{"id":61586,"date":"2017-01-16T06:30:03","date_gmt":"2017-01-15T22:30:03","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=61586"},"modified":"2017-01-15T17:36:18","modified_gmt":"2017-01-15T09:36:18","slug":"science%ef%bc%9a%e7%94%b5%e5%ad%90%e8%a1%8d%e5%b0%84%e8%ae%a9%e7%ba%b3%e7%b1%b3%e5%8d%95%e6%99%b6%e4%b8%ad%e7%9a%84%e6%b0%a2%e5%8e%9f%e5%ad%90%e6%97%a0%e6%89%80%e9%81%81%e5%bd%a2","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=61586","title":{"rendered":"Science\u6700\u65b0\u5c01\u9762\uff1a\u7535\u5b50\u884d\u5c04\u8ba9\u7eb3\u7c73\u5355\u6676\u4e2d\u7684\u6c22\u539f\u5b50\u65e0\u6240\u9041\u5f62"},"content":{"rendered":"<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-61743\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F1.medium-1.gif\" alt=\"\" width=\"346\" height=\"440\" \/><\/strong><\/p>\n<p><strong>\u3010\u5f15\u8bed\u3011<\/strong><\/p>\n<p>\u5317\u4eac\u65f6\u95f41\u670813\u65e5\uff0cScience\u7f51\u7ad9\u53d1\u8868\u4e86\u4e00\u7bc7\u9898\u4e3a\u201cHydrogen positions in single nanocrystals revealed by electron diffraction\u201d\u7684\u5c01\u9762\u6587\u7ae0\uff0c\u8bba\u6587<strong>\u901a\u8baf\u4f5c\u8005\u4e3a\u6377\u514b\u79d1\u5b66\u9662\u7269\u7406\u7814\u7a76\u6240\u7684L. Palatinus\u548c\u6cd5\u56fd\u56fd\u7acb\u5361\u6602\u9ad8\u7b49\u5de5\u7a0b\u5e08\u5b66\u9662\u7684P. Boullay<\/strong>\u3002<\/p>\n<p>\u7814\u7a76\u53d1\u73b0\uff0c\u901a\u8fc7\u4f7f\u7528\u52a8\u6001\u7cbe\u5316\u4e0e\u7535\u5b50\u884d\u5c04\u6570\u636e\u91c7\u96c6\u7684\u65b9\u6cd5\uff0c\u53ef\u5b9a\u4f4d\u5fae\u7c73\u7ea7\u4ee5\u4e0b\u6709\u673a\u6216\u65e0\u673a\u5355\u6676\u6750\u6599\u4e2d\u7684\u6c22\u539f\u5b50\u3002\u6c22\u539f\u5b50\u7684\u5b9a\u4f4d\u5411\u6765\u662f\u6676\u4f53\u7ed3\u6784\u5206\u6790\u4e2d\u7684\u5de8\u5927\u6311\u6218\u4e4b\u4e00\uff0c\u5982\u679c\u80fd\u591f\u6210\u529f\u68c0\u6d4b\uff0c\u5219\u9884\u793a\u7740\u7814\u7a76\u8005\u4eec\u80fd\u66f4\u6e05\u6670\u7684\u4e86\u89e3\u6676\u4f53\u6750\u6599\u7684\u6027\u8d28\u4e0e\u529f\u80fd\u3002\u800c\u8be5\u9879\u7814\u7a76\u5219\u6210\u529f\u5730\u83b7\u5f97\u4e86\u7a81\u7834\uff0c\u4e3a\u63ed\u793a\u63a2\u7a76\u6676\u4f53\u7ed3\u6784\u7684\u7ec6\u8282\u5f00\u8f9f\u4e86\u65b0\u8def\u5f84\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u6c22\u539f\u5b50\u7684\u4f4d\u7f6e\u5728\u6676\u4f53\u7ed3\u6784\u5206\u6790\u4e2d\u5341\u5206\u91cd\u8981\uff0c\u4f46\u5f80\u5f80\u5176\u6563\u5c04\u529f\u7387\u8fc7\u5c0f\u4ee5\u81f4\u5176\u4f4d\u7f6e\u96be\u4ee5\u786e\u5b9a\u3002\u672c\u6587\u4f5c\u8005\u62a5\u9053\u4e86\u4e00\u79cd\u6700\u65b0\u7814\u53d1\u7684\u52a8\u6001\u65cb\u8fdb\u7535\u5b50\u884d\u5c04\u7684\u6210\u50cf\u6570\u636e\u7ec6\u5316\u65b9\u6cd5\uff0c\u8be5\u65b9\u6cd5\u80fd\u76f4\u63a5\u663e\u793a\u51fa\u6c22\u539f\u5b50\u5728\u7eb3\u7c73\u6676\u6750\u6599\u4e2d\u7684\u4f4d\u7f6e\uff08\u5305\u62ec\u6c34\u5408\u7269\u4ee5\u53ca\u590d\u6742\u7684\u6709\u673a\u7269\uff09\u3002\u65e0\u8bba\u662f\u6709\u673a\u6750\u6599\uff08\u5bf9\u4e59\u9170\u6c28\u57fa\u915a\uff09\u8fd8\u662f\u65e0\u673a\u6750\u6599\uff08\u94b4\u94dd\u6846\u67b6\uff09\u4e2d\u7684\u6c22\u539f\u5b50\u7684\u4f4d\u7f6e\u90fd\u53ef\u786e\u5b9a\uff0c\u5e76\u4e14\u6e05\u6670\u51c6\u786e\u7684\u53cd\u5e94\u7ed3\u6784\u4e2d\u7684\u7ec6\u8282\uff08\u5176\u4e2d\u5305\u62ec\u5fae\u7c73\u751a\u81f3\u7eb3\u7c73\u7ea7\u522b\u5c3a\u5ea6\u7684\u5355\u6676\u4e2d\u6c22\u539f\u5b50\u7684\u4f4d\u7f6e\uff09\u3002<\/p>\n<p>\u672c\u6587\u4e2d\u4f5c\u8005\u5bf9\u4e24\u79cd\u4e4b\u524d\u96be\u4ee5\u786e\u5b9a\u6c22\u539f\u5b50\u65b9\u4f4d\u7684\u7ed3\u6784\u8fdb\u884c\u6210\u529f\u7684\u5b9a\u4f4d\uff0c\u5206\u522b\u662f\u6709\u673a\u7269\u5bf9\u4e59\u9170\u6c28\u57fa\u915a\uff08II\uff09\u6676\u4f53\u4e0e\u94b4\u94dd\u78f7\u9178\u76d0\uff08CAP\uff09\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>1 <\/strong><strong>\u5bf9\u4e59\u9170\u6c28\u57fa\u915a\u7684<\/strong><strong>PEDT<\/strong><strong>\u7ed3\u6784\u5206\u6790<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-61588 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F1.large_-1.jpg\" width=\"600\" height=\"333\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F1.large_-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F1.large_-1-300x167.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09\u5bf9\u4e59\u9170\u6c28\u57fa\u915a\uff08II\uff09\u6676\u4f53\u7684\u900f\u5c04\u7535\u5b50\u663e\u5fae\u955c\u6cd5\uff08TEM\uff09\u56fe\u50cf\u3002\u5982\u56fe\u6240\u793a\uff0c\u5706\u5708\u8868\u793a\u5728\u6570\u636e\u91c7\u96c6\u8fc7\u7a0b\u4e2d\uff0c\u7535\u5b50\u675f\u7684\u79fb\u52a8\u4ee5\u51cf\u5c0f\u8f90\u5c04\u635f\u4f24\u3002<\/p>\n<p>\uff08B\uff09\u8868\u793a\u6cbfa\u8f74\u7684\u4e00\u5c42\u6676\u4f53\u7ed3\u6784\uff0c\u5e76\u901a\u8fc7\u53e0\u52a0\u5dee\u5206\u7535\u4f4d\u56fe\u663e\u793a\u51fa\u6c22\u539f\u5b50\u4f4d\u7f6e\u7684\u6700\u5927\u503c\u3002\u5176\u4e2d\uff0c\u7b49\u503c\u9762\u6c34\u5e73\u5206\u522b\u4e3a2 \u03c3[\u25b3V(<strong>r<\/strong>)]\uff08\u4eae\u7070\u8272\u90e8\u5206\uff09\u548c3 \u03c3[\u25b3V(<strong>r<\/strong>)]\uff08\u9ec4\u8272\u90e8\u5206\uff09\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>2 <\/strong><strong>\u94b4\u94dd\u78f7\u9178\u76d0\uff08<\/strong><strong>CAP<\/strong><strong>\uff09\u6cbf\u6676\u76f8<\/strong><strong>[-2 -1 0]<\/strong><strong>\u7684\u7ed3\u6784\u56fe\uff08\u6b63\u516b\u9762\u4f53<\/strong><strong>Al(1)O<sub>6<\/sub>, Co(1)O<sub>6<\/sub>, <\/strong><strong>\u4e0e<\/strong><strong> Co(2)O<sub>6<\/sub><\/strong><strong>\u7684\u73af\u5883\uff09<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-61589 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F2.large_-1.jpg\" width=\"600\" height=\"437\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F2.large_-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F2.large_-1-300x219.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u6b63\u516b\u9762\u4f53Co(2)O<sub>6<\/sub>\u4ec5\u6709\u90e8\u5206\u88abCo\u5360\u636e\u3002\u56fe\u4e0a\u6807\u51fa\u4e86\u6bcf\u4e2a\u591a\u9762\u4f53\u4e2d\u592e\u9633\u79bb\u5b50\u7684\u7c7b\u578b\uff0c\u5176\u4e2d\u4ea6\u663e\u793a\u4e86\u6c22\u79bb\u5b50\u7684\u4f4d\u7f6e\uff08\u7ea2\u7403\u8868\u793aO\u539f\u5b50\uff09\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>3 CAP<\/strong><strong>\u7684<\/strong><strong>PEDT<\/strong><strong>\u7ed3\u6784\u5206\u6790<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-61590 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F3.large_-1.jpg\" width=\"600\" height=\"334\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F3.large_-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F3.large_-1-300x167.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09CAP\u5178\u578b\u6676\u4f53\u7684TEM\u56fe\u50cf\u3002\u5176\u4e2d\u9ed1\u8272\u5706\u5708\u8868\u793a\u5728\u6570\u636e\u91c7\u96c6\u8fc7\u7a0b\u4e2d\uff0c\u90e8\u5206\u6676\u4f53\u53d7\u5230\u7535\u5b50\u675f\u8f90\u7167\u3002<\/p>\n<p>\uff08B\uff09\u8868\u793a\u6cbf\u7740c\u8f74\uff0c\u5bf9CAP\u7ed3\u6784\u8fdb\u884c\u6295\u5f71\uff0c\u5e76\u901a\u8fc7\u53e0\u52a0\u5dee\u5206\u7535\u4f4d\u56fe\u663e\u793a\u51fa\u6c22\u539f\u5b50\u4f4d\u7f6e\u7684\u6700\u5927\u503c\u3002\u5176\u4e2d\uff0c\u7b49\u503c\u9762\u6c34\u5e73\u5206\u522b\u4e3a2 \u03c3[\u25b3V(r)]\uff08\u4eae\u7070\u8272\u90e8\u5206\uff09\u548c3 \u03c3[\u25b3V(r)]\uff08\u9ec4\u8272\u90e8\u5206\uff09\u3002\u865a\u7ebf\u753b\u7684\u692d\u5706\u5f62\u6807\u51fa\u4e86\u4e00\u4e2a\u6cbfc\u7684\u901a\u9053\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>4 CAP<\/strong><strong>\u5dee\u5206\u7535\u4f4d\u56fe\u663e\u793a\u7b49\u503c\u9762<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-61591 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F4.large_-1.jpg\" width=\"495\" height=\"1280\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F4.large_-1.jpg 495w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F4.large_-1-116x300.jpg 116w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/F4.large_-1-396x1024.jpg 396w\" sizes=\"(max-width: 495px) 100vw, 495px\" \/><\/p>\n<p>\u5dee\u5206\u70b9\u4f4d\u56fe\u7528\u4e8e\u8868\u793a\u4ee5\u4e0b\u7ed3\u6784\u9644\u8fd1\u7684\u7b49\u503c\u9762\u60c5\u51b5\uff08A\uff09AlO<sub>5<\/sub>\u00b7H<sub>2<\/sub>O\uff0c\uff08B\uff09CoO<sub>2<\/sub>\uff08OH\uff09<sub>2<\/sub>\u00b72H<sub>2<\/sub>O\u4ee5\u53ca\uff08C\uff09PO<sub>3<\/sub>OH\u57fa\u56e2\uff08\u5bf9\u5e94\u539f\u5b50\u989c\u8272\u89c1\u56fe\u4e09\uff09\u3002\u5176\u4e2d\uff0c\u7b49\u503c\u9762\u6c34\u5e73\u5206\u522b\u4e3a2 \u03c3[\u25b3V(r)]\uff08\u4eae\u7070\u8272\u90e8\u5206\uff09\u548c3 \u03c3[\u25b3V(r)]\uff08\u9ec4\u8272\u90e8\u5206\uff09\u3002\u901a\u8fc7DFT\u8ba1\u7b97\u4e0ePEDT\u7684\u7cbe\u5316\u83b7\u5f97\u6c22\u539f\u5b50\u7684\u4f4d\u7f6e\uff0c\u5206\u522b\u4ee5\u9ed1\u8272\u548c\u767d\u8272\u6807\u51fa\u3002<\/p>\n<p><strong>\u3010\u603b\u7ed3\u3011<\/strong><\/p>\n<p>\u8be5\u8bba\u6587\u4f7f\u7528\u52a8\u6001\u7cbe\u5316\u4e0e\u7535\u5b50\u884d\u5c04\u6570\u636e\u91c7\u96c6\u7684\u65b9\u6cd5\u6210\u529f\u5b9a\u4f4d\u5fae\u7c73\u7ea7\u4ee5\u4e0b\u6709\u673a\u6216\u65e0\u673a\u5355\u6676\u6750\u6599\u4e2d\u7684\u6c22\u539f\u5b50\uff0c\u4e3a\u7ec6\u81f4\u5206\u6790\u5e76\u900f\u5f7b\u4e86\u89e3\u6676\u4f53\u7684\u529f\u80fd\u4e0e\u6027\u80fd\u5f00\u8f9f\u4e86\u65b0\u7684\u8def\u5f84\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/science.sciencemag.org\/content\/355\/6321\/166\" target=\"_blank\">Hydrogen positions in single nanocrystals revealed by electron diffraction<\/a> (Science, 2017, DOI: 10.1126\/science.aak9652)<\/p>\n<p>\u540c\u671fPERSPECTIVE\u6587\u7ae0\u94fe\u63a5\uff1a<a href=\"http:\/\/science.sciencemag.org\/content\/355\/6321\/136?_ga=1.73925394.1488111892.1459129247\" target=\"_blank\">Electron diffraction and the hydrogen atom<\/a>\uff08Science, 2017, DOI: 10.1126\/science.aal4570\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7eb3\u7c73\u7ec4pengyuman\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/cailiaoren.mikecrm.com\/6qSdMU\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<\/strong><a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\"><strong>\u6d4b\u8bd5\u8c37<\/strong><\/a><strong>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8bed\u3011 \u5317\u4eac\u65f6\u95f41\u670813\u65e5\uff0cScience\u7f51\u7ad9\u53d1\u8868\u4e86\u4e00\u7bc7\u9898\u4e3a\u201cHydrogen positions in single nanocrystals reveal&#8230;<\/p>\n","protected":false},"author":1739,"featured_media":61745,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[155,56,33],"class_list":["post-61586","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-science","tag-crsytal","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/61586"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1739"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=61586"}],"version-history":[{"count":22,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/61586\/revisions"}],"predecessor-version":[{"id":61752,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/61586\/revisions\/61752"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/61745"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=61586"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=61586"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=61586"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}