{"id":66977,"date":"2017-02-27T06:30:34","date_gmt":"2017-02-26T22:30:34","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=66977"},"modified":"2017-03-18T21:49:29","modified_gmt":"2017-03-18T13:49:29","slug":"acc-chem-res-%e6%9c%80%e6%96%b0%e7%bb%bc%e8%bf%b0%ef%bc%9a%e8%a1%a8%e7%95%8c%e9%9d%a2%e6%9e%84%e7%ad%91%e9%9d%9e%e8%b4%b5%e9%87%91%e5%b1%9e%e7%94%b5%e5%82%ac%e5%8c%96%e5%89%82%e7%94%a8%e4%ba%8e","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=66977","title":{"rendered":"\u4e54\u4e16\u748bAcc. Chem. Res. \u6700\u65b0\u7efc\u8ff0\uff1a\u8868\/\u754c\u9762\u6784\u7b51\u975e\u8d35\u91d1\u5c5e\u7535\u50ac\u5316\u5242\u7528\u4e8e\u9ad8\u6548\u7684\u80fd\u91cf\u8f6c\u5316\u8fc7\u7a0b"},"content":{"rendered":"<p>\u3010<strong>\u5f15\u8a00<\/strong>\u3011<\/p>\n<p>\u5728\u5168\u7403\u80fd\u6e90\u5b89\u5168\u548c\u53ef\u6301\u7eed\u53d1\u5c55\u6280\u672f\u7684\u63a8\u52a8\u4e0b\uff0c\u79d1\u5b66\u5bb6\u4eec\u5f00\u59cb\u805a\u7126\u4e8e\u7814\u53d1\u5927\u91cf\u5b58\u5728\u4e8e\u5730\u7403\u4e2d\u7684\u5ec9\u4ef7\u975e\u8d35\u91d1\u5c5e\u6216\u975e\u91d1\u5c5e\u7535\u50ac\u5316\u5242\uff0c\u7528\u4e8e\u80fd\u91cf\u5b58\u50a8\u4e0e\u8f6c\u5316\u8fc7\u7a0b\uff0c\u5982\u6c22\u6790\u51fa\uff08HER\uff09\uff0c\u6c27\u6790\u51fa\uff08OER\uff09\u548c\u6c27\u8fd8\u539f\uff08ORR\uff09\u53cd\u5e94\uff0c\u5e76\u53d6\u5f97\u4e86\u4e00\u5b9a\u6210\u679c\u3002\u7814\u7a76\u53d1\u73b0\uff0c\u901a\u8fc7\u8868\u9762\u539f\u5b50\u8bbe\u8ba1\uff08\u6742\u539f\u5b50\u63ba\u6742\uff09\u6216\u8005\u754c\u9762\u539f\u5b50\u5206\u5b50\u8bbe\u8ba1\uff08\u754c\u9762\u952e\u5408\uff09\u53ef\u4ee5\u8bf1\u5bfc\u65b0\u7684\u7269\u7406\u5316\u5b66\u6027\u8d28\u548c\u534f\u540c\u4f5c\u7528\uff0c\u4ece\u800c\u589e\u5f3a\u7535\u50ac\u5316\u6d3b\u6027\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea<strong>\u6fb3\u5927\u5229\u4e9a\u963f\u5f97\u83b1\u5fb7\u5927\u5b66\u7684\u4e54\u4e16\u748b\u6559\u6388\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u4ee5<strong>\u201cSurface and Interface Engineering of Noble-Metal-Free Electrocatalysts for Efficient Energy Conversion Processes\u201d<\/strong>\u4e3a\u9898\u5728<strong>Accounts of Chemical Research<\/strong>\u4e0a\u53d1\u8868\u7efc\u8ff0\uff0c\u8be6\u7ec6\u603b\u7ed3\u4e86\u5173\u4e8e\u901a\u8fc7\u8868\/\u754c\u9762\u539f\u5b50\u5206\u5b50\u8bbe\u8ba1\uff0c\u6784\u7b51\u78b3\u57fa\u975e\u8d35\u91d1\u5c5e\u6216\u975e\u91d1\u5c5e\u9ad8\u6548\u7535\u50ac\u5316\u5242\u5728ORR, OER\u548cHER\u4e2d\u8fd0\u7528\u7684\u8fd1\u671f\u8fdb\u5c55\u3002\u901a\u8fc7\u63ba\u6742\u4e00\u79cd\u6216\u591a\u79cd\u4e0d\u540c\u7535\u8d1f\u6027\u7684\u6742\u539f\u5b50\u6765\u6539\u53d8\u78b3\u6750\u6599\u7684\u7535\u5b50\u7ed3\u6784\u4ee5\u589e\u5f3a\u7535\u5316\u5b66\u6d3b\u6027\u3002\u8fdb\u4e00\u6b65\u901a\u8fc7\u78b3\u6750\u6599\u4e0e\u5176\u4ed6\u6d3b\u6027\u50ac\u5316\u5242\u7684\u8026\u5408\u5f62\u6210\u590d\u5408\u7535\u50ac\u5316\u5242\u8fd8\u53ef\u4ee5\u589e\u52a0\u6d3b\u6027\u5bc6\u5ea6\uff0c\u589e\u5f3a\u7535\u50ac\u5316\u6d3b\u6027\uff0c\u8fd9\u4e9b\u975e\u91d1\u5c5e\u78b3\u57fa\u50ac\u5316\u5242\u5df2\u7ecf\u5c55\u73b0\u51fa\u548c\u91d1\u5c5e\u57fa\u50ac\u5316\u5242\u76f8\u5ab2\u7f8e\u7684\u7535\u50ac\u5316\u6d3b\u6027\u3002\u5f53\u7136\uff0c\u5177\u6709M-N-C\u7ed3\u6784\u7684\u91d1\u5c5e-\u78b3\u57fa\u590d\u5408\u6750\u6599\u5177\u6709\u5f88\u5f3a\u7684\u7535\u50ac\u5316\u6d3b\u6027\u3002\u56e0\u6b64\uff0c\u6211\u4eec\u53ef\u4ee5\u5bf9\u6750\u6599\u8fdb\u884c\u8868\u3001\u754c\u9762\u539f\u5b50\u5206\u5b50\u8bbe\u8ba1\uff0c\u53ef\u63a7\u6784\u7b51\u5177\u6709\u591a\u5b54\u7ed3\u6784\u3001\u91d1\u5c5e\u6d3b\u6027\u4e2d\u5fc3\u7ed3\u6784\u4ee5\u53ca\u5927\u5b54\u7ed3\u6784\u7684\u7535\u50ac\u5316\u5242\uff0c\u4ece\u800c\u6709\u52a9\u4e8e\u6211\u4eec\u4e86\u89e3\u6750\u6599\u7ed3\u6784-\u6027\u80fd\u4e4b\u95f4\u7684\u5173\u7cfb\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67116\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u7efc\u8ff0\u603b\u62ec\u56fe-1.png\" alt=\"\" width=\"600\" height=\"346\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u7efc\u8ff0\u603b\u62ec\u56fe-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/\u7efc\u8ff0\u603b\u62ec\u56fe-1-300x173.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u7efc\u8ff0\u603b\u89c8\u56fe<\/strong><\/p>\n<p><strong>1\u3001\u975e\u8d35\u91d1\u5c5e\u7535\u50ac\u5316\u5242\u7684\u7814\u7a76\u80cc\u666f\u3001\u8fdb\u5c55\u53ca\u5173\u952e\u95ee\u9898<\/strong><\/p>\n<p>\u51cf\u5c11\u793e\u4f1a\u5bf9\u4f20\u7edf\u5316\u77f3\u71c3\u6599\u4f9d\u8d56\u7684\u4e3b\u8981\u57fa\u7840\u7535\u5316\u5b66\u8fc7\u7a0b\u5305\u62ec\u6c22\u6790\u51fa\u53cd\u5e94\uff08HER\uff09\u3001\u6c27\u6790\u51fa\u53cd\u5e94\uff08OER\uff09\u4ee5\u53ca\u6c27\u8fd8\u539f\u53cd\u5e94\uff08ORR\uff09\u3002\u8fd9\u4e9b\u53cd\u5e94\u662f\u8bb8\u591a\u53ef\u6301\u7eed\u80fd\u91cf\u5b58\u50a8\u4e0e\u8f6c\u5316\u8bbe\u5907\u5982\u6c34\u5206\u89e3\u3001\u71c3\u6599\u7535\u6c60\u4ee5\u53ca\u91d1\u5c5e-\u7a7a\u6c14\u7535\u6c60\u7684\u57fa\u7840\u3002\u4f46\u662f\u56e0\u5176\u53cd\u5e94\u8fdf\u7f13\uff0c\u5927\u90e8\u5206\u90fd\u4ee5\u8d35\u91d1\u5c5e\u4f5c\u4e3a\u7535\u50ac\u5316\u5242\uff0c\u4f46\u4ef7\u683c\u6602\u8d35\u4e14\u50a8\u91cf\u5c11\uff0c\u56e0\u6b64\u4e9f\u9700\u5f00\u53d1\u5ec9\u4ef7\u7684\u66ff\u4ee3\u50ac\u5316\u5242\uff0c\u6700\u8fd1\u5728\u975e\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u9886\u57df\u53d6\u5f97\u4e86\u4e00\u5b9a\u8fdb\u5c55\uff0c\u5c55\u73b0\u51fa\u6781\u597d\u7684\u7535\u50ac\u5316\u6d3b\u6027\u3002<\/p>\n<p>\u5982\u4f55\u6539\u53d8\u50ac\u5316\u5242\u7684\u5316\u5b66\u7ec4\u6210\u662f\u63d0\u9ad8\u6d3b\u6027\u7684\u5173\u952e\u9014\u5f84\u3002\u78b3\u57fa\u6750\u6599\u56e0\u5176\u5177\u6709\u6613\u8c03\u8282\u7684\u5206\u5b50\u7ed3\u6784\u548c\u7269\u7406\u5316\u5b66\u6027\u8d28\u4ee5\u53ca\u9ad8\u7684\u7269\u7406\u5316\u5b66\u7a33\u5b9a\u6027\uff0c\u5728\u5f00\u53d1\u5148\u8fdb\u7535\u50ac\u5316\u5242\u4e2d\u626e\u6f14\u7740\u91cd\u8981\u89d2\u8272\u3002\u901a\u8fc7\u5bf9\u539f\u59cb\u78b3\u8fdb\u884c\u6742\u539f\u5b50\u63ba\u6742\u53ef\u4ee5\u83b7\u5f97\u4e00\u5b9a\u7684\u7535\u50ac\u5316\u6d3b\u6027\u3002 \u53e6\u5916\u4e5f\u53ef\u5c06\u4e0d\u540c\u7ed3\u6784\u78b3\u6750\u6599\u4e0e\u7535\u6d3b\u6027\u7269\u8d28\u590d\u5408\u5f62\u6210\u9ad8\u6d3b\u6027\u50ac\u5316\u5242\u3002\u4f46\u5e38\u89c4\u7684\u7269\u7406\u6df7\u5408\u56e0\u754c\u9762\u7ed3\u5408\u4e0d\u5bc6\u5207\uff0c\u56e0\u800c\u5927\u5927\u963b\u788d\u4e86\u5bf9\u50ac\u5316\u5242\u6709\u6548\u529f\u80fd\u57fa\u56e2\u7684\u7406\u89e3\u3002\u56e0\u6b64\uff0c\u754c\u9762\u8bbe\u8ba1\u5982\u6c22\u952e\u3001\u9759\u7535\u5438\u5f15\u3001\u8303\u5fb7\u74e6\u5c14\u65af\u4f5c\u7528\u3001\u5171\u4ef7\u952e\u7b49\u76f8\u4e92\u4f5c\u7528\u7684\u5f15\u5165\u53ef\u4ee5\u6539\u53d8\u5206\u5b50\u5c40\u90e8\u7684\u952e\u5408\u73af\u5883\u548c\u7535\u5b50\u72b6\u6001\u4ece\u800c\u63d0\u9ad8\u50ac\u5316\u6d3b\u6027\u3002<\/p>\n<p>\u56e0\u6b64\uff0c\u57fa\u4e8e\u8fd1\u5e74\u6765\u5728\u5236\u5907\u9ad8\u6d3b\u6027\u975e\u8d35\u91d1\u5c5e\u7535\u50ac\u5316\u5242\u6240\u53d6\u5f97\u7684\u6210\u5c31\uff0c\u5fc5\u987b\u6ee1\u8db3\u4ee5\u4e0b\u4e09\u4e2a\u6761\u4ef6\u6765\u5408\u6210\u51fa\u9ad8\u6548\u7535\u50ac\u5316\u5242\uff081\uff09\u901a\u8fc7\u8c03\u63a7\u5408\u6210\u53c2\u6570\u548c\u5316\u5b66\u4fee\u9970\u6765\u83b7\u5f97\u9ad8\u5bc6\u5ea6\u6d3b\u6027\u4f4d\u70b9\uff0c\uff082\uff09\u5177\u6709\u4f18\u5f02\u7684\u7535\u5b50\u8fc1\u79fb\u80fd\u529b\uff0c\u5373\u5bfc\u7535\u6027\u597d\uff0c\uff083\uff09\u4f18\u5f02\u7684\u7535\u6781\u7ed3\u6784\u3002<\/p>\n<p><strong>2\u3001\u78b3\u57fa\u7eb3\u7c73\u7ed3\u6784\u7535\u50ac\u5316\u5242<\/strong><\/p>\n<p><strong>2.1 \u6742\u539f\u5b50\u63ba\u6742\u78b3\u57fa\u7535\u50ac\u5316\u5242<\/strong><\/p>\n<p>\u901a\u8fc7\u6742\u539f\u5b50\u63ba\u6742\u53ef\u4ee5\u8c03\u8282\u78b3\u7eb3\u7c73\u7ed3\u6784\uff08\u77f3\u58a8\u70ef\uff0c\u78b3\u7eb3\u7c73\u7ba1\uff0c\u591a\u5b54\u78b3\uff09\u7684\u7535\u5b50\u7ed3\u6784\u548c\u7535\u5316\u5b66\u6027\u8d28\u3002\u4ee5ORR\u53cd\u5e94\u4e3a\u4f8b\uff0c\u901a\u8fc7\u6742\u539f\u5b50\u63ba\u6742\u4f7f\u5f97\u78b3\u6750\u6599\u7684\u7535\u5b50\u7ed3\u6784\u91cd\u65b0\u5206\u5e03\uff0c\u6539\u53d8\u4e86\u5bf9O<sub>2<\/sub>\u7684\u5316\u5b66\u5438\u9644\uff0c\u524a\u5f31\u4e86O-O\u952e\uff0c\u589e\u5f3a\u4e86ORR \u53cd\u5e94\u3002\u591a\u79cd\u6742\u539f\u5b50\u5171\u63ba\u6742\u78b3\u57fa\u6750\u6599\u4e5f\u88ab\u7528\u505aHER\u7535\u50ac\u5316\u5242\u3002\u901a\u8fc7\u5177\u6709\u4e0d\u540c\u7535\u8377\u5bc6\u5ea6\u7684\u591a\u79cd\u6742\u539f\u5b50\uff08N, S\uff09\u4fee\u9970\u77f3\u58a8\u70ef\u7ed3\u6784\u53ef\u4ee5\u6539\u53d8\u6750\u6599\u7684\u7ed9\u7535\u5b50\u6027\u8d28\u548c\u90bb\u8fd1\u78b3\u539f\u5b50\u7684\u7535\u5316\u5b66\u6d3b\u6027\uff0c\u5bfc\u81f4\u6d3b\u6027\u78b3\u539f\u5b50\u4ef7\u5e26\u4e0b\u79fb\uff0c\u6709\u5229\u4e8eH*\u7684\u5438\u8131\u9644\u3002\u901a\u8fc7\u5b9e\u9a8c\u548c\u7406\u8bba\u8ba1\u7b97\u8868\u660e\uff0c\u5171\u63ba\u6742\u53ef\u4ee5\u964d\u4f4eHER\u53cd\u5e94\u7684\u8d77\u59cb\u7535\u4f4d\u5e76\u63d0\u9ad8\u7535\u6d41\u5bc6\u5ea6\u3002\u5f53\u7136\uff0c\u4e0e\u542b\u91d1\u5c5e\u7c7b\u6750\u6599\u76f8\u6bd4\u5171\u63ba\u6742\u78b3\u57fa\u6750\u6599\u7684\u7535\u50ac\u5316\u5242\u6d3b\u6027\u8fd8\u662f\u6709\u4e00\u5b9a\u5dee\u8ddd\u7684\uff0c\u56e0\u4e3a\u63ba\u6742\u91cf\u8f83\u4f4e\uff0c\u50ac\u5316\u6d3b\u6027\u4f4d\u5c11\u3002\u56e0\u6b64\uff0c\u5236\u5907\u78b3\u7eb3\u7c73\u7ed3\u6784\u6750\u6599\u4e0e\u5177\u6709\u50ac\u5316\u6d3b\u6027\u7269\u8d28\u7684\u590d\u5408\u6750\u6599\u662f\u8fdb\u4e00\u6b65\u63d0\u9ad8\u50ac\u5316\u6d3b\u6027\u7684\u6709\u6548\u9014\u5f84\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67118\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/1-3.jpeg\" alt=\"\" width=\"600\" height=\"515\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/1-3.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/1-3-300x258.jpeg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe1 \u5171\u63ba\u6742\u77f3\u58a8\u70ef\u6750\u6599\u5728HER\u53cd\u5e94\u8fc7\u7a0b\u7684\u5e94\u7528<\/strong><\/p>\n<p><strong>2.2 \u78b3-\u6742\u539f\u5b50\u63ba\u6742\u78b3\u590d\u5408\u6750\u6599<\/strong><\/p>\n<p>\u975e\u91d1\u5c5e\u6750\u6599\u7a33\u5b9a\u6027\u597d\u4f46\u6d3b\u6027\u8f83\u5dee\uff0c\u4e0e\u78b3\u6750\u6599\u7684\u590d\u5408\u53ef\u4ee5\u8fdb\u4e00\u6b65\u589e\u5f3a\u50ac\u5316\u6d3b\u6027\u3002\u4e3b\u8981\u539f\u56e0\u5728\u4e8e\uff1a1\uff09\u53ef\u4ee5\u589e\u52a0\u50ac\u5316\u6d3b\u6027\u4f4d\u70b9\uff1b2\uff09\u63d0\u9ad8\u7535\u5b50\u7535\u5bfc\u7387\uff1b3\uff09\u6539\u53d8\u6750\u6599\u7684\u7ed9\u7535\u5b50\u6027\u8d28\u3002\u5bf9\u4e8e\u5316\u5b66\u63ba\u6742\u7684\u78b3\u7eb3\u7c73\u7ed3\u6784\uff0c\u5982N-\u63ba\u6742\u77f3\u58a8\u70ef\uff0c\u56e0\u5176\u4f4e\u7684\u6bd4\u8868\u9762\u79ef\u548c\u6d3b\u6027\u4e2d\u5fc3\u5bc6\u5ea6\uff0c\u8868\u73b0\u51fa\u4e00\u822c\u7684\u7535\u50ac\u5316\u6d3b\u6027\u3002\u867d\u7136\u901a\u8fc7\u7269\u7406\u6216\u5316\u5b66\u6d3b\u5316\u7684\u65b9\u6cd5\u53ef\u4ee5\u4e30\u5bcc\u5176\u591a\u5b54\u6027\uff0c\u4f46\u65e2\u4e0d\u7ecf\u6d4e\u4e5f\u4e0d\u73af\u4fdd\u3002\u4f46\u662f\u6211\u4eec\u901a\u8fc7\u5f15\u5165\u5177\u6709\u4ecb\u5b54\u3001\u5927\u5b54\u7684\u78b3\u591a\u7ea7\u7f51\u7edc\u7ed3\u6784\u4f5c\u4e3a\u8f7d\u4f53\u539f\u4f4d\u751f\u957fN\u63ba\u6742\u77f3\u58a8\u70ef\u6216\u78b3\u7eb3\u7c73\u7ba1\uff0c\u8fd9\u7c7b\u590d\u5408\u7ed3\u6784\u80fd\u591f\u4f7f\u8f7d\u4f53\u548cN\u63ba\u6742\u6750\u6599\u7d27\u5bc6\u63a5\u89e6\uff0c\u964d\u4f4e\u6d3b\u5316\u80fd\uff0c\u589e\u52a0\u5316\u5b66\u8868\u9762\u79ef\u548c\u6d3b\u6027\u4f4d\u70b9\uff0c\u540c\u65f6\u8fd8\u80fd\u9632\u6b62\u77f3\u58a8\u70ef\u7684\u5806\u53e0\uff0c\u8868\u73b0\u51fa\u4f18\u5f02\u7684\u7535\u50ac\u5316\u6d3b\u6027\u3002\u518d\u6bd4\u5982\u901a\u8fc7\u03c0-\u03c0\u5171\u8f6d\u4f5c\u7528\u5c06N\u63ba\u6742\u77f3\u58a8\u70ef\u548cCNT\u8026\u5408\u5f62\u6210\u590d\u5408\u7535\u50ac\u5316\u5242\u5c55\u73b0\u51fa\u5ab2\u7f8e\u5546\u4e1a\u5316<span lang=\"EN-US\" style=\"font-family: 'Georgia','serif'; color: #333333; background: white;\">IrO<sub>2<\/sub><\/span>\u7684\u6c34\u6c27\u5316\u6d3b\u6027\u3002\u56e0\u6b64\uff0c\u8fd9\u4e9b\u975e\u91d1\u5c5e\u78b3\u57fa\u6750\u6599\u901a\u8fc7\u5408\u7406\u8bbe\u8ba1\u83b7\u5f97\u76f8\u5e94\u7684\u7269\u7406\u5316\u5b66\u6027\u8d28\uff0c\u5176\u50ac\u5316\u6d3b\u6027\u6709\u6f5c\u529b\u8d85\u8d8a\u91d1\u5c5e\u57fa\u7535\u50ac\u5316\u5242\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67119\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/2-2.jpeg\" alt=\"\" width=\"600\" height=\"522\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/2-2.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/2-2-300x261.jpeg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe2 N\u63ba\u6742\u77f3\u58a8\u70ef-CNT\u590d\u5408\u50ac\u5316\u5242\u5728\u6c34\u6c27\u5316\u4e2d\u7684\u8fd0\u7528<\/strong><\/p>\n<p><strong>2.3 \u78b3-g-<\/strong><strong><span lang=\"EN-US\" style=\"color: #333333; background: white;\">C<sub>3<\/sub>N<sub>4<\/sub><\/span><\/strong><strong>\u590d\u5408\u6750\u6599<\/strong><\/p>\n<p>N-\u63ba\u6742\u78b3\u6750\u6599\u56e0N\u63ba\u6742\u91cf\u8fc7\u4f4e\u9650\u5236\u4e86\u50ac\u5316\u6d3b\u6027\u3002g-<span lang=\"EN-US\" style=\"color: #333333; background: white;\">C<sub>3<\/sub>N<sub>4<\/sub><\/span>\u5177\u6709\u5f88\u9ad8\u7684N\u542b\u91cf\uff0c\u4f46\u5176\u5bfc\u7535\u6027\u592a\u5dee\uff0c\u5728ORR\u53cd\u5e94\u8fc7\u7a0b\u4e2d\uff0c\u8fc7\u91cf\u7684\u8fc7\u6c27\u5316\u7269\u5806\u79ef\uff0c\u4e0d\u5229\u4e8e4e<sup>&#8211;<\/sup>\u53cd\u5e94\u5386\u7a0b\uff0c\u964d\u4f4e\u4e86\u50ac\u5316\u6d3b\u6027\u3002\u56e0\u6b64\uff0c\u5b9e\u9a8c\u4e2d\u5c06g-C<sub>3<\/sub>N<sub>4<\/sub>\u4e0e\u5177\u6709\u9ad8\u5bfc\u7535\u6027\u7684\u4ecb\u5b54\u78b3\u6750\u6599\u7ed3\u5408\u5f62\u6210\u590d\u5408\u6750\u6599\uff0c\u8868\u73b0\u51fa\u5353\u8d8a\u7684ORR\u6d3b\u6027\u3002\u5bfc\u7535\u78b3\u57fa\u5e95\u7684\u52a0\u5165\u63d0\u9ad8\u4e86\u7535\u5b50\u4f20\u9012\u901f\u7387\uff0c\u6d88\u9664\u4e86<span lang=\"EN-US\" style=\"font-family: 'Georgia','serif'; color: #333333; background: white;\">OH<sup>&#8211;<\/sup><\/span>\u8fdb\u4e00\u6b65\u8fd8\u539f\u7684\u58c1\u5792\uff0c\u8fdb\u800c\u63d0\u9ad8\u4e86O<sub>2<\/sub>\u5206\u5b50\u7684\u5438\u9644\uff0c\u5229\u4e8e4e<sup>&#8211;<\/sup>\u53cd\u5e94\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67120\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/3-2.jpeg\" alt=\"\" width=\"600\" height=\"628\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/3-2.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/3-2-287x300.jpeg 287w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe3 g-<span lang=\"EN-US\" style=\"color: #333333; background: white;\">C<sub>3<\/sub>N<sub>4<\/sub><\/span>-\u4ecb\u5b54\u78b3\u590d\u5408\u7535\u50ac\u5316\u5242\u5728ORR\u53cd\u5e94\u4e2d\u7684\u8fd0\u7528<\/strong><\/p>\n<p>\u5b9e\u9645\u4e0a\uff0c\u6211\u4eec\u53d1\u73b0\u4e0d\u540c\u7684\u5408\u6210\u65b9\u6cd5\u4f1a\u5f71\u54cdg-C<sub>3<\/sub>N<sub>4<\/sub>\u548cN\u63ba\u6742\u78b3\u6750\u6599\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\uff0c\u8fdb\u800c\u5f71\u54cd\u7535\u5316\u5b66\u6027\u80fd\u3002\u901a\u8fc7\u9759\u7535\u7ec4\u88c5\uff0c\u03c0-\u03c0\u5806\u79ef\u6548\u5e94\uff0c\u6211\u4eec\u53ef\u4ee5\u5236\u5907\u5177\u6709\u4e09\u7ef4\u7f51\u7edc\u7ed3\u6784\u9ad8\u542b\u6c2e\u91cf\u7684g-C<sub>3<\/sub>N<sub>4<\/sub>\u7eb3\u7c73\u7247\u548cCNT\u6742\u5316\u6750\u6599\uff0c\u56e0g-C<sub>3<\/sub>N<sub>4<\/sub>\u4e2d\u5b58\u5728\u5927\u91cf\u7684\u5421\u5576\u6c2e\u7c7b\u7269\u79cd\uff0c\u63d0\u9ad8\u4e86\u6b63\u7535\u8377\u5bc6\u5ea6\uff0c\u5229\u4e8e\u9634\u79bb\u5b50\uff08OH<sup>&#8211;<\/sup>\uff09\u7684\u5438\u9644\u548c\u7535\u5b50\u8f6c\u79fb\uff0c\u8fdb\u800c\u63d0\u9ad8\u4e86OER\u53cd\u5e94\u6d3b\u6027\u3002\u53e6\u5916\uff0c\u5c42\u72b6g-C<sub>3<\/sub>N<sub>4<\/sub>\u548cN\u63ba\u6742\u77f3\u58a8\u70ef\u7247\u5c42\u7ed3\u6784\u8026\u5408\u5f62\u6210\u7684\u6742\u5316\u6750\u6599\uff0c\u56e0\u5b58\u5728\u8f83\u597d\u7684H\u5438\u8131\u9644\u884c\u4e3a\uff0c\u663e\u793a\u51fa\u4f18\u4e8e\u91d1\u5c5e\u57fa\u6750\u6599\u7684HER\u53cd\u5e94\u6d3b\u6027\u3002\u6700\u540e\uff0c\u8fd8\u53ef\u4ee5\u8fdb\u884c\u6742\u539f\u5b50\u5982P\u63ba\u6742g-C<sub>3<\/sub>N<sub>4<\/sub>\u6765\u63d0\u9ad8\u6d3b\u6027\u4f4d\u70b9\uff0c\u6539\u53d8\u7535\u5b50\u7ed3\u6784\uff0c\u8fdb\u4e00\u6b65\u63d0\u5347\u50ac\u5316\u6027\u80fd\u3002\u8fd9\u79cd\u6742\u5316\u6750\u6599\u5728\u950c-\u7a7a\u6c14\u7535\u6c60\u4e2d\u8868\u73b0\u51fa\u4f4e\u7684\u8fc7\u7535\u52bf\u548c\u8f83\u597d\u7684\u8010\u4e45\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67121\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/4-2.jpeg\" alt=\"\" width=\"600\" height=\"518\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/4-2.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/4-2-300x259.jpeg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe4 g-<span lang=\"EN-US\" style=\"color: #333333; background: white;\">C<sub>3<\/sub>N<sub>4<\/sub><\/span>-N\u63ba\u6742\u77f3\u58a8\u70ef\u590d\u5408\u6750\u6599\u5728HER\u53cd\u5e94\u4e2d\u7684\u8fd0\u7528<\/strong><\/p>\n<p><strong>3\u3001\u91d1\u5c5e-\u975e\u91d1\u5c5e\u6742\u5316\u7535\u50ac\u5316\u5242<\/strong><\/p>\n<p><strong>\u00a03.1 \u4ee5M-N-C\u4e3a\u6d3b\u6027\u4f4d\u70b9\u7684\u91d1\u5c5e-\u975e\u91d1\u5c5e\u7535\u50ac\u5316\u5242<\/strong><\/p>\n<p>\u5f53\u524d\u5173\u4e8e\u91d1\u5c5e-\u6c2e\u7ed3\u6784\u7684\u7814\u7a76\u4e3b\u8981\u805a\u7126\u4e8e\u8fc7\u6e21\u91d1\u5c5e(Fe\u3001Co\u3001Ni)-\u5927\u73af\u5316\u5408\u7269\uff08\u915e\u83c1\uff0c\u90bb\u4e8c\u6c2e\u6742\u83f2\u7b49\uff09\u590d\u5408\u6750\u6599\u3002\u8fd9\u4e9b\u91d1\u5c5e-\u5927\u73af\u5316\u5408\u7269\u56e0\u4e3a\u7535\u5b50\u79bb\u57df\u6548\u5e94\u6709\u5229\u4e8e\u7535\u5b50\u4f20\u9012\uff0c\u4ea7\u751f\u4e86\u50ac\u5316\u6d3b\u6027\uff0c\u4f46\u7a33\u5b9a\u5dee\u963b\u788d\u4e86\u5b9e\u9645\u8fd0\u7528\u3002\u8fdb\u4e00\u6b65\u53ef\u4ee5\u5728\u60f0\u6027\u6c14\u6c1b\u4e0b\u76f4\u63a5\u78b3\u5316\u91d1\u5c5e\u5927\u73af\u5316\u5408\u7269\u5f62\u6210M-NX-C\u6750\u6599\uff0c\u5176\u8868\u73b0\u51fa\u8f83\u9ad8\u7684\u6d3b\u6027\u548c\u7a33\u5b9a\u6027\u3002\u901a\u8fc7DFT\u8ba1\u7b97\u8868\u660eN\u5143\u7d20\u7684\u63ba\u6742\u964d\u4f4e\u4e86\u8868\u9762\u78b3\u7684\u529f\u51fd\uff0c\u63d0\u9ad8\u4e86\u7535\u5b50\u4ece\u5185\u5d4c\u91d1\u5c5e\u7c92\u5b50\u5230\u5916\u5c42\u78b3\u7684\u4f20\u9012\u901f\u7387\uff0c\u8fdb\u800c\u63d0\u9ad8\u4e86\u50ac\u5316\u6d3b\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67122\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/5-2.jpeg\" alt=\"\" width=\"600\" height=\"190\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/5-2.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/5-2-300x95.jpeg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe5 M-NX-C\u6750\u6599\u7684\u5206\u5b50\u7ed3\u6784\u6a21\u578b<\/strong><\/p>\n<p>\u8fdb\u4e00\u6b65\u7814\u7a76\u53d1\u73b0\u540c\u65f6\u7145\u70e7\u6c2e\u6e90\u3001\u8fc7\u6e21\u91d1\u5c5e\u6e90\u548c\u78b3\u6e90\u4e5f\u53ef\u4ee5\u5f62\u6210M-Nx-C\u6750\u6599\uff0c\u56e0\u6b64\uff0c\u91d1\u5c5e\u5927\u73af\u5316\u5408\u7269\u53ef\u4ee5\u88ab\u4e00\u4e9b\u4f4e\u4ef7\u524d\u9a71\u4f53\u6240\u53d6\u4ee3\uff0c\u6bd4\u5982\u8fc7\u6e21\u91d1\u5c5e\u6e90\uff08\u785d\u9178\u76d0\u3001\u786b\u9178\u76d0\u3001\u918b\u9178\u76d0\u3001\u6c2f\u9178\u76d0\uff09\uff0c\u6c2e\u6e90\uff08\u805a\u82ef\u80fa\u3001\u4e09\u805a\u6c30\u80fa\u3001\u4e59\u8148\uff09\u548c\u78b3\u6e90\uff08\u77f3\u58a8\u70ef\u3001\u78b3\u7eb3\u7c73\u7ba1\u3001\u6d3b\u6027\u70ad\uff09\u3002\u7814\u7a76\u8868\u660e\uff0c\u9009\u62e9\u5408\u9002\u7684\u524d\u9a71\u4f53\u548c\u5408\u6210\u5de5\u827a\u53c2\u6570\uff08\u5982\u70ed\u89e3\u6e29\u5ea6\u3001\u4fdd\u6e29\u65f6\u95f4\u3001\u524d\u9a71\u4f53\u5728\u6eb6\u6db2\u4e2d\u7684\u53cd\u5e94\u548c\u540e\u5904\u7406\u5de5\u827a\u7b49\uff09\u5bf9\u5236\u5907\u51fa\u9ad8\u6d3b\u6027\u7535\u50ac\u5316\u5242\u5177\u6709\u91cd\u8981\u5f71\u54cd\u3002\u76ee\u524d\uff0c\u5bf9\u4e8eM-Nx-C\u6750\u6599\u7684\u50ac\u5316\u6d3b\u6027\u4e2d\u5fc3\u4e0d\u660e\u786e\uff0c\u4f46\u662f\u591a\u5b54\u6027\u548c\u5fae\u7eb3\u7c73\u7ed3\u6784\u5728\u5f88\u5927\u7a0b\u5ea6\u4e0a\u4f1a\u5f71\u54cd\u50ac\u5316\u6d3b\u6027\uff0c\u901a\u8fc7\u9178\u6d17\u5904\u7406\u53ef\u4ee5\u589e\u52a0\u4e00\u5b9a\u7684\u6bd4\u8868\u9762\u79ef\u3002\u4f46\u662f\uff0c\u6750\u6599\u5728\u9ad8\u6e29\u7145\u70e7\u548c\u9178\u6d17\u8fc7\u7a0b\u4f1a\u5bfc\u81f4\u7ed3\u6784\u574d\u584c\uff0c\u6d3b\u6027\u4f4d\u6d41\u5931\uff0c\u964d\u4f4e\u50ac\u5316\u6027\u80fd\u3002\u4e3a\u4e86\u907f\u514d\u4ee5\u4e0a\u95ee\u9898\uff0c\u7845\u7eb3\u7c73\u9897\u7c92\u3001\u9633\u6781\u6c27\u5316\u94dd\u7b49\u786c\u6a21\u677f\u88ab\u5f15\u5165\u81f3\u78b3\u5316\u8fc7\u7a0b\u3002\u4f46\u662f\u786c\u6a21\u677f\u7684\u540e\u5904\u7406\u548c\u5408\u6210\u6b65\u9aa4\u8d39\u65f6\u8d39\u529b\u963b\u788d\u4e86\u6279\u91cf\u751f\u4ea7\uff0c\u6240\u4ee5\u53c8\u5f15\u5165\u4e86PS\u7403\u548cF127\u7b49\u805a\u5408\u7269\u6a21\u677f\uff0c\u56e0\u4e3a\u5728\u9ad8\u6e29\u7145\u70e7\u8fc7\u7a0b\u4e2d\u591a\u5b54M-NX-C\u7ed3\u6784\u7684\u5f62\u6210\u548c\u6a21\u677f\u7684\u79fb\u9664\u662f\u540c\u65f6\u8fdb\u884c\u7684\u3002\u8fd9\u79cd\u5177\u6709\u591a\u7ea7\u5b54\u7ed3\u6784\u548c\u4f18\u826f\u7535\u5bfc\u7387\u7684\u590d\u5408\u6750\u6599\u8868\u73b0\u51fa\u5353\u8d8a\u7684ORR\u6d3b\u6027\u3002<\/p>\n<p>\u53e6\u5916\uff0c\u901a\u8fc7\u5229\u7528M-NX\u76f8\u4e92\u4f5c\u7528\uff0c\u81ea\u7ec4\u88c5\u5f62\u6210\u4e8c\u7ef4\u77f3\u58a8\u5316g-C<sub>3<\/sub>N<sub>4<\/sub>\u548c\u78b3\u5316\u949b\u7eb3\u7c73\u7247\u590d\u5408\u819c\u72b6\u7535\u50ac\u5316\u5242\uff0c\u5c55\u73b0\u51fa\u6781\u597d\u7684\u4ee5Ti-N \u7ed3\u6784\u4e3a\u6d3b\u6027\u4f4d\u70b9\u7684OER\u50ac\u5316\u6d3b\u6027\u3002\u4f46\u662f\uff0c\u91d1\u5c5e\u5728M-N-C\u7ed3\u6784\u4e2d\u6240\u8d77\u7684\u50ac\u5316\u4f5c\u7528\u4f9d\u7136\u6ca1\u6709\u76f4\u63a5\u8bc1\u636e\u3002\u5173\u4e8e\u6d3b\u6027\u4f4d\u70b9\u7684\u63a2\u7a76\u9700\u8981\u501f\u52a9\u7406\u8bba\u8ba1\u7b97\u548c\u5148\u8fdb\u7684\u6750\u6599\u5206\u6790\u624b\u6bb5\uff08\u5982X\u5c04\u7ebf\u8fd1\u8fb9\u5438\u6536\u8c31\uff0c\u7a46\u65af\u5821\u5c14\u8c31\uff09\u8fdb\u4e00\u6b65\u5206\u6790\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67123\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/6-2.jpeg\" alt=\"\" width=\"600\" height=\"544\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/6-2.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/6-2-300x272.jpeg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe6 g-<span lang=\"EN-US\" style=\"color: #333333; background: white;\">C<sub>3<\/sub>N<sub>4<\/sub><\/span>\u548c\u78b3\u5316\u949b\u590d\u5408\u6750\u6599\u5728OER\u4e2d\u7684\u8fd0\u7528<\/strong><\/p>\n<p><strong>3.2 \u91d1\u5c5e\u6c27\u5316\u7269\/\u6c22\u6c27\u5316\u7269-\u6c2e\u63ba\u6742\u78b3\u590d\u5408\u6750\u6599<\/strong><\/p>\n<p>\u9664\u4e86\u9ad8\u6e29\u7145\u70e7\u6cd5\u8fdb\u884c\u6c2e\u63ba\u6742\uff0c\u4e00\u4e9b\u6e29\u548c\u7684\u6c34\u70ed\u6cd5\u6216\u8005\u6eb6\u5242\u70ed\u6cd5\u4e5f\u53ef\u4ee5\u6709\u6548\u5236\u5907\u6c2e\u63ba\u6742\u7eb3\u7c73\u78b3\u6750\u6599\u3002\u901a\u8fc7\u4e0d\u540c\u5408\u6210\u65b9\u6cd5\uff0c\u5728\u78b3\u9aa8\u67b6\u4e2d\u7684\u6c2e\u5b98\u80fd\u56e2\u53ef\u4ee5\u5438\u9644\u91d1\u5c5e\u524d\u9a71\u4f53\uff0c\u4ece\u800c\u5728\u8868\u9762\u5f62\u6210\u91d1\u5c5e\u6c27\u5316\u7269\u6216\u8005\u6c22\u6c27\u5316\u7269\u7eb3\u7c73\u9897\u7c92\u3002\u91d1\u5c5e-\u78b3\u5177\u6709\u5f88\u5f3a\u7684\u8026\u5408\u4f5c\u7528\uff0c\u56e0\u800c\u5728\u91d1\u5c5e\u6d3b\u6027\u4f4d\u548c\u78b3\u57fa\u5e95\u4e4b\u95f4\u5f15\u53d1\u4e86\u7535\u5b50\u6216\u5316\u5b66\u4fee\u9970\uff0c\u534f\u540c\u4f5c\u7528\u4e0b\u589e\u5f3a\u4e86\u7535\u50ac\u5316\u6d3b\u6027<span style=\"color: #000000;\">\u3002\u4ee5<span lang=\"EN-US\" style=\"font-family: Georgia, serif; background: white;\">Mn<sub>3<\/sub>O<sub>4<\/sub><\/span><\/span><span style=\"color: #ff0000;\"><span style=\"color: #000000;\">\u4fee\u9970<\/span><\/span><span style=\"color: #000000;\">\u6c2e\u63ba\u6742\u77f3\u58a8\u70ef\u4e3a\u4f8b\uff0c\u5c55\u73b0\u51fa\u4f18\u5f02\u7684ORR\u6d3b\u6027\u3001\u7a33\u5b9a\u6027\u548c\u6297\u7532\u9187\u6bd2\u5316\u6027\u3002\u6211\u4eec\u53ef\u4ee5\u901a\u8fc7\u6539\u53d8\u6c34\u70ed\u53cd\u5e94\u6761\u4ef6\uff0c\u6765\u8c03\u63a7<span lang=\"EN-US\" style=\"font-family: Georgia, serif; background: white;\">Mn<sub>3<\/sub>O<sub>4<\/sub><\/span>\u7684\u5f62\u8c8c\uff0c\u8fdb<\/span>\u800c\u63a2\u7a76\u5f62\u8c8c\u5bf9\u7535\u50ac\u5316\u6d3b\u6027\u7684\u5f71\u54cd\u3002<\/p>\n<p>\u76ee\u524d\u7535\u50ac\u5316\u5242\u90fd\u662f\u6ef4\u6d82\u5230\u5bfc\u7535\u8f7d\u4f53\uff0c\u5982\u73bb\u78b3\uff0c\u91d1\u5c5e\u7b94\u4e0a\uff0c\u63a5\u89e6\u4e0d\u597d\uff0c\u8f7d\u91cf\u53d7\u9650\u548c\u4e0d\u53ef\u63a7\u7684\u5fae\u89c2\u7ed3\u6784\u4e0d\u5229\u4e8e\u7535\u5b50\u548c\u7269\u8d28\u7684\u4f20\u9012\u3002\u6700\u8fd1\uff0c\u7814\u7a76\u4eba\u5458\u5236\u5907\u4e86\u4e00\u79cd\u4e09\u7ef4\u81ea\u652f\u6491\u77f3\u58a8\u70ef\u819c\uff0c\u5177\u6709\u6781\u597d\u7684\u673a\u68b0\u5f39\u6027\u3002\u8fd9\u79cd\u81ea\u652f\u6491\u77f3\u58a8\u70ef\u819c\u53ef\u4ee5\u548c\u91d1\u5c5e\u56e2\u7c07\u76f8\u4e92\u4f5c\u7528\uff0c\u9650\u5236\u77f3\u58a8\u70ef\u7247\u5c42\u5806\u53e0\uff0c\u540c\u65f6\u4ea7\u751f\u5927\u91cf\u7684\u9762\u5916\u5b54\uff0c\u786e\u4fdd\u53cd\u5e94\u7269\u548c\u4ea7\u7269\u5728\u6574\u4e2a\u819c\u5185\u80fd\u591f\u5feb\u901f\u4f20\u9012\u3002\u901a\u8fc7\u6539\u53d8\u5b9e\u9a8c\u5904\u7406\u65b9\u6cd5\uff0c\u53ef\u4ee5\u63d2\u5165\u4e0d\u540c\u6d3b\u6027\u91d1\u5c5e\u4f4d\u70b9\u4e8e\u77f3\u58a8\u70ef\u819c\u5185\u6765\u8c03\u8282\u6750\u6599\uff0c\u4f7f\u5176\u5177\u6709\u4e0d\u540c\u529f\u80fd\u7684\u7535\u50ac\u5316\u6027\u80fd\u3002\u6bd4\u5982\uff0cNi\u7eb3\u7c73\u7c92\u5b50\u5d4c\u5165\u6c2e\u63ba\u6742\u77f3\u58a8\u70ef\u819c\u4e2d\uff0c\u8868\u73b0\u51fa\u5f88\u597d\u7684OER\u6d3b\u6027\u3002\u5982\u679c\u78b1\u6027\u6761\u4ef6\u4e0b\uff0c\u91d1\u5c5e\u524d\u9a71\u4f53\u951a\u5b9a\u5728\u77f3\u58a8\u70ef\u8868\u9762\uff0c\u5c31\u4f1a\u5f62\u6210Ni\u7684\u6c22\u6c27\u5316\u7269\uff1b\u53c8\u6bd4\u5982NiCo\u6c22\u6c27\u5316\u7269\u6c89\u79ef\u5728\u77f3\u58a8\u70ef\u819c\u4e0a\u8868\u73b0\u51fa\u4e00\u5b9a\u7684\u6c34\u5206\u89e3\u6027\u8d28\u3002\u8fdb\u4e00\u6b65\uff0c\u5728\u7a7a\u6c14\u4e2d\u9000\u706b\uff0c\u53c8\u53ef\u5f62\u6210NiCo\u6c27\u5316\u7269\u9897\u7c92\u3002<\/p>\n<p>\u8fd9\u79cd\u4e8c\u7ef4\u5c42\u72b6\u7ed3\u6784\uff0c\u56e0\u4e3a\u5177\u6709\u5171\u4ef7\u952e\u548c\u81ea\u7531\u952e\u7684\u5b58\u5728\uff0c\u80fd\u591f\u9694\u79bb\u6216\u5339\u914d\u4e0d\u540c\u5c42\u72b6\u7269\u8d28\uff0c\u5728\u65e0\u6676\u683c\u5339\u914d\u548c\u517c\u5bb9\u6027\u9650\u5236\u4e0b\uff0c\u5f62\u6210\u5927\u8303\u56f4\u7684\u6742\u5316\u6750\u6599\u3002<span style=\"color: #000000;\">\u6bd4\u5982WS<sub>2<\/sub>\u5c42<\/span>\u72b6\u7ed3\u6784\u8026\u5408\u6742\u539f\u5b50\u63ba\u6742\u77f3\u58a8\u70ef\u6750\u6599\uff0c\u4ea7\u751f\u5927\u91cf\u7684\u50ac\u5316\u6d3b\u6027\u4f4d\u548c\u9ad8\u7684\u7535\u5bfc\u7387\uff0c\u6709\u5229\u4e8e\u63d0\u9ad8HER\u53cd\u5e94\u6d3b\u6027\u3002<\/p>\n<p>\u4ee5\u4e0a\u7ed3\u679c\u8868\u660e\uff0c\u6c2e\u7684\u63ba\u6742\u52a0\u5f3a\u4e86\u91d1\u5c5e\u524d\u9a71\u4f53\u548c\u78b3\u8f7d\u4f53\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\uff0c\u540c\u65f6\u8fd9\u79cd\u4f5c\u7528\u5728M-N-C\u590d\u5408\u7ed3\u6784\u4e2d\u63d0\u5347\u4e86\u7535\u50ac\u5316\u6d3b\u6027\u3002\u7535\u50ac\u5316\u53cd\u5e94\u901f\u7387\u4e3b\u8981\u53d6\u51b3\u4e8e\u50ac\u5316\u5242\u7684\u51e0\u4f55\u6784\u578b\u548c\u7535\u5b50\u7ed3\u6784\uff0c\u4e8c\u8005\u5171\u540c\u5f71\u54cd\u53cd\u5e94\u4e2d\u95f4\u7269\u7684\u5438\u8131\u9644\u548c\u53cd\u5e94\u6d3b\u5316\u80fd\u3002\u56e0\u6b64\uff0c\u5bf9\u6742\u5316\u6750\u6599\u7684\u6d3b\u6027\u91d1\u5c5e\u6210\u5206\u8fdb\u884c\u539f\u5b50\u5c42\u9762\u7684\u7ed3\u6676\u5ea6\u548c\u8868\u9762\u7ed3\u6784\u8bbe\u8ba1\u5904\u7406\uff0c\u4e3a\u5148\u8fdb\u50ac\u5316\u5242\u5728\u7535\u50ac\u5316\u4e2d\u7684\u5e7f\u6cdb\u8fd0\u7528\u63d0\u4f9b\u4e86\u4e00\u6761\u65b0\u7684\u9014\u5f84\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-67124\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/7-2.jpeg\" alt=\"\" width=\"600\" height=\"845\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/7-2.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/7-2-213x300.jpeg 213w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe7 Ni\u3001NiCo-\u81ea\u652f\u6491\u4e8c\u7ef4\u77f3\u58a8\u70ef\u819c\u590d\u5408\u6750\u6599\u5728\u7535\u50ac\u5316\u53cd\u5e94\u4e2d\u7684\u8fd0\u7528<\/strong><\/p>\n<p>\u3010<strong>\u603b\u7ed3<\/strong>\u3011<\/p>\n<p>\u5229\u7528\u6750\u6599\u8bbe\u8ba1\u548c\u8868\u754c\u9762\u539f\u5b50\u5206\u5b50\u8bbe\u8ba1\u539f\u7406\uff0c\u5236\u5907\u51fa\u9ad8\u6548\u7535\u50ac\u5316\u5242\u7528\u4e8eOER, ORR\u548cHER\u7b49\u57fa\u7840\u7535\u50ac\u5316\u8fc7\u7a0b\u662f\u76ee\u524d\u7814\u7a76\u7684\u4e00\u5927\u8d8b\u52bf\uff0c\u8fd9\u53ef\u4ee5\u5c06\u5b9e\u9a8c\u548c\u7406\u8bba\u8fdb\u884c\u7ed3\u5408\uff0c\u63a2\u7a76\u9ad8\u6d3b\u6027\u4f4e\u4ef7\u7535\u50ac\u5316\u5242\u7684\u6709\u6548\u5408\u6210\u3002\u5177\u4f53\u6765\u8bf4\uff0c\u8fd9\u4e9b\u50ac\u5316\u5242\u7684\u7535\u50ac\u5316\u6d3b\u6027\u4e3b\u8981\u53d6\u51b3\u4e8e\u78b3\u6750\u6599\u4e2d\u7684\u63ba\u6742\u7c7b\u578b\u3001\u6d3b\u6027\u7ec4\u5206\u4e0e\u78b3\u57fa\u5e95\u7684\u8026\u5408\u5f62\u5f0f\u4ee5\u53ca\u524d\u9a71\u4f53\u7684\u9009\u62e9\u548c\u5408\u6210\u65b9\u6cd5\u3002\u6700\u7ec8\u5236\u5907\u8fd9\u4e9b\u9ad8\u6548\u7535\u50ac\u5316\u5242\u7684\u76ee\u7684\u662f\u7528\u4e8e\u53ef\u6301\u7eed\u80fd\u6e90\u8bbe\u5907\uff0c\u6bd4\u5982\u53ef\u5145\u7535\u91d1\u5c5e-\u7a7a\u6c14\u7535\u6c60\u3002\u76ee\u524d\u5df2\u7ecf\u6709\u4e00\u4e9b\u53cc\u529f\u80fd\u50ac\u5316\u5242\u7528\u4e8e\u91d1\u5c5e-\u7a7a\u6c14\u7535\u6c60\u548c\u6c34\u5206\u89e3\u8fc7\u7a0b\uff0c\u8fd9\u5c06\u8fdb\u4e00\u6b65\u5728\u6548\u7387\u548c\u5bff\u547d\u4e0a\u8fdb\u884c\u4f18\u5316\u63d0\u5347\u3002\u5bf9\u4e8e\u975e\u8d35\u91d1\u5c5e\u6216\u8005\u975e\u91d1\u5c5e\u7535\u50ac\u5316\u5242\u800c\u8a00\uff0c\u6df1\u5165\u4e86\u89e3\u50ac\u5316\u53cd\u5e94\u673a\u7406\u548c\u6d3b\u6027\u4f4d\u70b9\u662f\u5fc5\u8981\u7684\u3002\u8fd9\u5c31\u9700\u8981\u6211\u4eec\u501f\u52a9\u539f\u4f4d\u7b49\u5148\u8fdb\u6280\u672f\u5bf9\u6a21\u578b\u50ac\u5316\u5242\u6df1\u5165\u7814\u7a76\uff0c\u63d0\u5347\u6211\u4eec\u5bf9\u7535\u50ac\u5316\u53cd\u5e94\u673a\u5236\u5728\u5206\u5b50\u6c34\u5e73\u4e0a\u7684\u7406\u89e3\u3002\u6b64\u5916\uff0c\u901a\u8fc7\u5b9e\u9a8c\u548c\u8ba1\u7b97\u76f8\u7ed3\u5408\u8fdb\u884c\u539f\u5b50\u5206\u5b50\u6c34\u5e73\u8bbe\u8ba1\uff0c\u8fdb\u4e00\u6b65\u4e86\u89e3\u50ac\u5316\u53cd\u5e94\u672c\u8d28\uff0c\u8fd9\u6837\u624d\u80fd\u7814\u53d1\u51fa\u9ad8\u6548\u7535\u50ac\u5316\u5242\u7528\u4e8e\u5176\u4ed6\u7535\u5316\u5b66\u53cd\u5e94\uff0c\u6bd4\u5982CO<sub>2<\/sub>\u8fd8\u539f\u548c\u56fa\u6c2e\u53cd\u5e94\u7b49\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acs.accounts.6b00635\" target=\"_blank\">Surface and Interface Engineering of Noble-Metal-Free Electrocatalysts for Efficient Energy Conversion Processes<\/a> (Acc. Chem. Res., 2017, DOI: 10.1021\/acs.accounts.6b00635)<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u9ad8\u5206\u5b50\u6750\u6599\u5b66\u672f\u7ec4Star\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u5728\u5168\u7403\u80fd\u6e90\u5b89\u5168\u548c\u53ef\u6301\u7eed\u53d1\u5c55\u6280\u672f\u7684\u63a8\u52a8\u4e0b\uff0c\u79d1\u5b66\u5bb6\u4eec\u5f00\u59cb\u805a\u7126\u4e8e\u7814\u53d1\u5927\u91cf\u5b58\u5728\u4e8e\u5730\u7403\u4e2d\u7684\u5ec9\u4ef7\u975e\u8d35\u91d1\u5c5e\u6216\u975e\u91d1\u5c5e\u7535\u50ac\u5316\u5242\uff0c\u7528\u4e8e\u80fd\u91cf\u5b58\u50a8\u4e0e\u8f6c\u5316\u8fc7\u7a0b\uff0c\u5982\u6c22\u6790\u51fa\uff08HER&#8230;<\/p>\n","protected":false},"author":60,"featured_media":67125,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[533],"tags":[1414,18,76],"class_list":["post-66977","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zongshu","tag-qiaoshizhang","tag-xinnengyuan","tag-carbon"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66977"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/60"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=66977"}],"version-history":[{"count":13,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66977\/revisions"}],"predecessor-version":[{"id":68952,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/66977\/revisions\/68952"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/67125"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=66977"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=66977"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=66977"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}