{"id":90375,"date":"2017-07-10T14:00:58","date_gmt":"2017-07-10T06:00:58","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=90375"},"modified":"2017-07-09T12:52:14","modified_gmt":"2017-07-09T04:52:14","slug":"%e5%94%90%e6%9c%ac%e5%bf%a0%e9%99%a2%e5%a3%abadv-funct-mater-%ef%bc%9a%e7%ba%a2%e8%89%b2%e6%9c%89%e6%9c%ba%e7%ba%b3%e7%b1%b3%e7%b2%92%e5%ad%90%e7%94%a8%e4%ba%8e%e5%bc%82%e7%a7%8d%e7%a7%bb%e6%a4%8d","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=90375","title":{"rendered":"\u5510\u672c\u5fe0\u9662\u58ebAdv. Funct. Mater.\uff1a\u7ea2\u8272\u6709\u673a\u7eb3\u7c73\u7c92\u5b50\u7528\u4e8e\u5f02\u79cd\u79fb\u690d\u4f53\u5185\u8367\u5149\u6210\u50cf"},"content":{"rendered":"<p><strong>\u3010\u80cc\u666f\u4ecb\u7ecd\u3011<\/strong><\/p>\n<p>\u975e\u4fb5\u5165\u6027\u6d3b\u4f53\u8367\u5149\u6210\u50cf\u53ef\u4ee5\u4e3a\u75be\u75c5\u8bca\u65ad\u548c\u6cbb\u7597\u6280\u672f\u63d0\u4f9b\u6709\u4ef7\u503c\u7684\u4f53\u5185\u4fe1\u606f\u3002\u8367\u5149\u6210\u50cf\u7684\u8d28\u91cf\u548c\u5206\u8fa8\u7387\u9ad8\u5ea6\u4f9d\u8d56\u4e8e\u5f3a\u5149\u81f4\u53d1\u5149\uff08PL\uff09\uff0c\u9ad8\u5149\u7a33\u5b9a\u6027\uff0c\u826f\u597d\u751f\u7269\u76f8\u5bb9\u6027\u7684\u9020\u5f71\u5242 \uff0c\u4f18\u5f02\u7684\u7269\u7406\u7a33\u5b9a\u6027\u3002\u660e\u4eae\u7684\u548c\u7ea2\u8272\u7684\u6709\u673a\u7eb3\u7c73\u9897\u7c92\uff08NPs\uff09\u88ab\u8bc1\u660e\u53ef\u7528\u4e8e\u9ad8\u6548\u7387\u4f53\u5185\u8367\u5149\u6210\u50cf\u3002 \u7136\u800c\uff0c\u5927\u591a\u6570\u7ea2\u8272\u6709\u673a\u67d3\u6599\u5728\u805a\u96c6\u72b6\u6001\u4e0b\u663e\u793a\u51fa\u6781\u5f31\u7684\u91ca\u653e\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea<strong>\u534e\u5357\u7406\u5de5\u5927\u5b66<\/strong>\u7684<strong>\u5510\u672c\u5fe0\u9662\u58eb<\/strong>\u3001<strong>\u8d75\u7956\u91d1\u6559\u6388<\/strong>\u548c<strong>\u65b0\u52a0\u5761\u56fd\u7acb\u5927\u5b66<\/strong>\u7684<strong>Bin Liu\uff08\u5171\u540c\u901a\u8baf\uff09<\/strong>\u7b49\u4eba\u63d0\u51fa\u4e86\u5177\u6709\u5f3a\u805a\u96c6\u6001\u5149\u81f4\u53d1\u5149\u548c\u826f\u597d\u7684\u751f\u7269\u76f8\u5bb9\u6027\u7684\u7ea2\u8272\u8367\u5149\u56e2\uff08t-BPITBT-TPE\uff09\u3002\u7531\u5305\u542b\u57281,2-\u4e8c\u786c\u8102\u9170-sn-\u7518\u6cb9\u57fa-3-\u78f7\u9178\u4e59\u9187\u80fa-N- [\u7532\u6c27\u57fa\uff08\u805a\u4e59\u4e8c\u9187\uff09\uff08DSPE-mPEG\uff09\u80f6\u675f\u4e2d\u7684t-BPITBT-TPE\u805a\u96c6\u4f53\u7ec4\u6210\u7684NPs\u5728660nm\u5177\u6709\u9ad8\u7684\u5149\u81f4\u53d1\u5149\u5cf0\u503c\uff0c\u542b\u6c34\u4ecb\u8d28\u4e2d\u8367\u5149\u91cf\u5b50\u4ea7\u7387\u4e3a32\uff05\u3002\u901a\u8fc7\u4f7f\u7528\u5177\u6709\u4e0d\u540c\u672b\u7aef\u57fa\u56e2\u7684\u76f8\u540c\u805a\u5408\u7269\u57fa\u8d28\uff0c\u4f8b\u5982\u7532\u6c27\u57fa\uff08DSPE-mPEG\uff09\uff0c\u80fa\uff08DSPE-PEG-NH 2\uff09\u6216\u7fa7\u7532\u57fa\uff08DSPE-PEG-COOH\uff09\u57fa\u56e2\uff09\uff0cNPs\u53ef\u4ee5\u5bb9\u6613\u5730\u5e26\u7535\u3002\u76f8\u5173\u7814\u7a76\u7ed3\u679c\u4ee5\u9898\u4e3a\u201cRobust Red Organic Nanoparticles for In Vivo Fluorescence Imaging of Cancer Cell Progression in Xenografted Zebrafish\u201d\u53d1\u8868\u5728\u4e86Advanced Functional Materials\u4e0a\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe1\u00a0PITBT-TPE (CCDC 1502965) \u548ct-BPITBT-TPE (CCDC 1502964)\u7684\u6676\u4f53\u7ed3\u6784<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-90508\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/001-2.png\" alt=\"\" width=\"600\" height=\"574\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/001-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/001-2-300x287.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>PITBT-TPE\u4e2d\u7684TPE\u90e8\u5206\u91c7\u7528\u626d\u66f2\u6784\u8c61\uff0c\u4ee5\u9632\u6b62\u03c0-\u03c0\u5806\u53e0\u76f8\u4e92\u4f5c\u7528\uff0c\u4f46\u662f2,1,3-\u82ef\u5e76\u567b\u4e8c\u5511\uff08BT\uff09\uff0c\u567b\u5429\uff08Th\uff09\u548c9,10-\u83f2\u5e76\u54aa\u5511\uff08PI\uff09\u7247\u6bb5\u51e0\u4e4e\u6392\u5217\u5728\u76f8\u540c\u7684\u5e73\u9762<\/p>\n<p><strong>\u56fe2\u00a0\u03c0-\u03c0\u5806\u53e0\u76f8\u4e92\u4f5c\u7528\u7684\u56fe\u793a<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-90509\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/002-1.png\" alt=\"\" width=\"600\" height=\"436\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/002-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/002-1-300x218.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>A\uff09<\/strong>\u6676\u4f53\u586b\u5145\u548c \u00a0\u00a0<strong>B\uff09<\/strong>PITBT-TPE\u548ct-BPITBT-TPE\u7684\u5206\u5b50\u95f4\u03c0-\u03c0\u5806\u53e0\u76f8\u4e92\u4f5c\u7528\u7684\u56fe\u793a\uff0c\u4e3a\u4e86\u6e05\u695a\u8d77\u89c1\uff0c\u7701\u7565\u4e86\u6eb6\u5242\u5206\u5b50\u548c\u6c22\u539f\u5b50<\/p>\n<p><strong>\u56fe3\u00a0\u5438\u6536\u5149\u8c31\u548c\u5f52\u4e00\u5316\u5149\u81f4\u53d1\u5149\u5149\u8c31<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-90510\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/003-1.png\" alt=\"\" width=\"600\" height=\"312\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/003-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/003-1-300x156.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>A\uff09THF\u6eb6\u6db2\u4e2d\u7684\u5438\u6536\u5149\u8c31<\/p>\n<p>B\uff09THF\u6eb6\u6db2\u3001PITBT-TPE\u548ct-BPITBT-TPE\u819c\u7684\u5f52\u4e00\u5316\u5149\u81f4\u53d1\u5149\u5149\u8c31<\/p>\n<p><strong>\u56fe4 t-BPITBT NH<sub>2<\/sub>-TAT NPs\u7684\u79ef\u7d2f\u53caNPs\u5728\u4e0d\u540c\u5668\u5b98\u7ec4\u7ec7\u4e2d\u7684\u5206\u5e03<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-90511\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/004-1.png\" alt=\"\" width=\"520\" height=\"453\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/004-1.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/004-1-300x261.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>A\uff09\u4e0d\u540c\u65f6\u95f4\u9759\u8109\u6ce8\u5c04\u540e\u80bf\u7624\u5f02\u79cd\u79fb\u690d\u7269\u4e2dt-BPITBT NH<sub>2<\/sub>-TAT NPs\u7684\u79ef\u7d2f<\/p>\n<p>B\uff09NPs\u5728\u4e0d\u540c\u5668\u5b98\u7ec4\u7ec7\u4e2d\u7684\u5206\u5e03<\/p>\n<p><strong>\u3010\u603b\u7ed3\u3011<\/strong><\/p>\n<p>\u672c\u7814\u7a76\u8bbe\u8ba1\u5e76\u5408\u6210\u4e86\u5177\u6709\u9ad8\u56fa\u4f53\u8367\u5149\u6548\u7387\u7684\u7a33\u5b9a\u7684\u7ea2\u8272\u8367\u5149\u56e2BPITBT-TPE\u548ct-BPITBT-TPE\u3002\u5f15\u5165AIE\u6d3b\u6027TPE\u53ef\u6709\u6548\u7f13\u89e3\u805a\u5408\u72b6\u6001\u4e0b\u7535\u5b50D-A\u7ed3\u6784\u5206\u5b50\u7684\u53d1\u5c04\u731d\u706d\u3002\u8fd9\u4e9b\u7ed3\u679c\u8868\u660e\uff0c\u5177\u6709\u5f3a\u7ea2\u8272\u8367\u5149\u548c\u5404\u79cd\u5b98\u80fd\u56e2\u7684\u6709\u673a\u7eb3\u7c73\u9897\u7c92\u53ef\u80fd\u662f\u7528\u4e8e\u751f\u7269\u5e94\u7528\u6709\u5e0c\u671b\u7684\u5bf9\u6bd4\u5242\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201701418\/full\" target=\"_blank\" rel=\"noopener noreferrer\">Robust Red Organic Nanoparticles for In Vivo Fluorescence Imaging of Cancer Cell Progression in Xenografted Zebrafish<\/a>\uff08Adv. Funct. Mater.,2017,DOI:10.1002\/adfm.201701418\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u751f\u7269\u6750\u6599\u7ec4Allen\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u53c2\u4e0e\u751f\u7269\u6750\u6599\u8bdd\u9898\u8ba8\u8bba\u6216\u4e86\u89e3\u751f\u7269\u6750\u6599\u5c0f\u7ec4\u62db\u52df\u8be6\u60c5\uff0c\u8bf7\u52a0\u5165\u6750\u6599\u4eba\u751f\u7269\u6750\u6599\u4ea4\u6d41\u7fa4\uff08124806506\uff09\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<\/strong><a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\"><strong>\u6d4b\u8bd5\u8c37<\/strong><\/a><strong>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u80cc\u666f\u4ecb\u7ecd\u3011 \u975e\u4fb5\u5165\u6027\u6d3b\u4f53\u8367\u5149\u6210\u50cf\u53ef\u4ee5\u4e3a\u75be\u75c5\u8bca\u65ad\u548c\u6cbb\u7597\u6280\u672f\u63d0\u4f9b\u6709\u4ef7\u503c\u7684\u4f53\u5185\u4fe1\u606f\u3002\u8367\u5149\u6210\u50cf\u7684\u8d28\u91cf\u548c\u5206\u8fa8\u7387\u9ad8\u5ea6\u4f9d\u8d56\u4e8e\u5f3a\u5149\u81f4\u53d1\u5149\uff08PL\uff09\uff0c\u9ad8\u5149\u7a33\u5b9a\u6027\uff0c\u826f\u597d\u751f\u7269\u76f8\u5bb9\u6027\u7684&#8230;<\/p>\n","protected":false},"author":349,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-90375","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/90375"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/349"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=90375"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/90375\/revisions"}],"predecessor-version":[{"id":90644,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/90375\/revisions\/90644"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=90375"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=90375"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=90375"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}