{"id":91808,"date":"2017-07-21T06:30:48","date_gmt":"2017-07-20T22:30:48","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=91808"},"modified":"2017-07-20T15:13:19","modified_gmt":"2017-07-20T07:13:19","slug":"%e9%ad%8f%e5%bf%97%e7%a5%a5aem%e7%bb%bc%e8%bf%b0%ef%bc%9a%e6%9f%94%e6%80%a7%e5%82%a8%e8%83%bd%e8%a3%85%e7%bd%ae%e7%9a%84%e6%9c%ba%e6%a2%b0%e5%88%86%e6%9e%90%e5%92%8c%e7%bb%93%e6%9e%84%e8%ae%be","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=91808","title":{"rendered":"\u9b4f\u5fd7\u7965AEM\u7efc\u8ff0\uff1a\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u673a\u68b0\u5206\u6790\u548c\u7ed3\u6784\u8bbe\u8ba1\u8981\u6c42"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u4e3a\u63d0\u9ad8\u67d4\u6027\u7535\u5b50\u5143\u4ef6\u7684\u96c6\u6210\u5ea6\uff0c\u975e\u5e38\u9700\u8981\u5177\u6709\u51fa\u8272\u673a\u68b0\u53d8\u5f62\u6027\u80fd\u7684\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u3002\u4e0e\u4f20\u7edf\u7535\u6e90\u4e0d\u540c\uff0c\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u673a\u68b0\u53ef\u9760\u6027\uff0c\u5305\u62ec\u7535\u6c14\u6027\u80fd\u548c\u53d8\u5f62\u8010\u529b\u53d7\u5230\u4e86\u5f88\u591a\u5173\u6ce8\u3002\u4e3a\u4e86\u63d0\u4f9b\u8bbe\u5907\u7ed3\u6784\u8bbe\u8ba1\u7684\u6307\u5bfc\u539f\u5219\uff0c\u5e94\u5728\u673a\u68b0\u53d8\u5f62\u8fc7\u7a0b\u4e2d\u5bf9\u6574\u4e2a\u7ed3\u6784\u7684\u5e94\u53d8\u5206\u5e03\u548c\u5931\u6548\u6a21\u5f0f\u8fdb\u884c\u7efc\u5408\u7814\u7a76\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea<strong>\u56fd\u5bb6\u7eb3\u7c73\u79d1\u5b66\u4e2d\u5fc3<\/strong>\u7684<strong>\u9b4f\u5fd7\u7965\u7814\u7a76\u5458\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u7740\u91cd\u4e8e\u8fd1\u5e74\u6765\u67d4\u6027\u9502\u79bb\u5b50\u7535\u6c60\uff08LIBs\uff09\u548c\u8d85\u7ea7\u7535\u5bb9\u5668\uff08SCs\uff09\u7684\u673a\u68b0\u53d8\u5f62\u7279\u5f81\uff0c\u5206\u6790\u548c\u7ed3\u6784\u8bbe\u8ba1\u7b56\u7565\uff0c\u9996\u5148\u4ecb\u7ecd\u4e86\u5668\u4ef6\u4e2d\u5f2f\u66f2\u5e94\u53d8\u7684\u4e3b\u8981\u7406\u8bba\u8ba1\u7b97\uff0c\u7136\u540e\u603b\u7ed3\u4e86\u63cf\u8ff0\u5f2f\u66f2\u72b6\u6001\u7684\u51e0\u4e2a\u53c2\u6570\u3002\u5728\u8fd9\u4e9b\u53c2\u6570\u4e2d\uff0c\u7a81\u51fa\u4e86\u5f2f\u66f2\u534a\u5f84\u53ca\u5176\u76f8\u5e94\u7684\u6d4b\u8bd5\u65b9\u6cd5\u548c\u8bbe\u5907\u3002\u8be6\u7ec6\u56de\u987e\u4e86\u7ed3\u6784\u8bbe\u8ba1\u7684\u7b56\u7565\u53ca\u5176\u5e94\u7528\u8fdb\u5c55\uff0c\u5982\u57fa\u5e95\u9009\u62e9\u3001\u8bbe\u5907\u539a\u5ea6\u3001\u5c01\u88c5\u4f7f\u7528\u4ee5\u53ca\u65b0\u9896\u7684\u7ed3\u6784\u8bbe\u8ba1\u3002\u6700\u540e\uff0c\u8ba8\u8bba\u4e86\u5177\u6709\u53ef\u9760\u673a\u68b0\u6027\u80fd\u7684\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u6311\u6218\u548c\u524d\u666f\u3002\u76f8\u5173\u5185\u5bb9\u4ee5\u9898\u4e3a\u201c<strong>Mechanical Analyses and Structural Design Requirements for Flexible Energy Storage Devices<\/strong>\u201d\u53d1\u8868\u5728\u4e86<strong>Advanced Energy Materials<\/strong>\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92365\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/00-3.png\" alt=\"\" width=\"600\" height=\"446\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/00-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/00-3-300x223.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u7efc\u8ff0\u603b\u89c8\u56fe<\/strong><\/p>\n<h3>1 \u7b80\u4ecb<\/h3>\n<p>\u81ea\u53ef\u5f2f\u66f2\u5851\u6599\u7247\u4e0a\u7b2c\u4e00\u4e2a\u805a\u5408\u7269\u6676\u4f53\u7ba1\u4e0a\u7684\u5f00\u521b\u6027\u5de5\u4f5c\u5f00\u59cb\uff0c\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u53d7\u5230\u4e86\u76f8\u5f53\u5927\u7684\u5173\u6ce8\u3002\u5404\u79cd\u67d4\u6027\u7535\u5b50\u5143\u4ef6\uff0c\u5305\u62ec\u5377\u8d77\u663e\u793a\u5668\u3001\u67d4\u6027\u8584\u819c\u6676\u4f53\u7ba1\uff08TFT\uff09\u3001\u67d4\u6027\u592a\u9633\u80fd\u7535\u6c60\u3001\u67d4\u6027\u7eb3\u7c73\u53d1\u751f\u5668\uff0c\u4ee5\u53ca\u4e00\u4e9b\u67d4\u6027\u6307\u5c16\u7535\u5b50\u5668\u4ef6\uff0c\u8d85\u8584\u201c\u8868\u76ae\u201d\u7535\u5b50\u8bbe\u5907\u548c\u53ef\u690d\u5165\u533b\u7597\u8bbe\u5907\u7b49 \uff0c\u76ee\u524d\u53d1\u5c55\u826f\u597d\uff0c\u8fd9\u53cd\u6620\u4e86\u67d4\u6027\u7535\u5b50\u4ea7\u54c1\u7684\u589e\u957f\u8d8b\u52bf\u3002<\/p>\n<p>\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u7684\u53d1\u5c55\u8981\u6c42\u9ad8\u5ea6\u7075\u6d3b\u7684\u50a8\u80fd\u88c5\u7f6e\uff0c\u4e0d\u4ec5\u8981\u6709\u4e0e\u5e38\u89c4\u7535\u6e90\u7c7b\u4f3c\u7684\u9ad8\u80fd\u91cf\/\u529f\u7387\u5bc6\u5ea6\u548c\u901f\u7387\u6027\u80fd\uff0c\u800c\u4e14\u9700\u8981\u5177\u6709\u5f3a\u5927\u7684\u673a\u68b0\u6027\u80fd\u3002\u8fd9\u4e9b\u5668\u4ef6\u53ef\u4ee5\u8fdb\u4e00\u6b65\u63d0\u9ad8\u6574\u4e2a\u7535\u5b50\u7cfb\u7edf\u7684\u96c6\u6210\u5ea6\u3002\u5728\u7efc\u5408\u67d4\u6027\u7535\u5b50\u7cfb\u7edf\u4e2d\uff0c\u80fd\u91cf\u50a8\u5b58\u88c5\u7f6e\u5728\u8fde\u63a5\u5148\u524d\u7684\u80fd\u91cf\u91c7\u96c6\u88c5\u7f6e\u548c\u63a5\u4e0b\u6765\u7684\u80fd\u91cf\u5229\u7528\u88c5\u7f6e\u65b9\u9762\u8d77\u7740\u91cd\u8981\u7684\u4f5c\u7528\u3002\u53ef\u5145\u7535\u4e8c\u6b21\u7535\u6c60\u548c\u8d85\u7ea7\u7535\u5bb9\u5668\uff08SCs\uff09\u662f\u4e24\u79cd\u5178\u578b\u7684\u50a8\u80fd\u88c5\u7f6e\u3002\u901a\u8fc7\u5229\u7528\u65b0\u578b\u7535\u6781\u6750\u6599\uff0c\u96c6\u7535\u5668\u548c\u56fa\u6001\u7535\u89e3\u8d28\uff0c\u67d4\u6027\u9502\u79bb\u5b50\u7535\u6c60\uff08LIB\uff09\u548cSCs\u53d6\u5f97\u4e86\u663e\u8457\u8fdb\u5c55\u3002\u67d4\u6027\u7535\u6e90\u7684\u5e94\u7528\u9886\u57df\u548c\u4f7f\u7528\u5bff\u547d\u5f88\u5927\u7a0b\u5ea6\u4e0a\u53d6\u51b3\u4e8e\u5b83\u4eec\u7684\u673a\u68b0\u53d8\u5f62\u8010\u6027\u548c\u53d8\u5f62\u65f6\u7684\u7535\u6027\u80fd\u4fdd\u6301\u3002\u5408\u683c\u7684\u67d4\u6027\u7535\u6e90\u5e94\u80fd\u591f\u627f\u53d7\u5916\u90e8\u673a\u68b0\u53d8\u5f62\uff08\u5982\u5f2f\u66f2\uff0c\u538b\u7f29\uff0c\u62c9\u4f38\uff0c\u6298\u53e0\u548c\u626d\u8f6c\uff09\u5f15\u8d77\u7684\u9ad8\u5e94\u53d8\uff0c\u540c\u65f6\u4fdd\u6301\u5176\u7535\u5316\u5b66\u6027\u80fd\u7684\u7a33\u5b9a\u6027\u548c\u7ed3\u6784\u5b8c\u6574\u6027\u3002\u56e0\u6b64\uff0c\u5bf9\u4e8e\u672a\u6765\u7684\u5e94\u7528\uff0c\u67d4\u6027\u8bbe\u5907\u7684\u673a\u68b0\u53ef\u9760\u6027\u8bc4\u4f30\u548c\u7535\u6c14\u6027\u80fd\u5206\u6790\u5e94\u4e88\u4ee5\u91cd\u89c6\u3002<\/p>\n<p>\u5f2f\u66f2\u6210\u4e00\u5b9a\u66f2\u7387\u65f6\uff0c\u8010\u53d7\u6027\u662f\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u4e3b\u8981\u673a\u68b0\u53d8\u5f62\u7279\u6027\u3002\u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u4eba\u4eec\u5df2\u7ecf\u63d0\u51fa\u4e86\u51e0\u79cd\u5f2f\u66f2\u7279\u6027\u53c2\u6570\u548c\u5404\u79cd\u673a\u68b0\u65b9\u6cd5\u6765\u8bc4\u4f30\u67d4\u6027\u88c5\u7f6e\u7684\u8d28\u91cf\u548c\u5931\u6548\u6a21\u5f0f\u3002\u8fd9\u4e9b\u673a\u68b0\u8ba1\u91cf\u5b66\u4e2d\u7684\u4e00\u90e8\u5206\u6765\u6e90\u4e8e\u5bf9\u5fae\u673a\u7535\u7cfb\u7edf\uff08MEMS\uff09\u548cTFT\u7684\u67d4\u6027\u534a\u5bfc\u4f53\u5668\u4ef6\u7684\u65e9\u671f\u7814\u7a76\u3002\u7136\u800c\uff0c\u7531\u4e8e\u4e0d\u540c\u7814\u7a76\u7ec4\u91c7\u7528\u4e86\u5404\u79cd\u7406\u8bba\u548c\u65b9\u6cd5\uff0c\u56e0\u6b64\u96be\u4ee5\u6bd4\u8f83\u8fd9\u4e9b\u5927\u91cf\u7684\u6d4b\u91cf\u6570\u636e\uff0c\u7f3a\u4e4f\u7edf\u4e00\u7684\u8bc4\u4f30\u6807\u51c6\u3002\u67d4\u6027\u5668\u4ef6\u7684\u7075\u6d3b\u6027\u901a\u5e38\u4e0d\u4ec5\u901a\u8fc7\u4f7f\u7528\u76f4\u89c2\u7684\u8f6f\u7535\u6781\u6750\u6599\u800c\u4e14\u901a\u8fc7\u4f18\u5316\u5176\u673a\u68b0\u7ed3\u6784\u8bbe\u8ba1\u6765\u5b9e\u73b0\u3002\u7ed3\u5408\u5b9e\u9a8c\u548c\u7406\u8bba\u7ed3\u679c\u8be6\u7ec6\u5206\u6790\u4e0d\u4ec5\u63d0\u4f9b\u4e86\u53ef\u9760\u7684\u6d4b\u8bd5\u65b9\u6cd5\u6765\u63cf\u8ff0\u5f2f\u66f2\u72b6\u6001\uff0c\u800c\u4e14\u63d0\u4f9b\u4e86\u7ec4\u4ef6\u8bbe\u8ba1\u7684\u6307\u5bfc\uff0c\u9632\u6b62\u4e86\u673a\u68b0\u6545\u969c\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92316\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/01-5.png\" alt=\"\" width=\"600\" height=\"582\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/01-5.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/01-5-300x291.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe1\u00a0\u5404\u79cd\u7c7b\u578b\u7684\u96c6\u6210\u67d4\u6027\u7535\u5b50\u5668\u4ef6<\/strong><\/p>\n<h3>2\u00a0\u50a8\u80fd\u88c5\u7f6e\u7684\u5f2f\u66f2\u529b\u5b66<\/h3>\n<p>\u5355\u7ec4\u5206\u7cfb\u7edf\u4e2d\uff0c\u5728\u5668\u4ef6\u4e0a\u65bd\u52a0\u5916\u90e8\u5f2f\u66f2\u884c\u4e3a\u4e4b\u540e\uff0c\u6574\u4e2a\u7ed3\u6784\u5468\u56f4\u4f1a\u51fa\u73b0\u7269\u7406\u53d8\u5f62\u3002 \u7136\u540e\uff0c\u4ea7\u751f\u5185\u90e8\u5e94\u529b\u4ee5\u62b5\u6297\u5f62\u72b6\u53d8\u5316\u3002\u5047\u8bbe\u4e0d\u5747\u5300\u4f4d\u7f6e\u5bb9\u6613\u4f7f\u5e94\u529b\u5c40\u90e8\u5316\uff0c\u6574\u4e2a\u88c5\u7f6e\u7684\u5e94\u529b\u5206\u5e03\u5e94\u662f\u5f02\u8d28\u7684\u3002\u6839\u636e\u80e1\u514b\u5b9a\u5f8b\uff0c\u5f39\u6027\u6a21\u91cf\u901a\u8fc7\u7ebf\u6027\u5f39\u6027\u8303\u56f4\u5185\u7684\u7b80\u5355\u6bd4\u4f8b\u4f7f\u5e94\u529b\u548c\u5e94\u53d8\u76f8\u5173\u3002<\/p>\n<p>LIB\u7531\u4e24\u4e2a\u5c01\u88c5\u5c42\uff0c\u4e24\u4e2a\u96c6\u7535\u5668\uff0c\u4e24\u4e2a\u7535\u6781\uff0c\u5206\u79bb\u5668\/\u7535\u89e3\u8d28\u7b49\u7ec4\u6210\u3002\u5982\u679c\u4f5c\u4e3a\u673a\u68b0\u6881\u7684\u57fa\u7247\u5f2f\u66f2\u5230\u534a\u5f84\u4e3aR\u7684\u5706\u67f1\u4f53\u4e2d\uff0c\u5219\u5916\u8868\u9762\u627f\u53d7\u62c9\u4f38\u5e94\u53d8\u5e76\u4e14\u5185\u8868\u9762\u627f\u53d7\u538b\u7f29\u5e94\u53d8\u3002\u5728\u8bbe\u5907\u5185\u90e8\u5b58\u5728\u6ca1\u6709\u5355\u8f74\u5e94\u53d8\u7684\u673a\u68b0\u4e2d\u6027\u5e73\u9762\uff0c\u8be5\u5e73\u9762\u7684\u4f4d\u7f6e\u4e0e\u6bcf\u4e2a\u5c42\u7684\u6768\u6c0f\u6a21\u91cf\u548c\u539a\u5ea6\u6709\u5173\u3002\u5c06\u521a\u6027\u819c\u653e\u7f6e\u5728\u673a\u68b0\u4e2d\u6027\u5e73\u9762\u4e0a\u53ef\u5b9e\u73b0\u8d85\u67d4\u6027\u3002\u8003\u8651\u5230\u6750\u6599\u6027\u80fd\uff08\u5982\u5f39\u6027\u6a21\u91cf\u548c\u6cca\u677e\u6bd4\uff09\u7684\u5dee\u5f02\uff0c\u5f2f\u66f2\u529b\u5b66\u5728\u591a\u5c42\u7ed3\u6784\u4e2d\u662f\u590d\u6742\u7684\u3002\u521a\u6027\u819c\u548c\u67d4\u6027\u886c\u5e95\u7684\u4e0d\u5339\u914d\u5bfc\u81f4\u4e86\u819c\u4e0a\u6216\u5c42\u4e4b\u95f4\u754c\u9762\u7684\u5e94\u529b\u96c6\u4e2d\u3002<\/p>\n<p>\u5f53\u83b7\u5f97\u7684\u5e94\u529b\u8d85\u8fc7\u8010\u53d7\u6027\u6781\u9650\u65f6\uff0c\u7ed3\u6784\u7684\u7834\u574f\uff08\u5982\u88c2\u7eb9\u6216\u5206\u5c42\uff09\u4f1a\u968f\u5176\u7535\u6027\u80fd\u7684\u5f31\u5316\u800c\u53d1\u751f\u3002\u5728\u805a\u916f\u57fa\u677f\u4e0a\u7684\u6c27\u5316\u94df\u9521\uff08ITO\uff09\u819c\u4e2d\uff0c\u7834\u574f\u4f4d\u7f6e\u5bb9\u6613\u5728\u7f3a\u9677\u90e8\u4f4d\u5f00\u59cb\uff0c\u88c2\u7eb9\u6269\u5c55\u5bf9\u5e94\u4e8e\u7535\u963b\u589e\u52a0\u7ea610\uff05\u3002\u6b64\u5916\uff0c\u62c9\u4f38\u548c\u538b\u7f29\u5f2f\u66f2\u7684\u5931\u6548\u6a21\u5f0f\u4e5f\u4e0d\u540c\u3002\u5728\u62c9\u4f38\u5e94\u53d8\u4e0b\uff0c\u5728\u7ec4\u5206\u5c42\u7684\u7f3a\u9677\u90e8\u4f4d\u51fa\u73b0\u88c2\u7f1d\u3002\u5728\u538b\u7f29\u5e94\u53d8\u4e0b\uff0c\u819c\u5bb9\u6613\u53d1\u751f\u5f2f\u66f2\uff0c\u5e76\u4e14\u526a\u5207\u5e94\u529b\u53ef\u4ee5\u4fc3\u4f7f\u88c2\u7eb9\u7684\u4ea7\u751f\u3002\u56e0\u6b64\uff0c\u538b\u7f29\u5e94\u53d8\u8010\u53d7\u6027\u4e0e\u7ed3\u5408\u5f3a\u5ea6\uff08\u7c98\u5408\u529b\uff09\u6210\u6b63\u6bd4\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92321\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/02-4.png\" alt=\"\" width=\"600\" height=\"503\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/02-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/02-4-300x252.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe2 \u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u7ed3\u6784\u548c\u5f2f\u66f2\u529b\u5b66\u793a\u610f\u56fe<\/strong><\/p>\n<h3 style=\"text-align: left;\">3\u00a0\u5f2f\u66f2\u72b6\u6001\u7684\u673a\u68b0\u8868\u5f81\u548c\u5206\u6790<\/h3>\n<p>\u5c3d\u7ba1\u51e0\u4e2a\u673a\u68b0\u7279\u5f81\u53ef\u4ee5\u63cf\u8ff0\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u5f2f\u66f2\u72b6\u6001\uff0c\u4f46\u6700\u7b80\u5355\u7684\u6027\u8d28\u662f\u5b83\u4eec\u5728\u7ed9\u5b9a\u534a\u5f84\u4e0b\u7684\u5f2f\u66f2\u8010\u4e45\u6027\u3002\u56e0\u6b64\uff0c\u5e94\u8be5\u83b7\u5f97\u9002\u5f53\u7684\u53c2\u6570\uff0c\u5e76\u5f00\u53d1\u5176\u6d4b\u8bd5\u65b9\u6cd5\u548c\u8bbe\u5907\uff0c\u4ee5\u786e\u4fdd\u5728\u4e0d\u540c\u5f2f\u66f2\u72b6\u6001\u4e0b\u7684\u6d4b\u8bd5\u3002\u901a\u5e38\u4e09\u4e2a\u53c2\u6570\u53ef\u4ee5\u63cf\u8ff0\u8bbe\u5907\u7684\u5f2f\u66f2\u72b6\u6001\uff1a\uff081\uff09L\uff1a\u6cbf\u7740\u5f2f\u66f2\u65b9\u5411\u7684\u4e00\u7aef\u5230\u53e6\u4e00\u7aef\u8ddd\u79bb; \uff082\uff09\u03b8\uff1a\u5f2f\u66f2\u89d2\u5ea6; \uff083\uff09R\uff1a\u5f2f\u66f2\u66f2\u7387\u534a\u5f84\u3002<\/p>\n<h4>3.1 \u4e24\u7aef\u7684\u8ddd\u79bb\uff08L\uff09<\/h4>\n<p>L\u88ab\u5b9a\u4e49\u4e3a\u6cbf\u7740\u5f2f\u66f2\u65b9\u5411\u7684\u4e24\u7aef\u4e4b\u95f4\u7684\u8ddd\u79bb\u3002\u65e0\u8bba\u8bbe\u5907\u7684\u5f62\u72b6\u5982\u4f55\uff0c\u5305\u62ec\u4f20\u7edf\u7684\u7247\u72b6\u8bbe\u5907\u548c\u5177\u6709\u65b0\u9896\u7ed3\u6784\u8bbe\u8ba1\u7684\u7535\u5b50\u8bbe\u5907\uff0c\u8be5\u53c2\u6570\u90fd\u53ef\u5e94\u7528\u4e8e\u63cf\u8ff0\u5f2f\u66f2\u72b6\u6001\u3002L\u7684\u6d4b\u8bd5\u65b9\u6cd5\u7b80\u5355\uff0c\u53ef\u4ee5\u5728\u5927\u591a\u6570\u5b9e\u9a8c\u5ba4\u4e2d\u5b9e\u73b0\u3002L\u5728\u67d4\u6027LIB\u548cSCs\u4e0a\u7684\u5178\u578b\u5e94\u7528\u5982\u56fe3\u6240\u793a\u3002\u5728\u7535\u7f06\u578b\u67d4\u6027\u950c-\u7a7a\u6c14\u7535\u6c60\u4e2d\uff0c\u4ece\u521d\u59cbL\u4e3a7cm\u5230\u5f2f\u66f2\u52303cm\u5e76\u6062\u590d\u52307cm \uff0c\u671f\u95f4\u7684\u7535\u538b\u5728\u653e\u7535\u4e2d\u6ca1\u6709\u89c2\u5bdf\u5230\u660e\u663e\u7684\u5dee\u5f02\uff0c\u8868\u660e\u5916\u90e8\u5e94\u53d8\u4e0b\u826f\u597d\u7684\u673a\u68b0\u6027\u80fd\u3002<\/p>\n<p>\u5c3d\u7ba1\u64cd\u4f5c\u7b80\u5355\uff0c\u5e76\u4e14\u5e7f\u6cdb\u7528\u4e8e\u63cf\u8ff0\u67d4\u6027\u88c5\u7f6e\u7684\u5f2f\u66f2\u72b6\u6001\uff0c\u4f46L\u4ec5\u63d0\u4f9b\u5bf9\u5f2f\u66f2\u8fc7\u7a0b\u7684\u7b80\u5355\u7406\u89e3\uff0c\u5e76\u4e14\u4e0d\u9002\u5408\u4e8e\u5bf9\u83b7\u5f97\u7684\u5e94\u53d8\u548c\u6545\u969c\u6a21\u5f0f\u7684\u7efc\u5408\u5206\u6790\u3002\u5bf9\u4e8e\u5177\u6709\u4e0d\u5747\u5300\u673a\u68b0\u53d8\u5f62\u7684\u8d85\u8f6f\u548c\u8d85\u8584\u5668\u4ef6\uff0cL\u4e0d\u80fd\u63d0\u4f9b\u5f2f\u66f2\u72b6\u6001\u7684\u7cbe\u786e\u8868\u5f81\uff0c\u56e0\u4e3a\u5176\u5ffd\u7565\u4e86\u5cf0\u503c\u4f4d\u7f6e\u4e0a\u7684\u5b9e\u9645\u53d8\u5f62\u72b6\u6001\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92323\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/03-3.png\" alt=\"\" width=\"600\" height=\"402\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/03-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/03-3-300x201.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe3\u00a0 L\u5728\u67d4\u6027LIB\u548cSCs\u4e0a\u7684\u5178\u578b\u5e94\u7528 <\/strong><\/p>\n<h4>3.2\u00a0\u5f2f\u66f2\u89d2\u5ea6\uff08\u03b8\uff09<\/h4>\n<p>\u5f2f\u66f2\u89d2\u5ea6\u662f\u63cf\u8ff0\u5f2f\u66f2\u72b6\u6001\u7684\u53e6\u4e00\u4e2a\u5e38\u7528\u53c2\u6570\uff0c\u5176\u5b9a\u4e49\u4e3a\u79fb\u52a8\u7aef\u7684\u65cb\u8f6c\u89d2\u5ea6\u3002\u5728\u5f2f\u66f2\u89d2\u5ea6\u4e0d\u540c\u7684\u5f2f\u66f2\u72b6\u6001\u4e0b\u68c0\u6d4b\u6cb9\u58a8\u78b3\u6750\u6599\u7ea4\u7ef4SC\u7684CV\u66f2\u7ebf\uff0c\u7535\u5bb9\u5728\u9ad8\u5f2f\u66f2\u89d2\u5ea6\u4e0b\u7565\u5fae\u4e0b\u964d\uff0c\u8fd9\u53ef\u80fd\u662f\u7531\u4e8e\u6cb9\u58a8\u78b3\u6750\u6599\u5728\u9ad8\u5f2f\u66f2\u72b6\u6001\u4e0b\u7684\u635f\u574f\u9020\u6210\u7684\u3002\u5c06\u5177\u6709\u8f83\u5c0f\u6297\u5f2f\u521a\u5ea6\u7684\u67d4\u6027\u88c5\u7f6e\u56fa\u5b9a\u5728\u57fa\u6750\u4e0a\u4ee5\u786e\u4fdd\u5747\u5300\u7684\u53d8\u5f62\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u6d4b\u91cf\u8bbe\u5907\u7684\u957f\u5ea6\u5728\u786e\u5b9a\u5f2f\u66f2\u89d2\u5ea6\u65f6\u4f1a\u5f71\u54cd\u6240\u83b7\u5f97\u7684\u5e94\u53d8\u3002\u4f8b\u5982\uff0c\u5bf9\u4e8e\u8d85\u957f\u8bbe\u5907\uff0c\u5f2f\u66f2\u5f62\u72b6\u7684\u5cf0\u503c\u4f4d\u7f6e\u7531\u4e8e\u5f2f\u66f2\u76f4\u5f84\u5927\u800c\u5b9e\u9645\u4e0a\u627f\u53d7\u5f2f\u66f2\u5e94\u53d8\u4e5f\u4e0d\u4f1a\u592a\u5927\uff0c\u6240\u4ee5\u4e0eL\u76f8\u4f3c\uff0c\u5f2f\u66f2\u89d2\u5ea6\u53c2\u6570\u53ea\u80fd\u7c97\u7565\u5730\u8bc4\u4f30\u5f2f\u66f2\u72b6\u6001\uff0c\u5408\u9002\u7684\u8bbe\u5907\u548c\u8be6\u7ec6\u7684\u6d4b\u91cf\u8fc7\u7a0b\u4ecd\u9700\u8981\u8fdb\u884c\u8c03\u8282\uff0c\u4ee5\u786e\u4fdd\u89d2\u5ea6\u51c6\u786e\u7684\u4fe1\u606f\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92348\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/04-3.png\" alt=\"\" width=\"600\" height=\"421\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/04-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/04-3-300x211.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe4\u00a0\u5f2f\u66f2\u89d2\u5ea6\u5178\u578b\u6d4b\u91cf\u65b9\u6cd5\u7684\u539f\u7406\u56fe\u548c\u56fe\u7247<\/strong><\/p>\n<h4>3.3\u00a0\u5f2f\u66f2\u534a\u5f84\uff08R\uff09<\/h4>\n<p>\u867d\u7136\u7aef\u5bf9\u7aef\u8ddd\u79bbL\u548c\u5f2f\u66f2\u89d2\u03b8\u6d4b\u91cf\u53ef\u4ee5\u4e3a\u8bbe\u5907\u7684\u5f2f\u66f2\u72b6\u6001\u63d0\u4f9b\u7b80\u5355\u76f4\u89c2\u7684\u53c2\u8003\uff0c\u4f46\u5e94\u8be5\u5f00\u53d1\u9002\u7528\u4e8e\u5927\u591a\u6570\u67d4\u6027\u8bbe\u5907\u7684\u9002\u5f53\u53c2\u6570\u548c\u4e00\u822c\u65b9\u6cd5\u6765\u6bd4\u8f83\u5176\u6027\u80fd\u53ef\u9760\u6027\u548c\u6545\u969c\uff0c\u4ee5\u6b64\u6765\u4e86\u89e3\u8bbe\u5907\u914d\u7f6e\u4e0e\u673a\u68b0\u6027\u80fd\u4e4b\u95f4\u7684\u5173\u7cfb\uff0c\u5e76\u4e3a\u67d4\u6027\u88c5\u7f6e\u7684\u7ed3\u6784\u8bbe\u8ba1\u63d0\u4f9b\u53ef\u884c\u7684\u6307\u5bfc\u3002\u5f2f\u66f2\u66f2\u7387\u534a\u5f84R\u9664\u4e86\u5668\u4ef6\u7684\u56fa\u6709\u5f39\u6027\u6a21\u91cf\u548c\u539a\u5ea6\u5916\uff0c\u4e0e\u8bbe\u5907\u7684\u5f2f\u66f2\u5e94\u53d8\u5bc6\u5207\u76f8\u5173\u3002 \u56e0\u6b64\uff0c\u5f2f\u66f2\u534a\u5f84\u662f\u63cf\u8ff0\u5f2f\u66f2\u72b6\u6001\u6700\u5408\u9002\u7684\u53c2\u6570\u3002 \u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u5df2\u7ecf\u63d0\u51fa\u4e86\u51e0\u79cd\u8ba1\u7b97\u548c\u6d4b\u91cf\u65b9\u6cd5\u6765\u83b7\u5f97\u534a\u5f84\u503c\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92351\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/05-2.png\" alt=\"\" width=\"600\" height=\"610\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/05-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/05-2-295x300.png 295w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe5\u00a0\u57fa\u4e8eN-PCPE\u7684\u7535\u6c60\u548c\u9502\u79bb\u5b50\u7535\u6c60<\/strong><\/p>\n<h4 style=\"text-align: left;\">3.4 \u5f2f\u66f2\u8bd5\u9a8c\u88c5\u7f6e<\/h4>\n<p>\u9664\u4e86\u6587\u732e\u4e2d\u63d0\u5230\u7684\u5f2f\u66f2\u8bd5\u9a8c\u7684\u624b\u52a8\u64cd\u4f5c\u4e4b\u5916\uff0c\u8fd8\u9700\u8981\u4e00\u79cd\u81ea\u52a8\u5316\u88c5\u7f6e\u6765\u786e\u4fdd\u5728\u6570\u767e\u6b21\u5f2f\u66f2\u8fd0\u52a8\u671f\u95f4\u5f2f\u66f2\u53c2\u6570\u6570\u636e\u7684\u53ef\u9760\u6027\u3002\u7528\u4e8e\u5f2f\u66f2\u8bd5\u9a8c\u7684\u88c5\u7f6e\u901a\u5e38\u88ab\u8bbe\u8ba1\u6210\u6267\u884c\u591a\u6b21\u91cd\u590d\u7684\u5f2f\u66f2\u8fd0\u52a8\uff0c\u5e76\u4e14\u53ef\u4ee5\u4fdd\u8bc1\u79fb\u52a8\u901f\u5ea6\u548c\u7a0b\u5ea6\/\u957f\u5ea6\u7684\u7cbe\u5ea6\u3002\u67d4\u6027\u5668\u4ef6\u7535\u5316\u5b66\u7279\u6027\u7684\u539f\u4f4d\u6d4b\u91cf\u5728\u673a\u68b0\u5f2f\u66f2\u8fc7\u7a0b\u4e2d\u662f\u9996\u9009\u7684\uff0c\u5305\u62ecSC\u7684CV\u66f2\u7ebf\uff0cLIB\u7684\u5f00\u8def\u7535\u538b\u548c\u5bfc\u7535\u7535\u6781\u7684\u7535\u963b\u3002LIB\u7684\u5177\u4f53\u6027\u80fd\u548c\u7535\u5bb9\u7684\u6bd4\u5bb9\u91cf\u5728\u5145\u653e\u7535\u8fc7\u7a0b\u4e2d\u957f\u65f6\u95f4\u7684\u673a\u68b0\u53d8\u5f62\u540e\u4e5f\u5e94\u8be5\u6d4b\u91cf\u3002 \u56e0\u6b64\uff0c\u5e94\u901a\u8fc7\u7535\u6c14\u6027\u80fd\u53d8\u5316\u62a5\u544a\u6545\u969c\u7684\u60c5\u51b5\uff0c\u4ee5\u907f\u514d\u8bbe\u5907\u548c\u4eba\u5458\u64cd\u4f5c\u4ea7\u751f\u7684\u7cfb\u7edf\u9519\u8bef\u3002<\/p>\n<h4>3.5\u00a0\u6709\u9650\u5143\u5206\u6790<\/h4>\n<p>\u7efc\u5408\u8003\u5bdf\u53d8\u5f62\u529b\u5b66\uff0c\u53ef\u4ee5\u63ed\u793a\u590d\u6742\u7ed3\u6784\u67d4\u6027\u7535\u5b50\u88c5\u7f6e\u7684\u591a\u5c42\u548c\u4e09\u7ef4\u7ed3\u6784\u8bbe\u8ba1\u7684\u5e94\u53d8\u5206\u5e03\u548c\u6307\u5bfc\u539f\u5219\u3002\u7136\u800c\uff0c\u5bf9\u590d\u6742\u7ed3\u6784\u96c6\u6210\u53ef\u53d8\u5f62\u7535\u5b50\u8bbe\u5907\uff08\u5982\u6298\u7eb8\u7535\u5b50\u8bbe\u5907\uff09\u7684\u8be6\u7ec6\u53d8\u5f62\u8fc7\u7a0b\u63d0\u4f9b\u660e\u786e\u7684\u6570\u5b66\u5206\u6790\u662f\u56f0\u96be\u7684\u3002\u56e0\u6b64\uff0c\u9009\u62e9\u4f5c\u4e3a\u6570\u503c\u65b9\u6cd5\u7684\u6709\u9650\u5143\u5206\u6790\uff08FEA\uff09\u65b9\u6cd5\uff0c\u901a\u8fc7\u62df\u5408\u548c\u7ec4\u5408\u4e9a\u57fa\u7684\u4ee3\u6570\u65b9\u7a0b\uff0c\u4e3a\u590d\u6742\u51e0\u4f55\u7684\u67d4\u6027\u548c\u53ef\u62c9\u4f38\u88c5\u7f6e\u63d0\u4f9b\u4e86\u8fd1\u4f3c\u89e3\u3002FEA\u572820\u4e16\u7eaa40\u5e74\u4ee3\u521d\u88ab\u5f15\u5165\u65f6\u4e3b\u8981\u5206\u6790\u822a\u7a7a\u5de5\u7a0b\u7684\u590d\u6742\u7ed3\u6784\uff0c\u968f\u7740\u8ba1\u7b97\u673a\u6280\u672f\u7684\u8fdb\u6b65\uff0c\u8fc5\u901f\u53d1\u5c55\u3002\u6709\u9650\u5143\u6a21\u62df\u4e2d\uff0c\u5c06\u8fde\u7eed\u590d\u6742\u7ed3\u6784\u79bb\u6563\u5316\u4e3a\u4e00\u7ec4\u79bb\u6563\u5355\u5143\uff0c\u901a\u5e38\u79f0\u4e3a\u6709\u9650\u5143\uff0c\u6709\u9650\u5143\u7f51\u683c\u901a\u8fc7\u8fde\u63a5\u8fd9\u4e9b\u79bb\u6563\u6709\u9650\u5143\u7d20\u548c\u7ed3\u6784\u7279\u6027\u800c\u5f62\u6210\u3002\u6709\u9650\u5143\u7f51\u683c\u7684\u5bc6\u5ea6\u968f\u7740\u5e94\u529b\u7684\u53d8\u5316\u800c\u53d8\u5316\uff0c\u7ecf\u53d7\u9ad8\u5e94\u529b\u53d8\u5316\u7684\u7279\u5b9a\u533a\u57df\u9700\u8981\u6bd4\u5177\u6709\u8f83\u5c0f\u6216\u6ca1\u6709\u5e94\u529b\u53d8\u5316\u7684\u533a\u57df\u66f4\u9ad8\u7684\u7f51\u683c\u5bc6\u5ea6\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92353\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/06-1.png\" alt=\"\" width=\"600\" height=\"549\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/06-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/06-1-300x275.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe6\u00a0\u4e0d\u540c\u7535\u6781\u9635\u5217\u7684\u793a\u610f\u56fe<\/strong><\/p>\n<h3 style=\"text-align: left;\">4\u00a0\u67d4\u6027\u8bbe\u5907\u7684\u7ed3\u6784\u8981\u6c42\u548c\u8bbe\u8ba1<\/h3>\n<p>\u5668\u4ef6\u7684\u53d8\u5f62\u9650\u5236\u901a\u5e38\u53d6\u51b3\u4e8e\u83b7\u5f97\u7684\u5e94\u53d8\u4e0e\u6d3b\u6027\u6750\u6599\u7684\u8010\u53d7\u6027\u4e4b\u95f4\u7684\u5bf9\u5e94\u5173\u7cfb\u3002\u673a\u68b0\u53d8\u5f62\u8fc7\u7a0b\u5728\u5b9e\u9645\u5e94\u7528\u4e2d\u5f88\u590d\u6742\u3002\u56e0\u6b64\uff0c\u5bf9\u53d8\u5f62\u529b\u5b66\u548c\u7535\u6027\u80fd\u53d8\u5316\u7684\u8be6\u7ec6\u5206\u6790\u53ef\u4ee5\u6307\u5bfc\u67d4\u6027\u88c5\u7f6e\u7684\u8bbe\u8ba1\u3002<\/p>\n<h4>4.1\u00a0\u67d4\u6027\u57fa\u5e95\u548c\u819c<\/h4>\n<p>\u7535\u5b50\u819c\u901a\u5e38\u6c89\u79ef\u5728\u521a\u6027\u57fa\u5e95\u4e0a\u3002\u56e0\u6b64\uff0c\u5927\u591a\u6570\u5e94\u529b\u96c6\u4e2d\u5728\u6d3b\u6027\u819c\u6750\u6599\u4e0a\uff0c\u5e76\u4e14\u7535\u5b50\u5668\u4ef6\u4e0d\u80fd\u627f\u53d7\u663e\u8457\u7684\u5f2f\u66f2\u53d8\u5f62\u3002\u5f53\u819c\u7684\u6768\u6c0f\u6a21\u91cf\u5927\u4e8e\u886c\u5e95\u7684\u6768\u6c0f\u6a21\u91cf\u65f6\uff08E<sub>f<\/sub>&gt; E<sub>s<\/sub>\uff0c\u03c7&gt; 1\uff09\uff0c\u4e2d\u6027\u9762\u4ece\u4e2d\u5e73\u9762\u5411\u8584\u819c\u5c42\u79fb\u52a8\uff0c\u819c\u4e0a\u7684\u5e94\u53d8\u76f8\u5e94\u4e0b\u964d\u3002\u8fd9\u79cd\u6548\u5e94\u6fc0\u53d1\u4e86\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u5728\u4f4e\u6768\u6c0f\u6a21\u91cf\u7684\u5f39\u6027\u57fa\u5e95\u4e0a\u5370\u5237\u7535\u5b50\u8584\u819c\u6765\u51cf\u5c11\u5668\u4ef6\u5e94\u53d8\u7684\u601d\u8def\u3002\u4ee5\u8fd9\u79cd\u65b9\u5f0f\uff0c\u5f39\u6027\u57fa\u5e95\u627f\u53d7\u4e86\u5927\u90e8\u5206\u5f2f\u66f2\u5e94\u53d8\uff0c\u800c\u4e14\u5668\u4ef6\u7684\u6700\u5927\u5e94\u53d8\u6781\u9650\u4e3b\u8981\u53d6\u51b3\u4e8e\u57fa\u5e95\u7684\u67d4\u6027\u3002\u901a\u8fc7\u4f18\u5316\u6d3b\u6027\u7535\u6781\u6750\u6599\u7684\u7ed3\u6784\u914d\u7f6e\uff0c\u53ef\u4ee5\u514b\u670d\u5b83\u4eec\u7684\u5c40\u9650\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92355\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/07-1.png\" alt=\"\" width=\"600\" height=\"390\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/07-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/07-1-300x195.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe7\u00a0\u67d4\u6027\u77f3\u58a8\u7535\u6781\u7684\u56fe\u7247<\/strong><\/p>\n<h4 style=\"text-align: left;\">4.2 \u7ec4\u4ef6\u5c42\u539a\u5ea6<\/h4>\n<p>\u5b9e\u9a8c\u6240\u83b7\u5f97\u7684\u5f2f\u66f2\u72b6\u6001\u7684\u5e94\u53d8\u53ef\u4ee5\u901a\u8fc7\u51cf\u5c0f\u5c42\u539a\u800c\u7ebf\u6027\u51cf\u5c0f\u3002\u5bf9\u4e8e\u901a\u5e38\u7528\u4e8e\u67d4\u6027LIB\u548cSC\u7684\u539a\u5ea6\u8f83\u5c0f\u7684\u7eb3\u7c73\u7ea7\u6750\u6599\uff0c\u7531Eh<sup>3<\/sup>\/12\u7ed9\u51fa\u7684\u5f2f\u66f2\u521a\u5ea6\uff08E\u548ch\u5206\u522b\u8868\u793a\u5f39\u6027\u6a21\u91cf\u548c\u539a\u5ea6\uff09\u8fdc\u4f4e\u4e8e\u4f20\u7edf\u6750\u6599\uff0c \u5728\u5f2f\u66f2\u66f2\u7387\u534a\u5f84\u5c0f\u7684\u60c5\u51b5\u4e0b\uff0c\u5e94\u53d8\u6700\u5c0f\u3002Rogers\u7b49\u4eba\u63a2\u8ba8\u4e86\u8fd9\u4e00\u60f3\u6cd5\uff0c\u5e76\u53d1\u8868\u4e86\u4e00\u7cfb\u5217\u5173\u4e8e\u5c06\u5355\u6676\u7845\u5e26\u653e\u7f6e\u5728\u67d4\u6027\u57fa\u5e95\u4e0a\u5e76\u4f7f\u5176\u53ef\u62c9\u4f38\u7684\u62a5\u544a\u3002<\/p>\n<h4>4.3 \u5c01\u88c5\/\u673a\u68b0\u4e2d\u6027\u9762<\/h4>\n<p>\u673a\u68b0\u4e2d\u6027\u9762\u662f\u7a7f\u8fc7\u5668\u4ef6\u539a\u5ea6\u7684\u5e73\u9762\uff0c\u5728\u6700\u5c0f\u534a\u5f84\u66f2\u7387\u65f6\u6ca1\u6709\u5355\u8f74\u5f2f\u66f2\u5e94\u53d8\u3002\u5728\u6ca1\u6709\u5c01\u88c5\u5c42\u7684\u60c5\u51b5\u4e0b\uff0c\u673a\u68b0\u4e2d\u6027\u5e73\u9762\u901a\u5e38\u4f4d\u4e8e\u67d4\u6027\u57fa\u5e95\u4e2d\u800c\u4e0d\u662f\u51e0\u4f55\u4e2d\u5e73\u9762\uff0c\u8fd9\u662f\u7531\u4e8e\u7535\u6c14\u6750\u6599\u7684\u6a21\u91cf\u9ad8\u4e8e\u57fa\u5e95\u7684\u7f18\u6545\u3002Suo\u7b49\u4eba\u901a\u8fc7\u5f15\u5165\u5305\u542b\u57fa\u5e95\u548c\u5305\u5c01\u6750\u6599\u7684\u5939\u5c42\u7ed3\u6784\uff0c\u53ef\u4ee5\u8fdb\u4e00\u6b65\u964d\u4f4e\u5f2f\u66f2\u534a\u5f84\u3002\u6362\u53e5\u8bdd\u8bf4\uff0c\u901a\u8fc7\u5c06\u6ca1\u6709\u673a\u68b0\u5e94\u53d8\u7684\u4e2d\u6027\u5e73\u9762\u79fb\u52a8\u5230\u5177\u6709\u9ad8\u6297\u5f2f\u521a\u5ea6\u7684\u521a\u6027\u7535\u5c42\uff0c\u53ef\u4ee5\u63d0\u9ad8\u5f2f\u66f2\u6027\u80fd\uff0c\u8be5\u65b9\u6cd5\u53ef\u4ee5\u6307\u5bfc\u8bbe\u5907\u914d\u7f6e\u7684\u5b9e\u9a8c\u8bbe\u8ba1\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-92358\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/08-1.png\" alt=\"\" width=\"600\" height=\"363\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/08-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/08-1-300x182.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe8\u00a0\u5e94\u53d8\u51fd\u6570\u4ee5\u53ca\u8d85\u8584\u67d4\u6027Si-CMOS\u7535\u8def\u7684\u56fe\u50cf<\/strong><\/p>\n<h4 style=\"text-align: left;\">4.4 \u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u7ed3\u6784\u8bbe\u8ba1<\/h4>\n<p>\u67d4\u6027\u548c\u53ef\u62c9\u4f38\u7684\u7535\u5b50\u4ea7\u54c1\uff0c\u901a\u8fc7\u5408\u7406\u5229\u7528\u529b\u5b66\u548c\u7ed3\u6784\u8bbe\u8ba1\uff0c\u4e3a\u65e5\u5e38\u78e8\u635f\u63d0\u4f9b\u4e86\u4f18\u5f02\u7684\u9002\u5e94\u6027\uff0c\u751a\u81f3\u53ef\u4ee5\u4fee\u8865\u4eba\u4f53\u76ae\u80a4\u5e76\u8fdb\u5165\u4eba\u4f53\u3002 \u6700\u8fd1\uff0c\u4e00\u4e9b\u5173\u4e8e\u7ed3\u6784\u8bbe\u8ba1\u7684\u65b0\u60f3\u6cd5\u5df2\u7ecf\u88ab\u5f15\u5165\u5230\u4e86\u67d4\u6027\u7535\u5b50\u5b66\u4e2d\uff0c\u5e76\u4e14\u5728\u5177\u6709\u65b0\u9896\u7535\u8def\u914d\u7f6e\u7684\u53ef\u53d8\u5f62\u67d4\u6027LIB\u548cSC\u4e0a\u5df2\u7ecf\u53d6\u5f97\u4e86\u663e\u8457\u7684\u8fdb\u6b65\uff0c\u4f8b\u5982\u7535\u7ebf\/\u7535\u7f06\u56fe\u6848\uff0c\u6298\u7eb8\u8bbe\u8ba1\u548c\u6865\u5c9b\u8bbe\u8ba1 \uff0c\u901a\u8fc7\u4f7f\u7528\u590d\u6742\u7684\u673a\u68b0\u8bbe\u8ba1\u7b56\u7565\u7b49\u3002<\/p>\n<h3>5 \u603b\u7ed3\u4e0e\u5c55\u671b<\/h3>\n<p>\u4f5c\u4e3a\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u7684\u91cd\u8981\u7ec4\u6210\u90e8\u5206\uff0c\u67d4\u6027\u80fd\u6e90\uff08\u5305\u62ecLIB\u548cSC\uff09\u53d7\u5230\u4e86\u6781\u5927\u7684\u5173\u6ce8\u3002\u5efa\u7acb\u53ef\u9760\u7684\u67d4\u6027\u8868\u5f81\u662f\u63d0\u9ad8\u67d4\u6027\u80fd\u6e90\u673a\u68b0\u6027\u80fd\u7684\u5148\u51b3\u6761\u4ef6\u3002\u5bf9\u4e8e\u63cf\u8ff0\u5f2f\u66f2\u72b6\u6001\u7684\u53c2\u6570\uff0c\u5f2f\u66f2\u66f2\u7387\u534a\u5f84R\u662f\u9996\u9009\u7684\uff0c\u5177\u6709\u7ed9\u5b9a\u534a\u5f84\u7684\u5fc3\u8f74\u65b9\u6cd5\u5728\u6d4b\u91cfR\u7684\u5404\u79cd\u65b9\u6cd5\u4e2d\u662f\u6700\u51c6\u786e\u7684\uff0c\u56e0\u4e3a\u5b83\u7b80\u4fbf\uff0c\u5e76\u4e14\u4e0d\u8bba\u5f62\u72b6\u548c\u5c3a\u5bf8\u3002\u6b64\u5916\uff0c\u5bf9\u5f2f\u66f2\u529b\u5b66\u7684\u6df1\u5165\u5206\u6790\u53ef\u4ee5\u4e3a\u8bbe\u5907\u7684\u7ed3\u6784\u8bbe\u8ba1\u63d0\u4f9b\u5408\u7406\u7684\u6307\u5bfc\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/wol1\/doi\/10.1002\/aenm.201700535\/abstract\" target=\"_blank\" rel=\"noopener noreferrer\">Mechanical Analyses and Structural Design Requirements for Flexible Energy Storage Devices<\/a><span style=\"color: #ff0000;\"><span style=\"color: #000000;\">\uff08Adv. Energy Mater.,2017,DOI :10.1002\/aenm.201700535\uff09<\/span><\/span><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u65b0\u80fd\u6e90\u7ec4Allen\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002\u53c2\u4e0e\u65b0\u80fd\u6e90\u8bdd\u9898\u8ba8\u8bba\u8bf7\u52a0\u5165\u201c\u6750\u6599\u4eba\u65b0\u80fd\u6e90\u6750\u6599\u4ea4\u6d41\u7fa4 422065952\u201d\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8\u5927\u5bb6\u5ead<\/a>\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1axiaofire-18\uff0c\u5434\u73ab\uff0c\u6211\u4eec\u4f1a\u62c9\u5404\u4f4d\u8001\u5e08\u52a0\u5165\u4e13\u5bb6\u7fa4\u3002<\/strong><\/p>\n<p><strong>\u4eea\u5668\u8bbe\u5907\u3001\u8bd5\u5242\u8017\u6750\u3001\u6750\u6599\u6d4b\u8bd5\u3001\u6570\u636e\u5206\u6790\uff0c\u627e<a href=\"http:\/\/mai.cailiaoren.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6750\u6599\u4eba<\/a>\u3001\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u4e3a\u63d0\u9ad8\u67d4\u6027\u7535\u5b50\u5143\u4ef6\u7684\u96c6\u6210\u5ea6\uff0c\u975e\u5e38\u9700\u8981\u5177\u6709\u51fa\u8272\u673a\u68b0\u53d8\u5f62\u6027\u80fd\u7684\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u3002\u4e0e\u4f20\u7edf\u7535\u6e90\u4e0d\u540c\uff0c\u67d4\u6027\u50a8\u80fd\u88c5\u7f6e\u7684\u673a\u68b0\u53ef\u9760\u6027\uff0c\u5305\u62ec\u7535\u6c14\u6027\u80fd\u548c\u53d8\u5f62\u8010\u529b\u53d7\u5230\u4e86\u5f88\u591a\u5173\u6ce8&#8230;<\/p>\n","protected":false},"author":349,"featured_media":92361,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[533],"tags":[],"class_list":["post-91808","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zongshu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/91808"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/349"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=91808"}],"version-history":[{"count":11,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/91808\/revisions"}],"predecessor-version":[{"id":92502,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/91808\/revisions\/92502"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/92361"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=91808"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=91808"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=91808"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}