{"id":62012,"date":"2017-01-26T14:00:11","date_gmt":"2017-01-26T06:00:11","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=62012"},"modified":"2017-01-21T18:24:31","modified_gmt":"2017-01-21T10:24:31","slug":"%e4%ba%ba%e7%b1%bb%e5%92%8cnano%e7%9a%84%e4%b8%8d%e8%a7%a3%e4%b9%8b%e7%bc%98","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=62012","title":{"rendered":"\u4eba\u7c7b\u548c\u201cNano\u201d\u7684\u4e0d\u89e3\u4e4b\u7f18"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u201cNano\u201d\uff0c\u6253\u5f00\u79d1\u6280\u65b0\u95fb\u6ee1\u5929\u98de\u7684\u4e00\u4e2a\u8bcd\uff0c\u672a\u6765\u7684\u65e5\u5b50\u91cc\u6211\u4eec\u5c06\u89c1\u8bc1\u7eb3\u7c73\u6280\u672f\u5728\u822a\u7a7a\u822a\u5929\u3001\u751f\u7269\u533b\u5b66\u3001\u8ba1\u7b97\u548c\u901a\u4fe1\u7b49\u9886\u57df\u6539\u53d8\u4eba\u7c7b\u751f\u6d3b\u7684\u8fc7\u7a0b\uff0c\u8bf4\u4e0d\u5b9a\u8fd8\u6709\u52a9\u4e8e\u5ef6\u957f\u4eba\u7c7b\u5bff\u547d\u5462\uff0c\u7eb3\u7c73\uff0c\u4f60\u600e\u4e48\u770b\uff1f<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-62011\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/1-35.jpg\" alt=\"\" width=\"600\" height=\"310\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/1-35.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/1-35-300x155.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u6bcf\u5929\uff0c\u4f3c\u4e4e\u90fd\u4f1a\u5192\u51fa\u4e00\u53ea\u7528\u65b0\u65b9\u6cd5\u505a\u201c\u7eb3\u7c73\u201d\u7684\u56e2\u961f\uff0c\u5728\u4ed6\u4eec\u7684\u52aa\u529b\u4e0b\u4e00\u5207\u5c06\u4f1a\u53d8\u5f97\u66f4\u597d\u3002<\/p>\n<p>21\u4e16\u7eaa\u7684\u53d8\u9769\u4e0d\u4f1a\u7535\u89c6\u5316\uff0c\u800c\u662f\u4f1a\u88ab\u53d1\u5e03\u5230Snapchat\uff0cInstagram\uff0cTwitter\u548cYouTube\u4e0a\u3002\u4f46\u662f\u5982\u679c\u4f60\u6839\u672c\u770b\u4e0d\u5230\u5b83\u5462\uff1f\u8fd9\u5c31\u5982\u540c\u7eb3\u7c73\u7ea7\u522b\u4e0a\u53d1\u751f\u7684\u4e8b\u60c5\u53ea\u5b58\u5728\u4e8e\u7406\u8bba\u4e0a\u4e00\u6837\u3002<\/p>\n<p>\u4f46\u662f\uff0c\u4f46\u591a\u4e8f\u4e8620\u4e16\u7eaa\u8457\u540d\u7684\u7269\u7406\u5b66\u5bb6Richard Feynman\uff0c\u4ed6\u8ba9\u6211\u4eec\u770b\u5230\u4e86\u771f\u6b63\u7eb3\u7c73\u7ea7\u7684\u4e1c\u897f\u3002<\/p>\n<p>Feynman\u7684\u7406\u5ff5\u5728\u822a\u7a7a\u822a\u5929\u3001\u751f\u7269\u533b\u5b66\u3001\u8ba1\u7b97\u548c\u901a\u4fe1\u7b49\u4e0d\u540c\u9886\u57df\u4ecd\u5728\u4e0d\u65ad\u521b\u65b0\u3002\u4ed6\u5960\u5b9a\u4e86\u7531\u7eb3\u7c73\u7c92\u5b50\u5236\u9020\u78b3\u7eb3\u7c73\u7ba1\u3001\u5df4\u57fa\u7403\u3001\u5bcc\u52d2\u70ef\u3001\u77f3\u58a8\u70ef\u548c\u5176\u4ed6\u6750\u6599\u7684\u57fa\u7840\u3002<\/p>\n<p>1959\u5e74\uff0c\u7f8e\u56fd\u56fd\u5bb6\u7eb3\u7c73\u6280\u672f\u8ba1\u5212\uff08National Nanotechnology Initiative \uff0c\u7b80\u79f0NNI\uff09\u4e2dFeynman\u201c\u63cf\u8ff0\u4e86\u79d1\u5b66\u5bb6\u5c06\u80fd\u591f\u64cd\u7eb5\u548c\u63a7\u5236\u5355\u4e2a\u539f\u5b50\u548c\u5206\u5b50\u7684\u8fc7\u7a0b\u201d\uff0c\u6700\u65e9\u63d0\u51fa\u4e86\u7eb3\u7c73\u6280\u672f\u3002<\/p>\n<p>1984\u5e74\uff0c\u4ed6\u95ee\u9053\uff1a\u201c\u4f60\u80fd\u5236\u9020\u591a\u5c0f\u7684\u673a\u5668\uff1f\u201d \u4e8b\u5b9e\u8bc1\u660e\uff0c\u53ef\u4ee5\u5f88\u5c0f\u5f88\u5c0f\u3002<\/p>\n<p>\u800c\u4e14\uff0c\u6b63\u59822016\u5e7410\u67087\u65e5\u201c\u534e\u5c14\u8857\u65e5\u62a5\u201d\u62a5\u9053\uff0c\u6211\u4eec\u6b63\u5728\u89c1\u8bc1\u4e00\u4e9b\u771f\u6b63\u4f1f\u5927\u7684\u6210\u5c31\uff0c\u5305\u62ec\u5206\u5b50\u7535\u68af\u3001\u5206\u5b50\u808c\u8089\u3001\u5206\u5b50\u8ba1\u7b97\u673a\u82af\u7247\u3001\u5206\u5b50\u7535\u673a\u4ee5\u53ca\u7eb3\u7c73\u8f66\u3002<\/p>\n<p>\u8bd5\u7740\u60f3\u60f3\uff1a\u6839\u636eNNI\u63d0\u51fa\u7684\u7eb3\u7c73\u6280\u672f\uff0c\u201c\u7eb3\u7c73\u5c3a\u5ea6\u7684\u79d1\u5b66\uff0c\u5de5\u7a0b\u548c\u6280\u672f\u5927\u7ea6\u53ea\u67091-100\u7eb3\u7c73\u3002\u201d<\/p>\n<p>\u9664\u4e86\u8fd9\u4e9b\u8ff7\u4f60\u8d85\u7ea7\u673a\u5668\u5916\uff0c\u6211\u4eec\u6b63\u5728\u5c06\u201c\u7eb3\u7c73\u201d\u7eb3\u5165\u6280\u672f\u6750\u6599\u7684\u4ea7\u54c1\u5316\u8fdb\u7a0b\u4e2d\uff0c\u8fd9\u5c06\u4f7f\u73b0\u6709\u7684\u673a\u5668\u66f4\u8010\u7528\u3001\u5de5\u4f5c\u66f4\u9ad8\u6548\u3001\u79cd\u7c7b\u66f4\u4e30\u5bcc\u3002<\/p>\n<p>\u5f53\u6211\u4eec\u8c08\u5230\u4e0b\u4e00\u4ee3\u98de\u673a\u3001\u4e0b\u4e00\u4ee3\u53ef\u7a7f\u6234\u751f\u7269\u533b\u5b66\u8bbe\u5907\u548c\u4e0b\u4e00\u4ee3\u5149\u7ea4\u901a\u4fe1\u65f6\uff0c\u4e0d\u53d8\u7684\u4e3b\u9898\u662f\u7eb3\u7c73\uff1a\u7eb3\u7c73\u6280\u672f\u3001\u7eb3\u7c73\u6750\u6599\u3001\u7eb3\u7c73\u5149\u5b50\u5b66\u3002\u51e0\u5341\u5e74\u95f4\uff0c\u5236\u9020\u5546\u5df2\u80fd\u4f7f\u7528\u78b3\u7ea4\u7ef4\u5236\u9020\u66f4\u8f7b\u4fbf\u7684\u8fd0\u52a8\u5668\u6750\u3001\u66f4\u597d\u7684\u98de\u673a\u548c\u66f4\u4f18\u8d28\u7684\u7eba\u7ec7\u54c1\u3002<\/p>\n<p>\u6b63\u5982Dexter Johnson\u5728IEEE Spectrum\u7684\u62a5\u544a\u4e2d\u6240\u8bf4\uff0c\u78b3\u7eb3\u7c73\u7ba1\u5c06\u4f7f\u822a\u7a7a\u590d\u5408\u6750\u6599\u6027\u80fd\u66f4\u4f18\u8d8a\uff1a\u8428\u91cc\u5927\u5b66\u5148\u8fdb\u6280\u672f\u7814\u7a76\u6240\uff08Advanced Technology Institute\uff0c\u7b80\u79f0ATI\uff09\uff0c\u5e03\u91cc\u65af\u6258\u5927\u5b66\u521b\u65b0\u79d1\u5b66\u5148\u8fdb\u590d\u5408\u4e2d\u5fc3\uff08Advanced Composite Centre for Innovation and Science\uff0c\u7b80\u79f0ACCIS\uff09\u548c\u5e9e\u5df4\u8fea\u822a\u5929\u822a\u7a7a\u516c\u53f8\u7684\u7814\u7a76\u4eba\u5458\u6b63\u5728\u5408\u4f5c\u5f00\u53d1\u4e00\u79cd\u53d6\u4ee3\u805a\u5408\u7269\u80f6\u7684\u78b3\u7eb3\u7c73\u7ba1\u529f\u80fd\u6750\u6599\u3002\u7528\u8fd9\u79cd\u65b0\u6750\u6599\u751f\u4ea7\u7684\u589e\u5f3a\u805a\u5408\u7269\u5177\u6709\u8f83\u9ad8\u7684\u7535\u5bfc\u548c\u70ed\u5bfc\u7387\uff0c\u6709\u5f00\u8f9f\u65b0\u529f\u80fd\u7684\u53ef\u80fd\u6027\u3002\u82f1\u56fd\u7684\u7814\u7a76\u4eba\u5458\u8868\u793a\u5c06\u4f20\u611f\u5668\u548c\u80fd\u91cf\u91c7\u96c6\u5668\u7b49\u5c0f\u5de5\u5177\u76f4\u63a5\u5d4c\u5165\u6750\u6599\u4e2d\u5c06\u6210\u4e3a\u53ef\u80fd\u3002<\/p>\n<p>\u5f53\u6d89\u53ca\u5230\u98de\u673a\u9886\u57df\uff0c\u8f7b\u91cf\u5316\u662f\u8f83\u597d\u7684\uff0c\u6240\u4ee5\u5728\u673a\u8eab\u4e2d\u5d4c\u5165\u4f20\u611f\u5668\u548c\u80fd\u91cf\u6536\u96c6\u5668\u662f\u4e00\u4e2a\u91cd\u5927\u7684\u98de\u8dc3\u3002<\/p>\n<p>Johnson\u5728 IEEE Spectrum\u8fd8\u505a\u4e86\u57fa\u4e8e\u7535\u5b50\u632f\u8361\u7684\u201c\u65b0\u9896\u7684\u6df7\u5408\u7eb3\u7c73\u6750\u6599\u201d\u2014\u2014\u7eb3\u7c73\u5149\u5b50\u5b66\u7684\u4e3b\u8981\u8fdb\u6b65\u7684\u62a5\u544a\uff1a\u5fb7\u514b\u8428\u65af\u5927\u5b66\u5965\u65af\u6c40\u5206\u6821\u7684\u7814\u7a76\u4eba\u5458\u5f00\u53d1\u4e86\u4e00\u79cd\u6df7\u5408\u7eb3\u7c73\u6750\u6599\uff0c\u80fd\u591f\u8fdb\u884c\u5149\u5b66\u5143\u4ef6\u7684\u5199\u5165\uff0c\u64e6\u9664\u548c\u91cd\u5199\u3002\u7814\u7a76\u4eba\u5458\u8ba4\u4e3a\uff0c\u8fd9\u79cd\u7eb3\u7c73\u6750\u6599\u548c\u7528\u4e8e\u5f00\u53d1\u5b83\u7684\u6280\u672f\u53ef\u4ee5\u521b\u9020\u65b0\u4e00\u4ee3\u7684\u5149\u5b66\u82af\u7247\u548c\u7535\u8def\u3002<\/p>\n<p>\u5f53\u7136\uff0c\u53ef\u91cd\u5199\u5149\u5b66\u7684\u6982\u5ff5\u4e0d\u662f\u5168\u65b0\u7684\uff1b\u5b83\u662f\u8bf8\u5982CD\u548cDVD\u7684\u5149\u5b66\u5b58\u50a8\u4ecb\u8d28\u7684\u57fa\u7840\u3002\u7136\u800c\uff0cCD\u548cDVD\u9700\u8981\u5e9e\u5927\u7684\u5149\u6e90\uff0c\u5149\u5b66\u4ecb\u8d28\u548c\u5149\u68c0\u6d4b\u5668\u3002\u800c\u5168\u90e8\u57282-D\u6750\u6599\u4e0a\u64cd\u4f5c\u662f\u73b0\u5f00\u53d1\u7684\u53ef\u91cd\u5199\u96c6\u6210\u5149\u5b50\u7535\u8def\u7684\u4e00\u5927\u4eae\u70b9\u3002<\/p>\n<p>\u201c\u4e3a\u4e86\u5f00\u53d1\u53ef\u91cd\u5199\u7684\u96c6\u6210\u7eb3\u7c73\u5149\u5b50\u7535\u8def\u5c31\u5fc5\u987b\u5c06\u5149\u9650\u5236\u57282-D\u5e73\u9762\u5185\uff0c\u5176\u4e2d\u5149\u53ef\u4ee5\u5728\u5e73\u9762\u4e2d\u8fdb\u884c\u957f\u8ddd\u79bb\u4f20\u8f93\uff0c\u5e76\u4e14\u53ef\u4ee5\u5bf9\u5176\u4f20\u64ad\u65b9\u5411\uff0c\u5e45\u5ea6\uff0c\u9891\u7387\u548c\u76f8\u4f4d\u8fdb\u884c\u4efb\u610f\u8c03\u63a7\uff0c\u201d\u9879\u76ee\u7275\u5934\u4eba\uff0c\u5fb7\u514b\u8428\u65af\u5927\u5b66\u6559\u6388Yuebing Zheg\u8bf4\uff0c\u201c\u6211\u4eec\u7684\u6df7\u5408\u6750\u6599\uff0c\u4f7f\u5f97\u5f00\u53d1\u53ef\u91cd\u5199\u7684\u96c6\u6210\u7eb3\u7c73\u5149\u5b50\u7535\u8def\u6210\u4e3a\u53ef\u80fd\u3002\u201d<\/p>\n<p>\u8c01\u4f1a\u60f3\u5230\uff0c\u77f3\u58a8\u70ef\u4e0e\u81ea\u5236\u7684Silly Putty\uff08\u4e00\u79cd\u5f39\u6027\u6750\u6599\uff09\u6df7\u5408\u5c45\u7136\u4f1a\u521b\u5efa\u51fa\u4f7f\u201c\u53ef\u7a7f\u6234\u201d\u6210\u4e3a\u53ef\u80fd\u7684\u6781\u5177\u7a81\u7834\u6027\u7684\u65b0\u6750\u6599\u5462\uff1f<\/p>\n<p>\u4e0b\u4e00\u4ee3\u751f\u7269\u533b\u5b66\u8bbe\u5907\u65e0\u7591\u5c06\u4f1a\u4f7f\u7528\u4e00\u4e9b\u8fd9\u6837\u7684\u4e1c\u897f\uff1a<\/p>\n<p>\u4e00\u5757\u77f3\u58a8\u70ef\u53ef\u4ee5\u5c06\u88ab\u79f0\u4e3aSilly Putty\u7684\u5f39\u6027\u68d2\u72b6\u7269\u8f6c\u53d8\u4e3a\u80fd\u591f\u76d1\u6d4b\u4eba\u7c7b\u8109\u640f\u6216\u8005\u751a\u81f3\u53ef\u4ee5\u8ddf\u8e2a\u5c0f\u8718\u86db\u7cbe\u7ec6\u6b65\u4f10\u7684\u538b\u529b\u4f20\u611f\u5668\u3002<\/p>\n<p>\u8fd9\u79cd\u6750\u6599\u88ab\u79f0\u4e3aG-putty\uff0c\u5b83\u7684\u53d1\u660e\u8005\u5e0c\u671b\u53ef\u4ee5\u5c06\u5176\u5f00\u53d1\u6210\u4e00\u4e2a\u8fde\u7eed\u76d1\u6d4b\u8840\u538b\u7684\u88c5\u7f6e\u3002<\/p>\n<p>G-putty\u7684\u5236\u4f5c\u8005\u5728\u4ed6\u4eec\u7684\u7814\u7a76\u4e2d\u7ecf\u5e38\u4f9d\u8d56\u201c\u5bb6\u5ead\u7528\u54c1\u201d\u3002\u6b63\u5982Nature\u7684Mark Peplow\u8bf4\uff0c2014\u5e74\uff0c\u4ed6\u4eec\u901a\u8fc7\u201c\u5728\u53a8\u623f\u6405\u62cc\u673a\u4e2d\u70e7\u77f3\u58a8\u6765\u5236\u5907\u77f3\u58a8\u70ef\u201d\u3002<\/p>\n<p>\u4eba\u7c7b\u51fa\u4e8e\u5de5\u4e1a\u548c\u827a\u672f\u76ee\u7684\u7814\u7a76\u7eb3\u7c73\u6750\u6599\u5b9e\u9645\u4e0a\u5df2\u7ecf\u6709\u6570\u5343\u5e74\u4e86\u3002\u4f46\u662f\uff0c\u50cfFeynman\u8fd9\u6837\u53bb\u8bbe\u60f3\u5f00\u53d1\u8d85\u5c0f\u578b\u6280\u672f\u5c31\u9700\u8981\u6709\u8fdc\u89c1\u4e86\u3002\u4ed6\u7684\u52a9\u624b\u5728\u7eb3\u7c73\u6280\u672f\u548c\u7eb3\u7c73\u6750\u6599\u65b9\u9762\u53d6\u5f97\u7684\u8fdb\u5c55\u5c06\u63a8\u52a8\u661f\u9645\u63a2\u7d22\uff0c\u4fc3\u8fdb\u8d85\u7ea7\u8ba1\u7b97\uff0c\u5e76\u5ef6\u957f\u6211\u4eec\u4eba\u7c7b\u7684\u5bff\u547d\u3002<\/p>\n<p>Butterfly Sciences\u662f\u4e00\u4e2a\u4e2a\u4eba\u516c\u53f8\uff0c\u57fa\u4e8e\u4f7f\u7528\u57fa\u56e0\u6cbb\u7597\u6539\u5584\u827e\u6ecb\u75c5\u60a3\u8005\u751f\u6d3b\u7684\u7406\u5ff5\u800c\u521b\u7acb\u3002\u5b83\u662f\u5fae\u751f\u7269\u5b66\u5bb6Brian Hanley\u7684\u5fc3\u8840\u7ed3\u6676\u3002<\/p>\n<p>Hanley\u6f5c\u5fc3\u4e8e\u4ed6\u7684\u7814\u7a76\uff0c\u53bb\u5e746\u6708\uff0c\u4ed6\u81ea\u5df1\u6ce8\u5c04\u4e86\u4e00\u4e2a\u81ea\u5df1\u8bbe\u8ba1\u3001\u81ea\u5df1\u8d44\u52a9\u7684\u57fa\u56e0\uff0c\u4e14\u6ca1\u6709\u5f97\u5230FDA\u6279\u51c6\u3002<\/p>\n<p>\u6b63\u5982Antonio Regalado\u62a5\u9053\uff1a\u8fd9\u662f\u7b2c\u4e8c\u4f8bMIT\u6280\u672f\u8bc4\u8bba\u8bb0\u5f55\u7684\u4e0d\u53d7\u76d1\u7ba1\u7684\u57fa\u56e0\u6cbb\u7597\u6848\u4f8b\uff0c\u8fd9\u662f\u4e00\u4e2a\u88ab\u4e00\u4e9b\u5927\u80c6\u7684\u4eba\u6240\u63a5\u53d7\uff0c\u5bfb\u6c42\u5f00\u53d1\u6297\u8870\u8001\u6cbb\u7597\u7684\u6709\u98ce\u9669\u7684\u8bd5\u9a8c\u3002 Hanley\u6ce8\u5165\u4ed6\u7684\u808c\u8089\u7ec6\u80de\u7684\u57fa\u56e0\u4f1a\u4f7f\u4ed6\u7684\u8eab\u4f53\u4ea7\u751f\u66f4\u591a\u7684\u6709\u6548\u8377\u5c14\u8499\uff0c\u589e\u52a0\u4ed6\u7684\u529b\u91cf\uff0c\u8010\u529b\u548c\u5bff\u547d\u3002<\/p>\n<p>\u51e0\u4e4e\u6ca1\u6709\u6295\u8d44\u8005\u5bf9\u4ed6\u7684\u8fd9\u4e00\u6982\u5ff5\u611f\u5174\u8da3\u3002 \u4f4660\u5c81\u7684Hanley\u51b3\u5fc3\u770b\u770b\u4ed6\u7684\u65b9\u6cd5\u662f\u5426\u6709\u6548\u3002\u4ed6\u8bf4\uff1a\u201c\u6211\u60f3\u8bc1\u660e\u5b83\uff0c\u4e3a\u4e86\u81ea\u5df1\uff0c\u6211\u60f3\u8981\u53d6\u5f97\u8fdb\u5c55\uff0c\u201d\u3002<\/p>\n<p>\u6709\u4eba\u8bf4\uff0c\u4e00\u4e2a\u4ee3\u8868\u81ea\u5df1\u7684\u5f8b\u5e08\u662f\u4f1a\u6b3a\u9a97\u5ba2\u6237\u7684\u3002\u90a3\u4e48\u4ed6\u4eec\u5bf9\u81ea\u5df1\u505a\u57fa\u56e0\u6cbb\u7597\u8fd9\u4e00\u4e8b\u4ef6\u6709\u4ec0\u4e48\u770b\u6cd5\u5462\uff1f<\/p>\n<p>\u5965\u672c\u5927\u5b66\u4ece\u4e8b\u72d7\u57fa\u56e0\u7814\u7a76\u5de5\u4f5c\u7684Bruce Smith\u6559\u6388\u8bf4\uff1a\u201c\u6211\u8ba4\u4e3a\u8fd9\u662f\u75af\u4e86\uff0c\u4f46\u8fd9\u662f\u4eba\u7c7b\u4e0e\u6280\u672f\u78b0\u649e\u7684\u5929\u6027\u3002\u201d<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/www.trefis.com\/stock\/spy\/articles\/395255\/nanotechnology-how-miniscule-science-will-save-mankind\/2017-01-12\" target=\"_blank\">Nanotechnology: How Miniscule Science Will Save Mankind<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u9f99\u9a91\u58eb\u63d0\u4f9b\u7d20\u6750\uff0c\u8c37\u96e8\u661f\u7f16\u8bd1\uff0c\u4e01\u83f2\u83f2\u5ba1\u6838\uff0c\u70b9\u6211\u52a0\u5165<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u201cNano\u201d\uff0c\u6253\u5f00\u79d1\u6280\u65b0\u95fb\u6ee1\u5929\u98de\u7684\u4e00\u4e2a\u8bcd\uff0c\u672a\u6765\u7684\u65e5\u5b50\u91cc\u6211\u4eec\u5c06\u89c1\u8bc1\u7eb3\u7c73\u6280\u672f\u5728\u822a\u7a7a\u822a\u5929\u3001\u751f\u7269\u533b\u5b66\u3001\u8ba1\u7b97\u548c\u901a\u4fe1\u7b49\u9886\u57df\u6539\u53d8\u4eba\u7c7b\u751f\u6d3b\u7684\u8fc7\u7a0b\uff0c\u8bf4\u4e0d\u5b9a\u8fd8\u6709\u52a9\u4e8e\u5ef6\u957f\u4eba&#8230;<\/p>\n","protected":false},"author":230,"featured_media":62011,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[20,33],"class_list":["post-62012","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-zhineng","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/62012"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=62012"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/62012\/revisions"}],"predecessor-version":[{"id":62701,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/62012\/revisions\/62701"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/62011"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=62012"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=62012"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=62012"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}