{"id":55060,"date":"2016-12-10T06:30:17","date_gmt":"2016-12-09T22:30:17","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=55060"},"modified":"2016-12-09T20:30:24","modified_gmt":"2016-12-09T12:30:24","slug":"%e9%85%b7%ef%bc%81-%e8%8b%b1%e5%9b%bd%e7%a0%94%e5%8f%91%e5%a4%aa%e7%a9%ba3d%e6%89%93%e5%8d%b0%e8%ae%be%e5%a4%87","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=55060","title":{"rendered":"\u9177\uff01\u2014\u2014\u82f1\u56fd\u7814\u53d1\u592a\u7a7a3D\u6253\u5370\u8bbe\u5907"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u5728\u592a\u7a7a\u8fdb\u884c3D\u6253\u5370\uff01\u662f\u4e0d\u662f\u89c9\u5f97\u6709\u70b9\u4e0d\u53ef\u601d\u8bae\uff1f\u4f46\u662f\u8fd9\u5e76\u4e0d\u662f\u4e0d\u53ef\u80fd\u7684\u4e8b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-55847\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/iss-sts-3d_printer_nasa4.jpg\" alt=\"iss-sts-3d_printer_nasa4\" width=\"600\" height=\"353\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/iss-sts-3d_printer_nasa4.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/iss-sts-3d_printer_nasa4-300x177.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u7531\u4e8e\u5728\u592a\u7a7a\u4e2d\u5bf9\u53d7\u635f\u90e8\u4ef6\u8fdb\u884c\u4fee\u7406\u8f83\u4e3a\u56f0\u96be\uff0c\u4ece\u5730\u7403\u53d1\u9001\u5907\u4ef6\u7684\u8ddd\u79bb\u4e5f\u5c06\u53d8\u5f97\u8d8a\u6765\u8d8a\u8fdc\uff0c\u82f1\u56fd\u4f2f\u660e\u7ff0\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u5f00\u59cb\u7814\u53d1\u80fd\u7528\u4e8e\u592a\u7a7a3D\u6253\u5370\u7684\u8bbe\u5907\uff0c\u8fd9\u9879\u7814\u7a76\u6b27\u6d32\u822a\u5929\u5c40\u7684\u8d44\u52a9\u4e0b\u8fdb\u884c\u7684\u3002<\/p>\n<p>\u636e\u7814\u7a76\u4eba\u5458\u4ecb\u7ecd\uff0c\u5982\u679c\u4e00\u4e2a\u7ec4\u4ef6\uff0c\u4f8b\u5982\u652f\u67b6\u6216\u94f0\u94fe\uff0c\u5728\u592a\u7a7a\u4e2d\u88ab\u7834\u574f\uff0c\u60f3\u8981\u5bf9\u5176\u8fdb\u884c\u4fee\u7406\u53ef\u80fd\u5b58\u5728\u4e00\u5b9a\u7684\u56f0\u96be\uff0c\u4e0d\u4ec5\u6210\u672c\u8f83\u9ad8\uff0c\u800c\u4e14\u5177\u6709\u6f5c\u5728\u7684\u5371\u9669\u3002\u76ee\u524d\u7684\u89e3\u51b3\u529e\u6cd5\u662f\u5c06\u66ff\u6362\u96f6\u4ef6\u4ece\u5730\u7403\u53d1\u5c04\u5230\u56fd\u9645\u7a7a\u95f4\u7ad9\uff08ISS\uff09\u4e0a\u3002\u7136\u800c\uff0c\u968f\u7740\u4eba\u7c7b\u63a2\u7d22\u592a\u7a7a\u7684\u811a\u6b65\u8d8a\u884c\u8d8a\u8fdc\uff0c\u4ece\u5730\u7403\u4e0a\u53d1\u9001\u5907\u4ef6\u4e5f\u53d8\u5f97\u8d8a\u6765\u8d8a\u4e0d\u53ef\u884c\u3002\u592a\u7a7a3D\u6253\u5370\u7684\u53d1\u5c55\u5c06\u5e2e\u52a9\u5b87\u822a\u5458\u901a\u8fc7\u9ad8\u6548\u5236\u9020\u66ff\u4ee3\u54c1\u89e3\u51b3\u8fd9\u4e2a\u95ee\u9898\u3002\u76ee\u524d\u7684\u7814\u7a76\u53ef\u80fd\u610f\u5473\u7740\u67d0\u4e9b\u8bbe\u5907\u5728\u592a\u7a7a\u4e2d\u80fd\u591f\u88ab\u5b8c\u5168\u5236\u5907\u51fa\u6765\u3002<\/p>\n<p>\u8be5\u8fd1\u51c0\u6210\u5f62\u4e2d\u5fc3\u6b63\u5728\u4e0e\u67d0\u4e9b\u8bbe\u8ba1\u548c\u5236\u9020\u53d1\u52a8\u673a\u4ee5\u53ca\u5176\u4ed6\u98de\u673a\u90e8\u4ef6\u7684\u516c\u53f8\u53d1\u5c55\u6218\u7565\u4f19\u4f34\u5173\u7cfb\u3002\u5305\u62ec\u5171\u540c\u7814\u7a76\u98de\u673a\u7ec4\u4ef6\u7684\u65b0\u6750\u6599\u548c\u751f\u4ea7\u65b9\u6cd5\uff0c\u4ee5\u53ca\u5bfb\u627e\u80fd\u591f\u51cf\u5c11\u5236\u9020\u6240\u7528\u80fd\u91cf\u5e76\u51cf\u8f7b\u98de\u673a\u6574\u4f53\u91cd\u91cf\u7684\u65b9\u6cd5\u3002<\/p>\n<p>\u4e3a\u4e86\u6d4b\u8bd5PhotAM\u7cfb\u7edf\u7684\u53ef\u884c\u6027\uff0c\u5148\u8fdb\u6750\u6599\u4e0e\u52a0\u5de5\u5b9e\u9a8c\u5ba4\uff08AMPLab\uff09\u7684\u7814\u7a76\u5c0f\u7ec4\u5bf9\u5728\u4eba\u5de5\u5931\u91cd\u6761\u4ef6\u4e0b\u8fdb\u884c\u629b\u7269\u7ebf\u98de\u884c\u7684\u8bbe\u5907\u6a21\u578b\u8fdb\u884c\u4e86\u6d4b\u8bd5\u3002\u4e3a\u4e86\u68c0\u9a8c\u7406\u8bba\u4e0e\u6280\u672f\u4e0a\u7684\u53ef\u884c\u6027\uff0c\u79d1\u5b66\u5bb6\u4eec\u51cf\u5c0f\u91cd\u529b\uff0c\u4f7f\u7528\u914d\u6709\u4e13\u4e1a\u8bbe\u5907\u7684\u98de\u673a\uff0c\u5bf9\u8be5\u8bbe\u5907\u80fd\u5426\u5728\u96f6\u91cd\u529b\u6761\u4ef6\u4e0b\u6b63\u5e38\u8fd0\u884c\u8fdb\u884c\u4e86\u6d4b\u8bd5\uff0c\u4ece\u800c\u9a8c\u8bc1\u4e86\u5176\u6709\u6548\u6027\u3002<\/p>\n<p>\u4f2f\u660e\u7ff0\u5927\u5b66\u7684\u5b66\u8005\u4eec\u76ee\u524d\u4e5f\u5728\u8003\u8651\u5c06\u949b\u3001\u94dd\u548c\u954d\u8d85\u5408\u91d1\u7ed3\u6784\u7528\u4e8e\u5de5\u4e1a\u5b9e\u8df5\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.materialstoday.com\/additive-manufacturing\/news\/3d-printing-in-space\/\" target=\"_blank\">3D printing in space<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u6768\u8d85\u63d0\u4f9b\u7d20\u6750\uff0c\u9ec4\u4e9a\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u5728\u592a\u7a7a\u8fdb\u884c3D\u6253\u5370\uff01\u662f\u4e0d\u662f\u89c9\u5f97\u6709\u70b9\u4e0d\u53ef\u601d\u8bae\uff1f\u4f46\u662f\u8fd9\u5e76\u4e0d\u662f\u4e0d\u53ef\u80fd\u7684\u4e8b\u3002 \u7531\u4e8e\u5728\u592a\u7a7a\u4e2d\u5bf9\u53d7\u635f\u90e8\u4ef6\u8fdb\u884c\u4fee\u7406\u8f83\u4e3a\u56f0\u96be\uff0c\u4ece\u5730\u7403\u53d1\u9001\u5907\u4ef6\u7684\u8ddd\u79bb\u4e5f\u5c06\u53d8\u5f97\u8d8a\u6765\u8d8a\u8fdc\uff0c\u82f1&#8230;<\/p>\n","protected":false},"author":954,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[28],"class_list":["post-55060","post","type-post","status-publish","format-standard","hentry","category-keji","tag-3d"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/55060"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/954"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=55060"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/55060\/revisions"}],"predecessor-version":[{"id":55848,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/55060\/revisions\/55848"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=55060"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=55060"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=55060"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}