{"id":58502,"date":"2016-12-31T06:30:05","date_gmt":"2016-12-30T22:30:05","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=58502"},"modified":"2016-12-31T10:14:14","modified_gmt":"2016-12-31T02:14:14","slug":"%e7%9f%b3%e5%a2%a8%e7%83%af%e7%9a%84%e6%98%a5%e5%a4%a9%e6%9d%a5%e4%ba%86%ef%bc%81","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=58502","title":{"rendered":"\u77f3\u58a8\u70ef\u7684\u6625\u5929\u6765\u4e86\uff01\u82f1\u5f00\u53d1\u5ec9\u4ef7\u5546\u4e1a\u5316\u751f\u4ea7\u5de5\u827a"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u77f3\u58a8\u70ef\u6027\u80fd\u4f18\u8d8a\uff0c\u4f46\u5b83\u9020\u4ef7\u8d35\u554a\u3002\u94b1\u4e0d\u662f\u95ee\u9898\uff0c\u4f46\u6210\u54c1\u5668\u4ef6\u90a3\u53eb\u4e00\u4e2a\u96be\u4ea7\u554a\u3002\u522b\u6101\u4e86\uff0c\u65b0\u65b9\u6cd5\u9a6c\u4e0a\u89e3\u51b3\u6240\u6709\u95ee\u9898\uff0c\u77f3\u58a8\u70ef\u7684\u6625\u5929\u6765\u4e86\uff01<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-58503\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/1-59.jpg\" alt=\"\" width=\"580\" height=\"360\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/1-59.jpg 580w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/12\/1-59-300x186.jpg 300w\" sizes=\"(max-width: 580px) 100vw, 580px\" \/><\/p>\n<p>\u82f1\u56fd\u57c3\u514b\u585e\u7279\u77f3\u58a8\u70ef\u79d1\u5b66\u4e2d\u5fc3\u7684\u4e00\u4e2a\u5de5\u7a0b\u5e08\u56e2\u961f\u5f00\u53d1\u4e86\u4e00\u79cd\u5ec9\u4ef7\u3001\u7b80\u5355\u5b9e\u73b0\u77f3\u58a8\u70ef\u5546\u4e1a\u5316\u751f\u4ea7\u7684\u65b9\u6cd5\uff0c\u8be5\u65b9\u6cd5\u53ef\u76f4\u63a5\u5728\u7684\u94dc\u57fa\u4f53\u4e0a\u5236\u9020\u5b8c\u6574\u7684\u9635\u5217\u5668\u4ef6\u3002\u8fd9\u79cd\u5546\u7528\u5668\u4ef6\u53ef\u4ee5\u88ab\u76f4\u63a5\u8f6c\u79fb\u5230\u4f8b\u5982\u7845\u3001\u5851\u6599\u751a\u81f3\u7eba\u7ec7\u54c1\u8fd9\u6837\u7684\u57fa\u5e95\u4e0a\u3002<\/p>\n<p>\u6765\u81ea\u57c3\u514b\u585e\u7279\u5de5\u7a0b\u90e8\u3001\u540c\u65f6\u4e5f\u662f\u8bba\u6587\u4f5c\u8005\u4e4b\u4e00\u7684David Wright\u6559\u6388\u8bf4\uff1a\u201c\u4f7f\u7528\u77f3\u58a8\u70ef\u751f\u4ea7\u5668\u4ef6\u7684\u5e38\u89c4\u65b9\u6cd5\u5f88\u8017\u65f6\uff0c\u590d\u6742\u4e14\u6602\u8d35\uff0c\u5e76\u4e14\u6d89\u53ca\u8bb8\u591a\u5305\u62ec\u77f3\u58a8\u70ef\u751f\u957f\u3001\u819c\u7684\u8f6c\u79fb\u3001\u5149\u523b\u56fe\u6848\u5316\u548c\u91d1\u5c5e\u63a5\u89e6\u6c89\u79ef\u5de5\u827a\u6b65\u9aa4\u3002\u76f8\u6bd4\u4e4b\u4e0b\uff0c\u6211\u4eec\u7684\u65b0\u65b9\u6cd5\u7b80\u5355\u5f97\u591a\uff0c\u8fd9\u5f88\u53ef\u80fd\u5f00\u542f\u5ec9\u4ef7\u77f3\u58a8\u70ef\u5668\u4ef6\u5e94\u7528\u4e8e\u5305\u62ec\u6c14\u4f53\u548c\u751f\u7269\u533b\u5b66\u4f20\u611f\u5668\u4ee5\u53ca\u89e6\u6478\u5c4f\u663e\u793a\u5668\u7b49\u5f88\u591a\u91cd\u8981\u9886\u57df\u7684\u5927\u95e8\u3002\u201d<\/p>\n<p>\u4e3a\u4e86\u8bc1\u660e\u65b0\u5de5\u827a\uff0c\u8be5\u56e2\u961f\u4f7f\u7528\u5ec9\u4ef7\u7684\u666e\u901a\u6676\u5706\u548c\u5377\u5bf9\u5377\u5236\u9020\u6280\u672f\uff0c\u751f\u4ea7\u51fa\u4e86\u4e00\u79cd\u7075\u6d3b\u4e14\u5b8c\u5168\u900f\u660e\u7684\u6c27\u5316\u77f3\u58a8\u70ef\u57fa\u4f53\u6e7f\u5ea6\u4f20\u611f\u5668\uff0c\u4e14\u6027\u80fd\u4f18\u4e8e\u76ee\u524d\u4f7f\u7528\u7684\u5546\u4e1a\u4f20\u611f\u5668\u3002<\/p>\n<p>\u540c\u6837\u6765\u81ea\u57c3\u514b\u585e\u7279\u5de5\u7a0b\u90e8\u7684\u5408\u8457\u8005Moneter Craciun\u6559\u6388\u8865\u5145\u8bf4\uff1a\u201c\u57c3\u514b\u585e\u7279\u5927\u5b66\u662f\u5168\u7403\u4ece\u4e8b\u77f3\u58a8\u70ef\u7814\u7a76\u7684\u6743\u5a01\u673a\u6784\u4e4b\u4e00\uff0c\u8fd9\u9879\u65b0\u7684\u7814\u7a76\u53ea\u662f\u6211\u4eec\u63a8\u52a8\u77f3\u58a8\u70ef\u5de5\u4e1a\u9769\u547d\u613f\u666f\u4e2d\u7684\u6700\u65b0\u4e00\u6b65\u3002\u5236\u9020\u9ad8\u8d28\u91cf\uff0c\u4f4e\u6210\u672c\u7684\u77f3\u58a8\u70ef\u5668\u4ef6\u662f\u5b9e\u73b0\u8fd9\u4e00\u613f\u666f\u4e0d\u53ef\u6216\u7f3a\u7684\u4e00\u90e8\u5206\uff0c\u6211\u4eec\u6700\u65b0\u7684\u5de5\u4f5c\u662f\u6316\u6398\u77f3\u58a8\u70ef\u771f\u6b63\u6f5c\u529b\u7684\u4e00\u4e2a\u91cd\u5927\u8fdb\u6b65\u3002\u201d<\/p>\n<p>\u57c3\u514b\u585e\u7279\u5de5\u7a0b\u56e2\u961f\u7531Arseny Alexeev\u535a\u58eb\uff0cMatthew Barnes\uff0cKarthik Nagareddy\u535a\u58eb\u548cCraciun\u4ee5\u53caWright\u6559\u6388\u7ec4\u6210\uff0c\u8fd9\u9879\u5de5\u4f5c\u662f\u6b27\u76df\u8d44\u52a9\u7684FP7\u9879\u76eeCareRAMM\u7684\u4e00\u90e8\u5206\u3002<\/p>\n<p>\u7528\u4e8e\u5236\u9020\u5177\u6709\u9009\u62e9\u6027\u539f\u4f4d\u529f\u80fd\u5316\u548c\u56fe\u6848\u5316\u7684\u5927\u9762\u79efCVD\u77f3\u58a8\u70ef\u57fa\u5668\u4ef6\u7684\u7b80\u5355\u7684\u65b0\u5de5\u827a\u53d1\u8868\u5728\u4e86\u6700\u65b0\u7f51\u7edc\u7248\u82f1\u56fd\u7269\u7406\u5b66\u4f1a\uff08the Institute of Physics\uff09\u9876\u520a\u2014\u20142D Materials\u4e0a\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/scitechdaily.com\/new-method-could-accelerate-graphene-production\/\" target=\"_blank\">New Method Could Accelerate Graphene Production.<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/iopscience.iop.org\/article\/10.1088\/2053-1583\/4\/1\/011010\" target=\"_blank\">A simple process for the fabrication of large-area CVD graphene based devices via selective in situ functionalization and patterning.<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u5f20\u83b9\u63d0\u4f9b\u7d20\u6750\uff0c\u8c37\u661f\u96e8\u7f16\u8bd1\uff0c\u6731\u6653\u79c0\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u77f3\u58a8\u70ef\u6027\u80fd\u4f18\u8d8a\uff0c\u4f46\u5b83\u9020\u4ef7\u8d35\u554a\u3002\u94b1\u4e0d\u662f\u95ee\u9898\uff0c\u4f46\u6210\u54c1\u5668\u4ef6\u90a3\u53eb\u4e00\u4e2a\u96be\u4ea7\u554a\u3002\u522b\u6101\u4e86\uff0c\u65b0\u65b9\u6cd5\u9a6c\u4e0a\u89e3\u51b3\u6240\u6709\u95ee\u9898\uff0c\u77f3\u58a8\u70ef\u7684\u6625\u5929\u6765\u4e86\uff01 \u82f1\u56fd\u57c3\u514b\u585e\u7279\u77f3\u58a8\u70ef\u79d1\u5b66\u4e2d\u5fc3\u7684\u4e00&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[46],"class_list":["post-58502","post","type-post","status-publish","format-standard","hentry","category-keji","tag-graphene"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/58502"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=58502"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/58502\/revisions"}],"predecessor-version":[{"id":59456,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/58502\/revisions\/59456"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=58502"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=58502"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=58502"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}