{"id":51614,"date":"2016-11-15T06:30:46","date_gmt":"2016-11-14T22:30:46","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=51614"},"modified":"2016-11-14T23:34:10","modified_gmt":"2016-11-14T15:34:10","slug":"%e7%ba%b3%e7%b1%b3%e7%bb%93%e6%9e%84%e6%99%b6%e4%bd%93%e7%ae%a1-%e7%b3%96%e5%b0%bf%e7%97%85%e6%82%a3%e8%80%85%e7%9a%84%e7%a6%8f%e9%9f%b3","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=51614","title":{"rendered":"\u7eb3\u7c73\u7ed3\u6784\u6676\u4f53\u7ba1\u2014\u2014\u7cd6\u5c3f\u75c5\u60a3\u8005\u7684\u798f\u97f3"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8<\/strong>\uff1a\u4f20\u7edf\u7684\u8461\u8404\u7cd6\u4f20\u611f\u5668\u4ec5\u80fd\u5b9e\u65f6\u68c0\u6d4b\u8840\u7cd6\u9ad8\u4f4e\uff0c\u6765\u81ea\u4fc4\u52d2\u5188\u5dde\u7acb\u5927\u5b66\u7684\u7814\u7a76\u56e2\u961f\u81f4\u529b\u4e8e\u5c06\u8461\u8404\u7cd6\u4f20\u611f\u5668\u4e0e\u9690\u5f62\u773c\u955c\u6709\u673a\u7ed3\u5408\uff0c\u5b9e\u73b0\u5b9e\u65f6\u68c0\u6d4b\u548c\u6ce8\u5c04\u80f0\u5c9b\u7d20\u7684\u53cc\u91cd\u529f\u80fd\uff0c\u7eb3\u7c73\u7ed3\u6784\u6676\u4f53\u7ba1\u5728\u8fd9\u4e00\u6280\u672f\u4e2d\u8d77\u5230\u81f3\u5173\u91cd\u8981\u7684\u4f5c\u7528\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-51615 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/11\/\u65e0\u6807\u98981.png\" alt=\"%e6%97%a0%e6%a0%87%e9%a2%981\" width=\"500\" height=\"375\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/11\/\u65e0\u6807\u98981.png 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/11\/\u65e0\u6807\u98981-300x225.png 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u5404\u79cd\u7eb3\u7c73\u6750\u6599\u5df2\u7ecf\u88ab\u7528\u4e8e\u53ef\u4ee5\u5e2e\u52a9\u7cd6\u5c3f\u75c5\u60a3\u8005\u76d1\u6d4b\u5b9e\u65f6\u8840\u7cd6\u6c34\u5e73\u9ad8\u4f4e\u7684\u65b0\u578b\u8461\u8404\u7cd6\u4f20\u611f\u5668\u3002\u76ee\u524d\u5df2\u6709\u591a\u79cd\u6280\u672f\u5c06\u7eb3\u7c73\u6750\u6599\u6eb6\u5165\u9690\u5f62\u773c\u955c\u4ee5\u83b7\u5f97\u5404\u79cd\u65b0\u6027\u80fd\u3002<\/p>\n<p>\u5982\u4eca\uff0c\u4fc4\u52d2\u5188\u5dde\u7acb\u5927\u5b66\uff08OSU\uff09\u7684\u7814\u7a76\u56e2\u961f\u5c06\u7eb3\u7c73\u529f\u80fd\u7684\u9690\u5f62\u773c\u955c\u548c\u8461\u8404\u7cd6\u4f20\u611f\u5668\u96c6\u6210\u5230\u5355\u4e00\u5143\u4ef6\uff0c\u8fd9\u4e2a\u5143\u4ef6\u53ef\u80fd\u5728\u672a\u6765\u5b9e\u73b0\u68c0\u6d4b\u8840\u7cd6\u548c\u63a7\u5236\u80f0\u5c9b\u7d20\u6ce8\u5c04\u65f6\u95f4\u7684\u53cc\u91cd\u529f\u80fd\u3002\u7814\u7a76\u4eba\u5458\u6307\u51fa\u5143\u4ef6\u5c06\u4f1a\u4ee5\u900f\u660e\u4f20\u611f\u5668\u7684\u5f62\u5f0f\u5d4c\u5165\u9690\u5f62\u773c\u955c\u3002<\/p>\n<p>\u900f\u660e\u4f20\u611f\u5668\u7684\u5173\u952e\u662f\u7531\u94df\u9553\u950c\u6c27\u5316\u7269\u5236\u6210\u7684\u7eb3\u7c73\u7ed3\u6784\u573a\u6548\u5e94\u6676\u4f53\u7ba1\uff0c\u8fd9\u79cd\u6676\u4f53\u7ba1\u53ef\u4ee5\u7b80\u79f0\u4e3aIGZO-FET\u3002IGZO-FET\u7684\u5386\u53f2\u53ef\u4ee5\u8ffd\u6eaf\u52302014\u5e74\u5728\u4e1c\u4eac\u7684\u7814\u7a76\u4eba\u5458\u9996\u6b21\u53d1\u73b0\u7531\u94df\u9553\u950c\u6c27\u5316\u7269\u5236\u6210\u7684\u6676\u4f53\u7ba1\u3002\u8fd9\u4e9bIGZO\u6676\u4f53\u7ba1\u7684\u5de8\u5927\u6f5c\u529b\u5728\u4e8e\u5b83\u4eec\u7684\u900f\u660e\u5ea6\uff0c\u663e\u793a\u5668\u5236\u9020\u5546\u5f00\u53d1\u51fa\u8fd9\u79cd\u6676\u4f53\u7ba1\u662f\u4e3a\u4e86\u7528\u5b83\u4eec\u6765\u9a71\u52a8LCD\u548cOLED\u663e\u793a\u5668\u7684\u50cf\u7d20\u3002<\/p>\n<p>\u5728\u6700\u8fd1OSU\u7684\u7814\u7a76\u4e2d\uff0cIGZO\u6700\u5438\u5f15\u7814\u7a76\u56e2\u961f\u7684\u6027\u80fd\u6b63\u662f\u5b83\u7684\u900f\u660e\u5ea6\u3002OSU\u7684\u5316\u5b66\u5de5\u7a0b\u6559\u6388\uff0c\u7814\u7a76\u56e2\u961f\u6210\u5458\u4e4b\u4e00\u7684Greg Herman\u5728\u65b0\u95fb\u62a5\u544a\u4e2d\u8bf4\u9053\uff1a\u201c\u6211\u4eec\u53ef\u4ee5\u5b9e\u73b0\u4f20\u611f\u5668\u5de5\u4f5c\u65f6\u7684\u5b8c\u5168\u900f\u660e\u5316\u3002\u201d<\/p>\n<p>\u901a\u8fc7Nanoscale\u6742\u5fd7\u5bf9\u4e8e\u6b64\u9879\u7814\u7a76\u7684\u63cf\u8ff0\uff0cOSU\u56e2\u961f\u4f7f\u7528\u7d27\u5bc6\u5806\u53e0\u7684\u516d\u8fb9\u5f62IGZO FET\u7f51\u7edc\u5bf9IGZO\u8fdb\u884c\u56fe\u6848\u5316\u5904\u7406\u3002\u4f7f\u7528\u7684\u56fe\u6848\u5316\u6280\u672f\u5305\u62ec\u80f6\u4f53\u5149\u523b\u548c\u7535\u5b50\u55b7\u5c04\u5370\u5237\uff0c\u56e0\u6b64\u7814\u7a76\u4eba\u5458\u76f8\u4fe1\u8fd9\u79cdFET\u7684\u5236\u9020\u6210\u672c\u662f\u76f8\u5f53\u4f4e\u5ec9\u7684\u3002<\/p>\n<p>\u5728\u5b9e\u9645\u64cd\u4f5c\u4e2d\uff0c\u7814\u7a76\u4eba\u5458\u53d1\u73b0\u4e86\u6676\u4f53\u7ba1\u7684\u6f0f\u6781\u548c\u6e90\u6781\u968f\u7740\u8461\u8404\u7cd6\u6d53\u5ea6\u7684\u589e\u52a0\u5448\u73b0\u51fa\u7535\u5bfc\u964d\u4f4e\u7684\u73b0\u8c61\u3002\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u5b9e\u9645\u6d4b\u91cf\u8bc1\u5b9e\uff0c\u7eb3\u7c73\u7ed3\u6784IGZO FETs\u5728\u68c0\u6d4b\u8461\u8404\u7cd6\u6c34\u5e73\u53d8\u5316\u65b9\u9762\u6bd4\u975e\u7eb3\u7c73\u7ed3\u6784IGZO\u66f4\u7075\u654f\u3002<\/p>\n<p>\u201c\u6211\u4eec\u5c06\u4e00\u7cfb\u5217\u4f20\u611f\u5668\u96c6\u6210\u5230\u6c34\u6676\u4f53\u4e2d\uff0c\u5e76\u8fdb\u884c\u8bf8\u591a\u6d4b\u8bd5\uff1a\u5982\u538b\u529b\u6fc0\u7d20\uff0c\u5c3f\u9178\uff0c\u7eff\u5185\u969c\u538b\u529b\u611f\u6d4b\uff0c\u4ee5\u53ca\u5176\u4f59\u7c7b\u4f3c\u6307\u6807\u6d4b\u8bd5\u3002\u201dHerman\u63a5\u7740\u8bf4\u9053\uff0c\u201c\u6211\u4eec\u53ef\u4ee5\u76d1\u6d4b\u8bb8\u591a\u773c\u6cea\u4e2d\u7684\u5316\u5408\u7269\u3002\u4e14\u7531\u4e8e\u4f20\u611f\u5668\u662f\u900f\u660e\u7684\uff0c\u8fd9\u79cd\u76d1\u6d4b\u5e76\u4e0d\u4f1a\u963b\u788d\u89c6\u529b\u3002\u56e0\u6b64\u4e5f\u5728\u9690\u5f62\u773c\u955c\u4e0a\u83b7\u5f97\u4e86\u66f4\u591a\u7684\u611f\u6d4b\u7a7a\u95f4\u3002\u201d<\/p>\n<p>\u867d\u7136OSU\u7814\u7a76\u4eba\u5458\u6210\u529f\u4f7f\u7528\u900f\u660e\u6750\u6599IGZO\u7814\u5236\u51fa\u4f20\u611f\u5668\uff0c\u4f46\u8461\u8404\u7cd6\u76d1\u6d4b\u53ea\u662f\u4ed6\u4eec\u957f\u671f\u76ee\u6807\u91cc\u7684\u4e00\u90e8\u5206\u3002\u9664\u6b64\u4e4b\u5916\uff0c\u4ed6\u4eec\u8fd8\u5e0c\u671b\u80fd\u591f\u6839\u636e\u8461\u8404\u7cd6\u6307\u6807\u8bfb\u6570\u63d0\u4f9b\u6b63\u786e\u5242\u91cf\u7684\u80f0\u5c9b\u7d20\u3002\u8fd9\u9879\u6280\u672f\u8fd8\u9700\u8981\u5f00\u53d1\u5177\u6709\u4eba\u5de5\u80f0\u817a\u529f\u80fd\u7684\u6cf5\u9001\u88c5\u7f6e\uff0c\u4ee5\u53ca\u5c06\u8461\u8404\u7cd6\u8bfb\u6570\u53d1\u9001\u5230\u4eba\u5de5\u80f0\u817a\u7684\u901a\u4fe1\u7cfb\u7edf\u3002\u76ee\u524d\u8fd9\u9879\u6280\u672f\u8fd8\u505c\u7559\u5728\u8bbe\u60f3\u5c42\u9762\u3002<\/p>\n<p>Herman\u8865\u5145\u8bf4\u9053\uff1a\u201c\u6211\u4eec\u4e0b\u4e00\u6b65\u8981\u505a\u7684\u662f\u5145\u5206\u62d3\u5c55\u901a\u4fe1\u65b9\u9762\u7684\u529f\u80fd\uff0c\u56e2\u961f\u5c06\u81f4\u529b\u4e8e\u5c06\u611f\u6d4b\u548c\u901a\u4fe1\u5143\u4ef6\u5e94\u7528\u5230\u6574\u526f\u9690\u5f62\u773c\u955c\u3002\u201d<\/p>\n<p>\u539f\u6587\u94fe\u63a5: <a href=\"http:\/\/spectrum.ieee.org\/nanoclast\/semiconductors\/devices\/nanostructred-transistor-enables-glucose-sensing-contact-lenss\" target=\"_blank\">Nanostructred Transistor Enables Glucose Sensing Contact Lens<\/a>.<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.rsc.org\/en\/Content\/ArticleLanding\/2016\/NR\/C6NR05134K#!divAbstract\" target=\"_blank\">A field effect glucose sensor with a nanostructured amorphous In\u2013Ga\u2013Zn\u2013O network<\/a>.<\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u4e01\u83f2\u83f2\u4f9b\u7a3f\uff0c\u9a6c\u79cb\u6668\u7ffb\u8bd1\uff0c\u65f6\u51b0\u9065\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u4f20\u7edf\u7684\u8461\u8404\u7cd6\u4f20\u611f\u5668\u4ec5\u80fd\u5b9e\u65f6\u68c0\u6d4b\u8840\u7cd6\u9ad8\u4f4e\uff0c\u6765\u81ea\u4fc4\u52d2\u5188\u5dde\u7acb\u5927\u5b66\u7684\u7814\u7a76\u56e2\u961f\u81f4\u529b\u4e8e\u5c06\u8461\u8404\u7cd6\u4f20\u611f\u5668\u4e0e\u9690\u5f62\u773c\u955c\u6709\u673a\u7ed3\u5408\uff0c\u5b9e\u73b0\u5b9e\u65f6\u68c0\u6d4b\u548c\u6ce8\u5c04\u80f0\u5c9b\u7d20\u7684\u53cc\u91cd\u529f\u80fd\uff0c\u7eb3\u7c73\u7ed3&#8230;<\/p>\n","protected":false},"author":230,"featured_media":51615,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-51614","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/51614"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=51614"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/51614\/revisions"}],"predecessor-version":[{"id":51667,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/51614\/revisions\/51667"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/51615"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=51614"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=51614"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=51614"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}