{"id":60780,"date":"2017-01-15T14:00:39","date_gmt":"2017-01-15T06:00:39","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=60780"},"modified":"2017-01-10T15:20:21","modified_gmt":"2017-01-10T07:20:21","slug":"%e9%a3%9e%e6%9c%ba%e7%94%a8%e5%a4%8d%e5%90%88%e6%9d%90%e6%96%99%e7%9a%84%e5%8a%9f%e4%b8%8e%e8%bf%87","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=60780","title":{"rendered":"\u98de\u673a\u7528\u590d\u5408\u6750\u6599\u7684\u529f\u4e0e\u8fc7"},"content":{"rendered":"<p><span style=\"color: #000000;\"><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u590d\u5408\u6750\u6599\u4f5c\u4e3a\u73b0\u4ee3\u98de\u673a\u5236\u9020\u4e2d\u4e0d\u53ef\u6216\u7f3a\u7684\u90e8\u5206\u5df2\u7ecf\u5438\u5f15\u4e86\u8d8a\u6765\u8d8a\u591a\u4eba\u7684\u6ce8\u610f\uff0c\u90a3\u4e48\u98de\u673a\u4e0a\u4f7f\u7528\u7684\u590d\u5408\u6750\u6599\u6709\u54ea\u4e9b\u4f18\u70b9\u548c\u7f3a\u70b9\u5462\uff1f<\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-60781\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/\u56fe\u72471-1.jpg\" alt=\"\" width=\"700\" height=\"462\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/\u56fe\u72471-1.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/\u56fe\u72471-1-300x198.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><span style=\"color: #000000;\">\u98de\u673a\u4e0a\u4f7f\u7528\u4e86\u54ea\u4e9b\u590d\u5408\u6750\u6599\uff1f\u4e00\u822c\u6765\u8bf4\uff0c\u98de\u673a\u7528\u590d\u5408\u6750\u6599\u5305\u62ec\u73bb\u7483\u7ea4\u7ef4\u3001\u78b3\u7ea4\u7ef4\u548c\u7ea4\u7ef4\u589e\u5f3a\u57fa\u8d28\u4f53\u7cfb\uff0c\u6216\u8fd9\u4e9b\u6750\u6599\u4e2d\u7684\u4efb\u610f\u7ec4\u5408\u3002<\/span><\/p>\n<p><span style=\"color: #000000;\">\u6839\u636e\u7f8e\u56fd\u8054\u90a6\u822a\u7a7a\u7ba1\u7406\u5c40\uff08FAA\uff09\u7684\u62a5\u544a\uff0c\u7b2c\u4e8c\u6b21\u4e16\u754c\u5927\u6218\u540e\uff0c\u590d\u5408\u6750\u6599\u5f00\u59cb\u53d1\u5c55\u3002\u968f\u7740\u591a\u5e74\u6765\u7684\u53d1\u5c55\uff0c\u590d\u5408\u6750\u6599\u5df2\u53d8\u5f97\u66f4\u53d7\u6b22\u8fce\uff0c\u73b0\u5728\u88ab\u7528\u4e8e\u8bb8\u591a\u4e0d\u540c\u7c7b\u578b\u7684\u98de\u673a\u548c\u6ed1\u7fd4\u673a\u30022005\u5e74\uff0c\u7f8e\u56fd\u98de\u673a\u7ed3\u6784\u4e2d\u5927\u7ea6\u542b\u670935\uff05\u7684\u590d\u5408\u6750\u6599\u3002\u73b0\u5728\u7684\u98de\u673a\u7ed3\u6784\u901a\u5e38\u5305\u542b50\uff05\u81f370\uff05\u7684\u590d\u5408\u6750\u6599\u3002<\/span><\/p>\n<p><span style=\"color: #000000;\">\u7531\u4e8e\u590d\u5408\u6750\u6599\u5177\u6709\u8bb8\u591a\u4f18\u70b9\uff0c\u6240\u4ee5\u5b83\u7ecf\u5e38\u88ab\u7528\u4e8e\u822a\u7a7a\u9886\u57df\u4e2d\u3002\u6ce2\u97f3\u516c\u53f8\u57282012\u5e74\u63a8\u51fa\u4e86\u65b0\u7684787 Dreamliner\uff0c\u8fd9\u6b3e\u98de\u673a\u542b\u670950\uff05\u7684\u590d\u5408\u6750\u6599\u3002\u57282013\u5e74\u63a8\u51fa\u7684A350-XWB\u4e5f\u7531\u81f3\u5c1150\uff05\u7684\u590d\u5408\u6750\u6599\u5236\u6210\u3002\u73b0\u5728\u7684\u65b0\u98de\u673a\u51e0\u4e4e\u5168\u90e8\u5c06\u4e00\u4e9b\u590d\u5408\u6750\u6599\u878d\u5165\u5230\u4ed6\u4eec\u7684\u8bbe\u8ba1\u4e2d\u3002<\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u4f18\u70b9<\/strong><\/span><\/p>\n<p><span style=\"color: #000000;\">\u5927\u591a\u6570\u65f6\u5019\uff0c\u5728\u98de\u884c\u5668\u7ed3\u6784\u4e0a\u4f7f\u7528\u590d\u5408\u6750\u6599\u4f1a\u51cf\u5c11\u81ea\u91cd\u3002\u7ea4\u7ef4\u589e\u5f3a\u590d\u5408\u6750\u6599\u4f53\u7cfb\u6bd4\u5927\u591a\u6570\u98de\u673a\u4e2d\u7684\u4f20\u7edf\u94dd\u5f3a\u5ea6\u9ad8\uff0c\u5e76\u4e14\u5b83\u4eec\u80fd\u63d0\u4f9b\u5149\u6ed1\u7684\u8868\u9762\u5e76\u63d0\u9ad8\u71c3\u6cb9\u6548\u7387\u3002<\/span><\/p>\n<p><span style=\"color: #000000;\">\u590d\u5408\u6750\u6599\u4e0d\u4f1a\u50cf\u5176\u4ed6\u7c7b\u578b\u7684\u7ed3\u6784\u6750\u6599\u4e00\u6837\u6613\u88ab\u8150\u8680\u3002\u5b83\u4eec\u4e0d\u4f1a\u7531\u4e8e\u91d1\u5c5e\u75b2\u52b3\u800c\u7834\u88c2\uff0c\u5e76\u4e14\u5728\u7ed3\u6784\u6320\u66f2\u73af\u5883\u4e2d\u80fd\u591f\u4fdd\u6301\u826f\u597d\u3002\u590d\u5408\u6750\u6599\u7684\u5bff\u547d\u6bd4\u94dd\u957f\uff0c\u8fd9\u610f\u5473\u7740\u66f4\u4f4e\u7684\u7ef4\u62a4\u548c\u7ef4\u4fee\u6210\u672c\u3002<\/span><\/p>\n<p><span style=\"color: #000000;\">\u6709\u4eba\u79f0\uff0c\u590d\u5408\u6750\u6599\u7684\u4f7f\u7528\u4f1a\u5bf9\u822a\u7a7a\u6784\u6210\u5b89\u5168\u98ce\u9669\uff0c\u5e76\u4e14\u5217\u51fa\u4e86\u4e00\u4e9b\u7f3a\u70b9\u3002<\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u7f3a\u70b9<\/strong><\/span><\/p>\n<p><span style=\"color: #000000;\">\u590d\u5408\u6750\u6599\u4e0d\u5bb9\u6613\u65ad\u88c2\uff0c\u4f46\u662f\u7531\u6b64\u5e26\u6765\u7684\u95ee\u9898\u662f\u5f88\u96be\u5224\u65ad\u5185\u90e8\u7ed3\u6784\u662f\u5426\u5df2\u88ab\u635f\u574f\u3002\u76f8\u6bd4\u4e4b\u4e0b\uff0c\u94dd\u6613\u5f2f\u66f2\uff0c\u6613\u4e8e\u68c0\u6d4b\u7ed3\u6784\u635f\u574f\uff1b\u5bf9\u4e8e\u76f8\u540c\u7a0b\u5ea6\u7684\u635f\u4f24\uff0c\u590d\u5408\u6750\u6599\u7684\u66f4\u96be\u4ee5\u68c0\u6d4b\u3002\u5f53\u590d\u5408\u8868\u9762\u635f\u574f\u65f6\uff0c\u4fee\u590d\u53ef\u80fd\u4e5f\u66f4\u56f0\u96be\u3002<\/span><\/p>\n<p><span style=\"color: #000000;\">\u4f7f\u7528\u590d\u5408\u6750\u6599\u7684\u98de\u673a\u5e94\u8be5\u6ce8\u610f\u907f\u514d\u706b\u707e\uff0c\u56e0\u4e3a\u5176\u4e2d\u4f7f\u7528\u7684\u6811\u8102\u5728\u4f4e\u81f3150\u2103\u7684\u6e29\u5ea6\u4e0b\u5c31\u4f1a\u53d8\u5f31\u3002\u590d\u5408\u6750\u6599\u71c3\u70e7\u4f1a\u91ca\u653e\u6709\u6bd2\u7684\u70df\u96fe\u548c\u5fae\u7c92\u5b50\u3002\u9ad8\u4e8e300\u2103\u7684\u6e29\u5ea6\u53ef\u80fd\u5bfc\u81f4\u5176\u7ed3\u6784\u635f\u574f\u3002<\/span><\/p>\n<p><span style=\"color: #000000;\">\u6700\u540e\uff0c\u590d\u5408\u6750\u6599\u6bd4\u8f83\u6602\u8d35\uff0c\u4f46\u662f\u901a\u5e38\u540e\u671f\u8f83\u4f4e\u7684\u7ef4\u62a4\u6210\u672c\u4f1a\u62b5\u6d88\u5176\u9ad8\u521d\u59cb\u6210\u672c\u3002<\/span><\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/www.thebalance.com\/composite-materials-aircraft-structure-282777\" target=\"_blank\">Advantages and Disadvantages of Composite Materials on Airplanes.<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u9f99\u9a91\u58eb\u63d0\u4f9b\u7d20\u6750\uff0c\u5f90\u6d9b\u7f16\u8bd1\uff0c\u6731\u6653\u79c0\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u590d\u5408\u6750\u6599\u4f5c\u4e3a\u73b0\u4ee3\u98de\u673a\u5236\u9020\u4e2d\u4e0d\u53ef\u6216\u7f3a\u7684\u90e8\u5206\u5df2\u7ecf\u5438\u5f15\u4e86\u8d8a\u6765\u8d8a\u591a\u4eba\u7684\u6ce8\u610f\uff0c\u90a3\u4e48\u98de\u673a\u4e0a\u4f7f\u7528\u7684\u590d\u5408\u6750\u6599\u6709\u54ea\u4e9b\u4f18\u70b9\u548c\u7f3a\u70b9\u5462\uff1f \u98de\u673a\u4e0a\u4f7f\u7528\u4e86\u54ea\u4e9b\u590d\u5408\u6750\u6599\uff1f\u4e00\u822c\u6765\u8bf4\uff0c&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[43],"class_list":["post-60780","post","type-post","status-publish","format-standard","hentry","category-keji","tag-composite"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/60780"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=60780"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/60780\/revisions"}],"predecessor-version":[{"id":61010,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/60780\/revisions\/61010"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=60780"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=60780"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=60780"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}