{"id":81331,"date":"2017-05-18T14:00:46","date_gmt":"2017-05-18T06:00:46","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=81331"},"modified":"2017-05-18T14:06:14","modified_gmt":"2017-05-18T06:06:14","slug":"adv-energy-mater-%ef%bc%9a%e4%ba%8c%e7%bb%b4%e7%ba%b3%e7%b1%b3%e7%89%87%e5%85%89%e7%94%b5%e7%89%b9%e6%80%a7%e8%b0%83%e8%b0%90","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=81331","title":{"rendered":"Adv. Energy Mater. \uff1a\u4e8c\u7ef4\u7eb3\u7c73\u7247\u5149\u7535\u7279\u6027\u8c03\u8c10"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u4e8c\u7ef4\u534a\u5bfc\u4f53\u7eb3\u7c73\u7247\uff08NPLs\uff09\u4f5c\u4e3a\u4e00\u79cd\u65b0\u5174\u7684\u5149\u654f\u6750\u6599\uff0c\u7531\u4e8e\u5176\u9ad8\u5438\u6536\u7cfb\u6570\uff0c\u9ad8\u8f7d\u6d41\u5b50\u8fc1\u79fb\u7387\uff0c\u539a\u5ea6\u76f8\u5173\u7684\u5149\u900f\u5c04\u7387\u7b49\u7279\u70b9\uff0c\u4f7f\u5f97\u8fd9\u79cd\u6750\u6599\u5728\u5149\u7535\u5668\u4ef6\u9886\u57df\u5f97\u5230\u5927\u91cf\u5e94\u7528\u3002\u4f46\u662f\u4f20\u7edf\u7eb3\u7c73\u7247\u5927\u5c3a\u5bf8\u7684\u7f3a\u70b9\u5bfc\u81f4\u4e86\u7f3a\u9677\u7684\u5e26\u95f4\u80fd\u7ea7\u548c\u4f4e\u7684\u91cf\u5b50\u6536\u7387\uff08Quantum yield\uff0cQY\uff09<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u7535\u5b50\u79d1\u5927\u957f\u6c5f\u5b66\u8005Federico Rosei\u6559\u6388\uff08\u901a\u8baf\u4f5c\u8005\uff09\uff0c\u52a0\u62ff\u5927\u9b41\u5317\u514b\u5927\u5b66Haiguang Zhao\u535a\u58eb\uff08\u901a\u8baf\u4f5c\u8005\uff09\u548c\u745e\u5178\u5415\u52d2\u5965\u7406\u5de5\u5927\u5b66Alberto Vomiero\u6559\u6388\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u7814\u7a76\u53d1\u73b0\uff0c\u8d85\u5fae\u578b\u7684\u94c5\u786b\u65cf\u5316\u7269PbSe<sub>1-x<\/sub>S<sub>xn<\/sub>\u7eb3\u7c73\u7247\u7684\u91cf\u5b50\u4ea7\u989d\u53f2\u65e0\u524d\u4f8b\u7684\u8fbe\u5230\u4e8660%\uff0c\u5728\u4e00\u4e9b\u7ed3\u6784\u4e2d\u751a\u81f3\u8fd8\u53ef\u66f4\u9ad8\u3002\u5728\u5149\u5316\u5b66\u7cfb\u7edf\u4e2d\uff0c\u91c7\u7528\u8be5\u79cd\u7eb3\u7c73\u7247\u4f5c\u4e3a\u5149\u5438\u6536\u4f53\uff0c\u9971\u548c\u5149\u7535\u6d41\u53ef\u4ee5\u8fbe\u52305.0mA.cm<sup>-2<\/sup>\uff0c\u8fd9\u4e5f\u521b\u9020\u4e86\u592a\u9633\u80fd\u9a71\u52a8\u6c22\u6c14\u4ea7\u751f\u4e2d\u7eb3\u7c73\u7247\u7535\u6781\u7684\u65b0\u8bb0\u5f55\u3002\u5b9e\u9a8c\u7ed3\u679c\u8bc1\u660e\u8d85\u5fae\u578b\u7eb3\u7c73\u7247\u5728\u5149\u6d3b\u6027\u7eb3\u7c73\u6750\u6599\u9886\u57df\u5177\u6709\u91cd\u5927\u7684\u53d1\u5c55\u6f5c\u529b\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>1 \u8fd1<\/strong><strong>\u7ea2\u5916\u7eb3\u7c73\u7247\uff08<\/strong><strong>NIR NPLs<\/strong><strong>\uff09\u7684\u5f62\u6001\uff0c\u7ec4\u5408\u53ca\u8868\u5f81<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-81861 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/1-4-1.jpg\" alt=\"\" width=\"700\" height=\"781\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/1-4-1.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/1-4-1-269x300.jpg 269w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe\uff08A\uff09\u7eb3\u7c73\u7247\u7684\u5236\u5907\u6d41\u7a0b<\/p>\n<p>\u56fe\uff08B,C \uff06E-G\uff09PbSe<sub>1-x<\/sub>S<sub>xn<\/sub>\uff08Se:S=3:1\uff09\u7684TEM\u4eae\u573a\u56fe\u50cf, E,F,G\u4e2d\u7684Pb\u5206\u522b\u4f7f\u7528\u4e86PbBr<sub>2<\/sub>,PbCl<sub>2<\/sub>,PBbSe\u4f5c\u4e3a\u524d\u9a71\u4f53<\/p>\n<p>\u56fe\uff08D\uff09\u4f7f\u7528PbCl<sub>2<\/sub>\u4f5c\u4e3a\u524d\u9a71\u4f53\u7684PbSe<sub>1-x<\/sub>S<sub>xn<\/sub>\uff08Se:S=3:1\uff09\u7684EDS\u8c31<\/p>\n<p><strong>\u56fe<\/strong><strong>2 <\/strong><strong>\u7eb3\u7c73\u7247\u7684\u5149\u5b66\u7279\u6027<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-81864 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/2-4-2.jpg\" alt=\"\" width=\"700\" height=\"671\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/2-4-2.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/2-4-2-300x288.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe\uff08A\uff09PbSe<sub>1-x<\/sub>S<sub>xn\u7ecf\u8fc7<\/sub>\u9633\u79bb\u5b50\u4ea4\u6362\u5904\u7406\u524d\u540e\u7684\u5438\u6536\u8c31\u548cPL\u8c31<\/p>\n<p>\u56fe\uff08B\uff09\u4e0d\u540c\u53cd\u5e94\u6d53\u5ea6\u4e0b\u7684PbSe<sub>1-x<\/sub>S<sub>xn<\/sub>\u7684\u5178\u578bPL\u8870\u51cf\u66f2\u7ebf\u4ee5\u53ca\u5176\u62df\u5408\u66f2\u7ebf\uff0c\u6fc0\u53d1\u5149\u6ce2\u957f\u4e3a450nm<\/p>\n<p>\u56fe\uff08C\uff09PbSe<sub>1-x<\/sub>S<sub>xn<\/sub>\u91cf\u5b50\u70b9\u548c\u5706\u67f1\u4f53\u7eb3\u7c73\u7247\u7684\u793a\u610f\u56fe\uff0c\u4ee5\u53caPbSe<sub>1-x<\/sub>S<sub>xn<\/sub>\u91cf\u5b50\u70b9\u548c\u5706\u67f1\u4f53\u7eb3\u7c73\u7247\u7684\u5b9e\u9a8c\u548c\u4eff\u771f\u7684\u5e26\u9699\u4e0ePbS\u539a\u5ea6\u4e4b\u95f4\u7684\u5173\u7cfb<\/p>\n<p>\u56fe\uff08D\uff09\u8868\u4e2d\u5217\u51fa\u4e86\u4e0d\u540c\u7ec4\u4efd\u548c\u4f7f\u7528\u4e0d\u540c\u5148\u9a71\u4f53\u7684PbSe<sub>1-x<\/sub>S<sub>xn<\/sub>\u7684\u5149\u5b66\u7279\u70b9<\/p>\n<p><strong>\u56fe<\/strong><strong>3 <\/strong><strong>\u8d85\u5feb\u77ac\u6001\u4f20\u8f93\u6d4b\u91cf<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-81865 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/3-3-3.jpg\" alt=\"\" width=\"700\" height=\"1239\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/3-3-3.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/3-3-3-169x300.jpg 169w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/3-3-3-579x1024.jpg 579w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u56fe\uff08A\uff090.3 ps\u7684\u6cf5\u6d66\u63a2\u6d4b\u5ef6\u8fdf\u4e0b\uff0c\u5f52\u4e00\u5316\u7684\u0394T\/T\u8c31<\/p>\n<p>\u56fe\uff08B\uff09500ps\u7684\u6cf5\u6d66\u63a2\u6d4b\u5ef6\u8fdf\u4e0b\uff0c\u5f52\u4e00\u5316\u7684\u0394T\/T\u8c31<\/p>\n<p>\u56fe\uff08C\uff09\u6cf5\u6d66\u63a2\u6d4b\u6700\u5927\u5ef6\u8fdf\u4e0b\uff0c\u4e0d\u540c\u7ec4\u4efd\u6837\u54c1\u7684\u0394T\/T\u8c31\u7684\u52a8\u6001\u53d8\u5316<\/p>\n<p><strong>\u56fe<\/strong><strong>4 <\/strong><strong>\u7eb3\u7c73\u7247\u5149\u7535\u9633\u6781\u7684\u538b\u7535\u7279\u6027<\/strong><\/p>\n<p style=\"text-align: center;\"><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/4-3.bmp\"><img loading=\"lazy\" decoding=\"async\" class=\"alignnone size-full wp-image-81364\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/4-3.bmp\" alt=\"\" width=\"700\" height=\"196\" \/><\/a><\/p>\n<p>\u56fe\uff08A\uff09\u538b\u7535\u7cfb\u7edf\u7684\u7cbe\u786e\u80fd\u5e26\u6821\u51c6\uff0cTiO<sub>2<\/sub>\u548c\u7eb3\u7c73\u7247\u7684\u80fd\u7ea7\u4f30\u7b97\u90fd\u662f\u57fa\u4e8eUPS\u6d4b\u91cf\u7684\u57fa\u7840\u4e0a<\/p>\n<p>\u56fe\uff08B\uff09TiO2\/NPLs\/ZnS, TiO2\/PbS\/CdS QDs\/ZnS, \u548cTiO2\/Cd-NPLs\/ZnS \u5149\u7535\u9633\u6781\u8584\u819c\u5404\u81ea\u7684J-V\u66f2\u7ebf, \u5149\u7167\u5f3a\u5ea6\u662f100mW.cm<sup>-2<\/sup><\/p>\n<p>\u56fe\uff08C\uff09\u7535\u6d41\u5bc6\u5ea6\u4e0e\u5149\u7167\u65f6\u95f4\u7684\u5173\u7cfb\uff0c\u7535\u538b\u662f0.8V\uff0c\u5149\u7167\u5f3a\u5ea6\u662f100mW.cm<sup>-2<\/sup><\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u6587\u4e2d\u63d0\u51fa\u4e86\u4e00\u79cd\u7b80\u5355\u7684\u65b9\u6cd5\u6765\u5408\u6210\u8d85\u5fae\u578b\u7eb3\u7c73\u7247\uff0c\u5373\u901a\u8fc7\u6e29\u5ea6\u8f85\u52a9\u9633\u79bb\u5b50\u4ea4\u6362\u7684\u65b9\u6cd5\u3002\u8d85\u5fae\u578bNIR NPLs\u8868\u9762\u5177\u6709\u7d27\u51d1\u7684\u949d\u5316\u914d\u4f53\uff0c\u5e76\u4e14\u8868\u73b0\u51fa3D\u91cf\u5b50\u5316\u7535\u5b50\u884c\u4e3a\uff0c\u9ad8\u8fbe60%\u7684QY\uff0c\u4ee5\u53ca\u80fd\u5e26\u53ef\u8c03\u8c10\u7684\u7279\u70b9\uff0c\u5728LED\uff0c\u70ed\u4f20\u611f\u5668\uff0c\u53d1\u5149\u592a\u9633\u80fd\u96c6\u70ed\u5668\uff0c\u592a\u9633\u80fd\u7535\u6c60\uff0c\u6c22\u6c14\u4ea7\u751f\u7b49\u9886\u57df\u5177\u6709\u91cd\u5927\u7684\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/wol1\/doi\/10.1002\/aenm.201602728\/abstract\" target=\"_blank\" rel=\"noopener noreferrer\">Ultrasmall Nanoplatelets: The Ultimate Tuning of Optoelectronic Properties<\/a><\/strong>\uff08Adv. Energy Mater.\u00a0, 2017, DOI:10.1002\/aenm.201602728\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u5b66\u672f\u7ec4hxxurui\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002\u5982\u679c\u4f60\u5bf9\u7535\u5b50\u6750\u6599\u611f\u5174\u8da3\uff0c\u613f\u610f\u4e0e\u7535\u5b50\u7535\u5de5\u9886\u57df\u4eba\u624d\u4ea4\u6d41\uff0c\u8bf7\u52a0\u5165\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4\uff08QQ\u7fa4\uff1a482842474\uff09\u3002\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u4e8c\u7ef4\u534a\u5bfc\u4f53\u7eb3\u7c73\u7247\uff08NPLs\uff09\u4f5c\u4e3a\u4e00\u79cd\u65b0\u5174\u7684\u5149\u654f\u6750\u6599\uff0c\u7531\u4e8e\u5176\u9ad8\u5438\u6536\u7cfb\u6570\uff0c\u9ad8\u8f7d\u6d41\u5b50\u8fc1\u79fb\u7387\uff0c\u539a\u5ea6\u76f8\u5173\u7684\u5149\u900f\u5c04\u7387\u7b49\u7279\u70b9\uff0c\u4f7f\u5f97\u8fd9\u79cd\u6750\u6599\u5728\u5149\u7535\u5668\u4ef6\u9886\u57df\u5f97\u5230\u5927\u91cf\u5e94\u7528&#8230;<\/p>\n","protected":false},"author":1927,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-81331","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/81331"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1927"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=81331"}],"version-history":[{"count":16,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/81331\/revisions"}],"predecessor-version":[{"id":81866,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/81331\/revisions\/81866"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=81331"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=81331"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=81331"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}