{"id":62454,"date":"2017-01-28T14:00:33","date_gmt":"2017-01-28T06:00:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=62454"},"modified":"2017-01-24T17:02:21","modified_gmt":"2017-01-24T09:02:21","slug":"3d%e6%89%93%e5%8d%b0%e8%ae%a9%e5%8f%af%e4%bc%b8%e7%bc%a9%e7%94%b5%e5%ad%90%e8%ae%be%e5%a4%87%e6%9b%b4%e4%ba%b2%e6%b0%91%ef%bc%81","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=62454","title":{"rendered":"3D\u6253\u5370\u8ba9\u53ef\u4f38\u7f29\u7535\u5b50\u8bbe\u5907\u66f4\u4eb2\u6c11\uff01"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>3D\u6253\u5370\u6280\u672f\u81ea\u4ece\u95ee\u4e16\u4ee5\u6765\uff0c\u4fbf\u63a8\u52a8\u4e86\u8bb8\u591a\u4ea7\u4e1a\u7684\u9ad8\u901f\u53d1\u5c55\uff0c\u8d8a\u6765\u8d8a\u53d7\u5230\u79d1\u7814\u4eba\u5458\u7684\u91cd\u89c6\uff0c\u73b0\u5728\u5bc6\u82cf\u91cc\u5927\u5b66\u7406\u5de5\u5b66\u9662\u7684\u79d1\u7814\u4eba\u5458\u4eec\u5c063D\u6253\u5370\u6280\u672f\u76f4\u63a5\u5e94\u7528\u5728\u53ef\u4f38\u7f29\u7684\u7535\u5b50\u4ea7\u54c1\u4e2d\uff0c\u8fde\u63a5\u5851\u6027\u8f83\u597d\u7684\u5f39\u6027\u4f53\u4ee5\u53ca\u8106\u6027\u7684\u5bfc\u4f53\uff0c\u4e3a3D\u6253\u5370\u6280\u672f\u7684\u5e94\u7528\u5f00\u62d3\u51fa\u4e00\u6761\u65b0\u7684\u9053\u8def\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-62458\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/@DFMG7APBSF@VXLZCR9Y.jpg\" alt=\"\" width=\"498\" height=\"509\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/@DFMG7APBSF@VXLZCR9Y.jpg 498w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/01\/@DFMG7APBSF@VXLZCR9Y-294x300.jpg 294w\" sizes=\"(max-width: 498px) 100vw, 498px\" \/><\/p>\n<p>\u611f\u8c22\u5bc6\u82cf\u91cc\u5927\u5b66\u7406\u5de5\u5b66\u9662\u7684\u79d1\u7814\u4eba\u5458\u5bf93D\u6253\u5370\u6280\u672f\u7684\u7814\u7a76\uff0c\u4f7f\u5f97\u53ef\u4f38\u7f29\u7535\u5b50\u4ea7\u54c1\u8d70\u8fdb\u5343\u5bb6\u4e07\u6237\u3002<\/p>\n<p>\u5bc6\u82cf\u91cc\u5927\u5b66\u7406\u5de5\u5b66\u9662\u7684\u79d1\u7814\u4eba\u5458\u4eec\u9884\u6d4b\u53ef\u4f38\u7f29\u7535\u5b50\u4ea7\u54c1\u5c06\u4f1a\u96c6\u4e2d\u5728\u65b0\u7684\u5bfc\u4f53\u4e0a\uff0c\u53ef\u4ee5\u5728\u5f39\u6027\u4f53\u8fd9\u79cd\u9ad8\u5206\u5b50\u8868\u9762\u6216\u5185\u90e8\u96c6\u6210\u3002<\/p>\n<p>\u8fd9\u79cd\u5bfc\u4f53\u6216\u8bb8\u4f1a\u5728\u5c06\u6765\u7684\u67d0\u4e00\u5929\u53d6\u4ee3\u73b0\u5728\u5927\u591a\u6570\u7535\u5b50\u8bbe\u5907\u6240\u7528\u7684\u53c8\u786c\u53c8\u8106\u7684\u7535\u8def\u677f\u3002\u800c\u4e14\u5b83\u4eec\u7684\u7528\u6b66\u4e4b\u5730\u5f88\u591a\uff0c\u53ef\u4ee5\u4f5c\u4e3a\u53ef\u7a7f\u6234\u5f0f\u4f20\u611f\u5668\u7d27\u8d34\u76ae\u80a4\uff0c\u76d1\u6d4b\u5fc3\u810f\u548c\u5927\u8111\u7684\u6d3b\u52a8\uff0c\u8fd8\u53ef\u4ee5\u505a\u6210\u80fd\u591f\u8d34\u5728\u5f2f\u66f2\u8868\u9762\u7684\u8584\u592a\u9633\u80fd\u677f\u2026\u2026<\/p>\n<p>\u5bc6\u82cf\u91cc\u5927\u5b66\u7406\u5de5\u5b66\u9662\u7684\u79d1\u7814\u4eba\u5458\u4eec\u65ad\u8a00\uff0c\u672a\u6765\u53ef\u4f38\u7f29\u7535\u5b50\u4ea7\u54c1\u7684\u5173\u952e\u5728\u4e8e\u8868\u9762\u6216\u8005\u886c\u5e95\u3002\u5f39\u6027\u4f53\uff0c\u987e\u540d\u601d\u4e49\uff0c\u5b83\u662f\u4e00\u79cd\u5177\u6709\u9ad8\u5f39\u6027\u7684\u67d4\u6027\u6750\u6599\uff0c\u8fd9\u5c31\u610f\u5473\u7740\u5b83\u53ef\u4ee5\u5f2f\u66f2\u3001\u62c9\u4f38\u3001\u7d27\u6263\u4ee5\u53ca\u626d\u8f6c\uff0c\u4e14\u8fd9\u4e9b\u5f62\u53d8\u4e0d\u4f1a\u5bf9\u5b83\u7684\u6027\u80fd\u9020\u6210\u5f71\u54cd\u3002<\/p>\n<p>\u5bc6\u82cf\u91cc\u5927\u5b66\u7406\u5de5\u5b66\u9662\u7684\u673a\u68b0\u4e0e\u822a\u7a7a\u822a\u5929\u5de5\u7a0b\u7cfb\u7684\u52a9\u7406\u6559\u6388Heng Pan\u662f\u8be5\u7814\u7a76\u9879\u76ee\u7684\u9886\u5bfc\u8005\uff0c\u4ed6\u5728\u6587\u7ae0\u4e2d\u5199\u5230\uff1a\u5bf9\u4e8e\u53ef\u4f38\u7f29\u7535\u5b50\u4ea7\u54c1\uff0c\u6211\u4eec\u7684\u6311\u6218\u5728\u4e8e\u67d4\u6027\u5f39\u6027\u4f53\u548c\u8106\u6027\u5bfc\u4f53\u4e4b\u95f4\u7684\u4e0d\u5339\u914d\uff0c\u8fd9\u5c31\u662f\u9700\u8981\u6dfb\u52a0\u5242\u7684\u5e2e\u5fd9\u3002<\/p>\n<p>\u5728\u6587\u7ae0\u4e2d\uff0c\u7814\u7a76\u4eba\u5458\u8ba4\u4e3a\u53ef\u4ee5\u76f4\u63a5\u5728\u5f39\u6027\u4f53\u8868\u9762\u76f4\u63a5\u6253\u5370\u8584\u8584\u7684\u4e00\u5c42\u9ad8\u5bfc\u7535\u6027\u6750\u6599\u4f5c\u4e3a\u6dfb\u52a0\u5242\uff0c\u968f\u7740\u6dfb\u52a0\u5242\u5236\u9020\u4e1a\u7684\u53d1\u5c55\uff0c\u76f4\u63a5\u6253\u5370\u6280\u672f\u6b63\u9010\u6e10\u66ff\u4ee3\u4f20\u7edf\u7684\u65b9\u6cd5\u3002\uff08\u4f20\u7edf\u7684\u65b9\u6cd5\u5305\u62ec\u5149\u523b\u6280\u672f\uff0c\u5e38\u7528\u4e8e\u5236\u9020\u534a\u5bfc\u4f53\u6750\u6599\u3002\uff09<\/p>\n<p>Heng Pan\u548c\u4ed6\u7684\u540c\u4e8b\u4eec\u770b\u89c1\u4e86\u6dfb\u52a0\u5242\u5236\u9020\u4e1a\u5bf9\u8fd9\u4e9b\u65b0\u7684\u7535\u5b50\u8bbe\u5907\u7684\u7ecf\u6d4e\u6548\u5e94\uff0c\u56e0\u6b64\u4ed6\u4eec\u6d4b\u8bd5\u4e86\u4e00\u79cd\u79f0\u4e4b\u4e3a\u201c\u76f4\u63a5\u6c14\u6eb6\u80f6\u6253\u5370\u201d\u7684\u65b9\u6cd5\uff0c\u8be5\u65b9\u6cd5\u5728\u53ef\u4f38\u7f29\u7684\u886c\u5e95\u4e0a\u55b7\u6d82\u5bfc\u7535\u6750\u6599\uff0c\u4f7f\u5176\u6574\u5408\u5728\u4e00\u8d77\uff0c\u4ece\u800c\u5236\u9020\u51fa\u53ef\u4ee5\u653e\u7f6e\u5728\u76ae\u80a4\u4e0a\u7684\u4f20\u611f\u5668\u3002<\/p>\n<p>\u4ed6\u4eec\u5728\u6587\u7ae0\u4e2d\u5199\u5230\uff0c\u7531\u4e8e\u8bbe\u5907\u7684\u590d\u6742\u6027\u4ee5\u53ca\u5206\u8fa8\u7387\u7684\u589e\u52a0\uff0c\u4ece\u800c\u5bf9\u5de5\u827a\u6280\u672f\u63d0\u51fa\u4e86\u66f4\u9ad8\u7684\u8981\u6c42\uff0c\u76f4\u63a5\u6253\u5370\u6280\u672f\u4f5c\u4e3a\u4e00\u79cd\u6dfb\u52a0\u5242\u7684\u5236\u9020\u65b9\u6cd5\uff0c\u80fd\u591f\u6ee1\u8db3\u5bf9\u8bbe\u5907\u7684\u8981\u6c42\uff0c\u800c\u4e14\u6210\u672c\u4f4e\u5ec9\uff0c\u6548\u7387\u5927\u5e45\u5ea6\u63d0\u5347\uff0c\u8fd9\u53ef\u80fd\u662f\u5236\u9020\u51fa\u7ecf\u6d4e\u6548\u76ca\u9ad8\u3001\u5927\u89c4\u6a21\u53ef\u4f38\u7f29\u7535\u5b50\u8bbe\u5907\u4ea7\u4e1a\u7684\u89e3\u51b3\u65b9\u6848\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/worldindustrialreporter.com\/new-3d-printing-approach-could-make-stretchable-electronics-more-prelevant\/\" target=\"_blank\">New 3D Printing Approach could Make Stretchable Electronics More Prevalent<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u6708\u4eae\u63d0\u4f9b\u7d20\u6750\uff0c\u9648\u9732\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p><strong>\u4eea\u5668\u8bbe\u5907\u3001\u8bd5\u5242\u8017\u6750\u3001\u6750\u6599\u6d4b\u8bd5\u3001\u6570\u636e\u5206\u6790\uff0c\u627e<a href=\"http:\/\/mai.cailiaoren.com\/\" target=\"_blank\">\u6750\u6599\u4eba<\/a>\u3001\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a3D\u6253\u5370\u6280\u672f\u81ea\u4ece\u95ee\u4e16\u4ee5\u6765\uff0c\u4fbf\u63a8\u52a8\u4e86\u8bb8\u591a\u4ea7\u4e1a\u7684\u9ad8\u901f\u53d1\u5c55\uff0c\u8d8a\u6765\u8d8a\u53d7\u5230\u79d1\u7814\u4eba\u5458\u7684\u91cd\u89c6\uff0c\u73b0\u5728\u5bc6\u82cf\u91cc\u5927\u5b66\u7406\u5de5\u5b66\u9662\u7684\u79d1\u7814\u4eba\u5458\u4eec\u5c063D\u6253\u5370\u6280\u672f\u76f4\u63a5\u5e94\u7528\u5728\u53ef\u4f38\u7f29\u7684\u7535\u5b50&#8230;<\/p>\n","protected":false},"author":36,"featured_media":62455,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[28],"class_list":["post-62454","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-3d"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/62454"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/36"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=62454"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/62454\/revisions"}],"predecessor-version":[{"id":62995,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/62454\/revisions\/62995"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/62455"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=62454"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=62454"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=62454"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}