{"id":75549,"date":"2017-04-15T14:00:54","date_gmt":"2017-04-15T06:00:54","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=75549"},"modified":"2017-04-12T20:08:49","modified_gmt":"2017-04-12T12:08:49","slug":"acs-nano%ef%bc%9asi%e5%be%ae%e7%b1%b3%e7%ba%bf-zno%e7%ba%b3%e7%b1%b3%e8%96%84%e8%86%9c%e5%9f%ba%e7%9a%84%e6%9f%94%e6%80%a7led%e9%98%b5%e5%88%97%e5%99%a8%e4%bb%b6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=75549","title":{"rendered":"ACS Nano\uff1aSi\u5fae\u7c73\u7ebf-ZnO\u7eb3\u7c73\u8584\u819c\u57fa\u7684\u67d4\u6027LED\u9635\u5217\u5668\u4ef6"},"content":{"rendered":"<p><strong><b>\u3010\u5f15\u8a00\u3011<\/b><\/strong><\/p>\n<p>Si\u662f\u6700\u5177\u6709\u4ee3\u8868\u6027\u7684\u534a\u5bfc\u4f53\u6750\u6599\uff0c\u8fdb\u5165\u4fe1\u606f\u65f6\u4ee3\u4ee5\u6765\uff0cSi\u4f5c\u4e3a\u7b2c\u4e00\u4ee3\u534a\u5bfc\u4f53\u6750\u6599\u5728\u4e8c\u6781\u7ba1\uff0cCMOS\u7b49\u65b9\u9762\u53d6\u5f97\u4e86\u957f\u8db3\u7684\u53d1\u5c55\u3002\u8fd1\u5e74\u6765\u67d4\u6027\u5668\u4ef6\u7531\u4e8e\u5176\u53ef\u5f2f\u66f2\u6027\u3001\u80fd\u66f4\u597d\u7684\u7684\u8d34\u5408\u5728\u7269\u4f53\u8868\u9762\u7684\u6027\u80fd\u9010\u6e10\u5f15\u8d77\u4eba\u4eec\u7684\u5173\u6ce8\uff0c\u5f53\u7136\uff0c\u7845\u8fd8\u662f\u9996\u9009\u7684\u57fa\u5e95\u6750\u6599\u3002\u4f46\u662f\uff0c\u7531\u4e8eSi\u7684\u6027\u8d28\u8f83\u8106\u548c\u8f83\u5f31\u7684\u5149\u7535\u5b50\u5b66\u6027\u80fd\uff0c\u4f7f\u5f97\u7814\u7a76\u5236\u5907\u67d4\u6027\u57fa\u5e95\u7684LED\u9635\u5217\u6210\u4e3a\u4e86\u4e00\u5927\u6311\u6218\uff0c\u540c\u65f6\u8fd9\u4e00\u6311\u6218\u4e5f\u5f15\u8d77\u4e86\u7814\u7a76\u4eba\u5458\u7684\u7814\u53d1\u70ed\u60c5\u3002<\/p>\n<p><strong><b>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/b><\/strong><\/p>\n<p>\u6765\u81ea<strong><b>\u6e05\u534e\u5927\u5b66\u6750\u6599\u5b66\u9662<\/b><\/strong><strong><b>\u7684<\/b><\/strong><strong><b>\u6731\u9759<\/b><\/strong><strong><b>\u9662\u58eb\u3001<\/b><\/strong><strong><b>\u4e2d\u79d1\u9662\u5317\u4eac\u7eb3\u7c73\u80fd\u6e90\u4e0e\u7cfb\u7edf\u7814\u7a76\u6240\u7684\u738b\u4e2d\u6797\u9662\u58eb\u3001\u6f58\u66f9\u5cf0<\/b><\/strong><strong><b>\u7814\u7a76\u5458<\/b><\/strong><strong><b>\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/b><\/strong>\u7b49\u4eba\u7814\u5236\u51fa\u4e86\u96c6\u67d4\u6027\u3001\u7a33\u5b9a\u3001\u8d28\u91cf\u8f7b\u548c\u53ef\u8fdb\u884c\u80fd\u91cf\u6536\u96c6\u7b49\u4f18\u70b9\u4e3a\u4e00\u8eab\u7684Si\u5fae\u7c73\u7ebf-ZnO\u7eb3\u7c73\u8584\u819c\u57fa\u7684\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\uff0c\u8be5\u5668\u4ef6\u53ef\u4ee5\u7528\u4f5c\u6d4b\u4e8c\u7ef4\u538b\u529b\u5206\u5e03\u7684\u4f5c\u538b\u529b\u4f20\u611f\u5668\u3002\u57fa\u4e8e\u538b\u7535\u6548\u5e94\uff0c\u67d4\u6027LED\u9635\u5217\u4eae\u5ea6\u53ef\u4ee5\u63d0\u9ad8\u4e09\u500d\uff08\u5728\u4f4e\u4e8e60Mpa\u7684\u538b\u529b\u4e0b\uff09\u3002\u6b64\u5916\uff0c\u8be5\u5668\u4ef6\u6027\u80fd\u7a33\u5b9a\u5e76\u53ef\u8fdb\u884c\u80fd\u91cf\u6536\u96c6\u5b9e\u73b0\u81ea\u4f9b\u7535\uff0c\u57281000\u6b21\u5f2f\u66f2\u5faa\u73af\u548c\u5728\u7a7a\u6c14\u4e2d\u653e\u7f6e6\u4e2a\u6708\u4e4b\u540e\u4f9d\u7136\u53ef\u4ee5\u5f88\u597d\u5730\u5de5\u4f5c\u3002\u4e14\u8be5\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u7684\u529f\u8017\u4ec5\u662f\u5e73\u5e38LED\u529f\u8017\u76848%\u3002\u8fd9\u79cd\u67d4\u6027\u7845\u57fa\u5668\u4ef6\u5177\u6709\u5e7f\u9614\u7684\u5e94\u7528\u5e76\u4e14\u6709\u53ef\u80fd\u5f15\u53d1\u67d4\u6027\u663e\u793a\u5c4f\u3001\u89e6\u5c4f\u6280\u672f\u548c\u667a\u80fd\u76ae\u80a4\u76f8\u5173\u7684\u6280\u672f\u9769\u547d\u3002<\/p>\n<p><strong><b>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe1.\u67d4\u6027<\/b><\/strong><strong><b>\u805a\u5408\u7269<\/b><\/strong><strong><b>\/Si\/ZnO LEDs\u9635\u5217\u5668\u4ef6\u7684\u5236\u5907\u8fc7\u7a0b<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-75550\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72471-7.jpg\" alt=\"\" width=\"600\" height=\"225\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72471-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72471-7-300x113.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>\uff08a-e\uff09\u5782\u76f4Si\u5fae\u7c73\u7ebf\u9635\u5217\u7684\u8f6c\u79fb\u8fc7\u7a0b<\/p>\n<p>\uff08f\uff09\u67d4\u6027\u805a\u5408\u7269\/Si\/ZnO LEDs\u9635\u5217\u5668\u4ef6\u7684\u539f\u7406\u56fe<\/p>\n<p><strong><b>\u56fe2.\u67d4\u6027LED\u9635\u5217\u7ed3\u6784\u7279\u70b9<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-75551\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72472-6.jpg\" alt=\"\" width=\"600\" height=\"302\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72472-6.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72472-6-300x151.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>\uff08a\uff09Si\u5fae\u7c73\u7ebf\u7684SEM\u4fa7\u9762\u56fe\uff0c\u5176\u4e2d\u7684\u5c0f\u63d2\u56fe\u662fSi\u5fae\u7c73\u7ebf\u7684\u4fef\u89c6\u56fe\uff0c\u6807\u5c3a\u4e3a15um<\/p>\n<p>\uff08b\uff09\u8f6c\u79fb\u4e2d\u7684\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u548cSi\u886c\u5e95\u7684\u793a\u610f\u56fe<\/p>\n<p>\uff08c\uff09\u805a\u5408\u7269\/Si\u5fae\u7c73\u7ebf\u9635\u5217\u805a\u5408\u7269\u8584\u819c\u7684\u80cc\u9762<\/p>\n<p>\uff08d\uff09\u8f6c\u79fb\u7684\u67d4\u6027\u8584\u819c\uff0c\u53ef\u5377\u6210\u5706\u7b52\u72b6<\/p>\n<p>\uff08e\uff09\u8f6c\u79fb\u540e\u7684Si\u5f7b\u5e95\u7684SEM\u56fe<\/p>\n<p>\uff08f\uff09\u572810V\u7535\u538b\u4e0b\u7684LED\u9635\u5217\u7684\u5149\u5b66\u56fe\u50cf<\/p>\n<p><strong><b>\u56fe3.\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u7684\u67d4\u97e7\u5ea6<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-75552\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72473-5.jpg\" alt=\"\" width=\"600\" height=\"316\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72473-5.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72473-5-300x158.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>\uff08a\uff09\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u7ed3\u6784\u793a\u610f\u56fe<\/p>\n<p>\uff08b\uff09LEDs\u7684\u4e0d\u540c\u533a\u57df\u7684\u53d1\u5149\u4eae\u5ea6<\/p>\n<p>\uff08c\uff09\u5728\u4e0d\u540c\u5f2f\u66f2\u89d2\u5ea6\u4e0b\u7684I-V\u66f2\u7ebf<\/p>\n<p>\uff08d\uff09\u57281MHz\u9891\u7387\u4e0b\u7684\u8109\u51b2\u7535\u538b\u4f5c\u7528\u4e0b\uff0cLEDs\u9635\u5217\u5668\u4ef6\u5728\u8fde\u7eed\u4eae24h\u4ee5\u540e\u7684\u4e0d\u540cLEDs\u7684\u53d1\u5149\u4eae\u5ea6<\/p>\n<p>\uff08e\uff09\u57281000\u6b21\u5faa\u73af\u540e\u7684LED\u9635\u5217\u5668\u4ef6\u7684\u673a\u68b0\u7a33\u5b9a\u6027<\/p>\n<p><strong><b>\u56fe4.\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u7684\u53d1\u5149\u6027\u80fd<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-75553\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72474-5.jpg\" alt=\"\" width=\"600\" height=\"278\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72474-5.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72474-5-300x139.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>\uff08a\uff09\u5728\u4e0d\u540c\u8f93\u5165\u7535\u6d41\u4e0b\u67d4\u6027\u5668\u4ef6\u7684EL\u5149\u8c31<\/p>\n<p>\uff08b\uff09\u5f53\u8f93\u5165\u7535\u6d41\u4e3a30mA\u65f6\uff0c\u7528\u9ad8\u65af\u65b9\u7a0b\u6765\u8ba1\u7b97\u5149\u8c31\u7684\u5cf0\u503c<\/p>\n<p>\uff08c-f\uff09\u6bd4\u8f83\u4e09\u79cd\u4e0d\u540c\u4f46\u76f8\u4f3c\u7684ZnO\/Si LED\u9635\u5217\u5668\u4ef6\u7684\u4e0d\u540c\u70b9\uff1a\uff08d\uff09SC LED\uff0c\uff08e\uff09DCSS\uff0c\uff08f\uff09\u67d4\u6027LED<\/p>\n<p><strong><b>\u56fe5.LED\u9635\u5217\u5668\u4ef6\u7684\u5de5\u4f5c\u673a\u7406\u53ca\u5176\u538b\u7535\u53d1\u5149\u7684\u589e\u5f3a\u6548\u5e94<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-75554\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72476-3.jpg\" alt=\"\" width=\"600\" height=\"416\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72476-3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/\u56fe\u72476-3-300x208.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>\uff08a\uff09\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u6d4b\u8bd5\u538b\u529b\u5206\u5e03\u7684\u5de5\u4f5c\u673a\u5236<\/p>\n<p>\uff08b\uff09\u5929\u84dd\u8272\u7684NANO\u56fe\u6848\uff0c\u6807\u5c3a150um<\/p>\n<p>\uff08c\uff09LED\u4e0a\u7684\u538b\u529b\u5206\u5e03\u663e\u793aNANO\u56fe\u6848<\/p>\n<p>\uff08d\uff09\u5728\u6ca1\u6709\u504f\u7f6e\u7535\u538b\u548c\u6ca1\u6709\u5e94\u529b\u4f5c\u7528\u4e0b\u7684\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u7684\u80fd\u5e26\u7ed3\u6784\u56fe<\/p>\n<p>\uff08e\uff09\u5728\u6709\u504f\u7f6e\u7535\u538b\u548c\u5e94\u529b\u4f5c\u7528\u4e0b\u7684\u67d4\u6027LED\u9635\u5217\u5668\u4ef6\u7684\u80fd\u5e26\u7ed3\u6784\u56fe<\/p>\n<p>\uff08f\uff09\u5728\u4e0d\u540c\u538b\u529b\u4e0bLEDs\u9635\u5217\u5668\u4ef6\u7684\u538b\u529b\u5206\u5e03\u56fe\uff08\u901a\u8fc7\u4eae\u5ea6\u6765\u663e\u793a\uff09<\/p>\n<p><strong><b>\u3010<\/b><\/strong><strong><b>\u5c0f<\/b><\/strong><strong><b>\u7ed3\u3011<\/b><\/strong><\/p>\n<p>\u8be5\u7814\u7a76\u56e2\u961f\u5728\u5ba4\u6e29\u4e0b\u8bbe\u8ba1\u5236\u9020\u4e86Si\u5fae\u7c73\u7ebf\u9635\u5217\u6765\u5236\u5907n-ZnO\/p-Si \u5f02\u8d28\u7ed3LEDs\uff0c\u8be5\u5668\u4ef6\u5177\u6709\u67d4\u6027\u3001\u957f\u4f7f\u7528\u5bff\u547d\u548c\u81ea\u4f9b\u7535\u53ca\u53d1\u51fa\u53ef\u89c1\u5149\u4eae\u5ea6\u8f83\u5f3a\u7b49\u4f18\u70b9\u3002\u8be5LEDs\u9635\u5217\u6709\u5f88\u597d\u7684\u673a\u68b0\u67d4\u6027\uff0c\u5728\u5f00\u5173\u6b21\u6570\u8d85\u8fc710<sup>11<\/sup>\u548c\u6301\u7eed\u53d1\u514924h\u540e\u4f9d\u7136\u53ef\u4ee5\u5f88\u597d\u7684\u5de5\u4f5c\u3002\u4e0e\u4f20\u7edf\u7684SC LED\u76f8\u6bd4\u67d4\u6027LEDs\u76f8\u5f53\u7684\u8282\u80fd\u3002\u5f53\u5176\u572860Mpa\u7684\u538b\u529b\u4f5c\u7528\u4e0bLEDs\u9635\u5217\u5668\u4ef6\u7684EL\u4eae\u5ea6\u4f1a\u589e\u59273\u500d\u4ee5\u4e0a\u3002\u6839\u636eLEDs\u7684\u589e\u5f3a\u53d1\u5149\u533a\u53ef\u4ee5\u7528\u6765\u6d4b\u5b9a\u538b\u529b\u5206\u5e03\u3002<\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5<\/b><\/strong>\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.7b00272\" target=\"_blank\">Flexible Light Emission Diode Arrays Made of Transferred Si Microwires-ZnO Nanofilm ith Piezo-Phototronic Effect Enhanced Lighting<\/a> (ACS Nano, 2017, DOI:\u00a010.1021\/acsnano.7b00272)\u00a0<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u5b66\u672f\u7ec4\u738b\u5a75\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002\u5982\u679c\u4f60\u5bf9\u7535\u5b50\u6750\u6599\u611f\u5174\u8da3\uff0c\u613f\u610f\u4e0e\u7535\u5b50\u7535\u5de5\u9886\u57df\u4eba\u624d\u4ea4\u6d41\uff0c\u8bf7\u52a0\u5165\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4\uff08QQ\u7fa4\uff1a482842474\uff09<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong><b>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/b><\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 Si\u662f\u6700\u5177\u6709\u4ee3\u8868\u6027\u7684\u534a\u5bfc\u4f53\u6750\u6599\uff0c\u8fdb\u5165\u4fe1\u606f\u65f6\u4ee3\u4ee5\u6765\uff0cSi\u4f5c\u4e3a\u7b2c\u4e00\u4ee3\u534a\u5bfc\u4f53\u6750\u6599\u5728\u4e8c\u6781\u7ba1\uff0cCMOS\u7b49\u65b9\u9762\u53d6\u5f97\u4e86\u957f\u8db3\u7684\u53d1\u5c55\u3002\u8fd1\u5e74\u6765\u67d4\u6027\u5668\u4ef6\u7531\u4e8e\u5176\u53ef\u5f2f\u66f2\u6027\u3001\u80fd\u66f4&#8230;<\/p>\n","protected":false},"author":99,"featured_media":75555,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[31],"class_list":["post-75549","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-dianzi"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/75549"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/99"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=75549"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/75549\/revisions"}],"predecessor-version":[{"id":75865,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/75549\/revisions\/75865"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/75555"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=75549"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=75549"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=75549"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}