{"id":68322,"date":"2017-03-03T14:00:54","date_gmt":"2017-03-03T06:00:54","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=68322"},"modified":"2017-02-27T18:29:11","modified_gmt":"2017-02-27T10:29:11","slug":"%e4%ba%8c%e7%bb%b4%e6%9d%90%e6%96%99%e7%a9%b6%e7%ab%9f%e6%98%af%e5%a6%82%e4%bd%95%e6%96%ad%e8%a3%82%e7%9a%84%ef%bc%9f","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=68322","title":{"rendered":"\u4e8c\u7ef4\u6750\u6599\u7a76\u7adf\u662f\u5982\u4f55\u65ad\u88c2\u7684\uff1f"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u4e8c\u7ef4\u6750\u6599\u4f5c\u4e3a\u73b0\u4eca\u6750\u6599\u5b66\u754c\u7684\u70ed\u95e8\u65b9\u5411\uff0c\u6709\u7740\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u4f46\u5bf9\u4e8c\u7ef4\u6750\u6599\u7684\u63a2\u7d22\u4eba\u7c7b\u8fd8\u6709\u5f88\u957f\u7684\u8def\u8981\u8d70\uff0c\u6bd4\u5982\uff0c\u4f60\u77e5\u9053\u4e8c\u7ef4\u6750\u6599\u7684\u65ad\u88c2\u673a\u5236\u5417\uff1fIBS\u79d1\u7814\u56e2\u961f\u7684\u6700\u65b0\u53d1\u73b0\u4e3a\u6211\u4eec\u63ed\u5f00\u4e86\u5b83\u7684\u795e\u79d8\u9762\u7eb1\u3002<br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-68323\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/20170207-tensile-stress-visualization-.jpg\" alt=\"\" width=\"650\" height=\"385\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/20170207-tensile-stress-visualization-.jpg 650w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/20170207-tensile-stress-visualization--300x178.jpg 300w\" sizes=\"(max-width: 650px) 100vw, 650px\" \/><\/p>\n<p>\u8bb8\u591a\u79d1\u5b66\u5bb6\u63d0\u51fa\uff0c\u82e5\u60f3\u7406\u89e3\u7ea4\u8584\u7684\u4e8c\u7ef4\u6750\u6599\u7a76\u7adf\u662f\u5982\u4f55\u65ad\u88c2\u7684\uff0c\u6211\u4eec\u5c31\u5f97\u63a2\u7d22\u5f97\u6bd4\u73b0\u6709\u7406\u8bba\u66f4\u8fdc\u3002<\/p>\n<p>AsianScientist\uff082017\u5e742\u670813\u65e5\uff09\u6d88\u606f\uff0c\u57fa\u7840\u79d1\u5b66\u7814\u7a76\u6240\uff08IBS\uff09\u7efc\u5408\u7eb3\u7c73\u7ed3\u6784\u7269\u7406\u4e2d\u5fc3(CINAP)\u7684\u79d1\u5b66\u5bb6\u4eec\u9996\u6b21\u89c2\u5bdf\u5230\u4e8c\u7ef4\u4e8c\u786b\u5316\u94bc\uff08MoS2\uff09\u7684\u65ad\u88c2\u3002\u76ee\u524d\u4ed6\u4eec\u5df2\u5c06\u8be5\u53d1\u73b0\u53d1\u8868\u5728Nature Communications\u671f\u520a\u4e0a\uff0c\u4ed6\u4eec\u7684\u53d1\u73b0\u6709\u671b\u7528\u4e8e\u6307\u5bfc\u8bbe\u8ba1\u65b0\u7684\u4e8c\u7ef4\u6750\u6599\u3002<\/p>\n<p>\u5982\u4eca\uff0c\u5e94\u7528MoS2\u7b49\u4e8c\u7ef4\u6750\u6599\u5df2\u88ab\u770b\u4f5c\u672a\u6765\u7535\u5b50\u53ca\u5149\u7535\u5668\u4ef6\u9886\u57df\u7684\u91cd\u8981\u53d1\u5c55\u65b9\u5411\u3002\u7136\u800c\u53ef\u4ee5\u9884\u89c1\u7684\u662f\uff0c\u4e8c\u7ef4\u6750\u6599\u7684\u673a\u68b0\u6027\u8d28\u4e0e\u6211\u4eec\u5e38\u89c1\u7684\u4e09\u7ef4\u6750\u6599\u5927\u76f8\u5f84\u5ead\u3002\u7279\u522b\u662f\u6211\u4eec\u96be\u4ee5\u5e94\u7528\u73b0\u4eca\u7684\u7406\u8bba\u53bb\u9884\u6d4b\u548c\u89e3\u91ca\u4e8c\u7ef4\u6750\u6599\u65ad\u88c2\u7684\u4e25\u91cd\u6027\u53ca\u65ad\u53e3\u5f62\u72b6\u3002<\/p>\n<p>\u91d1\u7b49\u5ef6\u5c55\u6027\u8f83\u597d\u7684\u6750\u6599\u53ef\u5728\u65ad\u88c2\u524d\u53d1\u751f\u8f83\u5927\u5e94\u53d8\uff0c\u800c\u73bb\u7483\u7b49\u8106\u6027\u6750\u6599\u5728\u7a81\u7136\u65ad\u88c2\u4e4b\u524d\u53ea\u80fd\u5438\u6536\u76f8\u5bf9\u8f83\u5c0f\u7684\u80fd\u91cf\uff0c\u4e14\u57fa\u672c\u6ca1\u6709\u4f38\u5c55\u548c\u53d8\u5f62\u3002\u5728\u7eb3\u7c73\u5c3a\u5ea6\u4e0b\uff0c\u5ef6\u6027\u6750\u6599\u4e2d\u7684\u539f\u5b50\u8fd0\u52a8\u6bd4\u8106\u6027\u6750\u6599\u4e2d\u7684\u66f4\u4e3a\u81ea\u7531\uff0c\u56e0\u6b64\u5728\u5916\u90e8\u65bd\u52a0\u62c9\u529b\uff08\u62c9\u4f38\u5e94\u529b\uff09\u7684\u60c5\u51b5\u4e0b\uff0c\u8fd9\u4e9b\u539f\u5b50\u53ef\u80fd\u79bb\u5f00\u539f\u672c\u6709\u5e8f\u7684\u6676\u683c\uff0c\u5373\u6750\u6599\u4e13\u4e1a\u672f\u8bed\u4e2d\u7684\u4f4d\u9519\u3002\u8fd9\u5c31\u662f\u683c\u91cc\u83f2\u65af\u6a21\u578b\uff0c\u5b83\u4ece\u8bde\u751f\u4e4b\u65e5\u8d77\u5df2\u88ab\u4eba\u4eec\u5e94\u7528\u4e8e\u89e3\u91ca\u5927\u91cf\u6750\u6599\u65ad\u88c2\u73b0\u8c61\uff0c\u4f46\u5176\u6b63\u786e\u6027\u4ecd\u7f3a\u5c11\u539f\u5b50\u6216\u7eb3\u7c73\u5c3a\u5ea6\u7684\u5b9e\u9a8c\u6570\u636e\u652f\u6301\u3002<\/p>\n<p>\u5728\u4e0a\u8ff0\u7814\u7a76\u4e2d\uff0cIBS\u7684\u79d1\u5b66\u5bb6\u4eec\u89c2\u5bdf\u5230\u4e86\u4e8c\u7ef4MoS2\u4e0a\u81ea\u7136\u5f62\u6210\u6216\u7ecf\u7535\u5b50\u675f\u7a7f\u5b54\u5f62\u6210\u7684\u88c2\u7eb9\u662f\u5982\u4f55\u6269\u5c55\u7684\u3002\u8be5\u7814\u7a76\u8bba\u6587\u7684\u7b2c\u4e00\u4f5c\u8005Ly Thuc Hue\u535a\u58eb\u5411\u6211\u4eec\u9610\u8ff0\uff1a\u201c\u6211\u4eec\u5728\u8fdb\u884c\u8bd5\u9a8c\u65f6\u9047\u5230\u7684\u6700\u5927\u56f0\u96be\u5728\u4e8e\u5982\u4f55\u4f7f\u7535\u5b50\u675f\u4ec5\u80fd\u7a7f\u5b54\u3001\u800c\u4e0d\u5bfc\u81f4\u6750\u6599\u4ea7\u751f\u5176\u4ed6\u7f3a\u9677\u53c8\u6216\u662f\u4f7f\u6750\u6599\u88ab\u7834\u574f\u3002\u6240\u4ee5\u6211\u4eec\u53ea\u80fd\u8fc5\u901f\u5b8c\u6210\u64cd\u4f5c\uff0c\u5e76\u4f7f\u7528\u5c3d\u53ef\u80fd\u4f4e\u7684\u80fd\u91cf\u3002\u201d<\/p>\n<p>\u8fd9\u4e2a\u7814\u7a76\u91c7\u7528\u900f\u5c04\u7535\u955c\u5bf9\u539f\u5b50\u8fdb\u884c\u5b9e\u65f6\u89c2\u5bdf\u3002\u5c3d\u7ba1MoS2\u662f\u4e00\u79cd\u8106\u6027\u6750\u6599\uff0c\u4f46\u4ee4\u4eba\u60ca\u8bb6\u7684\u662f\uff0c\u7814\u7a76\u56e2\u961f\u4f9d\u65e7\u5728\u8ddd\u79bb\u5b83\u7684\u88c2\u7eb9\u524d\u6cbf\u6216\u88c2\u7eb9\u5c16\u7aef3-5nm\u7684\u5730\u65b9\u89c2\u5bdf\u5230\u4e86\u539f\u5b50\u4f4d\u9519\u7684\u5b58\u5728\u3002\u8fd9\u4e2a\u73b0\u8c61\u663e\u7136\u4e0d\u80fd\u7528\u683c\u91cc\u83f2\u65af\u6a21\u578b\u6765\u89e3\u91ca\u3002<\/p>\n<p>\u4e3a\u6a21\u62df\u81ea\u7136\u6761\u4ef6\u4e0b\u7684\u5f00\u88c2\uff0c\u7814\u7a76\u56e2\u961f\u5c06\u4e8c\u7ef4MoS2\u6837\u54c1\u66b4\u9732\u5728\u7d2b\u5916\u5149\u4e0b\uff0c\u4f7f\u5176\u6c27\u5316\uff0c\u7531\u6b64\u52a0\u901f\u539f\u5b50\u4f4d\u9519\u5f62\u6210\uff0c\u5e76\u4f7f\u62c9\u4f38\u533a\u57df\u6269\u5c55\u81f3\u8ddd\u88c2\u7eb9\u5c16\u7aef5-10nm\u5904\u3002<\/p>\n<p>\u201c\u6211\u4eec\u7684\u7814\u7a76\u8868\u660e\uff0c\u4e8c\u7ef4\u6750\u6599\u7684\u5f00\u88c2\u4e0e\u4e09\u7ef4\u8106\u6027\u6216\u97e7\u6027\u6750\u6599\u7684\u5f00\u88c2\u5728\u672c\u8d28\u4e0a\u662f\u4e0d\u540c\u7684\uff0c\u201dCINAP\u6559\u6388Lee Young Hee\u5bf9\u6b64\u89e3\u91ca\u9053\uff0c\u201c\u8fd9\u4e9b\u73b0\u8c61\u65e0\u6cd5\u518d\u7528\u5e38\u89c4\u7684\u6750\u6599\u5931\u6548\u7406\u8bba\u6765\u89e3\u91ca\uff0c\u6240\u4ee5\u6211\u4eec\u8ba4\u4e3a\u5f88\u6709\u5fc5\u8981\u4e3a\u4e4b\u5efa\u7acb\u4e00\u5957\u65b0\u7684\u7406\u8bba\u4f53\u7cfb\u3002\u201d<\/p>\n<p>\u611f\u5174\u8da3\u7684\u8bfb\u8005\u53ef\u4ee5\u81ea\u884c\u9605\u8bfb\u5173\u4e8e\u8be5\u9879\u7814\u7a76\u7684\u8bba\u6587\uff0c\u6587\u732e\u9898\u76ee\u4e3a\uff1a Dynamical Observations on the Crack Tip Zone and Stress Corrosion of Two-dimensional MoS2\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/www.asianscientist.com\/2017\/02\/in-the-lab\/2d-material-crack-atomic\/\" target=\"_blank\">How Do 2D Materials Crack?<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.nature.com\/articles\/ncomms14116\" target=\"_blank\">Dynamical Observations on the Crack Tip Zone and Stress Corrosion of Two-dimensional MoS2<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u6708\u4eae\u63d0\u4f9b\u7d20\u6750\uff0c\u5510\u601d\u54f2\u7f16\u8bd1\uff0c\u96ea\u7430\u5ba1\u6838\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u4e8c\u7ef4\u6750\u6599\u4f5c\u4e3a\u73b0\u4eca\u6750\u6599\u5b66\u754c\u7684\u70ed\u95e8\u65b9\u5411\uff0c\u6709\u7740\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u4f46\u5bf9\u4e8c\u7ef4\u6750\u6599\u7684\u63a2\u7d22\u4eba\u7c7b\u8fd8\u6709\u5f88\u957f\u7684\u8def\u8981\u8d70\uff0c\u6bd4\u5982\uff0c\u4f60\u77e5\u9053\u4e8c\u7ef4\u6750\u6599\u7684\u65ad\u88c2\u673a\u5236\u5417\uff1fIBS\u79d1\u7814\u56e2\u961f\u7684\u6700\u65b0&#8230;<\/p>\n","protected":false},"author":230,"featured_media":68324,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[258],"class_list":["post-68322","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-2d"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/68322"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=68322"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/68322\/revisions"}],"predecessor-version":[{"id":68457,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/68322\/revisions\/68457"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/68324"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=68322"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=68322"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=68322"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}