{"id":66457,"date":"2017-02-25T14:00:18","date_gmt":"2017-02-25T06:00:18","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=66457"},"modified":"2017-02-21T09:25:17","modified_gmt":"2017-02-21T01:25:17","slug":"%e5%8f%af%e5%9b%9e%e6%94%b6%e7%a2%b3%e7%ba%a4%e7%bb%b4%e8%bf%9b%e5%86%9b%e6%b1%bd%e8%bd%a6%e8%a1%8c%e4%b8%9a","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=66457","title":{"rendered":"\u53ef\u56de\u6536\u78b3\u7ea4\u7ef4\u8fdb\u519b\u6c7d\u8f66\u884c\u4e1a"},"content":{"rendered":"<p><strong><b>\u6750\u6599\u725b\u6ce8<\/b><\/strong><strong><b>\uff1a<\/b><\/strong>\u8bf4\u4e2d\u56fd\u5730\u5927\u7269\u535a\uff0c\u8bf4\u4e2d\u56fd\u8d44\u6e90\u4e30\u5bcc\uff0c\u4f46\u662f\uff0c\u518d\u8fc7100\u5e74\u5462\uff1f\u518d\u8fc71000\u5e74\u5462\uff1f\u4e2d\u56fd\u4eba\u53e3\u5728\u9010\u6e10\u589e\u591a\uff0c\u4e2d\u56fd\u7684\u4eba\u5747\u6d88\u8017\u4e5f\u5728\u9010\u6e10\u589e\u591a\uff0c\u5728\u53ef\u6301\u7eed\u6027\u53d1\u5c55\u7684\u9053\u8def\u4e0a\uff0c\u5947\u745e\u662f\u8fd9\u6837\u505a\u7684\u2026\u2026<\/p>\n<p>\u4e2d\u56fd\u5947\u745e\u65b0\u80fd\u6e90\u6c7d\u8f66\u6280\u672f\u6709\u9650\u516c\u53f8\u5df2\u627f\u8bfa\u5b83\u7684eQ1\u7535\u52a8\u6c7d\u8f66\u5c06\u4f7f\u7528ELG\u78b3\u7ea4\u7ef4\u6709\u9650\u516c\u53f8\u7684\u53ef\u56de\u6536\u78b3\u7ea4\u7ef4\u3002\u5176\u7ec8\u6781\u76ee\u6807\u662f\u5c06\u78b3\u7ea4\u7ef4\u5e7f\u6cdb\u5e94\u7528\u4e8e\u9ad8\u5bb9\u91cf\u6c7d\u8f66\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-66458\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u56fe\u72471-8.jpg\" alt=\"\" width=\"500\" height=\"417\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u56fe\u72471-8.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u56fe\u72471-8-300x250.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>ELG\u78b3\u7ea4\u7ef4\u6709\u9650\u516c\u53f8\uff08Coseley, UK\uff09\u548c\u827e\u8fbe\u7d22\u9ad8\u65b0\u6750\u6599\u829c\u6e56\u6709\u9650\u516c\u53f8\uff08\u829c\u6e56\uff0c\u4e2d\u56fd\uff09\u7b7e\u7f72\u4e86\u6709\u5173\u5728\u6c7d\u8f66\u884c\u4e1a\u57fa\u4e8eELG\u516c\u53f8\u7684\u53ef\u56de\u6536\u78b3\u7ea4\u7ef4\u6750\u6599\u5408\u4f5c\u5f00\u53d1\u8f7b\u8d28\u590d\u5408\u7ec4\u4ef6\u7684\u5408\u4f5c\u5907\u5fd8\u5f55\u3002<\/p>\n<p>\u5408\u4f5c\u7684\u6700\u521d\u7126\u70b9\u662f\u8c03\u67e5\u5df2\u901a\u8fc7\u5947\u745e\u516c\u53f8\u8ba4\u5b9a\u7684\u5947\u745eeQ1\u7535\u52a8\u6c7d\u8f66\u7684\u5e94\u7528\u7a0b\u5e8f\u3002\u5947\u745eeQ1\u5df2\u5e7f\u6cdb\u91c7\u7528\u94dd\u5408\u91d1\u6280\u672f\u6765\u51cf\u8f7b\u8d28\u91cf\uff0c\u5408\u4f5c\u7684\u73b0\u9636\u6bb5\u76ee\u6807\u662f\u9009\u62e9\u6027\u5730\u4f7f\u7528\u78b3\u7ea4\u7ef4\u590d\u5408\u6750\u6599\uff0c\u8fdb\u4e00\u6b65\u51cf\u8f7b\u8f66\u8eab\u8d28\u91cf\u3002\u957f\u8fdc\u7684\u76ee\u6807\u5219\u662f\u5c06\u8fd9\u4e9b\u9879\u76ee\u6210\u679c\u5e94\u7528\u4e8e\u5947\u745e\u4f20\u7edf\u8f66\u4e0a\u3002<\/p>\n<p>\u6839\u636e\u4e2d\u56fd\u673a\u68b0\u79d1\u5b66\u6280\u672f\u7814\u7a76\u9662\u5148\u8fdb\u5236\u9020\u6280\u672f\u4e2d\u5fc3\uff08CAMTA\uff09\u7684\u6a0a\u5e7f\u5b8f\u6559\u6388\u56e2\u961f\u5bf9ELS\u6750\u6599\u7684\u521d\u6b65\u8bc4\u4f30\uff0c\u5947\u745e\u58f0\u660e\u5c06\u5bf9\u6750\u6599\u7684\u521d\u7ea7\u5e94\u7528\u8fdb\u884c\u8c03\u7814\uff0c\u5e76\u9884\u8bbe\u4e86\u6280\u672f\u76ee\u6807\u548c\u5546\u4e1a\u76ee\u6807\u3002ELG\u3001\u827e\u8fbe\u7d22\u548c\u5947\u745e\u6253\u7b97\u8fbe\u6210\u4e00\u9879\u5168\u9762\u7684\u534f\u8bae\uff0c\u5728\u829c\u6e56\u8fdb\u884c\u76f8\u5173\u96f6\u90e8\u4ef6\u7684\u5168\u89c4\u6a21\u751f\u4ea7\u3002\u5f53\u56fd\u5185\u5f00\u59cb\u5927\u91cf\u751f\u4ea7\u53ef\u56de\u6536\u78b3\u7ea4\u7ef4\u6750\u6599\u65f6\uff0c\u6839\u636e\u8fd9\u9879\u534f\u8bae\uff0cELG\u5c06\u5728\u4e2d\u56fd\u5efa\u7acb\u78b3\u7ea4\u7ef4\u6750\u6599\u56de\u6536\u4e2d\u5fc3\u3002\u4f7f\u7528\u7684ELG\u6750\u6599\u4e3b\u8981\u662fCARBISO M\u548cCARBISO TM\u3002<\/p>\n<p>ELG\u7684\u603b\u7ecf\u7406Frazer Barnes\u8bf4\uff1a\u201c\u901a\u8fc7\u5927\u91cf\u4f7f\u7528\u94dd\u5408\u91d1\uff0ceQ1\u5728\u4e2d\u56fd\u6c7d\u8f66\u884c\u4e1a\u5c31\u8f7b\u8d28\u5316\u65b9\u9762\u8bb2\u5df2\u7ecf\u6709\u5f88\u5927\u7684\u8fdb\u6b65\u4e86\uff0c\u6211\u4eec\u5f88\u9ad8\u5174\u80fd\u4e0e\u827e\u8fbe\u7d22\u548c\u5947\u745e\u7684\u521b\u65b0\u5de5\u7a0b\u56e2\u961f\u5408\u4f5c\uff0c\u5c06\u78b3\u7ea4\u7ef4\u590d\u5408\u6750\u6599\u5e94\u7528\u4e8e\u6c7d\u8f66\u884c\u4e1a\uff0c\u534f\u52a9\u4ed6\u4eec\u66f4\u4e0a\u4e00\u5c42\u697c\u3002\u201d<\/p>\n<p>\u827e\u8fbe\u7d22\u7684\u8463\u4e8b\u957f\u517c\u9996\u5e2d\u6267\u884c\u5b98\u6881\u6ce2\u535a\u58eb\u8bf4\uff1a\u201c\u901a\u8fc7\u5229\u7528\u53ef\u56de\u6536\u78b3\u7ea4\u7ef4\uff0c\u52a0\u4e0a\u4e0e\u7ecf\u9a8c\u5982\u6b64\u4e30\u5bcc\u7684\u5408\u4f5c\u4f19\u4f34\u5408\u4f5c\uff0c\u8fd9\u4e2a\u9879\u76ee\u80fd\u4f7f\u6211\u4eec\u89e3\u51b3\u5728\u6c7d\u8f66\u884c\u4e1a\u5927\u89c4\u6a21\u4f7f\u7528\u78b3\u7ea4\u7ef4\u5e26\u6765\u7684\u6210\u672c\u9ad8\u96be\u9898\uff0c\u6211\u4eec\u7684\u613f\u666f\u662f\u6b64\u6b21\u5408\u4f5c\u80fd\u5728\u829c\u6e56\u5efa\u7acb\u4e00\u4e2a\u6c7d\u8f66\u590d\u5408\u6750\u6599\u4e2d\u5fc3\uff0c\u8fd9\u4e5f\u54cd\u5e94\u4e86\u4e2d\u56fd\u590d\u5408\u6750\u6599\u884c\u4e1a\u7684\u53ef\u6301\u7eed\u53d1\u5c55\u6218\u7565\u3002\u201d<\/p>\n<p>\u5947\u745e\u6c7d\u8f66\u6709\u9650\u516c\u53f8\u526f\u603b\u7ecf\u7406\uff0c\u5947\u745e\u65b0\u80fd\u6e90\u6c7d\u8f66\u6280\u672f\u6709\u9650\u516c\u53f8\u603b\u7ecf\u7406\u9ad8\u7acb\u65b0\u8bf4\uff1a\u201c\u4e3a\u4e86\u6ee1\u8db3\u73af\u5883\u548c\u6027\u80fd\u4e24\u4e2a\u65b9\u9762\u7684\u9700\u6c42\uff0c\u51cf\u8f7b\u65b0\u80fd\u6e90\u6c7d\u8f66\u548c\u4f20\u7edf\u8f66\u7684\u8d28\u91cf\u90fd\u975e\u5e38\u6709\u5fc5\u8981\u3002\u6211\u4eec\u76f8\u4fe1\u78b3\u7ea4\u7ef4\u590d\u5408\u6750\u6599\u5c06\u4f1a\u5728\u8fd9\u65b9\u9762\u626e\u6f14\u975e\u5e38\u91cd\u8981\u7684\u89d2\u8272\uff0c\u800c\u4e14\u901a\u8fc7\u6211\u4eec\u4e0eELG\u548c\u827e\u8fbe\u7d22\u5728eQ1\u9879\u76ee\u4e0a\u7684\u5408\u4f5c\uff0c\u6211\u4eec\u5c06\u4f1a\u83b7\u5f97\u975e\u5e38\u91cd\u8981\u7684\u9879\u76ee\u7ecf\u9a8c\uff0c\u4ee5\u4fbf\u66f4\u597d\u5730\u670d\u52a1\u4e8e\u6211\u4eec\u7684\u4f20\u7edf\u8f66\u3002\u201d<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.compositesworld.com\/blog\/post\/recycled-carbon-fiber-moves-into-automotive\" target=\"_blank\">Recycled carbon fiber moves into automotive<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u6708\u4eae\u63d0\u4f9b\u7d20\u6750\uff0c\u674e\u4e00\u51e1\u7f16\u8bd1\uff0c\u859b\u6587\u5609\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u8bf4\u4e2d\u56fd\u5730\u5927\u7269\u535a\uff0c\u8bf4\u4e2d\u56fd\u8d44\u6e90\u4e30\u5bcc\uff0c\u4f46\u662f\uff0c\u518d\u8fc7100\u5e74\u5462\uff1f\u518d\u8fc71000\u5e74\u5462\uff1f\u4e2d\u56fd\u4eba\u53e3\u5728\u9010\u6e10\u589e\u591a\uff0c\u4e2d\u56fd\u7684\u4eba\u5747\u6d88\u8017\u4e5f\u5728\u9010\u6e10\u589e\u591a\uff0c\u5728\u53ef\u6301\u7eed\u6027\u53d1\u5c55\u7684\u9053\u8def\u4e0a\uff0c\u5947\u745e\u662f&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-66457","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66457"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=66457"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66457\/revisions"}],"predecessor-version":[{"id":66918,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66457\/revisions\/66918"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=66457"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=66457"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=66457"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}