{"id":66426,"date":"2017-02-27T14:00:35","date_gmt":"2017-02-27T06:00:35","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=66426"},"modified":"2017-02-21T09:33:42","modified_gmt":"2017-02-21T01:33:42","slug":"3d%e6%89%93%e5%8d%b0%e6%9d%90%e6%96%99%e7%9a%84%e6%8e%a7%e5%88%b6%e5%ae%9e%e7%8e%b0%e6%96%b0%e9%ab%98%e5%ba%a6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=66426","title":{"rendered":"3D\u6253\u5370\u6750\u6599\u7684\u63a7\u5236\u5b9e\u73b0\u65b0\u9ad8\u5ea6"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8<\/strong>\uff1a\u672c\u6587\u4ecb\u7ecd\u4e86\u4e00\u79cd\u65b0\u578b3D\u6253\u5370\u6750\u6599\u7684\u65b9\u6cd5\u3002\u8fd9\u79cd\u65b9\u6cd5\u5229\u7528\u9676\u74f7\u6ce1\u6cab\u6cb9\u58a8\u8bbe\u8ba1\u51fa\u4e86\u5177\u6709\u72ec\u7acb\u8c03\u63a7\u5b8f\u89c2\u548c\u5fae\u89c2\u5b54\u9699\u7387\u76843D\u6750\u6599\uff0c\u8fd9\u9879\u6280\u672f\u672a\u6765\u6709\u671b\u5e94\u7528\u4e86\u5177\u6709\u591a\u529f\u80fd\u7684\u8f7b\u8d28\u7ed3\u6784\u6750\u6599\u7684\u5236\u5907\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-66723 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u65e0\u6807\u9898-1-1.png\" width=\"600\" height=\"471\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u65e0\u6807\u9898-1-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u65e0\u6807\u9898-1-1-300x236.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u5927\u81ea\u7136\u7528\u6709\u9650\u7684\u8bbe\u8ba1\u6750\u6599\u521b\u9020\u5947\u5999\u7684\u4ea7\u7269\u3002\u4f8b\u5982\uff0c\u8349\u53ef\u4ee5\u652f\u6491\u5176\u81ea\u8eab\u91cd\u91cf\uff0c\u62b5\u6297\u5f3a\u98ce\u529b\u8d1f\u8377\uff0c\u5e76\u4e14\u80fd\u5728\u88ab\u5439\u5012\u4e4b\u540e\u6062\u590d\u3002\u690d\u7269\u7684\u8010\u5bd2\u6027\u6765\u81ea\u5b83\u4e2d\u7a7a\u3001\u7ba1\u72b6\u5b8f\u89c2\u7ed3\u6784\u548c\u591a\u5b54\u6216\u7ec6\u80de\u5fae\u7ed3\u6784\u7684\u7ec4\u5408\u3002\u8fd9\u4e9b\u7ed3\u6784\u7279\u5f81\u5171\u540c\u4f5c\u7528\uff0c\u4f7f\u5f97\u8349\u5177\u6709\u5f3a\u5927\u7684\u673a\u68b0\u6027\u80fd\u3002<\/p>\n<p>\u53d7\u81ea\u7136\u754c\u7ec6\u80de\u7ed3\u6784\u7684\u542f\u53d1\uff0c\u54c8\u4f5b\u5927\u5b66\u751f\u7269\u542f\u53d1\u5de5\u7a0b\u6000\u65af\u7814\u7a76\u6240\uff0c\u54c8\u4f5b\u5927\u5b66\u7ea6\u7ff0\u00b7\u9c8d\u5c14\u68ee\u5de5\u7a0b\u4e0e\u5e94\u7528\u79d1\u5b66\u5b66\u9662\uff08SEAS\uff09\u548c\u9ebb\u7701\u7406\u5de5\u5b66\u9662\u7684\u7814\u7a76\u4eba\u5458\u5f00\u53d1\u4e86\u4e00\u79cd\u5236\u5907\u65b0\u578b3D\u6253\u5370\u6750\u6599\u7684\u65b9\u6cd5\u3002\u8fd9\u4e2a\u65b9\u6cd5\u5229\u7528\u9676\u74f7\u6ce1\u6cab\u6cb9\u58a8\u6765\u5b9e\u73b0\u5b8f\u89c2\u548c\u5fae\u89c2\u5b54\u9699\u7387\u7684\u72ec\u7acb\u8c03\u63a7\u3002\u4ed6\u4eec\u7684\u65b9\u6cd5\u53ef\u4ee5\u7528\u4e8e\u5236\u9020\u8f7b\u8d28\u7ed3\u6784\u6750\u6599\u3001\u9694\u70ed\u6216\u7ec4\u7ec7\u652f\u67b6\u3002<\/p>\n<p>\u6000\u65af\u7814\u7a76\u6240\u6838\u5fc3\u6559\u5458\uff0cSEAS\u751f\u7269\u542f\u53d1\u5de5\u7a0b\u7684Hansj\u00f6rg Wyss\u6559\u6388\uff0c\u540c\u65f6\u4e5f\u662f\u672c\u6587\u7684\u8d44\u6df1\u4f5c\u8005Jennifer Lewis\u63d0\u5230\uff1a\u201c\u901a\u8fc7\u6269\u5927\u53ef\u5370\u5237\u6750\u6599\u7684\u7ec4\u6210\u7a7a\u95f4\uff0c\u6211\u4eec\u53ef\u4ee5\u751f\u4ea7\u51fa\u5177\u6709\u7279\u6b8a\u521a\u5ea6\u7684\u8f7b\u8d28\u7ed3\u6784\u201d\u3002<\/p>\n<p>Lewis\u5b9e\u9a8c\u5ba4\u4f7f\u7528\u7684\u9676\u74f7\u6ce1\u6cab\u6cb9\u58a8\u542b\u6709\u6c27\u5316\u94dd\u9897\u7c92\uff0c\u6c34\u548c\u7a7a\u6c14\u3002<\/p>\n<p>Lewis\u5b9e\u9a8c\u5ba4\u7684\u7814\u7a76\u751f\uff0c\u4e5f\u662f\u672c\u6587\u7684\u7b2c\u4e00\u4f5c\u8005Joseph Muth\u8bf4\uff1a\u201c\u6ce1\u6cab\u6cb9\u58a8\u5f88\u6709\u8da3\uff0c\u56e0\u4e3a\u4f60\u53ef\u4ee5\u5728\u66f4\u5927\u7684\u7ec6\u80de\u5b8f\u89c2\u7ed3\u6784\u4e2d\u5bf9\u5176\u5fae\u89c2\u7ed3\u6784\u8fdb\u884c\u6570\u5b57\u56fe\u6848\u5316\u3002\u6cb9\u58a8\u51dd\u56fa\u540e\uff0c\u5f97\u5230\u7684\u7ed3\u6784\u7531\u88ab\u591a\u4e2a\u957f\u5ea6\u5c3a\u5ea6\u7684\u9676\u74f7\u6750\u6599\u5305\u56f4\u7684\u7a7a\u6c14\u7ec4\u6210\u3002\u5f53\u4f60\u5728\u7ed3\u6784\u4e2d\u52a0\u5165\u5b54\u9699\u65f6\uff0c\u4f60\u5c06\u8d4b\u4e88\u5b83\u672c\u6765\u4e0d\u4f1a\u6709\u7684\u6027\u8d28\u3002\u201d<\/p>\n<p>\u901a\u8fc7\u63a7\u5236\u6ce1\u6cab\u7684\u5fae\u89c2\u7ed3\u6784\uff0c\u7814\u7a76\u4eba\u5458\u53ef\u4ee5\u8c03\u63a7\u6cb9\u58a8\u7684\u6027\u80fd\uff0c\u4ee5\u53ca\u5b83\u5728\u5fae\u89c2\u5c3a\u5ea6\u4e0a\u5982\u4f55\u53d8\u5f62\u3002 \u901a\u8fc7\u4f18\u5316\uff0c\u56e2\u961f\u53ef\u4ee5\u6253\u5370\u5177\u6709\u53ef\u8c03\u51e0\u4f55\u5f62\u72b6\uff0c\u5bc6\u5ea6\u548c\u521a\u5ea6\u7684\u8f7b\u8d28\u516d\u89d2\u5f62\u548c\u4e09\u89d2\u5f62\u8702\u7a9d\u3002<\/p>\n<p>\u9ebb\u7701\u7406\u5de5\u5927\u5b66\u6750\u6599\u79d1\u5b66\u548c\u5de5\u7a0b\u7684Matoula S. Salapatas\u6559\u6388\uff0c\u4e5f\u662f\u672c\u6587\u7684\u5171\u540c\u4f5c\u8005Lorna Gibson\u535a\u58eb\u8bf4\uff0c\u201c\u8fd9\u4e2a\u8fc7\u7a0b\u7ed3\u5408\u4e86\u4e24\u4e2a\u4e16\u754c\u7684\u4f18\u52bf\uff0c\u4f60\u53ef\u4ee5\u901a\u8fc7\u6ce1\u6cab\u5904\u7406\u548c\u5168\u5c40\u67b6\u6784\u63a7\u5236\u6765\u5b9e\u73b0\u5fae\u89c2\u7ed3\u6784\u63a7\u5236\u3002\u56e0\u4e3a\u6211\u4eec\u6b63\u5728\u6253\u5370\u5df2\u7ecf\u5305\u542b\u7279\u5b9a\u5fae\u7ed3\u6784\u7684\u4e1c\u897f\uff0c\u6240\u4ee5\u4e0d\u5fc5\u5bf9\u6bcf\u4e2a\u5355\u72ec\u7684\u6837\u54c1\u8fdb\u884c\u56fe\u6848\u5316\u3002\u8fd9\u5c31\u4f7f\u6211\u4eec\u80fd\u591f\u4ee5\u6bd4\u4ee5\u524d\u66f4\u53ef\u63a7\u7684\u65b9\u5f0f\u6765\u83b7\u5f97\u5177\u6709\u7279\u5b9a\u5c42\u6b21\u7684\u7ed3\u6784\u3002<\/p>\n<p>Muth\u8bf4\uff0c\u201c\u73b0\u5728\u6211\u4eec\u53ef\u4ee5\u5236\u9020\u591a\u529f\u80fd\u6750\u6599\uff0c\u5728\u8fd9\u4e9b\u6750\u6599\u4e2d\uff0c\u5305\u62ec\u673a\u68b0\u6027\u80fd\u3001\u70ed\u6027\u80fd\u548c\u4f20\u8f93\u7279\u6027\u5728\u5185\u7684\u8bb8\u591a\u4e0d\u540c\u7684\u6750\u6599\u7279\u6027\u53ef\u4ee5\u5728\u4e00\u4e2a\u7b80\u5355\u7684\u6253\u5370\u6b65\u9aa4\u4e2d\u8fdb\u884c\u7ed3\u6784\u4f18\u5316\u3002\u201d<\/p>\n<p>\u867d\u7136\u8be5\u56e2\u961f\u4e13\u6ce8\u4e8e\u7528\u4e8e\u8be5\u7814\u7a76\u7684\u5355\u4e00\u9676\u74f7\u6750\u6599\uff0c\u4f46\u53ef\u5370\u5237\u6ce1\u6cab\u6cb9\u58a8\u8fd8\u662f\u53ef\u4ee5\u7531\u8bb8\u591a\u6750\u6599\u5236\u6210\u7684\uff0c\u5305\u62ec\u5176\u4ed6\u9676\u74f7\u3001\u91d1\u5c5e\u548c\u805a\u5408\u7269\u3002<\/p>\n<p>Lewis\u8bf4\uff0c\u201c\u8fd9\u9879\u5de5\u4f5c\u4ee3\u8868\u4e86\u8fc8\u5411\u6784\u5efa\u591a\u5b54\u6750\u6599\u7684\u53ef\u6269\u5c55\u5236\u9020\u7684\u91cd\u8981\u4e00\u6b65\u3002\u201d<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.3dprintingprogress.com\/articles\/10595\/new-level-of-control-over-the-structure-of-3d-printed-materials\" target=\"_blank\">New level of control over the structure of 3D-printed materials<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u6708\u4eae\u63d0\u4f9b\u7d20\u6750\uff0c\u51af\u5a1c\u7f16\u8bd1\uff0c\u65f6\u51b0\u9065\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a><\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u672c\u6587\u4ecb\u7ecd\u4e86\u4e00\u79cd\u65b0\u578b3D\u6253\u5370\u6750\u6599\u7684\u65b9\u6cd5\u3002\u8fd9\u79cd\u65b9\u6cd5\u5229\u7528\u9676\u74f7\u6ce1\u6cab\u6cb9\u58a8\u8bbe\u8ba1\u51fa\u4e86\u5177\u6709\u72ec\u7acb\u8c03\u63a7\u5b8f\u89c2\u548c\u5fae\u89c2\u5b54\u9699\u7387\u76843D\u6750\u6599\uff0c\u8fd9\u9879\u6280\u672f\u672a\u6765\u6709\u671b\u5e94\u7528\u4e86\u5177\u6709\u591a\u529f\u80fd\u7684\u8f7b\u8d28\u7ed3&#8230;<\/p>\n","protected":false},"author":230,"featured_media":66429,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[28],"class_list":["post-66426","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-3d"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66426"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=66426"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66426\/revisions"}],"predecessor-version":[{"id":66923,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66426\/revisions\/66923"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/66429"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=66426"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=66426"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=66426"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}