{"id":7709,"date":"2016-04-15T08:00:14","date_gmt":"2016-04-15T00:00:14","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=7709"},"modified":"2017-03-04T22:39:03","modified_gmt":"2017-03-04T14:39:03","slug":"%e7%8e%8b%e4%b8%ad%e6%9e%97acs-nano%ef%bc%9a%e4%bc%a0%e7%bb%9f%e5%89%aa%e7%ba%b8%e8%89%ba%e6%9c%af%e8%b5%a0%e4%ba%88%e7%9a%84%e7%a4%bc%e7%89%a9-%e5%8f%af%e4%bc%b8%e7%bc%a9","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=7709","title":{"rendered":"\u738b\u4e2d\u6797ACS nano\uff1a\u4f20\u7edf\u526a\u7eb8\u827a\u672f\u8d60\u4e88\u7684\u201c\u793c\u7269\u201d\u2014\u53ef\u4f38\u7f29\u6027\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a"},"content":{"rendered":"<p>\u3010<strong>\u80cc\u666f\u7b80\u4ecb<\/strong>\u3011<\/p>\n<p>\u5728\u8fc7\u53bb\u7684\u51e0\u5341\u5e74\u95f4\uff0c\u4f5c\u4e3a\u4e0b\u4e00\u4ee3\u529f\u80fd\u5668\u4ef6\u7684\u67d4\u6027\u7535\u5b50\u5b66\u4e00\u76f4\u5728\u4e0d\u65ad\u53d1\u5c55\uff0c\u5e76\u5438\u5f15\u4e86\u5de5\u4e1a\u754c\u548c\u5b66\u672f\u754c\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u76f8\u6bd4\u4f20\u7edf\u5668\u4ef6\uff0c\u5728\u4e0d\u727a\u7272\u5668\u4ef6\u6027\u80fd\u548c\u53ef\u9760\u6027\u7684\u60c5\u51b5\u4e0b\uff0c\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u6709\u826f\u597d\u7684\u53ef\u53d8\u5f62\u6027\u3002\u56e0\u6b64\uff0c\u67d4\u6027\u7535\u5b50\u5b66\u5728\u53ef\u7a7f\u6234\u5668\u4ef6\u3001\u7535\u5b50\u76ae\u80a4\u3001\u690d\u5165\u5f0f\u7535\u5b50\u5668\u4ef6\u7b49\u65b9\u9762\u6709\u7740\u5de8\u5927\u7684\u5e94\u7528\u524d\u666f\u3002\u4f5c\u4e3a\u67d4\u6027\u7535\u5b50\u7cfb\u7edf\u4e2d\u5fc5\u4e0d\u53ef\u5c11\u7684\u4f9b\u80fd\u6a21\u5757\u4e5f\u5728\u98de\u901f\u7684\u53d1\u5c55\uff0c\u79d1\u5b66\u5bb6\u4eec\u5df2\u7ecf\u7814\u7a76\u4e86\u4f17\u591a\u53ef\u53d8\u5f62\u7684\u80fd\u91cf\u5b58\u50a8\u5668\u4ef6\uff0c\u6bd4\u5982\u57fa\u4e8e\u8584\u819c\u53ef\u5f2f\u66f2\u7684\u8d85\u7ea7\u7535\u5bb9\u5668\u548c\u7535\u6c60\uff0c\u8d34\u5728\u8863\u670d\u4e0a\u7684\u53ef\u4f38\u7f29\u7684\u8d85\u7ea7\u7535\u5bb9\u5668\u548c\u53ef\u4f38\u7f29\u7684\u9502\u79bb\u5b50\u7535\u6c60\u7b49\u3002\u7136\u800c\uff0c\u53ef\u4f38\u7f29\u7684\u53d1\u7535\u5668\u4ef6\u5728\u67d4\u6027\u81ea\u4f9b\u80fd\u7535\u5b50\u7cfb\u7edf\u4e2d\u6709\u7740\u66f4\u9ad8\u6c34\u5e73\u7684\u5e94\u7528\u6f5c\u529b\uff0c\u56e0\u6b64\uff0c<strong>\u67d4\u6027\u53d1\u7535\u5668\u4ef6<\/strong>\u4e5f\u662f\u56fd\u9645\u79d1\u7814\u9886\u57df\u4e2d\u7684\u70ed\u70b9\u3002<\/p>\n<p>\u5728\u65e5\u5e38\u751f\u6d3b\u4e2d\uff0c\u673a\u68b0\u80fd\u662f\u4e00\u79cd\u666e\u904d\u5b58\u5728\u7684\u80fd\u91cf\u3002\u79d1\u5b66\u5bb6\u5728\u5229\u7528\u673a\u68b0\u80fd\u53d1\u7535\u65b9\u9762\u505a\u4e86\u5f88\u591a\u5de5\u4f5c\uff0c\u4f8b\u5982\u7535\u78c1\u53d1\u7535\u673a\u3001\u538b\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u548c\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u7b49\u3002\u5176\u4e2d<strong>\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\uff08TENG\uff09\u662f\u5229\u7528\u6469\u64e6\u5e26\u7535\u548c\u9759\u7535\u611f\u5e94\u4e4b\u95f4\u7684\u8026\u5408\u6548\u5e94\u5c06\u673a\u68b0\u80fd\u8f6c\u6362\u6210\u7535\u80fd\u7684\uff0c\u6709\u7740\u4f4e\u6210\u672c\u548c\u5145\u88d5\u7684\u539f\u6599\u9009\u62e9\u7b49\u4f18\u70b9<\/strong>\uff0c\u56e0\u6b64\uff0c\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u5728\u4e3a\u67d4\u6027\u7535\u5b50\u7cfb\u7edf\u63d0\u4f9b\u53ef\u4f38\u7f29\u80fd\u91cf\u65b9\u9762\u5b58\u5728\u5f88\u5927\u7684\u53ef\u80fd\u6027\u3002<\/p>\n<p>\u76ee\u524d\uff0c\u8fd9\u4e2a\u9886\u57df\u7684\u96be\u9898\u5728\u4e8e\u6469\u64e6\u7535\u53d1\u7535\u673a\u7684\u53ef\u5f2f\u66f2\u6027\u4f9d\u8d56\u4e8e\u7ec4\u6210\u6750\u6599\uff0c\u8981\u6c42\u7ec4\u6210\u6750\u6599\uff08\u50cfPDMS\u548c\u6a61\u80f6\uff09\u5fc5\u987b\u8981\u4fdd\u8bc1\u56fa\u6709\u7684\u5f39\u6027\u3002\u4f46\u662f\uff0c\u79d1\u5b66\u5bb6\u5229\u7528\u8fd9\u4e9b\u5f39\u6027\u6750\u6599\u5236\u4f5c\u7684\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u7684\u53ef\u4f38\u7f29\u6548\u679c\u5e76\u4e0d\u7406\u60f3\u3002\u8be5\u600e\u4e48\u63d0\u9ad8\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u7684\u53ef\u4f38\u7f29\u6027\u5462\uff1f<\/p>\n<p>\u8fd1\u65e5\uff0c\u7f8e\u56fd\u4f50\u6cbb\u4e9a\u7406\u5de5\u5b66\u9662<strong>\u738b\u4e2d\u6797<\/strong>\u6559\u6388\u7b49\u4eba\uff0c<strong>\u4ece\u4e2d\u56fd\u4f20\u7edf\u7684\u526a\u7eb8\u827a\u672f\u4e2d\u83b7\u5f97\u7075\u611f\uff0c\u901a\u8fc7\u5bf9\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u7ec4\u6210\u6750\u6599\u7684\u7ed3\u6784\u5165\u624b\uff0c\u8bbe\u8ba1\u4e86\u4e00\u79cd\u9ad8\u5ea6\u53ef\u4f38\u7f29\u7684\u8054\u9501\u526a\u7eb8\u56fe\u6848\u7ed3\u6784\u7684\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\uff08\u7eb8\u57faK-TENG\uff09<\/strong>\u3002<\/p>\n<p>\u3010<strong>\u4e3b\u8981\u4eae\u70b9<\/strong>\u3011<\/p>\n<p><strong>\u8fd9\u79cd\u5177\u6709\u4f18\u826f\u4f38\u7f29\u6027\u7684\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\uff08TENG\uff09\u501f\u7528\u4e86\u4f20\u7edf\u7684\u526a\u7eb8\u56fe\u6848\uff0c\u5b83\u7684\u53ef\u4f38\u7f29\u6027\u6e90\u81ea\u4e8e\u7ed3\u6784\u7684\u8bbe\u8ba1\uff0c\u800c\u4e0d\u662f\u7ec4\u6210\u6750\u6599\u3002<\/strong>\u5229\u7528\u8fd9\u79cd\u8bbe\u8ba1\u65b9\u6cd5\uff0c\u5bf9\u4e8e<strong>\u6ca1\u6709\u5f39\u6027\u7684\u6750\u6599\u4e5f\u53ef\u4ee5\u88ab\u7528\u6765\u5236\u4f5cTENG<\/strong>\u3002\u56e0\u6b64\uff0c\u8fd9\u79cd\u8bbe\u8ba1\u65b9\u6cd5\u5177\u6709\u5f88\u9ad8\u7684<strong>\u666e\u9002\u6027<\/strong>\u3002\u6587\u732e\u4e2d\u5236\u4f5c\u7684\u7eb8\u57faK-TENG\u7684<strong>\u53ef\u5f2f\u66f2\u6027\u53ef\u8fbe\u5230100%<\/strong>\uff0c<strong>\u53ef\u4ee5\u901a\u8fc7\u5404\u79cd\u5f62\u5f0f\u7684\u8fd0\u52a8\uff08\u4f8b\u5982\u4f38\u7f29\u3001\u6324\u538b\u548c\u626d\u8f6c\u7b49\uff09\u8fdb\u884c\u5de5\u4f5c<\/strong>\u3002\u5728\u8be5\u5668\u4ef6\u4e0a\u505a\u4e00\u4e2a\u7b80\u5355\u7684\u62cd\u624b\u52a8\u4f5c\u5c31\u53ef\u4ee5\u4ea7\u751f\u9ad8\u8fbe<strong>115.49V<\/strong>\u7684\u5f00\u8def\u7535\u538b\u548c<strong>39.87nC<\/strong>\u7684\u8f6c\u79fb\u7535\u8377\u3002\u6b64\u5916\uff0c\u8fd9\u79cdK-TENG\u6709\u7740\u5e7f\u6cdb\u7684\u5e94\u7528\uff0c\u4f8b\u5982\u6db2\u6676\u663e\u793a\u5c4f\u3001LED\u7167\u660e\u9635\u5217\u548c\u81ea\u4f9b\u7535\u52a0\u901f\u4f20\u611f\u7b49\u3002\u8fd9\u9879\u5de5\u4f5c\u663e\u8457\u63d0\u9ad8\u4e86\u53ef\u4f38\u7f29TENG\u7684\u53ef\u4f38\u7f29\u5ea6\uff0c\u4fc3\u8fdb\u4e86\u53ef\u4f38\u7f29TENG\u5728\u67d4\u6027\u7535\u5b50\u5b66\u9886\u57df\u7684\u5f15\u7528\uff0c\u5f00\u8f9f\u4e86\u57fa\u4e8e\u526a\u7eb8\u8bbe\u8ba1\u5728\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u5e94\u7528\u7684\u53d1\u5c55\u65b9\u5411\u3002<\/p>\n<p>\u3010<strong>\u7ed3\u679c\u548c\u8ba8\u8bba<\/strong>\u3011<img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-7711\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/1-6.png\" alt=\"1\" width=\"604\" height=\"492\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/1-6.png 604w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/1-6-300x244.png 300w\" sizes=\"(max-width: 604px) 100vw, 604px\" \/><\/p>\n<p><strong>\u56fe1<\/strong> \uff08a\uff09\u7eb8\u57faK-TENG\u7684\u7ed3\u6784\u793a\u610f\u56fe\uff1a\u4e0a\u9762\u7684\u63d2\u56fe\u662fFEP\u8584\u819c\u7684SEM\u56fe\u7247\uff0c\u4e0b\u9762\u7684\u63d2\u56fe\u662f\u8054\u9501\u7ed3\u6784\u7684\u5256\u89c6\u56fe\u3002\uff08b\uff09\u4e0d\u540c\u62c9\u529b\u6761\u4ef6\u4e0b\u7684\u7ec4\u5408\u5668\u4ef6\u7684\u56fe\u7247\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-7712\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/2-6.png\" alt=\"2\" width=\"837\" height=\"504\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/2-6.png 837w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/2-6-300x181.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/2-6-768x462.png 768w\" sizes=\"(max-width: 837px) 100vw, 837px\" \/><br \/>\n<strong>\u56fe2<\/strong>\u3000\u7eb8\u57faK-TENG\u7684\u5de5\u4f5c\u673a\u7406\uff1a\u8fd9\u79cd\u8054\u9501\u526a\u7eb8\u56fe\u6848\u7ed3\u6784\u9650\u5236\u4e86FEP\u5c42\u7684\u53d8\u5f62\uff0c\u786e\u4fdd\u5f20\u529b\u91ca\u653e\u540e\uff0c\u5668\u4ef6\u53ef\u4ee5\u590d\u539f\uff0c\u6781\u5927\u5730\u63d0\u9ad8\u4e86\u5668\u4ef6\u7684\u7a33\u5b9a\u6027\u548c\u53ef\u9760\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-7713\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/3-7.png\" alt=\"3\" width=\"620\" height=\"578\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/3-7.png 620w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/3-7-300x280.png 300w\" sizes=\"(max-width: 620px) 100vw, 620px\" \/><\/p>\n<p><strong>\u56fe3<\/strong> \u00a0 \u5728\u62c9\u4f38\u5e94\u53d8\u4e3a16%\u300128%\u548c40%\u7684\u60c5\u51b5\u4e0b\uff0c\u7eb8\u57faK-TENG\u7684\u5178\u578b\u7535\u5b66\u53c2\u6570\u8f93\u51fa\uff1a(a) \u5f00\u8def\u7535\u538bVoc\uff0c\uff08b\uff09\u77ed\u8def\u7535\u6d41Isc\u548c\uff08c\uff09\u8f6c\u79fb\u7535\u8377\u91cfQtr\u3002\u4e0a\u9762\u7684\u63d2\u56fe\u662f\u5728\u76f8\u5e94\u5e94\u53d8\u503c\u7684\u6761\u4ef6\u4e0b\uff0c\u7eb8\u57faK-TENG\u7684\u5256\u89c6\u56fe\u3002\u4ece\u4e0a\u56fe\u53ef\u4ee5\u770b\u51fa\uff1a\u5e94\u53d8\u4e3a16%\u300128%\u548c40%\u7684\u4e09\u79cd\u60c5\u51b5\u5206\u522b\u5bf9\u5e94\u7740\u5668\u4ef6\u5904\u4e8e\u8f7b\u5fae\u62c9\u4f38\u3001\u6ee1\u8f7d\u62c9\u4f38\u548c\u8d85\u8f7d\u62c9\u4f38\u7684\u72b6\u6001\uff0c\u901a\u8fc7\u5bf9\u8fd9\u4e09\u79cd\u4ee3\u8868\u72b6\u6001\u7684\u6d4b\u8bd5\uff0c\u53ef\u4ee5\u5f97\u5230\u5668\u4ef6\u7684\u6700\u5927\u5de5\u4f5c\u6781\u9650\u3002\u5728\u524d\u4e24\u79cd\u72b6\u6001\u4e0b\uff0c\u7535\u8377\u5206\u79bb\u8ddd\u79bb\u968f\u62c9\u4f38\u5e94\u53d8\u589e\u5927\u5355\u8c03\u589e\u52a0\uff0c\u6545\u5f00\u8def\u7535\u538bVoc\u548c\u8f6c\u79fb\u7535\u8377Qtr\u4e5f\u5355\u8c03\u589e\u52a0\uff1b\u5728\u8d85\u8f7d\u62c9\u4f38\u72b6\u6001\u4e0b\uff0c\u7535\u8377\u5206\u79bb\u8ddd\u79bb\u968f\u62c9\u4f38\u5e94\u53d8\u589e\u5927\u5f00\u59cb\u4e0b\u964d\u3002\u53ef\u4ee5\u5f97\u51fa\uff0c\u5728\u6ee1\u8f7d\u62c9\u4f38\u72b6\u6001\u4e0b\uff0c\u5668\u4ef6\u7684\u5f00\u8def\u7535\u538bVoc \u8fbe\u5230\u6700\u5927\u503c\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-7714\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/4-6.png\" alt=\"4\" width=\"763\" height=\"542\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/4-6.png 763w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/4-6-300x213.png 300w\" sizes=\"(max-width: 763px) 100vw, 763px\" \/><br \/>\n<strong>\u56fe4<\/strong> \u00a0 K-TENG\u7684\u4e0d\u540c\u5de5\u4f5c\u6a21\u5f0f\uff1a\uff08a-c\uff09\u62c9\u4f38\u6a21\u5f0f\u4e0b\u5e94\u53d8\u503c\u4e3a28%\u7684\u7eb8\u57faK-TENG\u7684\u5256\u89c6\u56fe\uff0c\u5f00\u8def\u7535\u538bVoc\u548c\u8f6c\u79fb\u7535\u8377Qtr\uff1b\uff08d-f\uff09\u538b\u7f29\u6a21\u5f0f\u4e0b\u7eb8\u57faK-TENG\u7684\u5256\u89c6\u56fe\uff0c\u5f00\u8def\u7535\u538bVoc\u548c\u8f6c\u79fb\u7535\u8377Qtr\uff1b\uff08g-i\uff09\u626d\u8f6c\u6a21\u5f0f\u4e0b\u7eb8\u57faK-TENG\u7684\u5256\u89c6\u56fe\uff0c\u5f00\u8def\u7535\u538bVoc\u548c\u8f6c\u79fb\u7535\u8377Qtr\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-7715\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/5-6.png\" alt=\"5\" width=\"701\" height=\"503\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/5-6.png 701w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/5-6-300x215.png 300w\" sizes=\"(max-width: 701px) 100vw, 701px\" \/><br \/>\n<strong>\u56fe5<\/strong> \u00a0 \u7eb8\u57faK-TENG\u5728\u81ea\u4f9b\u80fd\u52a0\u901f\u4f20\u611f\u5668\u7684\u5e94\u7528\uff1a\uff08a\uff09\u5728\u4e0d\u540c\u52a0\u901f\u5ea6\u503c\u4e0b\u5bf9\u5e94\u7684\u5f00\u8def\u7535\u538bVoc\uff1b\uff08b\uff09\u88c5\u6709\u7eb8\u57faK-TENG\u7684\u52a0\u901f\u4f20\u611f\u5668\u7684\u56fe\u7247\uff1b\uff08c\uff09\u5f00\u8def\u7535\u538bVoc\u548c\u52a0\u901f\u5ea6a\u7684\u5173\u7cfb\u56fe\uff1a\u8d8b\u52bf\u7ebf\u6e05\u6670\u5730\u8868\u660e\u5f00\u8def\u7535\u538b\u548c\u52a0\u901f\u5ea6\u5448\u73b0<strong>\u7ebf\u6027<\/strong>\u7684\u5173\u7cfb\uff0c\u6bd4\u4f8b\u7cfb\u6570\u4e3a0.080V\u2022s2\/m\uff0c\u572810\u81f340m\/s2\u7684\u8303\u56f4\u4e2d\uff0c\u8868\u73b0\u51fa\u4f18\u826f\u7684\u6027\u80fd\u3002<\/p>\n<p>\u3010<strong>\u603b\u7ed3<\/strong>\u3011<\/p>\n<p>\u738b\u4e2d\u6797\u6559\u6388\u7b49\u4eba\u63d0\u51fa\u7684\u8fd9\u79cd\u901a\u7528\u65b9\u6cd5\uff0c\u53ef\u4ee5\u5236\u5907\u51fa<strong>\u9ad8\u4f38\u7f29\u6027\u3001\u73af\u5883\u53cb\u597d\u578b\u548c\u8054\u9501\u526a\u7eb8\u56fe\u6848\u7ed3\u6784\u7684\u7eb8\u57faK-TENG<\/strong>\u3002\u7531\u56fa\u6709\u5f39\u6027\u6750\u6599\u5236\u5907\u51fa\u7684K-TENG\u7684\u6700\u5927\u62c9\u4f38\u5e94\u53d8\u53ef\u8fbe100%\uff0c\u6700\u5927\u53ef\u8f93\u51fa7.32\u4f0f\u7684\u5f00\u8def\u7535\u538b\u548c2.64nC\u7684\u8f6c\u79fb\u7535\u8377\u91cf\u3002\u8fd9\u79cd\u8054\u9501\u526a\u7eb8\u56fe\u6848\u7ed3\u6784\u8bbe\u8ba1\u4e0d\u4f46\u53ef\u4ee5<strong>\u663e\u8457\u5730\u589e\u5f3a\u5668\u4ef6\u7684\u786c\u5ea6\u548c\u53ef\u9760\u6027<\/strong>\uff0c\u800c\u4e14<strong>\u6d88\u9664\u4e86\u8fc7\u53bb\u7684TENG\u5728\u7535\u8377\u5206\u79bb\u8fc7\u7a0b\u5bf9\u989d\u5916\u7a7a\u95f4\u7684\u9700\u8981<\/strong>\u3002\u7531\u4e8e\u8fd9\u79cd\u8bbe\u8ba1\u672c\u8eab\u5448\u73b0\u5f62\u72b6\u9002\u5e94\u6027\u7684<strong>\u8584\u819c\u7ed3\u6784<\/strong>\uff0c\u4f7f\u5f97K-TENG\u53ef\u4ee5\u5728\u4e0d\u540c\u7c7b\u578b\u7684\u8fd0\u52a8\u6a21\u5f0f\uff08\u62c9\u4f38\u3001\u538b\u7f29\u548c\u626d\u8f6c\uff09\u4e0b\u5de5\u4f5c\uff0c\u6269\u5927K-TENG\u7684\u5e94\u7528\u8303\u56f4\u3002\u8fd9\u9879\u5de5\u4f5c\u4ece\u4f20\u7edf\u827a\u672f\u4e2d\u5f97\u5230\u542f\u53d1\uff0c\u5e94\u7528\u5230\u7eb3\u7c73\u53d1\u7535\u673a\u884c\u4e1a\uff0c\u4fc3\u8fdb\u4e86\u67d4\u6027\u7535\u5b50\u884c\u4e1a\u7684\u53d1\u5c55\u3002<\/p>\n<p>\u3010<strong>\u4f5c\u8005\u7b80\u4ecb<\/strong>\u3011<\/p>\n<p>\u738b\u4e2d\u6797\ufe501982\u6bd5\u4e1a\u4e8e\u897f\u5317\u7535\u8baf\u5de5\u7a0b\u5b66\u9662(\u73b0\u540d\u897f\u5b89\u7535\u5b50\u79d1\u6280\u5927\u5b66)\ufe50\u5e76\u4e8e\u540c\u4e00\u5e74\u8003\u53d6\u4e2d\u7f8e\u8054\u5408\u62db\u6536\u7684\u7269\u7406\u7814\u7a76\u751f(CUSPEA)\u30021987 \u5e74\u83b7\u4e9a\u5229\u6851\u90a3\u5dde\u7acb\u5927\u5b66\u7269\u7406\u5b66\u535a\u58eb, \u4ece\u5e08\u4e8e\u56fd\u9645\u7535\u5b50\u663e\u5fae\u5b66\u6743\u5a01 John Cowley \u6559\u6388\u3002\u738b\u6559\u6388\u73b0\u662f\u4f50\u6cbb\u4e9a\u7406\u5de5\u5b66\u9662\u7ec8\u8eab\u6821\u8463\u4e8b\u8bb2\u5e2d\u6559\u6388\uff0cHightower\u7ec8\u8eab\u8bb2\u5e2d\u6559\u6388\uff0c\u5de5\u5b66\u9662\u6770\u51fa\u8bb2\u5e2d\u6559\u6388\u548c\u7eb3\u7c73\u7ed3\u6784\u8868\u5f81\u4e2d\u5fc3\u4e3b\u4efb\u3002\u738b\u6559\u6388\u5df2\u5f53\u9009\u4e3a\u4e2d\u56fd\u79d1\u5b66\u9662\u5916\u7c4d\u9662\u58eb\u548c\u6b27\u6d32\u79d1\u5b66\u9662\u9662\u58eb\u3002<\/p>\n<p>\u738b\u4e2d\u6797\u662f\u56fd\u9645\u7eb3\u7c73\u79d1\u6280\u9886\u57df\u5177\u6709\u91cd\u8981\u5b66\u672f\u5f71\u54cd\u7684\u79d1\u5b66\u5bb6\u3002\u4ed6\u7684\u7814\u7a76\u5177\u6709\u539f\u521b\u6027\uff0c\u524d\u77bb\u6027\u548c\u5f15\u9886\u6027\u3002\u8fd1\u5e74\u6765\uff0c\u4ed6\u5728<strong>\u7eb3\u7c73\u6750\u6599\u53ef\u63a7\u751f\u957f\u3001\u8868\u5f81\u548c\u5e94\u7528<\/strong>\u7b49\u591a\u65b9\u9762\u53d6\u5f97\u4e86\u591a\u9879\u6709\u56fd\u9645\u91cd\u8981\u5f71\u54cd\u529b\u7684\u539f\u521b\u6027\u7814\u7a76\u6210\u679c\u3002\u738b\u6559\u6388\u5df2\u5728\u56fd\u9645\u4e00\u6d41\u520a\u7269\u4e0a\u53d1\u8868\u4e86<strong>1000<\/strong>\u591a\u7bc7\u671f\u520a\u8bba\u6587\uff08\u5176\u4e2d<strong>16<\/strong>\u7bc7\u53d1\u8868\u5728\u7f8e\u56fd\u300a<strong>Science<\/strong>\u300b\u548c\u300a<strong>Nature<\/strong> \u300b\u671f\u520a\u4e0a\uff1b\u516d\u7bc7\u53d1\u8868\u5728\u300aNature\u300b\u5b50\u520a\u4e0a\uff09\ufe50<strong>45<\/strong>\u7bc7\u7efc\u8ff0\u548c\u4e66\u7ae0\u8282\ufe50<strong>100<\/strong>\u9879\u4e13\u5229\u7b49\u3002\u4ed6\u5df2\u88ab\u9080\u8bf7\u505a\u8fc7<strong>850<\/strong>\u591a\u6b21\u5b66\u672f\u8bb2\u6f14\u548c\u5927\u4f1a\u7279\u9080\u62a5\u544a\u3002\u4ed6\u7684\u5b66\u672f\u8bba\u6587\u5df2\u88ab\u5f15\u7528<strong>84,000<\/strong>\u6b21\u4ee5\u4e0a\u3002\u4ed6\u8bba\u6587\u88ab\u5f15\u7528\u7684H\u56e0\u5b50(h-index)\u662f<strong>140<\/strong>\u3002\u4ed6\u662f\u4e16\u754c\u4e0a\u5728\u6750\u6599\u548c\u7eb3\u7c73\u6280\u672f\u8bba\u6587\u5f15\u7528\u6b21\u6570\u6700\u591a\u7684\u524d\u4e94\u4f4d\u4f5c\u8005\u4e4b\u4e00\u3002\u738b\u6559\u6388\u5728\u5f53\u4eca\u4e16\u754c\u6700\u6770\u51fa\u7684\u79d1\u5b66\u5bb6\u6392\u540d\u699c\u4e0a\u7b2c<strong>25<\/strong>\u540d \u3002<\/p>\n<p>\u8bfe\u9898\u7ec4\u7f51\u9875\uff1a<a href=\"http:\/\/www.nanoscience.gatech.edu\/\" target=\"_blank\">http:\/\/www.nanoscience.gatech.edu\/<\/a><\/p>\n<p>\u3010<strong>\u5907\u6ce8<\/strong>\u3011<\/p>\n<p>\u8be5\u7814\u7a76\u6210\u679c\u8fd1\u671f\u53d1\u8868\u5728ACS nano (IF: 12.881) \u4e0a\uff0c\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b00949\" target=\"_blank\">Paper-Based Triboelectric Nanogenerators Made of Stretchable Interlocking Kirigami Patterns<\/a>\u3002<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u79d1\u666e\u56e2\u961f\u5b66\u672f\u7ec4<strong>\u7075\u5bf8<\/strong>\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6b22\u8fce\u52a0\u5165\u6750\u6599\u4eba\u79d1\u666e\u56e2\u961f\uff0c\u4e00\u8d77\u8fdb\u884c\u6750\u6599\u9876\u520a\u5b66\u672f\u52a8\u6001\u7684\u8ddf\u8e2a\u548c\u62a5\u9053\u4ee5\u53caSCI\u76f8\u5173\u77e5\u8bc6\u79d1\u666e\u7b49\u3002\u52a0\u5165\u65b9\u5f0f\uff1a\uff081\uff09\u52a0\u5165\u6750\u6599\u4eba\u6587\u732e\u68c0\u7d22\u7fa4\uff08410109144\uff09\uff0c\u79c1\u4fe1\u7ba1\u7406\u5458\u201c\u6210\u90fd-\u5c0f\u5c0f\uff08QQ:763044722\uff09\u201d\u62a5\u540d\uff1b\uff082\uff09<a href=\"http:\/\/cailiaoren.mikecrm.com\/f.php?t=6qSdMU\" target=\"_blank\">\u70b9\u6b64\u5904\u62a5\u540d<\/a>\u3002<\/p>\n<p>\u6b22\u8fce\u5404\u5927\u8bfe\u9898\u7ec4\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u80cc\u666f\u7b80\u4ecb\u3011 \u5728\u8fc7\u53bb\u7684\u51e0\u5341\u5e74\u95f4\uff0c\u4f5c\u4e3a\u4e0b\u4e00\u4ee3\u529f\u80fd\u5668\u4ef6\u7684\u67d4\u6027\u7535\u5b50\u5b66\u4e00\u76f4\u5728\u4e0d\u65ad\u53d1\u5c55\uff0c\u5e76\u5438\u5f15\u4e86\u5de5\u4e1a\u754c\u548c\u5b66\u672f\u754c\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u76f8\u6bd4\u4f20\u7edf\u5668\u4ef6\uff0c\u5728\u4e0d\u727a\u7272\u5668\u4ef6\u6027\u80fd\u548c\u53ef\u9760\u6027\u7684\u60c5\u51b5\u4e0b\uff0c&#8230;<\/p>\n","protected":false},"author":372,"featured_media":7711,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[1302,31,33,32],"class_list":["post-7709","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-wangzhonglin","tag-dianzi","tag-nano","tag-film"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/7709"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/372"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=7709"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/7709\/revisions"}],"predecessor-version":[{"id":7727,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/7709\/revisions\/7727"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/7711"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=7709"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=7709"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=7709"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}