{"id":9256,"date":"2016-04-22T08:00:30","date_gmt":"2016-04-22T00:00:30","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=9256"},"modified":"2016-04-21T21:53:49","modified_gmt":"2016-04-21T13:53:49","slug":"%e9%a3%9e%e7%a7%92%e6%88%90%e5%83%8f-%e8%ae%b0%e5%bd%95%e7%83%ad%e9%87%8f%e5%9c%a8%e6%9d%90%e6%96%99%e5%86%85%e7%9a%84%e4%bc%a0%e6%92%ad%e8%bf%87%e7%a8%8b","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=9256","title":{"rendered":"\u201c\u98de\u79d2\u6210\u50cf\u201d\u2014\u8bb0\u5f55\u70ed\u91cf\u5728\u6750\u6599\u5185\u7684\u4f20\u64ad\u8fc7\u7a0b"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-9258\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/160415125941_1_540x360.jpg\" alt=\"160415125941_1_540x360\" width=\"540\" height=\"360\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/160415125941_1_540x360.jpg 540w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/04\/160415125941_1_540x360-300x200.jpg 300w\" sizes=\"(max-width: 540px) 100vw, 540px\" \/><\/p>\n<p><strong>\u6750\u6599\u725b\u6ce8\uff1a<\/strong>\u660e\u5c3c\u82cf\u8fbe\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u91c7\u7528\u6700\u5148\u8fdb\u7684\u8d85\u5feb\u7535\u5b50\u663e\u5fae\u955c\u9996\u6b21\u8bb0\u5f55\u4e0b\u4e86\u70ed\u91cf\u4ee5\u97f3\u901f\u7a7f\u8fc7\u7eb3\u7c73\u5c3a\u5bf8\u6750\u6599\u7684\u89c6\u9891\uff0c\u8fd9\u5bf9\u7406\u89e3\u6750\u6599\u5185\u90e8\u7684\u8fd0\u52a8\u5177\u6709\u91cd\u8981\u610f\u4e49\uff0c\u6709\u5229\u4e8e\u8bbe\u8ba1\u7814\u7a76\u51fa\u7528\u9014\u66f4\u5e7f\u6cdb\u7684\u6750\u6599\u3002<\/p>\n<p>\u80fd\u91cf\u5177\u6709\u591a\u79cd\u5f62\u5f0f\uff0c\u5176\u4e2d\u70ed\u662f\u6700\u5176\u5e38\u89c1\u7684\u5f62\u5f0f\u4e4b\u4e00\u3002\u70ed\u80fd\u662f\u8bf8\u5982\u7535\u529b\u4f20\u8f93\u4ee5\u53ca\u4ea4\u901a\u8fd0\u8f93\u7b49\u91cd\u8981\u573a\u5408\u4e2d\u80fd\u91cf\u635f\u5931\u7684\u6700\u4e3b\u8981\u5f62\u5f0f\u3002\u4f8b\u5982\uff0c\u6c7d\u8f66\u4e2d\u6c7d\u6cb9\u7684\u80fd\u91cf\u5ba4\u53cb70%\u4ee5\u70ed\u7684\u5f62\u5f0f\u635f\u8017\u6389\u7684\u3002\u56e0\u800c\uff0c\u5728\u516c\u5171\u57fa\u7840\u8bbe\u65bd\u5efa\u8bbe\u65f6\u5f80\u5f80\u4f1a\u8003\u8651\u5230\u6563\u70ed\u7b49\u95ee\u9898\u3002<\/p>\n<p>\u6750\u6599\u79d1\u5b66\u5bb6\u548c\u5de5\u7a0b\u5e08\u4eec\u65e9\u5df2\u5f00\u59cb\u7814\u7a76\u5982\u4f55\u5728\u539f\u5b50\u5c42\u9762\u4e0a\u63a7\u5236\u70ed\u80fd\uff0c\u5e0c\u671b\u80fd\u591f\u5c06\u70ed\u80fd\u8fdb\u884c\u5faa\u73af\u4f7f\u7528\u3001\u63d0\u9ad8\u80fd\u91cf\u4f7f\u7528\u6548\u7387\uff0c\u5e76\u6700\u7ec8\u51cf\u5c11\u5316\u77f3\u71c3\u6599\u7684\u4f7f\u7528\u3002\u53ea\u6709\u4e86\u89e3\u4e86\u70ed\u91cf\u7a7f\u8fc7\u6750\u6599\u7684\u8fc7\u7a0b,\u7814\u7a76\u624d\u4f1a\u6709\u8fdb\u4e00\u6b65\u7a81\u7834\u3002\u4e0d\u5c3d\u5982\u4eba\u610f\u7684\u662f\u6355\u83b7\u70ed\u91cf\u8fd0\u52a8\u8fd9\u4e00\u57fa\u672c\u7269\u7406\u8fc7\u7a0b\u7684\u6210\u50cf\u5e76\u4e0d\u662f\u4ef6\u6613\u4e8b\u3002\u8fd9\u662f\u56e0\u4e3a\u70ed\u91cf\u6210\u50cf\u65f6\u5206\u8fa8\u7387\u5e94\u5728\u7eb3\u7c73\u5c3a\u5bf8\u4e0a\uff0c\u800c\u70ed\u8fd0\u52a8\u7684\u901f\u5ea6\u5374\u8fbe\u6570\u82f1\u91cc\u6bcf\u79d2\uff0c\u8fd9\u65e0\u7591\u7ed9\u6210\u50cf\u5e26\u6765\u4e86\u5de8\u5927\u7684\u56f0\u96be\u3002<\/p>\n<p>\u4e3a\u4e86\u89e3\u51b3\u51fa\u73b0\u7684\u96be\u9898\uff0c\u5bf9\u70ed\u80fd\u7684\u8fd0\u52a8\u8fdb\u884c\u6210\u50cf\uff0c\u7814\u7a76\u4eba\u5458\u4f7f\u7528\u4e86\u4e00\u79cd\u5148\u8fdb\u7684\u8d85\u5feb\u7535\u5b50\u663e\u5fae\u955c\u3002\u5b83\u80fd\u5728\u6570\u98de\u79d2\u5185\u68c0\u6d4b\u5230\u6750\u6599\u5185\u90e8\u539f\u5b50\u548c\u5206\u5b50\u5c3a\u5ea6\u7684\u8fd0\u52a8\u3002\u5728\u8fd9\u9879\u7814\u7a76\u4e2d\uff0c\u4ed6\u4eec\u7528\u4e00\u4e2a\u7b80\u6613\u7684\u6fc0\u5149\u8109\u51b2\u6fc0\u53d1\u7535\u5b50\uff0c\u8fd9\u4e5f\u5feb\u901f\u52a0\u70ed\u4e86\u8054\u7852\u5316\u94a8\u548c\u9517\u6676\u4f53\u3002\u5c31\u6b64\uff0c\u4ed6\u4eec\u6355\u83b7\u5230\u4e86\u70ed\u80fd\u6ce2\u7a7f\u8fc7\u6676\u4f53\u7684\u6162\u52a8\u4f5c\u89c6\u9891\u3002<\/p>\n<p>\u6ce2\u9635\u9762\u7a7f\u900f\u6750\u6599\u7684\u8fc7\u7a0b\u770b\u8d77\u6765\u5c31\u5982\u540c\u77f3\u5934\u6389\u5165\u6c34\u4e2d\u6cdb\u8d77\u7684\u6d9f\u6f2a\u4e00\u822c\u3002\u89c6\u9891\u4e2d\u663e\u793a\u7684\u6ce2\u662f\u4ee56\u7eb3\u7c73\/\u76ae\u79d2\u7684\u901f\u5ea6\u79fb\u52a8\u3002\u6620\u5c04\u7684\u632f\u52a8\u80fd\u91cf\uff0c\u4e5f\u5373\u662f\u58f0\u5b50\uff0c\u5b83\u5bf9\u8be6\u7ec6\u7406\u89e3\u70ed\u8fd0\u52a8\u7684\u672c\u8d28\u6709\u5f88\u91cd\u8981\u7684\u4f5c\u7528\u3002<\/p>\n<p>\u79d1\u5b66\u5bb6\u4eec\u60f3\u4e86\u89e3\u3001\u63a7\u5236\u3001\u4ee5\u53ca\u5229\u7528\u70ed\u8fd0\u52a8\uff0c\u671f\u671b\u7cbe\u786e\u5f15\u5bfc\u5b83\u53bb\u5b8c\u6210\u6709\u7528\u7684\u5de5\u4f5c\u4ee5\u53ca\u5c06\u5b83\u5feb\u901f\u4ece\u654f\u611f\u7ec4\u4ef6\u79fb\u8d70\u3002\u7531\u4e8e\u70ed\u8fd0\u52a8\u5728\u65f6\u95f4\u5c3a\u5ea6\u6781\u5feb\uff0c\u5728\u7a7a\u95f4\u5c3a\u5ea6\u53c8\u6781\u5fae\u5c0f\uff0c\u56e0\u4e3a\u5145\u5206\u4e86\u89e3\u6750\u6599\u5185\u90e8\u7684\u70ed\u8fd0\u52a8\u90fd\u662f\u6781\u5176\u56f0\u96be\u7684\u3002<\/p>\n<p>\u6b64\u6b21\u89c2\u5bdf\u5230\u6ce2\u9635\u9762\u8fd0\u52a8\u7684\u89c6\u9891\u5c06\u6709\u52a9\u4e8e\u6211\u4eec\u7406\u89e3\u5176\u5185\u90e8\u8fd0\u52a8\u3002\u5b83\u5bf9\u5355\u4e2a\u539f\u5b50\u5728\u632f\u52a8\u6240\u626e\u6f14\u7684\u89d2\u8272\u548c\u7eb3\u7c73\u5c3a\u5ea6\u7279\u6027\u63d0\u4f9b\u4e86\u4e00\u4e2a\u5168\u65b0\u7684\u8ba4\u8bc6\uff0c\u8fd9\u53ef\u4ee5\u5e2e\u52a9\u5de5\u7a0b\u5e08\u66f4\u597d\u7684\u8bbe\u8ba1\u51fa\u7528\u9014\u66f4\u5e7f\u6cdb\u7684\u6750\u6599\u3002<\/p>\n<p>\u8be5\u9879\u7814\u7a76\u6700\u8fd1\u5df2\u53d1\u8868\u5728<a href=\"http:\/\/www.nature.com\/ncomms\/2016\/160415\/ncomms11230\/full\/ncomms11230.html\" target=\"_blank\">Nature Communications<\/a>\u4e0a\u3002<\/p>\n<p>\u5168\u6587\u53c2\u8003\u94fe\u63a5\uff1a<a href=\"https:\/\/www.sciencedaily.com\/releases\/2016\/04\/160415125941.htm\" target=\"_blank\">https:\/\/www.sciencedaily.com\/releases\/2016\/04\/160415125941.htm<\/a><\/p>\n<p>\u611f\u8c22\u6750\u6599\u4eba\u7f51\u7f16\u8f91\u90e8\u9ec4\u8bed\u5ae3\u4f9b\u7a3f\uff01<\/p>\n<p style=\"text-align: left;\">\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u660e\u5c3c\u82cf\u8fbe\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u91c7\u7528\u6700\u5148\u8fdb\u7684\u8d85\u5feb\u7535\u5b50\u663e\u5fae\u955c\u9996\u6b21\u8bb0\u5f55\u4e0b\u4e86\u70ed\u91cf\u4ee5\u97f3\u901f\u7a7f\u8fc7\u7eb3\u7c73\u5c3a\u5bf8\u6750\u6599\u7684\u89c6\u9891\uff0c\u8fd9\u5bf9\u7406\u89e3\u6750\u6599\u5185\u90e8\u7684\u8fd0\u52a8\u5177\u6709\u91cd\u8981\u610f\u4e49\uff0c\u6709\u5229\u4e8e\u8bbe\u8ba1\u7814\u7a76\u51fa\u7528\u9014&#8230;<\/p>\n","protected":false},"author":171,"featured_media":9258,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[113,31,33,32],"class_list":["post-9256","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-semiconductor","tag-dianzi","tag-nano","tag-film"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/9256"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/171"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=9256"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/9256\/revisions"}],"predecessor-version":[{"id":9297,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/9256\/revisions\/9297"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/9258"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=9256"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=9256"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=9256"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}