{"id":86953,"date":"2017-06-20T14:00:14","date_gmt":"2017-06-20T06:00:14","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=86953"},"modified":"2017-06-26T19:35:41","modified_gmt":"2017-06-26T11:35:41","slug":"%e4%b8%ad%e7%a7%91%e9%99%a2%e4%b8%8a%e6%b5%b7%e5%be%ae%e7%b3%bb%e7%bb%9f%e6%89%80%e7%8b%84%e5%a2%9e%e5%b3%b0%e5%9b%a2%e9%98%9f%ef%bc%9a%e9%94%97%e8%be%85%e5%8a%a9%e7%bb%9d%e7%bc%98%e4%bd%93%e4%b8%8a","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=86953","title":{"rendered":"\u4e2d\u79d1\u9662\u4e0a\u6d77\u5fae\u7cfb\u7edf\u6240\u72c4\u589e\u5cf0\u56e2\u961f\uff1a\u9517\u8f85\u52a9\u7edd\u7f18\u4f53\u4e0a\u77f3\u58a8\u70ef\u6750\u6599\u751f\u957f\u7814\u7a76\u83b7\u8fdb\u5c55"},"content":{"rendered":"<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u671f\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u4e0a\u6d77\u5fae\u7cfb\u7edf\u4e0e\u4fe1\u606f\u6280\u672f\u7814\u7a76\u6240\u4fe1\u606f\u529f\u80fd\u6750\u6599\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4<em><i>SOI<\/i><\/em>(\u7edd\u7f18\u4f53\u4e0a\u7845)\u6750\u6599\u4e0e\u5668\u4ef6\u8bfe\u9898\u7ec4\u5728\u7edd\u7f18\u4f53\u886c\u5e95\u4e0a\u76f4\u63a5\u5236\u5907\u77f3\u58a8\u70ef\u7814\u7a76\u65b9\u9762\u53d6\u5f97\u65b0\u8fdb\u5c55\u3002\u5236\u5907\u7edd\u7f18\u4f53\u4e0a\u77f3\u58a8\u70ef\u662f\u63a8\u52a8\u77f3\u58a8\u70ef\u5728\u5fae\u7535\u5b50\u9886\u57df\u5e94\u7528\u7684\u91cd\u8981\u57fa\u7840\u6761\u4ef6\uff0c\u9488\u5bf9\u8fd9\u4e00\u9700\u6c42\uff0c<em><i>SOI<\/i><\/em>\u6750\u6599\u4e0e\u5668\u4ef6\u8bfe\u9898\u7ec4\u7684\u7814\u7a76\u4eba\u5458\u4f7f\u7528\u9517\u8584\u819c\u505a\u50ac\u5316\u5242\uff0c\u901a\u8fc7\u5316\u5b66\u6c14\u76f8\u6c89\u79ef\uff08<em><i>CVD<\/i><\/em>\uff09\u65b9\u6cd5\u6210\u529f\u5728\u4e8c\u6c27\u5316\u7845\u3001\u84dd\u5b9d\u77f3\u3001\u77f3\u82f1\u73bb\u7483\u7b49\u7edd\u7f18\u886c\u5e95\u4e0a\u5236\u5907\u51fa\u9ad8\u8d28\u91cf\u5355\u5c42\u77f3\u58a8\u70ef\u6750\u6599\uff0c\u5e76\u5c06\u5176\u6210\u529f\u5e94\u7528\u4e8e\u9664\u96fe\u5668\u7b49\u7535\u52a0\u70ed\u5668\u4ef6\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c<em><i><strong>Germanium-assisted Direct Growth of Graphene on Arbitrary Dielectric Substrates for Heating Devices<\/strong>\u201d<\/i><\/em>\u4e3a\u9898\u8fd1\u671f\u5728<strong><em><i>Small<\/i><\/em><\/strong>\u4e0a\u53d1\u8868\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe1\u00a0Ge\u84b8\u53d1\u548c\u77f3\u58a8\u70ef\u5f62\u6210\u65f6\u95f4\u7684\u6f14\u53d8<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-86957\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/01-9.png\" alt=\"\" width=\"600\" height=\"535\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/01-9.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/01-9-300x268.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a1-e1\uff09\u5728920\u2103\u4e0b\u5728\u4e0d\u540c\u65f6\u95f4\u5728SiO<sub>2<\/sub>\/Si\u4e0a\u751f\u957f\u7684\u77f3\u58a8\u70ef\u7684\u5149\u5b66\u56fe\u50cf<\/p>\n<p>a2-e2\uff09\u4f5c\u4e3a\u751f\u957f\u65f6\u95f4\u51fd\u6570\u7684Ge\u5cf0\u5f3a\u5ea6\u7684\u62c9\u66fc\u6620\u5c04<\/p>\n<p>a3-e3\uff09\u77f3\u58a8\u70ef\u7684I<sub>2D<\/sub>\/I<sub>G<\/sub>\u6bd4\u7684\u62c9\u66fc\u6620\u5c04<\/p>\n<p>f\uff09\u5728920\u2103\u4e0b\u4e0d\u540cCVD\u65f6\u95f4\u7684Ge\u7684\u62c9\u66fc\u5149\u8c31<\/p>\n<p>g\uff09\u5728920\u2103\u4e0b\u4e0d\u540cCVD\u65f6\u95f4\u7684\u77f3\u58a8\u70ef\u7684\u62c9\u66fc\u5149\u8c31<\/p>\n<p>h\uff09\u7edf\u8ba1I<sub>2D<\/sub>\/I<sub>G<\/sub>\u548cI<sub>D<\/sub>\/I<sub>G<\/sub>\u6bd4\u503c\u4f5c\u4e3a\u65f6\u95f4\u7684\u51fd\u6570<\/p>\n<p><strong>\u56fe2\u00a0Ge\u84b8\u53d1\u548c\u77f3\u58a8\u70ef\u5f62\u6210\u4e0eCVD\u6e29\u5ea6\u7684\u6f14\u53d8<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-86959\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/02-8.png\" alt=\"\" width=\"600\" height=\"607\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/02-8.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/02-8-297x300.png 297w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a1-d1\uff09\u5728\u4e0d\u540c\u6e29\u5ea6\u4e0b\u5728SiO<sub>2<\/sub>\/Si\u4e0a\u751f\u957f300\u5206\u949f\u7684\u77f3\u58a8\u70ef\u7684\u5149\u5b66\u56fe\u50cf<\/p>\n<p>a2-d2\uff09\u4f5c\u4e3a\u6e29\u5ea6\u7684\u51fd\u6570\u7684Ge\u5cf0\u5f3a\u5ea6\u7684\u62c9\u66fc\u6620\u5c04<\/p>\n<p>a3-d3\uff09\u77f3\u58a8\u70efI<sub>2D<\/sub>\/I<sub>G<\/sub>\u6bd4\u7684\u62c9\u66fc\u6620\u5c04<\/p>\n<p>e\uff09\u5728\u4e0d\u540c\u6e29\u5ea6\u4e0b\u77f3\u58a8\u70ef\u751f\u957f300\u5206\u949f\u540e\u7684Ge\u7684\u62c9\u66fc\u5149\u8c31<\/p>\n<p>f\uff09\u5728\u4e0d\u540c\u6e29\u5ea6\u4e0b\u751f\u957f300\u5206\u949f\u7684\u77f3\u58a8\u70ef\u7684\u62c9\u66fc\u5149\u8c31<\/p>\n<p>g\uff09\u7edf\u8ba1I<sub>2D<\/sub>\/I<sub>G<\/sub>\u548cI<sub>D<\/sub>\/I<sub>G<\/sub>\u6bd4\u503c\u4f5c\u4e3a\u6e29\u5ea6\u7684\u51fd\u6570<\/p>\n<p><strong>\u3010\u7814\u7a76\u5185\u5bb9\u3011<\/strong><\/p>\n<p>\u77f3\u58a8\u70ef\uff0c\u7531\u4e8e\u5176\u4f18\u5f02\u7684\u7269\u7406\u6027\u8d28\u4e00\u76f4\u53d7\u5230\u5b66\u672f\u754c\u7684\u5e7f\u6cdb\u5173\u6ce8\uff0c\u4e3a\u4e86\u5b9e\u73b0\u5728\u5fae\u7535\u5b50\u9886\u57df\u7684\u5e94\u7528\uff0c\u77f3\u58a8\u70ef\u8584\u819c\u9700\u8981\u8f6c\u79fb\u6216\u76f4\u63a5\u751f\u957f\u5230\u7edd\u7f18\u886c\u5e95\u4e0a\u3002\u76f4\u63a5\u5728\u7edd\u7f18\u886c\u5e95\u4e0a\u751f\u957f\u77f3\u58a8\u70ef\uff0c\u6709\u5229\u4e8e\u83b7\u5f97\u6676\u5706\u7ea7\u77f3\u58a8\u70ef\u6750\u6599\uff0c\u5bf9\u63a8\u52a8\u77f3\u58a8\u70ef\u6750\u6599\u5728\u96c6\u6210\u7535\u8def\u7b49\u9886\u57df\u7684\u5e94\u7528\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002\u4f46\u7531\u4e8e\u7edd\u7f18\u886c\u5e95\u672c\u8eab\u4e0d\u5177\u6709\u50ac\u5316\u80fd\u529b\uff0c\u4f7f\u7528<em><i>Cu<\/i><\/em>\uff08\u94dc\uff09\u3001<em><i>Ni<\/i><\/em>\uff08\u954d\uff09\u7b49\u91d1\u5c5e\u50ac\u5316\u5242\u53c8\u96be\u514d\u5f15\u5165\u91d1\u5c5e\u6cbe\u6c61\uff0c\u56e0\u6b64\u8be5\u9879\u7814\u7a76\u4e00\u76f4\u9762\u4e34\u8bb8\u591a\u6311\u6218\u3002\u4e0a\u6d77\u5fae\u7cfb\u7edf\u6240\u4fe1\u606f\u529f\u80fd\u6750\u6599\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u7684\u6c6a\u5b50\u6587\u3001\u859b\u5fe0\u8425\u7b49\u4eba\u57fa\u4e8e\u9517\u886c\u5e95\u4e0a\u751f\u957f\u9ad8\u8d28\u91cf\u5355\u5c42\u77f3\u58a8\u70ef\u7684\u7814\u7a76\u57fa\u7840\uff0c\u5728\u7edd\u7f18\u886c\u5e95\u4e0a\u9884\u5148\u6c89\u79ef\u9517\u8584\u819c\u4f5c\u4e3a\u50ac\u5316\u5242\uff0c\u901a\u8fc7\u4f18\u5316\u77f3\u58a8\u70ef\u751f\u957f\u6e29\u5ea6\u548c\u751f\u957f\u65f6\u95f4\uff0c\u5728\u5b8c\u5168\u84b8\u53d1\u6389\u9517\u8584\u819c\u7684\u540c\u65f6\u5b9e\u73b0\u5355\u5c42\u77f3\u58a8\u70ef\u5728\u7edd\u7f18\u886c\u5e95\u8868\u9762\u7684\u5168\u8986\u76d6\u3002\u5728\u7814\u7a76\u4e2d\u4ed6\u4eec\u8fd8\u53d1\u73b0\uff0c\u77f3\u58a8\u70ef\u7684\u5f62\u72b6\u5b8c\u5168\u4f9d\u8d56\u4e8e\u9517\u8584\u819c\u7684\u5f62\u72b6\uff0c\u56e0\u6b64\u8be5\u65b9\u6cd5\u65e2\u53ef\u4ee5\u5b9e\u73b0\u6676\u5706\u7ea7\u77f3\u58a8\u70ef\u8584\u819c\u7684\u751f\u957f\uff0c\u4e5f\u53ef\u4ee5\u901a\u8fc7\u9884\u5148\u8bbe\u8ba1\u7684\u9517\u56fe\u5f62\u5b9a\u4e49\u540e\u7eed\u77f3\u58a8\u70ef\u5668\u4ef6\u6240\u9700\u56fe\u5f62\u5316\u7684\u751f\u957f\u3002\u83b7\u5f97\u7684\u7edd\u7f18\u4f53\u4e0a\u77f3\u58a8\u70ef\u6750\u6599\u8868\u73b0\u51fa\u826f\u597d\u7684\u7535\u5b66\u6027\u80fd\uff0c\u521d\u6b65\u5c55\u793a\u4e86\u5176\u5728\u9664\u96fe\u3001\u7535\u81f4\u53d8\u8272\u7b49\u52a0\u70ed\u5668\u4ef6\u65b9\u9762\u7684\u5e94\u7528\u3002\u8be5\u9879\u7814\u7a76\u4e3a\u83b7\u5f97\u6676\u5706\u7ea7\u7edd\u7f18\u4f53\u4e0a\u77f3\u58a8\u70ef\u5960\u5b9a\u4e86\u57fa\u7840\uff0c\u6709\u52a9\u4e8e\u63a8\u52a8\u77f3\u58a8\u70ef\u6750\u6599\u5728\u5fae\u7535\u5b50\u9886\u57df\u7684\u5e94\u7528\u3002<\/p>\n<p>\u8be5\u9879\u5de5\u4f5c\u5f97\u5230\u4e86\u201c\u4e07\u4eba\u8ba1\u5212\u201d\u9752\u5e74\u62d4\u5c16\u4eba\u624d\u9879\u76ee\u3001\u4e2d\u79d1\u9662\u524d\u6cbf\u79d1\u5b66\u91cd\u70b9\u7814\u7a76\u9879\u76ee\u548c\u4e0a\u6d77\u5e02\u4f18\u79c0\u5b66\u79d1\u5e26\u5934\u4eba\u8ba1\u5212\u7684\u8d44\u52a9\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.cas.cn\/syky\/201706\/t20170615_4605042.shtml\" target=\"_blank\" rel=\"noopener noreferrer\">http:\/\/www.cas.cn\/syky\/201706\/t20170615_4605042.shtml<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/smll.201700929\/full\" target=\"_blank\" rel=\"noopener noreferrer\">Germanium-assisted Direct Growth of Graphene on Arbitrary Dielectric Substrates for Heating Devices<\/a>\uff08Small,2017,DOI\uff1a10.1002\/smll.201700929\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8Allen\u7f16\u8f91\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u6210\u679c\u7b80\u4ecb\u3011 \u8fd1\u671f\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u4e0a\u6d77\u5fae\u7cfb\u7edf\u4e0e\u4fe1\u606f\u6280\u672f\u7814\u7a76\u6240\u4fe1\u606f\u529f\u80fd\u6750\u6599\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4SOI(\u7edd\u7f18\u4f53\u4e0a\u7845)\u6750\u6599\u4e0e\u5668\u4ef6\u8bfe\u9898\u7ec4\u5728\u7edd\u7f18\u4f53\u886c\u5e95\u4e0a\u76f4\u63a5\u5236\u5907\u77f3\u58a8\u70ef\u7814\u7a76\u65b9\u9762\u53d6\u5f97\u65b0&#8230;<\/p>\n","protected":false},"author":349,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[46],"class_list":["post-86953","post","type-post","status-publish","format-standard","hentry","category-keji","tag-graphene"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/86953"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/349"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=86953"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/86953\/revisions"}],"predecessor-version":[{"id":86960,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/86953\/revisions\/86960"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=86953"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=86953"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=86953"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}