{"id":87787,"date":"2017-06-23T14:30:41","date_gmt":"2017-06-23T06:30:41","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=87787"},"modified":"2017-06-23T14:47:55","modified_gmt":"2017-06-23T06:47:55","slug":"%e3%80%90%e6%8a%95%e7%a8%bf%e5%be%85%e5%ae%9a%e3%80%91%e3%80%8a%e5%be%b7%e5%9b%bd%e5%ba%94%e7%94%a8%e5%8c%96%e5%ad%a6%e3%80%8b%e5%9b%9b%e5%b7%9d%e5%a4%a7%e5%ad%a6%e9%ab%98%e5%88%86%e5%ad%90%e7%a0%94","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=87787","title":{"rendered":"\u300a\u5fb7\u56fd\u5e94\u7528\u5316\u5b66\u300b\u56db\u5ddd\u5927\u5b66\u9ad8\u5206\u5b50\u7814\u7a76\u6240\u5f20\u65b0\u661f\u8bfe\u9898\u7ec4\uff1a\u5b9e\u65f6\u3001\u591a\u6b21\u81ea\u4fee\u590d\u7684\u67d4\u6027\u4f20\u611f\u5668\u7528\u4e8e\u4eba\u673a\u4ea4\u4e92\u7cfb\u7edf"},"content":{"rendered":"<p>\u968f\u7740\u667a\u80fd\u7ec8\u7aef\u7684\u666e\u53ca\uff0c\u5f00\u53d1\u548c\u5236\u5907\u5177\u6709\u4f18\u5f02\u529b\u5b66\u6027\u80fd\u548c\u54cd\u5e94\u7075\u654f\u6027\u7684\u67d4\u6027\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u6750\u6599\u5728\u5065\u5eb7\u76d1\u6d4b\u3001\u7535\u5b50\u76ae\u80a4\u3001\u4eff\u751f\u673a\u5668\u4eba\u3001\u4eba\u673a\u4ea4\u4e92\u7b49\u9886\u57df\u5177\u6709\u6781\u5927\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p>\u8fd1\u5e74\u6765\uff0c<strong>\u56db\u5ddd\u5927\u5b66\u9ad8\u5206\u5b50\u7814\u7a76\u6240\u5f20\u65b0\u661f\u526f\u6559\u6388<\/strong>\u548c<strong>\u5362\u707f\u8f89\u6559\u6388<\/strong>\u8bfe\u9898\u7ec4\u5229\u7528\u5177\u6709\u72ec\u7279\u4e24\u4eb2\u6027\u548c\u7eb3\u7c73\u5c3a\u5bf8\u7ed3\u6784\u7684\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6676\uff08CNC\uff09\u7684\u7ed3\u6784\u5bfc\u5411\u4f5c\u7528\uff0c\u8bf1\u5bfc\u5bfc\u7535\u586b\u6599\u81ea\u7ec4\u88c5\u5b9e\u73b0\u5728\u6a61\u80f6\u57fa\u4f53\u4e2d\u7684\u6709\u5e8f\u6392\u5217\u548c\u5b9a\u6784\u52a0\u5de5\uff0c\u83b7\u5f97\u529b\u5b66\u6027\u80fd\u4f18\u5f02\uff0c\u5bf9\u5e94\u53d8\u3001\u5316\u5b66\u6eb6\u5242\u7b49\u5916\u573a\u4f5c\u7528\u54cd\u5e94\u7075\u654f\u7684\u6709\u5e8f\u591a\u5c42\u6b21\u7ed3\u6784\u6a61\u80f6\u590d\u5408\u6750\u6599 (J. Mater. Chem. A, 2015, 3, 13317; ACS Sustainable Chem. Eng., 2015, 3, 675; Soft Matter, 2016, 12, 845; Compos. Sci. Technol., 2016, 124, 44; Compos. Sci. Technol., 2016, 125; Green Chem. 2017, DOI: 10.1039\/C7GC01138E.)\u3002\u5e76\u901a\u8fc7\u5c42\u5c42\u7ec4\u88c5\u52a0\u5de5\u65b9\u6cd5\u5c06\u5fae\u7ed3\u6784\u53ef\u63a7\u7684\u5bfc\u7535\u80f6\u4e73\u6d82\u8986\u4e8ePU\u7eb1\u7ebf\u3001\u6d77\u7ef5\u7b49\u5f39\u6027\u57fa\u6750\u8868\u9762\uff0c\u5236\u5907\u4e86\u5177\u6709\u8d85\u9ad8\u7075\u654f\u5ea6\u7684\u62c9\u4f38\u5e94\u53d8\u4ee5\u53ca\u5316\u5b66\u6eb6\u5242\u4f20\u611f\u6750\u6599 (ACS Appl. Mater. Interfaces, 2016, 8, 9936; ACS Appl. Mater. Interfaces, 2017, 9, 13657; Phys. Chem. Chem. Phys., 2017, 19, 16198.)\uff0c\u5728\u667a\u80fd\u670d\u88c5\u3001\u8f93\u6cb9\u7ba1\u9053\u6e17\u6f0f\u76d1\u6d4b\u4e0e\u667a\u80fd\u5835\u6f0f\u7b49\u9886\u57df\u5177\u6709\u91cd\u8981\u7684\u5e94\u7528\u4ef7\u503c\u3002<\/p>\n<p>\u76ee\u524d\uff0c\u5927\u90e8\u5206\u67d4\u6027\u4f20\u611f\u5668\u53d7\u9650\u4e8e\u54cd\u5e94\u7075\u654f\u6027\u5dee\u4ee5\u53ca\u906d\u53d7\u4e0d\u53ef\u907f\u514d\u7684\u5916\u529b\u7834\u574f\u65f6\u529b\u5b66\u7535\u5b66\u7a33\u5b9a\u6027\u5dee\uff0c\u53ea\u80fd\u5b9e\u73b0\u4fe1\u53f7\u91c7\u96c6\uff0c\u800c\u65e0\u6cd5\u8fdb\u884c\u4e0b\u4e00\u6b65\u7684\u4fe1\u53f7\u8bc6\u522b\u3001\u5904\u7406\u548c\u6307\u4ee4\u7684\u8f93\u51fa\u3002\u56e0\u6b64\uff0c\u5f00\u53d1\u5177\u6709\u4eff\u751f\u81ea\u6108\u5408\u529f\u80fd\u7684\u81ea\u4fee\u590d\u67d4\u6027\u4f20\u611f\u5668\u6750\u6599\u53ca\u5176\u53ef\u7a7f\u6234\u7535\u5b50\u662f\u529f\u80fd\u5f39\u6027\u4f53\u6750\u6599\u9886\u57df\u4e9f\u5f85\u89e3\u51b3\u7684\u6838\u5fc3\u95ee\u9898\u4e4b\u4e00\u3002\u5df2\u62a5\u9053\u7684\u81ea\u4fee\u590d\u67d4\u6027\u4f20\u611f\u5668\u7684\u5e94\u53d8\u654f\u611f\u5143\u4ef6\u591a\u4e3a\u65e0\u673a\u5bfc\u7535\u6d82\u5c42\uff0c\u5982\u78b3\u7eb3\u7c73\u7ba1\u3001\u91d1\u7eb3\u7c73\u9897\u7c92\u7b49\uff0c\u5176\u672c\u8eab\u5e76\u4e0d\u5177\u5907\u81ea\u4fee\u590d\u529f\u80fd\uff0c\u5bfc\u81f4\u957f\u671f\u4f7f\u7528\u7684\u53ef\u9760\u6027\u548c\u7a33\u5b9a\u6027\u53d7\u5230\u5f71\u54cd\uff0c\u4e25\u91cd\u963b\u788d\u4e86\u5176\u5b9e\u9645\u5e94\u7528\u3002<\/p>\n<p>\u57fa\u4e8e\u4ee5\u4e0a\u80cc\u666f\uff0c<strong>\u5f20\u65b0\u661f\u526f\u6559\u6388\u7814\u7a76\u56e2\u961f<\/strong>\u4ece\u8bbe\u8ba1\u548c\u6784\u5efa\u5177\u6709\u81ea\u4fee\u590d\u6027\u80fd\u7684\u6709\u673a\u5e94\u53d8\u654f\u611f\u6750\u6599\u51fa\u53d1\uff0c\u901a\u8fc7\u5bf9CNC\u8fdb\u884c\u8868\u9762\u63a5\u679d\u6216\u5316\u5b66\u4fee\u9970\uff0c\u5728\u586b\u6599\u5bfc\u7535\u7f51\u7edc\u4e0e\u6a61\u80f6\u57fa\u4f53\u95f4\u6784\u5efa\u5177\u6709\u81ea\u4fee\u590d\u529f\u80fd\u7684\u52a8\u6001\u79bb\u5b50\u952e\u3001\u914d\u4f4d\u952e\u3001\u591a\u91cd\u6c22\u952e\u7b49\u8d85\u5206\u5b50\u53ef\u9006\u4ea4\u8054\u7f51\u7edc\uff0c \u5728\u5ba4\u6e29\u4e0b\u5b9e\u73b0\u6750\u6599\u7684\u5b9e\u65f6\uff08\u2264 30 s\uff09\u3001\u591a\u6b21\u81ea\u4fee\u590d\uff08\u81ea\u4fee\u590d3\u6b21\u540e\u7684\u4fee\u590d\u6548\u7387\u4e3a93%\uff09\uff0c\u5e76\u5229\u7528\u5c42\u5c42\u7ec4\u88c5\u52a0\u5de5\u65b9\u6cd5\u5236\u5907\u5177\u6709\u8d85\u9ad8\u7075\u654f\u5ea6\u3001\u53ef\u76d1\u6d4b\u5fae\u5c0f\u751f\u7406\u6d3b\u52a8\uff08\u5982\u5589\u7ed3\u53d1\u97f3\u3001\u9762\u90e8\u8868\u60c5\u3001\u5480\u56bc\u3001\u54b3\u55fd\u3001\u541e\u54bd\u7b49\uff09\u7684\u81ea\u4fee\u590d\u6709\u673a\u67d4\u6027\u4f20\u611f\u6750\u6599\uff0c\u4e3a\u53ef\u7a7f\u6234\u7535\u5b50\u7684\u5e94\u7528\u63d0\u4f9b\u5173\u952e\u6750\u6599\u548c\u6280\u672f\u3002(J. Mater. Chem. A, 2017, 5, 9824.; ACS Appl. Mater. Interfaces, 2017, 9, 20106.)<\/p>\n<p><strong>\u56fe1.\uff08a\uff09\u8d85\u5206\u5b50\u591a\u91cd\u6c22\u952e\u53ef\u9006\u4ea4\u8054\u7f51\u7edc\u6a21\u578b\u793a\u610f\u56fe\uff1b\uff08b\uff09\u529b\u5b66\u6027\u80fd\u81ea\u4fee\u590d\u6548\u7387\u5bf9\u6bd4\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-87789 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u56fe\u72471-16.png\" alt=\"\" width=\"530\" height=\"139\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u56fe\u72471-16.png 530w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u56fe\u72471-16-300x79.png 300w\" sizes=\"(max-width: 530px) 100vw, 530px\" \/><\/p>\n<p>\n <strong>\u56fe2. \u529b\u5b66\u6027\u80fd\u81ea\u4fee\u590d\u6f14\u793a<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-87790 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u56fe2.gif\" alt=\"\" width=\"146\" height=\"82\" \/><\/p>\n<p>\u7531\u4e8e\u8be5\u67d4\u6027\u4f20\u611f\u6750\u6599\u51fa\u8272\u7684\u529b\u5b66\u3001\u7535\u5b66\u53ef\u9760\u6027\u4e0e\u54cd\u5e94\u7075\u654f\u6027\uff0c\u8be5\u56e2\u961f\u901a\u8fc7\u4e0e\u56db\u5ddd\u5927\u5b66\u7535\u5b50\u4fe1\u606f\u5b66\u9662\u4f59\u8273\u6885\u526f\u6559\u6388\u3001\u9676\u9752\u5ddd\u526f\u6559\u6388\u4ee5\u53ca\u56db\u5ddd\u5927\u5b66\u9526\u57ce\u5b66\u9662\u5e84\u5065\u8001\u5e08\u5408\u4f5c\uff0c\u8bbe\u8ba1\u548c\u5f00\u53d1\u4e86\u9762\u90e8\u8868\u60c5\u63a7\u5236\u673a\u5668\u4eba\u539f\u578b\u7cfb\u7edf\u4ee5\u53ca\u540c\u6b65\u53d1\u97f3\u539f\u578b\u7cfb\u7edf\uff0c\u5b9e\u73b0\u4e86\u67d4\u6027\u4f20\u611f\u5668\u4e0e\u7535\u5b50\u63a7\u5236\u7cfb\u7edf\u7684\u96c6\u6210\u5316\u5e94\u7528\u548c\u4eba\u673a\u4ea4\u4e92\u3002<\/p>\n<p><strong>\u56fe3.\uff08a\uff09\u81ea\u4fee\u590d\u67d4\u6027\u4f20\u611f\u5668\u7528\u4e8e\u9762\u90e8\u8868\u60c5\u8bc6\u522b\uff0c\u8bed\u97f3\u8bc6\u522b\uff1b\uff08b\uff09\u9762\u90e8\u8868\u60c5\u63a7\u5236\u673a\u5668\u4eba\u7cfb\u7edf\u548c\u540c\u6b65\u53d1\u97f3\u7cfb\u7edf\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-87791 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u56fe\u72473-6.png\" alt=\"\" width=\"698\" height=\"244\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u56fe\u72473-6.png 698w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/06\/\u56fe\u72473-6-300x105.png 300w\" sizes=\"(max-width: 698px) 100vw, 698px\" \/><\/p>\n<p>\u8fd9\u4e00\u7814\u7a76\u6210\u679c\u5df2\u5728\u7ebf\u53d1\u8868\u5728<strong>Angewandte Chemie International Edition<\/strong>\uff08\u5fb7\u56fd\u5e94\u7528\u5316\u5b66\uff0cIF:11.994\uff09\u671f\u520a\u4e0a\uff0c\u56db\u5ddd\u5927\u5b66\u9ad8\u5206\u5b50\u7814\u7a76\u6240\u7855\u58eb\u7814\u7a76\u751f<strong>\u66f9\u6770<\/strong>\u4e3a\u7b2c\u4e00\u4f5c\u8005\uff0c<strong>\u5f20\u65b0\u661f\u526f\u6559\u6388<\/strong>\u548c<strong>\u4f59\u8273\u6885\u526f\u6559\u6388<\/strong>\u4e3a\u8bba\u6587\u7684\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002\u672c\u7814\u7a76\u5de5\u4f5c\u5f97\u5230\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\uff08\u9879\u76ee\u7f16\u53f7\uff1a51673121\uff09\u548c\u9ad8\u5206\u5b50\u6750\u6599\u5de5\u7a0b\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u63a2\u7d22\u9879\u76ee\uff08\u9879\u76ee\u7f16\u53f7\uff1asklpme2017-2-06\uff09\u7b49\u9879\u76ee\u7684\u8d44\u52a9\u3002<\/p>\n<p><strong>\u53c2\u8003\u6587\u732e\uff1a<\/strong><br \/>\n Jie Cao, Canhui Lu, Xinxing Zhang*, et al., Multiple hydrogen bonding enables the self-healing of sensors for human-machine interaction. Angewandte Chemie International Edition, 2017, DOI: 10.1002\/anie.201704217.<\/p>\n<p>\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u968f\u7740\u667a\u80fd\u7ec8\u7aef\u7684\u666e\u53ca\uff0c\u5f00\u53d1\u548c\u5236\u5907\u5177\u6709\u4f18\u5f02\u529b\u5b66\u6027\u80fd\u548c\u54cd\u5e94\u7075\u654f\u6027\u7684\u67d4\u6027\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u6750\u6599\u5728\u5065\u5eb7\u76d1\u6d4b\u3001\u7535\u5b50\u76ae\u80a4\u3001\u4eff\u751f\u673a\u5668\u4eba\u3001\u4eba\u673a\u4ea4\u4e92\u7b49\u9886\u57df\u5177\u6709\u6781\u5927\u5e94\u7528\u524d\u666f\u3002 \u8fd1\u5e74\u6765\uff0c\u56db\u5ddd&#8230;<\/p>\n","protected":false},"author":24,"featured_media":87789,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[42],"class_list":["post-87787","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-gaofenzi"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/87787"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/24"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=87787"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/87787\/revisions"}],"predecessor-version":[{"id":87794,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/87787\/revisions\/87794"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/87789"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=87787"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=87787"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=87787"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}