{"id":65736,"date":"2017-02-22T14:00:23","date_gmt":"2017-02-22T06:00:23","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=65736"},"modified":"2017-02-16T08:19:40","modified_gmt":"2017-02-16T00:19:40","slug":"%e8%ae%a1%e7%ae%97%e6%9c%ba%e6%a8%a1%e6%8b%9f%ef%bc%8c%e9%81%87%e8%a7%81%e6%af%94%e7%9f%b3%e5%a2%a8%e7%83%af%e6%9b%b4%e5%a5%bd%e7%9a%84%e4%b8%80%e7%bb%b4%e7%a1%bc%e9%93%be","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=65736","title":{"rendered":"\u8ba1\u7b97\u673a\u6a21\u62df\uff0c\u9047\u89c1\u6bd4\u77f3\u58a8\u70ef\u66f4\u597d\u7684\u4e00\u7ef4\u787c\u94fe"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u77f3\u58a8\u70ef\u56e0\u5176\u7279\u6b8a\u7684\u7269\u7406\u5316\u5b66\u6027\u8d28\u800c\u5e7f\u53d7\u5173\u6ce8\uff0c\u73b0\u5728\u79d1\u5b66\u5bb6\u4eec\u901a\u8fc7\u8ba1\u7b97\u673a\u6a21\u62df\u53d1\u73b0\u4e86\u53e6\u4e00\u79cd\u6027\u80fd\u751a\u81f3\u66f4\u597d\u7684\u6750\u6599\u2014\u2014\u4e00\u7ef4\u787c\u94fe\uff0c\u5176\u673a\u68b0\u5f3a\u5ea6\u53ef\u4ee5\u4e0e\u6700\u597d\u7684\u7eb3\u7c73\u6750\u6599\u76f8\u5ab2\u7f8e\uff0c\u5176\u88ab\u62c9\u4f38\u65f6\u4f1a\u53d8\u6210\u53cd\u94c1\u78c1\u6027\u534a\u5bfc\u4f53\uff0c\u800c\u62c9\u4f38\u4e00\u534a\u65f6\u5219\u4f1a\u5f62\u6210\u7c7b\u4f3c\u4e8c\u6781\u7ba1\u7684\u7ed3\u6784\u3002\u4e0d\u8fc7\u76ee\u524d\u8be5\u6750\u6599\u8fd8\u5904\u4e8e\u7406\u8bba\u7814\u7a76\u9636\u6bb5\uff0c\u5c1a\u672a\u88ab\u5408\u6210\u51fa\u6765\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-65738\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/Carbyne_web_1024.jpg\" alt=\"\" width=\"600\" height=\"243\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/Carbyne_web_1024.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/Carbyne_web_1024-300x122.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u4eba\u4eec\u90fd\u7231\u77f3\u58a8\u70ef\u2014\u2014\u8fd9\u79cd\u4ec5\u6709\u4e00\u4e2a\u539f\u5b50\u539a\u5ea6\u7684\u78b3\u8584\u819c\u4e0d\u4ec5\u7279\u522b\u67d4\u8f6f\uff0c\u800c\u4e14\u6bd4\u94bb\u77f3\u66f4\u786c\uff0c\u6bd4\u94a2\u66f4\u575a\u56fa\uff0c\u6700\u8fd1\u8fd8\u6210\u4e3a\u4e86\u8d85\u5bfc\u6750\u6599\u3002\u7136\u800c\u5b83\u5e76\u4e0d\u662f\u552f\u4e00\u8d85\u51fa\u671f\u671b\u7684\u7eb3\u7c73\u6750\u6599\uff0c\u7814\u7a76\u4eba\u5458\u6700\u8fd1\u6a21\u62df\u51fa\u4e86\u4e00\u79cd\u53ef\u62c9\u4f38\u7684\u4e00\u7ef4\u787c\u94fe\uff0c\u636e\u9884\u6d4b\u8be5\u6750\u6599\u751a\u81f3\u5177\u6709\u6bd4\u77f3\u58a8\u70ef\u66f4\u597d\u7684\u6027\u80fd\u3002<\/p>\n<p>\u9700\u8981\u8bf4\u660e\u7684\u662f\uff0c\u8fc4\u4eca\u4e3a\u6b62\u8fd9\u79cd\u4e00\u7ef4\u787c\u94fe\u8fd8\u5c1a\u672a\u88ab\u5236\u5907\u51fa\u6765\uff0c\u76ee\u524d\u5bf9\u8fd9\u79cd\u6750\u6599\u7684\u7814\u7a76\u8fd8\u5904\u4e8e\u8ba1\u7b97\u673a\u6a21\u62df\u9636\u6bb5\u3002<\/p>\n<p>\u4f46\u662f\u5b9e\u9a8c\u5ba4\u4e2d\u5df2\u7ecf\u6210\u529f\u5730\u5408\u6210\u4e86\u5355\u5c42\u539f\u5b50\u3001\u5bcc\u52d2\u70ef\u7b3c\u72b6\u5df4\u57fa\u7403\u5f62\u5f0f\u7684\u787c\uff0c\u4ee5\u53ca\u88ab\u79f0\u4e3a\u78b3\u7094\u7684\u5355\u5c42\u539f\u5b50\u78b3\u94fe\uff08\u5982\u4e0a\u56fe\u6240\u793a\uff09\u3002\u56e0\u6b64\uff0c\u7814\u7a76\u4eba\u5458\u9884\u6d4b\uff0c\u4e00\u7ef4\u5355\u539f\u5b50\u787c\u94fe\u8fdf\u65e9\u4f1a\u6210\u4e3a\u73b0\u5b9e\u3002<\/p>\n<p>\u5982\u679c\u6210\u771f\u7684\u8bdd\uff0c\u6211\u4eec\u5c06\u56e0\u6b64\u53d7\u76ca\u3002\u56e0\u4e3a\u6a21\u62df\u7ed3\u679c\u8868\u660e\uff1a\u4e00\u7ef4\u787c\u94fe\u6709\u4e00\u4e9b\u975e\u5e38\u4e0d\u53ef\u601d\u8bae\u7684\u6027\u8d28\u3002\u4f8b\u5982\uff0c\u5f53\u5b83\u4eec\u88ab\u62c9\u4f38\u65f6\uff0c\u8fd9\u4e9b\u91d1\u5c5e\u94fe\u4f1a\u53d8\u6210\u53cd\u94c1\u78c1\u6027\u534a\u5bfc\u4f53\u2014\u2014\u8fd9\u610f\u5473\u7740\u975e\u78c1\u6027\u91d1\u5c5e\u90fd\u53ef\u4ee5\u53d8\u6210\u6ca1\u6709\u7535\u963b\u7684\u8d85\u5bfc\u4f53\u3002\u800c\u5f53\u5b83\u4eec\u88ab\u91ca\u653e\u65f6\uff0c\u5b83\u4eec\u5c06\u6062\u590d\u5230\u6574\u9f50\u7684\u53cc\u539f\u5b50\u539a\u5ea6\u7684\u5e26\u72b6\u7ed3\u6784\u3002<\/p>\n<p>\u636e\u9884\u6d4b\uff0c\u8be5\u6750\u6599\u7684\u673a\u68b0\u521a\u5ea6\u53ef\u4ee5\u4e0e\u76ee\u524d\u6027\u80fd\u6700\u597d\u7684\u7eb3\u7c73\u6750\u6599\u5ab2\u7f8e\u3002\u5b83\u4eec\u53ef\u4ee5\u4f5c\u4e3a\u8ff7\u4f60\u7684\u6052\u529b\u5f39\u7c27\u2014\u2014\u4e00\u79cd\u4e0d\u540c\u5e38\u89c4\u7684\u5f39\u7c27\uff0c\u5728\u5176\u62c9\u4f38\u8303\u56f4\u5185\u6240\u9700\u65bd\u52a0\u7684\u529b\u6052\u5b9a\uff08\u5927\u591a\u6570\u5f39\u7c27\u62c9\u4f38\u8d8a\u957f\uff0c\u6240\u9700\u65bd\u52a0\u7684\u529b\u8d8a\u5927\uff09\u3002<\/p>\n<p>\u867d\u7136\u8fd9\u9879\u5de5\u4f5c\u8fd8\u5904\u4e8e\u7406\u8bba\u9636\u6bb5\uff0c\u4f46\u5b83\u5e76\u975e\u4e0d\u5207\u5b9e\u9645\u3002\u8fd9\u4e9b\u6a21\u62df\u5de5\u4f5c\u662f\u7531\u83b1\u65af\u5927\u5b66\u7684\u4e00\u4e2a\u56e2\u961f\u8fdb\u884c\u7684\uff0c\u5176\u64c5\u957f\u5bf9\u8fd8\u4e0d\u5b58\u5728\u7684\u6750\u6599\u8fdb\u884c\u539f\u5b50\u7ea7\u522b\u7684\u8ba1\u7b97\u673a\u6a21\u62df\u3002<\/p>\n<p>\u4ed6\u4eec\u5df2\u6709\u6210\u7ee9\u76f8\u5f53\u4e0d\u9519\u3002\u8be5\u56e2\u961f\u4e4b\u524d\u5df2\u7ecf\u9884\u6d4b\u5e76\u6a21\u62df\u4e86\u79f0\u4e3a\u201c\u787c\u5429\u201d\u7684\u4e8c\u7ef4\u787c\u8584\u819c\u7684\u884c\u4e3a\uff0c\u5176\u4e0e\u77f3\u58a8\u70ef\u3001\u78b3\u94fe\u4ee5\u53ca\u787c\u5bcc\u52d2\u70ef\u7b49\u5df2\u7ecf\u88ab\u5b9e\u9a8c\u5ba4\u5408\u6210\u51fa\u7684\u6750\u6599\u5f88\u76f8\u4f3c\u3002<\/p>\n<p>\u9996\u5e2d\u7814\u7a76\u5458Boris Yakobson\u8bf4\uff1a\u201c\u6211\u4eec\u5173\u4e8e\u78b3\u7094\u4ee5\u53ca\u5e73\u9762\u787c\u7684\u5de5\u4f5c\u4f7f\u6211\u4eec\u76f8\u4fe1\u787c\u539f\u5b50\u7ec4\u6210\u7684\u4e00\u7ef4\u957f\u94fe\u662f\u4e00\u79cd\u53ef\u80fd\u5b9e\u73b0\u7684\u6709\u8da3\u7ed3\u6784\u3002\u201d<\/p>\n<p>\u201c\u6211\u4eec\u60f3\u77e5\u9053\u5b83\u662f\u5426\u7a33\u5b9a\u4ee5\u53ca\u5177\u6709\u4ec0\u4e48\u6027\u8d28\u3002\u8fd9\u5c31\u662f\u73b0\u4ee3\u7406\u8bba\u8ba1\u7b97\u65b9\u6cd5\u4ee4\u4eba\u5370\u8c61\u6df1\u523b\u7684\u5730\u65b9\uff0c\u56e0\u4e3a\u4eba\u4eec\u53ef\u4ee5\u5bf9\u8fd8\u4e0d\u5b58\u5728\u7684\u7ed3\u6784\u505a\u76f8\u5f53\u73b0\u5b9e\u7684\u8bc4\u4f30\u3002\u201d<\/p>\n<p>\u77f3\u58a8\u70ef\u662f\u6574\u5c42\u78b3\u539f\u5b50\u6784\u6210\u7684\u4e8c\u7ef4\u7ed3\u6784\uff0c\u4e0e\u4e4b\u4e0d\u540c\u7684\u662f\uff0c\u83b1\u65af\u5927\u5b66\u56e2\u961f\u6b63\u5728\u6a21\u62df\u7684\u787c\u7ed3\u6784\u53ea\u5b58\u5728\u4e8e\u4e00\u7ef4\u65b9\u5411\u4e0a\uff0c\u7531\u5355\u539f\u5b50\u94fe\u6216\u53cc\u539f\u5b50\u5e26\u7ec4\u6210\u3002<\/p>\n<p>\u5e26\u548c\u94fe\u4e0e\u5176\u8bf4\u662f\u4e24\u79cd\u4e0d\u540c\u7684\u7ed3\u6784\uff0c\u5b9e\u9645\u4e0a\u66f4\u50cf\u662f\u4e00\u7ef4\u787c\u7684\u4e24\u79cd\u660e\u786e\u5b9a\u4e49\u7684\u76f8\u3002<\/p>\n<p>\u8fd9\u610f\u5473\u7740\u5f53\u4e00\u7ef4\u787c\u88ab\u62c9\u4f38\u65f6\uff0c\u5176\u4ece\u53cc\u539f\u5b50\u5e26\u72b6\u7ed3\u6784\u8f6c\u53d8\u4e3a\u5355\u539f\u5b50\u94fe\uff0c\u7136\u540e\u968f\u7740\u538b\u529b\u7684\u91ca\u653e\u53c8\u4f1a\u518d\u6b21\u8f6c\u53d8\u56de\u6765\u3002<\/p>\n<p>\u4f60\u53ef\u4ee5\u770b\u5230\uff0c\u5728\u4e0b\u9762\u7684\u6a21\u62df\u4e2d\u4e00\u4e2a64\u4e2a\u539f\u5b50\u7684\u787c\u94fe\u5c31\u5728\u53d1\u751f\u8fd9\u6837\u7684\u8f6c\u53d8\uff0c\u5b83\u88ab\u62c9\u4f38\u5230\u65ad\u70b9\uff1a<\/p>\n<p>\u201c\u787c\u4e0e\u78b3\u975e\u5e38\u4e0d\u540c\uff0c\u201dYakobson\u8bf4\uff0c\u201c\u5b83\u559c\u6b22\u5f62\u6210\u4e24\u6392\u539f\u5b50\uff0c\u5c31\u50cf\u7528\u4e8e\u6865\u6881\u6784\u9020\u7684\u6841\u67b6\uff0c\u8fd9\u4f3c\u4e4e\u662f\u5176\u6700\u7a33\u5b9a\u3001\u80fd\u91cf\u6700\u4f4e\u7684\u72b6\u6001\u3002\u201d<\/p>\n<p>\u201c\u5982\u679c\u4f60\u62c9\u5b83\uff0c\u5b83\u5c31\u5f00\u59cb\u4f38\u5c55\uff0c\u5176\u539f\u5b50\u5c48\u4ece\u4e8e\u8fd9\u4e2a\u5355\u539f\u5b50\u7ebf\uff0c\u5982\u679c\u4f60\u6536\u56de\u8fd9\u4e2a\u529b\uff0c\u5b83\u5c31\u6298\u53e0\u56de\u6765\uff0c\u201d\u4ed6\u8865\u5145\u8bf4\uff0c\u201c\u4ece\u7ed3\u6784\u4e0a\u770b\u8fd9\u5f88\u6709\u610f\u601d\uff0c\u540c\u65f6\u5b83\u4e5f\u6539\u53d8\u4e86\u5176\u7535\u5b50\u6027\u80fd\u3002\u201d<\/p>\n<p>\u5f88\u9177\u7684\u662f\uff0c\u8fd9\u4e24\u79cd\u72b6\u6001\u90fd\u6709\u5176\u72ec\u7279\u7684\u6027\u8d28\u2014\u2014\u5355\u539f\u5b50\u94fe\u662f\u4e00\u4e2a\u534a\u5bfc\u4f53\uff0c\u800c\u53cc\u539f\u5b50\u5e26\u662f\u4e00\u79cd\u96be\u4ee5\u7f6e\u4fe1\u575a\u786c\u7684\u91d1\u5c5e\uff0c\u80fd\u62b5\u6297\u5f62\u53d8\u3002<\/p>\n<p>\u201c\u8fd9\u4f7f\u5176\u6210\u4e3a\u4e00\u4e2a\u6709\u8da3\u7684\u7ec4\u5408\uff1a\u5f53\u4f60\u62c9\u4f38\u4e00\u534a\uff0c\u4f60\u4f1a\u5f97\u5230\u4e00\u90e8\u5206\u5e26\u548c\u4e00\u90e8\u5206\u94fe\u3002\u7531\u4e8e\u5176\u4e2d\u4e00\u79cd\u662f\u91d1\u5c5e\uff0c\u53e6\u4e00\u79cd\u662f\u534a\u5bfc\u4f53\uff0c\u5176\u5c31\u6210\u4e3a\u4e00\u79cd\u4e00\u7ef4\u3001\u53ef\u8c03\u8282\u7684\u2018\u8096\u7279\u57fa\u7ed3\u2019\u201dYakobson\u8bf4\u3002<\/p>\n<p>\u201c\u8096\u7279\u57fa\u7ed3\u201d\u662f\u7535\u5b50\u5728\u91d1\u5c5e\u548c\u534a\u5bfc\u4f53\u8fde\u63a5\u521d\u7684\u52bf\u5792\uff0c\u5e76\u4e14\u901a\u5e38\u7528\u4f5c\u4e8c\u6781\u7ba1\u6765\u63a7\u5236\u7535\u6d41\uff0c\u4e14\u4ec5\u5141\u8bb8\u5176\u5355\u5411\u6d41\u52a8\u3002<\/p>\n<p>\u8fd9\u79cd\u6750\u6599\u4e2d\u539f\u5b50\u7684\u81ea\u65cb\u4e5f\u5f88\u6709\u8da3\uff0c\u5f53\u88ab\u62c9\u4f38\u6210\u5355\u539f\u5b50\u94fe\u65f6\uff0c\u539f\u5b50\u7684\u201c\u4e0a\u201d\u6216\u201c\u4e0b\u201d\u81ea\u65cb\u72b6\u6001\u7684\u65b9\u5411\u5728\u76f8\u53cd\u7684\u65b9\u5411\u5bf9\u51c6\uff0c\u4f7f\u5176\u62e5\u6709\u53cd\u94c1\u78c1\u6027\u3002<\/p>\n<p>\u7814\u7a76\u4eba\u5458\u76ee\u524d\u5bf9\u53cd\u94c1\u78c1\u6750\u6599\u975e\u5e38\u611f\u5174\u8da3\uff0c\u7279\u522b\u662f\u90a3\u4e9b\u5bfc\u7535\u6027\u4e5f\u5f88\u597d\u7684\u6750\u6599\uff0c\u53ef\u7528\u4e8e\u81ea\u65cb\u7535\u5b50\u5b66\u7684\u53d1\u5c55\uff0c\u5c06\u6210\u4e3a\u672a\u6765\u7684\u9ad8\u6027\u80fd\u7535\u5b50\u5668\u4ef6\u3002<\/p>\n<p>\u76ee\u524d\u6211\u4eec\u8fd8\u4e0d\u77e5\u9053\u8fd9\u4e9b\u4e00\u7ef4\u787c\u94fe\u662f\u5426\u53ef\u4ee5\u5b58\u5728\u3002\u4f46\u4e8b\u5b9e\u4e0a\uff0c\u9884\u6d4b\u5230\u8be5\u6750\u6599\u5177\u6709\u8fd9\u4e48\u68d2\u7684\u6027\u8d28\uff0c\u610f\u5473\u7740\u79d1\u5b66\u5bb6\u4eec\u5f88\u6709\u53ef\u80fd\u5c3d\u6700\u5927\u52aa\u529b\u5728\u5b9e\u9a8c\u5ba4\u5408\u6210\u5b83\u4eec\u3002<\/p>\n<p>\u4f60\u6c38\u8fdc\u4e0d\u77e5\u9053\u4ed6\u4eec\u53ef\u80fd\u4f1a\u5728\u8fd9\u4e2a\u8fc7\u7a0b\u4e2d\u5076\u7136\u53d1\u73b0\u5176\u4ed6\u4ec0\u4e48\u72ec\u7279\u7684\u53d1\u73b0\u3002\u201c\u5373\u4f7f\u5b83\u4eec\u4ece\u6765\u90fd\u4e0d\u5b58\u5728\uff0c\u5b83\u4eec\u4ecd\u7136\u5f88\u91cd\u8981\uff0c\u56e0\u4e3a\u6211\u4eec\u5728\u63a2\u7d22\u6240\u6709\u7684\u53ef\u80fd\uff0c\u201d\u96c5\u5404\u5e03\u68ee\u8bf4\u3002\u8be5\u7814\u7a76\u5df2\u53d1\u8868\u5728\u7f8e\u56fd\u5316\u5b66\u5b66\u4f1a\u6742\u5fd7\u4e0a\u3002<\/p>\n<p>\u6807\u9898\uff1a<a href=\"http:\/\/www.sciencealert.com\/scientists-simulate-a-new-1d-material-that-could-be-even-weirder-than-graphene\" target=\"_blank\">Scientists simulate a new material that could be even weirder than grapheme<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/jacs.6b12750\" target=\"_blank\"><span class=\"hlFld-Title\">Mechanochemistry of One-Dimensional Boron: Structural and Electronic Transitions<\/span><\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u4e01\u83f2\u83f2\u63d0\u4f9b\u7d20\u6750\uff0c\u738b\u6668\u7f16\u8bd1\uff0c \u9ec4\u8d85\u5ba1\u6838\uff1b<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u77f3\u58a8\u70ef\u56e0\u5176\u7279\u6b8a\u7684\u7269\u7406\u5316\u5b66\u6027\u8d28\u800c\u5e7f\u53d7\u5173\u6ce8\uff0c\u73b0\u5728\u79d1\u5b66\u5bb6\u4eec\u901a\u8fc7\u8ba1\u7b97\u673a\u6a21\u62df\u53d1\u73b0\u4e86\u53e6\u4e00\u79cd\u6027\u80fd\u751a\u81f3\u66f4\u597d\u7684\u6750\u6599\u2014\u2014\u4e00\u7ef4\u787c\u94fe\uff0c\u5176\u673a\u68b0\u5f3a\u5ea6\u53ef\u4ee5\u4e0e\u6700\u597d\u7684\u7eb3\u7c73\u6750\u6599\u76f8\u5ab2\u7f8e\uff0c\u5176&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-65736","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/65736"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=65736"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/65736\/revisions"}],"predecessor-version":[{"id":65740,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/65736\/revisions\/65740"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=65736"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=65736"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=65736"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}