{"id":56677,"date":"2016-12-18T14:06:11","date_gmt":"2016-12-18T06:06:11","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=56677"},"modified":"2016-12-18T14:06:54","modified_gmt":"2016-12-18T06:06:54","slug":"%e6%9c%ba%e5%99%a8%e5%ad%a6%e4%b9%a0%e9%a2%84%e6%b5%8b2%e7%bb%b4%e6%9d%90%e6%96%99%e5%bb%ba%e6%a8%a1","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=56677","title":{"rendered":"\u673a\u5668\u5b66\u4e60\u53ef\u4ee5\u9884\u6d4b2\u7ef4\u6750\u6599\u5efa\u6a21\u4e86"},"content":{"rendered":"<p><strong><b>\u6750\u6599\u725b\u6ce8<\/b><\/strong>\uff1a\u4f5c\u4e3a\u4eba\u5de5\u667a\u80fd\u7684\u6838\u5fc3\u2014\u2014\u673a\u5668\u5b66\u4e60\uff0c\u5176\u5e94\u7528\u904d\u5e03\u4eba\u5de5\u667a\u80fd\u7684\u5404\u4e2a\u9886\u57df\u3002\u65e5\u524d\uff0c\u7f8e\u56fd\u963f\u8d21\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u53d1\u73b0\u4e86\u673a\u5668\u5b66\u4e60\u7684\u65b0\u5e94\u7528\uff0c\u7387\u5148\u5229\u7528\u673a\u5668\u5b66\u4e60\u8fdb\u884c\u4e8c\u7ef4\u6750\u6599\u7684\u5efa\u6a21\uff0c\u8fd9\u5c06\u5bf9\u53d1\u73b0\u548c\u5f00\u53d1\u65b0\u6750\u6599\u6709\u5de8\u5927\u4fc3\u8fdb\u4f5c\u7528\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-56678\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/\u56fe\u7247\u4e0a\u5927\u90d1\u4e3d11.jpg\" alt=\"%e5%9b%be%e7%89%87%e4%b8%8a%e5%a4%a7%e9%83%91%e4%b8%bd11\" width=\"650\" height=\"300\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/\u56fe\u7247\u4e0a\u5927\u90d1\u4e3d11.jpg 650w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/\u56fe\u7247\u4e0a\u5927\u90d1\u4e3d11-300x138.jpg 300w\" sizes=\"(max-width: 650px) 100vw, 650px\" \/><br \/>\n\u4e0a\u56fe\u4e3a\u9521\u70ef\u7684\u201c\u8352\u539f\u201d\uff1a\u9521\u70ef\u6bd4\u5b83\u7684\u201c\u8868\u4eb2\u201d\u77f3\u58a8\u70ef\u548c\u7845\u70f7\u66f4\u67d4\u8f6f\u3001\u6ce2\u7eb9\u66f4\u591a\u3002\u673a\u5668\u5b66\u4e60\uff0c\u662f\u901a\u8fc7\u5927\u91cf\u6570\u636e\u8bad\u7ec3\u4f7f\u8ba1\u7b97\u673a\u8fdb\u884c\u6a21\u5f0f\u8bc6\u522b\u548c\u9884\u6d4b\uff0c\u53ef\u4ee5\u5e2e\u52a9\u533b\u751f\u66f4\u51c6\u786e\u5730\u8bca\u65ad\u75be\u75c5\uff0c\u5728\u91d1\u878d\u5e02\u573a\u4e2d\u9884\u6d4b\u80a1\u7968\u7684\u6da8\u8dcc\u3002\u73b0\u5728\u6750\u6599\u79d1\u5b66\u5bb6\u5f00\u521b\u4e86\u673a\u5668\u5b66\u4e60\u7684\u53e6\u4e00\u4e2a\u91cd\u8981\u5e94\u7528\u2014\u2014\u52a0\u5feb\u65b0\u6750\u6599\u7684\u53d1\u73b0\u548c\u5f00\u53d1\u3002<\/p>\n<p>\u7f8e\u56fd\u80fd\u6e90\u90e8\uff08DOE\uff09\u963f\u8d21\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u7684\u7eb3\u7c73\u6750\u6599\u548c\u5148\u8fdb\u5149\u5b50\u6e90\u4e2d\u5fc3\u7684\u7814\u7a76\u4eba\u5458\uff08\u7531\u8ba1\u7b97\u79d1\u5b66\u5bb6Subramanian Sankaranarayanan\u9886\u5bfc\u7684\u4e00\u4e2a\u7814\u7a76\u56e2\u961f\uff09\u5728<em><i>The Journal of Physical Chemistry Letters<\/i><\/em>\u4e0a\u53d1\u8868\u4e86\u4e00\u9879\u7814\u7a76\uff0c\u58f0\u79f0\u5229\u7528\u673a\u5668\u5b66\u4e60\u53ef\u4ee5\u51c6\u786e\u9884\u6d4b\u7eb3\u7c73\u6750\u6599\u7684\u7269\u7406\u3001\u5316\u5b66\u548c\u673a\u68b0\u6027\u80fd\u3002\u4ed6\u4eec\u7528\u673a\u5668\u5b66\u4e60\u521b\u5efa\u4e86\u9996\u4e2a\u539f\u5b50\u7ea7\u6a21\u578b\uff0c\u51c6\u786e\u9884\u6d4b\u4e86\u9521\u70ef\u8fd9\u79cd\u7531\u5355\u539f\u5b50\u539a\u7684\u9521\u7247\u5236\u6210\u7684\u4e8c\u7ef4\u6750\u6599\u7684\u70ed\u6027\u80fd\u3002<\/p>\n<p>\u8fd9\u9879\u7814\u7a76\u662f\u5e94\u7528\u673a\u5668\u5b66\u4e60\u8fdb\u884c\u6750\u6599\u5efa\u6a21\u7684\u9996\u4f8b\uff0c\u4e0e\u8fc7\u53bb\u7684\u5efa\u6a21\u65b9\u6cd5\u76f8\u6bd4\uff0c\u8fd9\u79cd\u5efa\u6a21\u65b9\u6cd5\u53ef\u4ee5\u66f4\u51c6\u786e\u5730\u9884\u6d4b\u6750\u6599\u7279\u6027\u3002<\/p>\n<p>\u963f\u8d21\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u7684\u535a\u58eb\u540e\u7814\u7a76\u8005Mathew Cherukara\u8bf4\uff1a\u201c\u9884\u6d4b\u5efa\u6a21\u5bf9\u65b0\u6750\u6599\u7684\u5f00\u53d1\u975e\u5e38\u91cd\u8981\uff0c\u5305\u62ec\u6295\u8d44\u751f\u4ea7\u524d\u7684\u4e00\u5207\u51c6\u5907\u5de5\u4f5c\uff0c\u6bd4\u5982\u4e86\u89e3\u65b0\u6750\u6599\u7684\u7279\u70b9\u3001\u5bf9\u4e0d\u540c\u7684\u523a\u6fc0\u7684\u54cd\u5e94\u72b6\u6001\uff0c\u4ee5\u53ca\u5982\u4f55\u6709\u6548\u63d0\u9ad8\u5546\u4e1a\u5e94\u7528\u6027\u3002\u201d<\/p>\n<p>\u4f20\u7edf\u7684\u539f\u5b50\u5c3a\u5ea6\u7684\u6750\u6599\u5efa\u6a21\u4e00\u822c\u9700\u8981\u5f00\u53d1\u6570\u5e74\u65f6\u95f4\uff0c\u800c\u4e14\u7814\u7a76\u4eba\u5458\u8fd8\u4e0d\u5f97\u4e0d\u5f88\u5927\u7a0b\u5ea6\u4e0a\u4f9d\u9760\u76f4\u89c9\u6765\u786e\u5b9a\u5efa\u6a21\u7684\u53c2\u6570\u3002\u7136\u800c\uff0cCherukara\u53ca\u5176\u540c\u4e8b\u901a\u8fc7\u4f7f\u7528\u673a\u5668\u5b66\u4e60\uff0c\u4e0d\u4ec5\u51cf\u5c11\u4e86\u4eba\u5458\u6295\u5165\uff0c\u800c\u4e14\u5c06\u7cbe\u786e\u5efa\u6a21\u7684\u65f6\u95f4\u7f29\u77ed\u5230\u4e86\u51e0\u4e2a\u6708\u3002<\/p>\n<p>\u963f\u8d21\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u535a\u58eb\u540e\u7814\u7a76\u5458Badri Narayanan\u8bf4\uff1a\u201c\u6211\u4eec\u5c06\u6765\u81ea\u5b9e\u9a8c\u6216\u57fa\u4e8e\u7406\u8bba\u8ba1\u7b97\u5f97\u5230\u7684\u6570\u636e\u8f93\u5165\u7535\u8111\uff0c\u7136\u540e\u5411\u673a\u5668\u63d0\u95ee\uff0c\u6bd4\u5982\u53ef\u4ee5\u7ed9\u51fa\u6750\u6599\u6240\u6709\u6027\u80fd\u7684\u6a21\u578b\u5417\uff1f\u53ef\u4ee5\u901a\u8fc7\u4f18\u5316\u6750\u6599\u7ed3\u6784\uff0c\u63a7\u5236\u7f3a\u9677\u6216\u662f\u5b9a\u5236\u6750\u6599\u6765\u83b7\u5f97\u7279\u5b9a\u7684\u6240\u9700\u6027\u80fd\u5417\uff1f\u201d<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-56679\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/\u56fe\u7247\u4e0a\u5927\u90d1\u4e3d22.jpg\" alt=\"%e5%9b%be%e7%89%87%e4%b8%8a%e5%a4%a7%e9%83%91%e4%b8%bd22\" width=\"650\" height=\"300\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/\u56fe\u7247\u4e0a\u5927\u90d1\u4e3d22.jpg 650w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/\u56fe\u7247\u4e0a\u5927\u90d1\u4e3d22-300x138.jpg 300w\" sizes=\"(max-width: 650px) 100vw, 650px\" \/><br \/>\n\u963f\u8d21\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u7814\u7a76\u56e2\u961f\u7387\u5148\u4f7f\u7528\u673a\u5668\u5b66\u4e60\u8fdb\u884c\u4e8c\u7ef4\u6750\u6599\u5efa\u6a21\u3002\u4e0e\u5927\u591a\u6570\u4f20\u7edf\u6a21\u578b\u4e0d\u540c\uff0c\u673a\u5668\u5b66\u4e60\u6a21\u578b\u80fd\u591f\u51c6\u786e\u6355\u6349\u952e\u7684\u5f62\u6210\u548c\u65ad\u88c2\u8fc7\u7a0b\uff0c\u673a\u5668\u5b66\u4e60\u6a21\u578b\u4e0d\u4ec5\u53ef\u4ee5\u66f4\u53ef\u9760\u5730\u9884\u6d4b\u6750\u6599\u6027\u80fd\uff08\u4f8b\u5982\u70ed\u5bfc\u7387\uff09\uff0c\u800c\u4e14\u53ef\u4ee5\u4f7f\u7814\u7a76\u4eba\u5458\u51c6\u786e\u83b7\u53d6\u5316\u5b66\u53cd\u5e94\uff0c\u4ece\u800c\u66f4\u597d\u5730\u4e86\u89e3\u7279\u6b8a\u6750\u6599\u7684\u5408\u6210\u65b9\u6cd5\u3002<\/p>\n<p>\u673a\u5668\u5b66\u4e60\u6784\u5efa\u6a21\u578b\u7684\u53e6\u4e00\u4e2a\u4f18\u70b9\uff0c\u662f\u8fc7\u7a0b\u4e0d\u53d7\u6750\u6599\u79cd\u7c7b\u9650\u5236\uff0c\u8fd9\u610f\u5473\u7740\u7814\u7a76\u4eba\u5458\u53ef\u4ee5\u540c\u65f6\u7814\u7a76\u591a\u79cd\u4e0d\u540c\u7684\u6750\u6599\uff0c\u5e76\u7528\u673a\u5668\u5b66\u4e60\u7814\u7a76\u5404\u79cd\u4e0d\u540c\u5143\u7d20\u53ca\u5176\u5316\u5408\u8fc7\u7a0b\u3002<\/p>\n<p>\u8fd9\u9879\u7814\u7a76\u4e2d\u7684\u8ba1\u7b97\u6a21\u578b\u7814\u7a76\u5bf9\u8c61\u9521\u70ef\uff0c\u662f\u4e00\u79cd\u7531\u9521\u5236\u6210\u7684\u6750\u6599\uff0c\u8fd1\u5e74\u6765\u5907\u53d7\u5173\u6ce8\u3002\u4ece2004\u5e74\u77f3\u58a8\u70ef\u7684\u53d1\u73b0\u5230\u73b0\u5728\u7684\u9521\u70ef\uff0c\u53ef\u4ee5\u770b\u51fa\u4eba\u4eec\u5bf9\u4e8c\u7ef4\u6750\u6599\u7684\u5174\u8da3\u65e5\u76ca\u589e\u957f\u3002\u867d\u7136\u9521\u70ef\u79bb\u5546\u4e1a\u5316\u5e94\u7528\u8fd8\u975e\u5e38\u9065\u8fdc\uff0c\u4f46\u7814\u7a76\u4eba\u5458\u53d1\u73b0\u5b83\u5728\u4e00\u4e9b\u7eb3\u7c73\u5668\u4ef6\u7684\u70ed\u7ba1\u7406\uff08\u70ed\u8c03\u8282\uff09\u4e2d\u5177\u6709\u5de8\u5927\u7684\u6f5c\u5728\u5e94\u7528\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/phys.org\/news\/2016-12-machine-enables-d-materials.html\" target=\"_blank\">Machine learning enables predictive modeling of 2-D materials<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acs.jpclett.6b01562\" target=\"_blank\"><span class=\"hlFld-Title\"><i>Ab Initio<\/i>-Based Bond Order Potential to Investigate Low Thermal Conductivity of Stanene Nanostructures<\/span><\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u9f99\u9a91\u58eb\u63d0\u4f9b\u7d20\u6750\uff0c\u90d1\u4e3d\u4ed9\u7f16\u8bd1\uff0c\u5218\u5b87\u9f99\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u4f5c\u4e3a\u4eba\u5de5\u667a\u80fd\u7684\u6838\u5fc3\u2014\u2014\u673a\u5668\u5b66\u4e60\uff0c\u5176\u5e94\u7528\u904d\u5e03\u4eba\u5de5\u667a\u80fd\u7684\u5404\u4e2a\u9886\u57df\u3002\u65e5\u524d\uff0c\u7f8e\u56fd\u963f\u8d21\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\u53d1\u73b0\u4e86\u673a\u5668\u5b66\u4e60\u7684\u65b0\u5e94\u7528\uff0c\u7387\u5148\u5229\u7528\u673a\u5668\u5b66\u4e60\u8fdb\u884c\u4e8c\u7ef4\u6750\u6599\u7684\u5efa\u6a21\uff0c\u8fd9\u5c06&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[258],"class_list":["post-56677","post","type-post","status-publish","format-standard","hentry","category-keji","tag-2d"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/56677"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=56677"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/56677\/revisions"}],"predecessor-version":[{"id":57374,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/56677\/revisions\/57374"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=56677"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=56677"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=56677"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}