{"id":85454,"date":"2017-06-10T06:30:33","date_gmt":"2017-06-09T22:30:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=85454"},"modified":"2017-06-09T08:09:45","modified_gmt":"2017-06-09T00:09:45","slug":"%e7%a7%91%e6%8a%80%e8%b5%84%e8%ae%af%e5%86%99%e4%bd%9c%e5%a4%a7%e8%b5%9b%ef%bd%9cnatl-sci-rev-%ef%bc%9a%e5%a4%9a%e5%85%83%e9%87%91%e5%b1%9e%e6%9c%89%e6%9c%ba%e6%a1%86%e6%9e%b6%e5%8c%96%e5%90%88","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=85454","title":{"rendered":"\u79d1\u6280\u8d44\u8baf\u5199\u4f5c\u5927\u8d5b\uff5cNatl. Sci. Rev.\uff1a\u591a\u5143\u91d1\u5c5e\u6709\u673a\u6846\u67b6\u5316\u5408\u7269\uff08MTV-MOFs\uff09"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-81477 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/\u8d44\u8baf\u5927\u8d5b-\u526f\u672c-2-1.png\" alt=\"\" width=\"740\" height=\"416\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/\u8d44\u8baf\u5927\u8d5b-\u526f\u672c-2-1.png 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/\u8d44\u8baf\u5927\u8d5b-\u526f\u672c-2-1-300x169.png 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/p>\n<p>\u6750\u6599\u4eba\u9996\u5c4a\u79d1\u6280\u8d44\u8baf\u5199\u4f5c\u5927\u8d5b\u81ea5\u670813\u65e5\u53d1\u5e03\u5f81\u7a3f\u901a\u77e5\u4ee5\u6765\uff08<a href=\"http:\/\/www.cailiaoniu.com\/80668.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u53c2\u8d5b\u8be6\u60c5\u8bf7\u6233\u6211<\/a>\uff09\uff0c\u53d7\u5230\u8bfb\u8005\u4eec\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u672c\u6587\u7531SCI\u671f\u520aNational Science Review\u7f16\u8f91\u90e8\u6295\u7a3f\u3002<\/p>\n<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u7f51\u72b6\u5316\u5b66\u662f\u5c06\u7b80\u5355\u7684\u6709\u673a\u5355\u5143\u4e0e\u65e0\u673a\u5355\u5143\u901a\u8fc7\u952e\u8fde\u63a5\u6210\u7684\u957f\u7a0b\u3001\u591a\u5b54\u6676\u4f53\uff0c\u5982MOFs\u3002\u8be5\u9886\u57df\u901a\u8fc7\u5236\u9020\u65b0\u7ed3\u6784\u6765\u7814\u7a76\u7f51\u72b6\u7269\u8d28\u5728\u6c14\u4f53\u5b58\u50a8\u4e0e\u5206\u79bb\u3001\u50ac\u5316\u7b49\u65b9\u9762\u7684\u5e94\u7528\u3002\u8fc4\u4eca\u4e3a\u6b62\u7814\u7a76\u7684MOFs\u76f8\u5bf9\u6765\u8bf4\u5177\u6709\u8f83\u5c0f\u7684\u7ed3\u6784\uff0c\u5373\u6676\u4f53\u4e2d\u53ea\u6709\u5c11\u91cf\u7684\u91cd\u590d\u5355\u5143\u3002\u672a\u6765\u7684MOFs\u53ef\u4ee5\u4ece\u62e5\u6709\u5927\u91cf\u91cd\u590d\u5355\u5143\u7684\u751f\u7269\u7cfb\u7edf\u4e2d\u83b7\u5f97\u7075\u611f\u3002\u4e3a\u4e86\u4f7fMOFs\u7684\u53d1\u5c55\u8fbe\u5230\u66f4\u9ad8\u7684\u6c34\u5e73\uff0c\u5f88\u6709\u5fc5\u8981\u53d1\u5c55\u51fa\u53ef\u4ee5\u4f7fMOFs\u7ed3\u6784\u66f4\u590d\u6742\u7684\u65b9\u6cd5\u3002\u5728\u8fd9\u79cd\u80cc\u666f\u4e0b\uff0c\u5982\u4f55\u5728\u6709\u5e8f\u7ed3\u6784\u4e2d\u5f15\u5165\u5f02\u8d28\u6027\uff0c\u5e76\u4e14\u53ef\u4ee5\u6210\u529f\u7684\u5e94\u7528\u8fd9\u79cd\u6750\u6599\u5c31\u6210\u4e3a\u4e86\u5de8\u5927\u7684\u6311\u6218\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u6c99\u7279\u963f\u62c9\u4f2f\u6cd5\u8d6b\u5fb7\u56fd\u738b\u77f3\u6cb9\u77ff\u4ea7\u5927\u5b66<\/strong><strong>\u7684<\/strong><strong>Aasif Helal<\/strong><strong>\u548c<\/strong><strong>Omar M. Yaghi<\/strong><strong>\uff08\u5171\u540c\u901a\u8baf\uff09<\/strong>\u7b49\u4eba\u5728<strong>National Science Review<\/strong>\u4e0a\u53d1\u8868\u4e86\u4e00\u7bc7\u9898\u4e3a<strong>\u201c<\/strong><strong>Multivariate metal-organic frameworks<\/strong><strong>\u201d<\/strong>\u7684\u5c55\u671b\uff0c\u8fd9\u7bc7\u6587\u7ae0\u4e3b\u8981\u603b\u7ed3\u4e86\u5728\u6709\u5e8fMOFs\u4e2d\u5f15\u5165\u5f02\u8d28\u6027\u7684\u591a\u79cd\u65b9\u6cd5\uff0c\u4ece\u800c\u4f7f\u5176\u529f\u80fd\u66f4\u52a0\u4f18\u5316\u7684\u7814\u7a76\u8fdb\u5c55\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>1 <\/strong><strong>\u5728\u6709\u5e8f<\/strong><strong>MOFs<\/strong><strong>\u4e2d\u5f15\u5165<\/strong><strong>MTV<\/strong><strong>\u7684\u4ee3\u8868\u6027\u53d1\u73b0<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-85455 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u6731\u6653\u79c0.jpg\" alt=\"\" width=\"600\" height=\"436\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u6731\u6653\u79c0.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u6731\u6653\u79c0-300x218.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe\u4e2d\u4e0d\u540c\u989c\u8272\u4ee3\u8868\u7684\u7269\u8d28\uff1a\u5176\u4e2d\uff0c\u9ed1\u8272\uff1a<\/strong><strong>C<\/strong><strong>\uff1b\u7ea2\u8272\uff1a<\/strong><strong>O<\/strong><strong>\uff1b\u7eff\u8272\uff1a\u5f15\u5165\u7684\u5b98\u80fd\u56e2\uff1b\u5404\u79cd\u6709\u8272\u591a\u9762\u4f53\uff1b\u91d1\u5c5e\u539f\u5b50\uff1b\uff08<\/strong><strong>H<\/strong><strong>\u539f\u5b50\u672a\u663e\u793a\uff09<\/strong><strong>TCPP<\/strong><strong>\uff1a\u56db\uff08<\/strong><strong>4 &#8211;<\/strong><strong>\u7fa7\u57fa\u82ef\u57fa\uff09\u535f\u5549<\/strong><\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u672c\u6587\u4ec5\u662f\u73b0\u62a5\u9053\u7684\u5728\u6709\u5e8f\u7ed3\u6784\u4e2d\u5b9e\u73b0\u5f02\u8d28\u6027\u7684\u51e0\u4e2a\u4f8b\u5b50\u3002\u5728\u8be5\u9886\u57df\uff0c\u8fd8\u6709\u5f88\u5927\u7684\u7a7a\u95f4\u6709\u5f85\u5f00\u53d1\u3002\u901a\u8fc7\u5bf9\u5408\u6210\u540e\u7684MOF\u8fdb\u884c\u4fee\u9970\uff0c\u53ef\u4ee5\u5b9e\u73b0\u201c\u6a21\u62df\u9176\u7684\u590d\u6742\u6027\u201d\u3002\u4f8b\u5982\uff0c\u901a\u8fc7\u5bf9MOF-74\u8fdb\u884c7\u6b65\u540e\u5904\u7406\u53cd\u5e94\uff0c\u53ef\u4ee5\u5f62\u6210\u5177\u6709\u4e09\u80bd\u529f\u80fd\u7684\u6750\u6599\u3002\u53e6\u5916\u4e00\u4e9b\u7814\u7a76\u4e13\u6ce8\u4e8eMOFs\u4e2d\u7f3a\u9677\u7684\u5f15\u5165\u3001\u63a7\u5236\u548c\u5229\u7528\u3002\u6b64\u5916\uff0c\u4e3a\u5ba2\u4f53\u5206\u5b50\u8bbe\u8ba1\u4e0d\u540c\u6570\u76ee\u548c\u4e0d\u540c\u987a\u5e8f\u7684\u52a8\u6001\u6846\u67b6\u4e5f\u53ef\u4ee5\u8d4b\u4e88MOFs\u66f4\u591a\u4e0d\u540c\u7684\u7269\u7406\u6027\u8d28\u3002<\/p>\n<p>\u53ef\u4ee5\u8fd9\u4e48\u8bf4\uff0c\u5f15\u5165\u5f02\u8d28\u6027\u53ef\u80fd\u662f\u5c06\u4eba\u9020\u6750\u6599\u4e0e\u81ea\u7136\u754c\u7684\u6750\u6599\u8054\u7cfb\u8d77\u6765\u7684\u7b2c\u4e00\u6b65\u3002\u7684\u786e\uff0c\u4eba\u5de5\u5408\u6210\u6750\u6599\u7684\u8fc7\u7a0b\u4e3b\u8981\u662f\u6309\u987a\u5e8f\u64cd\u4f5c\uff0c\u800c\u81ea\u7136\u754c\u5374\u662f\u591a\u79cd\u65b9\u5f0f\u4e00\u8d77\u8fd0\u4f5c\uff0c\u4ece\u800c\u5b9e\u73b0\u66f4\u5e7f\u6cdb\u7684\u7ec4\u5408\u3002\u56e0\u6b64\uff0c\u5bf9\u4e8e\u5408\u6210\u5316\u5b66\u5bb6\u800c\u8a00\uff0c\u5982\u4f55\u5c06\u5b64\u7acb\u7684\u7269\u8d28\u5efa\u7acb\u8054\u7cfb\u5c31\u663e\u5f97\u81f3\u5173\u91cd\u8981\uff0c\u800c\u8fd9\u4e3b\u8981\u4f9d\u8d56\u4e8e\u5177\u6709\u591a\u4e2a\u7ed3\u6784\u7684\u5f02\u8d28\u7cfb\u7edf\u6750\u6599\u7684\u6210\u529f\u5b9e\u73b0\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"https:\/\/academic.oup.com\/nsr\/article\/3052680\/Multivariate-metal-organic-frameworks?searchresult=1\" target=\"_blank\" rel=\"noopener noreferrer\">Multivariate metal-organic frameworks<\/a>. \uff08Natl Sci Rev, 2017, DOI: 10.1093\/nsr\/nwx013\uff09<\/p>\n<div class=\"middles\">\n<div id=\"subright\">\n<div class=\"personbox\">\n<div class=\"middles\">\n<div id=\"subright\">\n<div class=\"personbox\">\n<div class=\"middles\">\n<div>\n<div id=\"subright\">\n<div class=\"personbox\">\n<p><strong><span style=\"color: #ff0000;\">National\u00a0Science\u00a0Review\u4ecb\u7ecd<\/span><\/strong><\/p>\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n<\/div>\n<p>National Science Review\u4e3a\u4e2d\u56fd\u7b2c\u4e00\u4efd\u82f1\u6587\u7248\u7efc\u8ff0\u6027\u5b66\u672f\u671f\u520a\uff0c\u5b9a\u4f4d\u4e8e\u4e00\u4efd\u5177\u6709\u6218\u7565\u6027\u3001\u5bfc\u5411\u6027\u7684\u7efc\u8ff0\u671f\u520a\uff0c\u81f4\u529b\u4e8e\u5168\u9762\u5c55\u793a\u4e2d\u56fd\u5404\u79d1\u5b66\u9886\u57df\u7684\u4ee3\u8868\u6027\u7814\u7a76\u6210\u679c\uff0c\u8ffd\u8e2a\u62a5\u9053\u91cd\u5927\u79d1\u6280\u4e8b\u4ef6\uff0c\u6df1\u5ea6\u89e3\u8bfb\u70ed\u70b9\u7814\u7a76\u548c\u91cd\u8981\u79d1\u6280\u653f\u7b56\u7b49\u3002\u4e8e2014\u5e743\u6708\u6b63\u5f0f\u51fa\u7248\uff0c2016\u5e74NSR\u521b\u520a\u4ee5\u6765\u7684\u9996\u4e2aSCI\u5f71\u54cd\u56e0\u5b50\u8fbe\u52308.0\uff0c\u4f4d\u4e8e63\u79cd\u591a\u5b66\u79d1\u7efc\u5408\u7c7b\u671f\u520a\u7684\u7b2c5\u540d\u3002\u672c\u520a\u53d1\u8868\u7684\u6240\u6709\u8bba\u6587\u5168\u6587\u53ef\u4ee5\u5728\u7ebf\u514d\u8d39\u9605\u8bfb\u548c\u4e0b\u8f7d\u3002<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4ebaMOF\u7ec4\u6731\u6653\u79c0\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<\/strong><a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\"><strong>\u6d4b\u8bd5\u8c37<\/strong><\/a><strong>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u4eba\u9996\u5c4a\u79d1\u6280\u8d44\u8baf\u5199\u4f5c\u5927\u8d5b\u81ea5\u670813\u65e5\u53d1\u5e03\u5f81\u7a3f\u901a\u77e5\u4ee5\u6765\uff08\u53c2\u8d5b\u8be6\u60c5\u8bf7\u6233\u6211\uff09\uff0c\u53d7\u5230\u8bfb\u8005\u4eec\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u672c\u6587\u7531SCI\u671f\u520aNational Science Review\u7f16&#8230;<\/p>\n","protected":false},"author":1369,"featured_media":85455,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[1592,245],"class_list":["post-85454","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-nsr","tag-mof"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/85454"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1369"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=85454"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/85454\/revisions"}],"predecessor-version":[{"id":85480,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/85454\/revisions\/85480"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/85455"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=85454"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=85454"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=85454"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}