd9\u610f\u5473\u7740\u5b83\u53ef\u4ee5\u4e0d\u9700\u592a\u591a\u989d\u5916\u7684\u80fd\u91cf\u6d6a\u8d39\u5c31\u80fd\u5b9e\u73b0\u53cd\u5e94\u7684\u201c\u6253\u5f00\u548c\u5173\u95ed\u201d\u3002<\/p>\n<p>\u56e0\u6b64\uff0c\u7814\u7a76\u4eba\u5458\u4eec\u8ba4\u4e3a\u8be5\u65b9\u6cd5\u53ef\u4ee5\u6269\u5c55\u5230\u5de5\u4e1a\u76f8\u5173\u7684\u5e94\u7528\u9886\u57df\u3002\u4f8b\u5982\uff0c\u8be5\u8fc7\u7a0b\u53ef\u4ee5\u7528\u6765\u5b58\u50a8\u6765\u81ea\u98ce\u80fd\u548c\u592a\u9633\u80fd\u7b49\u53ef\u53d8\u529f\u7387\u6e90\u4ea7\u751f\u7684\u591a\u4f59\u7684\u7535\u529b\u3002\u4e59\u9187\u53ef\u4ee5\u7528\u4e8e\u5305\u62ec\u6297\u83cc\u6d17\u624b\u6db2\u51dd\u80f6\u7684\u5404\u79cd\u4ea7\u54c1\uff0c\u4e5f\u53ef\u4f5c\u4e3a\u4e00\u79cd\u4e3a\u7532\u9187\u3001\u9152\u7cbe\u996e\u6599\u3001\u53d1\u52a8\u673a\u71c3\u6599\u548c\u706b\u7bad\u71c3\u6599\u7b49\u7684\u89e3\u6bd2\u5242\u3002<\/p>\n<p>\u539f\u6587\u8fde\u63a5\uff1a<a href=\"http:\/\/www.rdmag.com\/article\/2016\/10\/scientists-turn-carbon-dioxide-alcohol-single-spark\" target=\"_blank\">Scientists Turn Carbon Dioxide into Alcohol with a Single Spark.<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/slct.201601169\/full\" target=\"_blank\">High-Selectivity Electrochemical Conversion of CO2 to Ethanol using a Copper Nanoparticle\/N-Doped Graphene Electrode.<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u4e01\u83f2\u83f2\u63d0\u4f9b\u7d20\u6750\uff0c\u5218\u51a0\u65d7\u7f16\u8bd1\uff0c\u6731\u6653\u79c0\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u8fd0\u7528\u7eb3\u7c73\u6280\u672f\uff0c\u6a61\u6811\u5cad\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u7684\u7814\u7a76\u4eba\u5458\u6210\u529f\u5730\u5c06\u4e8c\u6c27\u5316\u78b3\u8f6c\u5316\u6210\u4e59\u9187\uff0c\u8be5\u5b9e\u9a8c\u5177\u6709\u975e\u5e38\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u770b\u8d77\u6765\u4f3c\u4e4e\u4e0d\u53ef\u601d\u8bae\uff0c\u8fd9\u662f\u5982\u4f55\u5b9e\u73b0\u7684\u5462\uff1f\u4e0b\u9762\u5c31\u968f\u5c0f\u7f16\u4e00&#8230;<\/p>\n","protected":false},"author":230,"featured_media":49711,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[81],"class_list":["post-49709","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-clearenergy"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/49709"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=49709"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/49709\/revisions"}],"predecessor-version":[{"id":49725,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/49709\/revisions\/49725"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/49711"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=49709"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=49709"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=49709"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}