{"id":60239,"date":"2017-01-11T06:30:13","date_gmt":"2017-01-10T22:30:13","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=60239"},"modified":"2017-01-08T16:02:45","modified_gmt":"2017-01-08T08:02:45","slug":"%e9%87%91%e5%b1%9e%e4%b8%8e%e6%b6%82%e5%b1%82%e4%b9%8b%e9%97%b4%e7%9a%84%e8%9c%9c%e6%b1%81%e7%88%b1%e6%81%8b","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=60239","title":{"rendered":"\u91d1\u5c5e\u4e0e\u6d82\u5c42\u4e4b\u95f4\u7684\u871c\u6c41\u7231\u604b"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u5c06\u6d82\u5c42\u4e0e\u91d1\u5c5e\u7ed3\u5408\u5e76\u4e0d\u7a00\u5947\uff0c\u53ef\u5c06\u5b83\u5e94\u7528\u4e8e\u6027\u80fd\u8981\u6c42\u6781\u9ad8\u7684\u822a\u7a7a\u9886\u57df\u5462<strong>\uff1f<\/strong>\u90a3\u4e48\u5982\u4f55\u63d0\u9ad8\u6d82\u5c42\u548c\u91d1\u5c5e\u4e4b\u95f4\u7ed3\u5408\uff1f\u4fc4\u7f57\u65af\u79d1\u5b66\u5bb6\u7ed9\u51fa\u4e86\u65b0\u65b9\u6cd5\uff0c\u800c\u4e14\u6240\u9700\u8981\u7684\u65f6\u95f4\u4ec5\u4e3a\u5fae\u79d2\u7ea7\u522b\uff01\u8ba9\u6211\u4eec\u62ed\u76ee\u4ee5\u5f85\uff01<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-60685 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/Modified-metals-for-space-engineering-produced-in-microseconds_popup.jpg\" width=\"600\" height=\"399\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/Modified-metals-for-space-engineering-produced-in-microseconds_popup.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/Modified-metals-for-space-engineering-produced-in-microseconds_popup-300x200.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u6258\u6728\u65af\u514b\u7406\u5de5\u5927\u5b66\uff08TPU\uff09\u548c\u9ad8\u7535\u6d41\u7535\u5b50\u5b66\u9662\u7684\u4fc4\u7f57\u65af\u79d1\u5b66\u5bb6\u4eec\u5df2\u7ecf\u5f00\u53d1\u51fa\u4e86\u4e00\u79cd\u5c06\u8010\u78e8\u6d82\u5c42\u7194\u5408\u5728\u57fa\u5e95\u91d1\u5c5e\u4e0a\u7684\u65b0\u65b9\u6cd5\u3002\u8fd9\u79cd\u96c6\u8d28\u8f7b\u3001\u9ad8\u5f3a\u5ea6\u548c\u8010\u8150\u8680\u6027\u4e8e\u4e00\u4f53\u7684\u6539\u6027\u6750\u6599\uff0c\u88ab\u5e7f\u6cdb\u5e94\u7528\u4e8e\u673a\u68b0\u5de5\u7a0b\uff0c\u822a\u7a7a\u548c\u7a7a\u95f4\u5de5\u7a0b\u9886\u57df\u3002<\/p>\n<p>\u8fd9\u4e00\u65b0\u6750\u6599\u662f\u57fa\u4e8e\u7845\u548c\u94dd\u7684\u94dd\u7845\u5408\u91d1\u3002TPU\u7eb3\u7c73\u6750\u6599\u548c\u6280\u672f\u7cfb\u7684\u7814\u7a76\u751fMaria Rygina\u8ba4\u4e3a\uff1a\u201c\u8fd9\u4e9b\u91d1\u5c5e\u8f7b\u8d28\u4e14\u8010\u8150\u8680\u3002\u4e3a\u4e86\u4f7f\u5b83\u4eec\u5728\u822a\u5929\u5de5\u7a0b\u4e2d\u5927\u663e\u8eab\u624b\uff0c\u6211\u4eec\u53ea\u9700\u8981\u6539\u53d8\u5b83\u4eec\u7684\u5f3a\u5ea6\u548c\u6469\u64e6\u6027\u80fd\uff0c\u6362\u53e5\u8bdd\u8bf4\u5c31\u662f\u63d0\u9ad8\u786c\u5ea6\u548c\u8010\u78e8\u6027\u3002\u201d<\/p>\n<p>\u8be5\u6d82\u5c42\u4e0d\u662f\u6c89\u79ef\u5728\u57fa\u5e95\u4e0a\uff0c\u800c\u662f\u901a\u8fc7\u5f3a\u8109\u51b2\u7535\u5b50\u675f\u7194\u878d\u5230\u57fa\u5e95\u4e2d\u3002\u5b9e\u9a8c\u7814\u7a76\u8868\u660e\uff0c\u5b83\u4f7f\u91d1\u5c5e\u7684\u786c\u5ea6\u63d0\u9ad8\u4e86\u8fd16\u500d\uff0c\u8010\u78e8\u6027\u63d0\u9ad8\u4e863\u500d\u3002<\/p>\n<p>\u201c\u73b0\u5728\u6700\u5927\u7684\u96be\u9898\u662f\u6d82\u5c42\u548c\u57fa\u6750\u4e4b\u95f4\u7684\u7c98\u9644\u6027\u3002\u5982\u679c\u6d82\u5c42\u88ab\u7b80\u5355\u5730\u6c89\u79ef\u5728\u57fa\u5e95\u4e0a\uff0c\u90a3\u4e48\u5b83\u53ef\u4ee5\u5f88\u5bb9\u6613\u5730\u88ab\u6e05\u9664\uff0c\u201d\u9879\u76ee\u7684\u79d1\u5b66\u5e26\u5934\u4ebaYuri Ivanov\u6559\u6388\u8865\u5145\u9053\uff0c\u201c\u5916\u56fd\u7814\u7a76\u56e2\u961f\u6b63\u5728\u901a\u8fc7\u5f62\u6210\u591a\u5c42\u6d82\u5c42\u7684\u65b9\u5f0f\u6765\u5bfb\u627e\u89e3\u51b3\u8fd9\u4e2a\u95ee\u9898\u7684\u65b9\u6cd5\u3002\u7136\u800c\uff0c\u591a\u5c42\u6c89\u79ef\u9700\u8981\u6d88\u8017\u5927\u91cf\u65f6\u95f4\u3002\u6211\u4eec\u5219\u5728\u57fa\u6750\u8868\u9762\u6dfb\u52a0\u7194\u878d\u6d82\u5c42\u5373\u53ef\uff0c\u8fd9\u4ec5\u4ec5\u9700\u8981\u51e0\u5fae\u79d2\u7684\u65f6\u95f4\u5c31\u53ef\u4ee5\u5c06\u7c98\u9644\u529b\u663e\u7740\u63d0\u9ad8\u3002\u201d<\/p>\n<p>\u636e\u79d1\u5b66\u5bb6\u6240\u8bf4\uff0c\u6539\u6027\u91d1\u5c5e\u53ef\u4ee5\u7528\u4e8e\u5236\u9020\u822a\u5929\u5668\u7684\u5185\u90e8\u673a\u6784\u90e8\u4ef6\u3002\u76ee\u524d\uff0c\u8be5\u65b9\u6cd5\u5df2\u7ecf\u88ab\u7528\u4e8e\u751f\u4ea7\u6728\u5de5\u5de5\u5177\u548c\u673a\u68b0\u5de5\u7a0b\u7684\u96f6\u90e8\u4ef6\u3002\u76f8\u4fe1\u5728\u4e0d\u4e45\u7684\u5c06\u6765\uff0c\u5b83\u7684\u821e\u53f0\u4f1a\u66f4\u52a0\u5bbd\u5e7f\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.materialsforengineering.co.uk\/engineering-materials-news\/modified-metals-for-space-engineering-produced-in-microseconds\/149414\/\" target=\"_blank\">Modified metals for space engineering produced in microseconds<\/a>.<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u987e\u73a5\u63d0\u4f9b\u7d20\u6750\uff0c\u535c\u4fee\u660e\u7f16\u8bd1\uff0c\u725b\u857e\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\"><span style=\"color: #0b619c;\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/span><\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\"><span style=\"color: #0b619c;\">\u6d4b\u8bd5\u8c37<\/span><\/a>\uff01<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u5c06\u6d82\u5c42\u4e0e\u91d1\u5c5e\u7ed3\u5408\u5e76\u4e0d\u7a00\u5947\uff0c\u53ef\u5c06\u5b83\u5e94\u7528\u4e8e\u6027\u80fd\u8981\u6c42\u6781\u9ad8\u7684\u822a\u7a7a\u9886\u57df\u5462\uff1f\u90a3\u4e48\u5982\u4f55\u63d0\u9ad8\u6d82\u5c42\u548c\u91d1\u5c5e\u4e4b\u95f4\u7ed3\u5408\uff1f\u4fc4\u7f57\u65af\u79d1\u5b66\u5bb6\u7ed9\u51fa\u4e86\u65b0\u65b9\u6cd5\uff0c\u800c\u4e14\u6240\u9700\u8981\u7684\u65f6\u95f4\u4ec5\u4e3a\u5fae\u79d2\u7ea7\u522b&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-60239","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/60239"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=60239"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/60239\/revisions"}],"predecessor-version":[{"id":60687,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/60239\/revisions\/60687"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=60239"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=60239"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=60239"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}