{"id":93805,"date":"2017-07-30T09:00:53","date_gmt":"2017-07-30T01:00:53","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=93805"},"modified":"2017-07-29T22:03:57","modified_gmt":"2017-07-29T14:03:57","slug":"cool-nasa%e5%8f%91%e6%98%8e%e5%8f%af%e4%bb%a5%e5%9c%a8%e7%81%ab%e6%98%9f%e4%b8%8a%e4%bd%bf%e7%94%a8%e7%9a%84%e6%91%a9%e6%93%a6%e7%ba%b3%e7%b1%b3%e5%8f%91%e7%94%b5%e6%9c%ba","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=93805","title":{"rendered":"Cool! NASA\u53d1\u660e\u53ef\u4ee5\u5728\u706b\u661f\u4e0a\u4f7f\u7528\u7684\u6469\u64e6\u7eb3\u7c73\u53d1\u7535\u673a"},"content":{"rendered":"<p><span style=\"color: #3366ff;\"><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/span><\/p>\n<p>\u63a2\u7d22\u706b\u661f\u662f\u4eba\u7c7b\u957f\u4e45\u4ee5\u6765\u7684\u68a6\u60f3\uff0c\u8fc4\u4eca\u4e3a\u6b62\u5df2\u6709\u56db\u53f0\u63a2\u6d4b\u8f66\u6210\u529f\u767b\u9646\u706b\u661f\uff0c\u5176\u4e2d\u7684\u4e24\u53f0\u4ecd\u5728\u6267\u884c\u4efb\u52a1\u3002\u7535\u529b\u7684\u751f\u4ea7\u548c\u7ba1\u7406\u5bf9\u4e8e\u706b\u661f\u8f66\u7eed\u822a\u3001\u4eea\u5668\u8fd0\u884c\u4ee5\u53ca\u4e0e\u5730\u7403\u901a\u8baf\u662f\u81f3\u5173\u91cd\u8981\u7684\u3002\u800c\u5e38\u7528\u7684\u592a\u9633\u80fd\u7535\u6c60\u548c\u653e\u5c04\u6027\u540c\u4f4d\u7d20\u53d1\u7535\u673a\uff08RTG\uff09\u5177\u6709\u4e00\u5b9a\u7684\u5c40\u9650\u6027\u3002\u5728\u706b\u661f\u4e0a\uff0c\u9891\u9891\u5149\u987e\u7684\u6c99\u5c18\u66b4\u4e0d\u4ec5\u4f1a\u963b\u6321\u592a\u9633\u5149\u5165\u5c04\uff0c\u8fd8\u4f1a\u6781\u5927\u5730\u51cf\u5c11\u706b\u661f\u8868\u9762\u592a\u9633\u5149\u5f3a\u5ea6\u3002\u539a\u539a\u7684\u7c89\u5c18\u8986\u76d6\u5728\u592a\u9633\u80fd\u7535\u6c60\u677f\u4e0a\u4f1a\u81f4\u4f7f\u5176\u65e0\u6cd5\u6709\u6548\u5de5\u4f5c\u3002\u5b63\u8282\u6027\u7684\u9633\u5149\u4e0b\u964d\u548c\u5317\u6781\u5730\u533a\u7684\u4f4e\u9633\u5149\u5f3a\u5ea6\u4e5f\u6210\u4e3a\u9650\u5236\u56e0\u7d20\u3002\u5c3d\u7ba1RTG\u7684\u8f93\u51fa\u7a33\u5b9a\uff0c\u4f46\u662f\u906d\u9047\u7206\u70b8\u3001\u8fdb\u5165\u5927\u6c14\u5c42\u3001\u4e0b\u964d\u548c\u7740\u9646\u7b49\u6781\u7aef\u6761\u4ef6\u65f6\u4ecd\u53ef\u80fd\u9020\u6210\u653e\u5c04\u6027\u6c61\u67d3\u3002\u6b64\u5916\uff0c\u653e\u5c04\u6027\u540c\u4f4d\u7d20\u7684\u5236\u9020\u548c\u4f7f\u7528\u5728\u4e16\u754c\u8303\u56f4\u5185\u662f\u8fdd\u53cd\u653e\u5c04\u6027\u8d44\u6e90\u7684\u51cf\u6392\u548c\u63a7\u5236\u534f\u8bae\u7684\u3002\u56e0\u6b64\uff0c\u4eba\u7c7b\u8feb\u5207\u9700\u8981\u53ef\u6301\u7eed\u7a33\u5b9a\u7684\u7535\u6e90\u7cfb\u7edf\u6765\u5f25\u8865\u5f53\u524d\u706b\u661f\u80fd\u6e90\u53d1\u7535\u7cfb\u7edf\u7684\u4e0d\u8db3\u3002<\/p>\n<p>\u5c3d\u7ba1\u7535\u78c1\u53d1\u7535\u673a\u662f\u5730\u7403\u4e0a\u6700\u53d7\u6b22\u8fce\u7684\u673a\u68b0\u80fd\u91cf\u6536\u96c6\u5668\uff0c\u4f46\u662f\u8fd9\u79cd\u91cd\u91cf\u578b\u7684\u53d1\u7535\u673a\u6781\u5927\u5730\u9650\u5236\u4e86\u706b\u661f\u63a2\u6d4b\u7684\u53d1\u5c04\u3001\u63a8\u8fdb\u6210\u672c\u4ee5\u53ca\u65c5\u884c\u65f6\u95f4\u3002\u65e5\u76ca\u5174\u8d77\u7684\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\uff08TENG\uff09\u5177\u6709\u8f7b\u8d28\u5316\u548c\u8f93\u51fa\u529f\u7387\u5927\u7684\u4f18\u826f\u7279\u6027\uff0c\u8fd9\u4f7f\u5f97\u5176\u6709\u671b\u6210\u4e3a\u706b\u661f\u4e0a\u8fdb\u884c\u673a\u68b0\u80fd\u91cf\u6536\u96c6\u7684\u5f3a\u6709\u529b\u7684\u66ff\u4ee3\u8005\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/span><\/p>\n<p>\u8fd1\u65e5\uff0cNASA\u7814\u7a76\u5458Jin-Woo Han\uff08\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u5229\u7528\u706b\u661f\u6a21\u62df\u6c14\u8c61\u5ba4\uff0c\u6df1\u5165\u7814\u7a76\u4e86\u706b\u661f\u4e0a\u7684\u5404\u79cd\u73af\u5883\u56e0\u7d20\u5bf9TENG\u8f93\u51fa\u6027\u80fd\u7684\u5f71\u54cd\u3002\u5e76\u6839\u636e\u5b9e\u9a8c\u7ed3\u679c\uff0c\u5bf9TENG\u5e94\u7528\u4e8e\u706b\u661f\u63a2\u6d4b\u7684\u524d\u666f\u7ed9\u4e88\u4e86\u5408\u7406\u5c55\u671b\u3002\u8be5\u6210\u679c\u4ee5\u201cTriboelectric nanogenerator for Mars environment\u201d\u4e3a\u9898\u4e8e2017\u5e747\u6708\u53d1\u8868\u4e8eNano Energy\u4e0a\u3002<\/p>\n<p>\u4ee5\u4e0b\u662f\u6587\u7ae0\u7684\u56fe\u6587\u89e3\u8bfb\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u3010\u56fe\u6587\u89e3\u8bfb\u3011<\/strong><\/span><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u706b\u661f\u4e0a\u7684\u73af\u5883\u56e0\u7d20<\/strong><\/span><\/p>\n<p>\u5982\u88681\u6240\u793a\uff0c\u5730\u7403\u4e0e\u706b\u661f\u7684\u73af\u5883\u5dee\u5f02\u53ef\u5206\u4e3a\u4ee5\u4e0b\u4e94\u4e2a\u56e0\u7d20\u3002\u7b2c\u4e00\uff0c\u706b\u661f\u7684\u5927\u6c14\u538b\u529b\u4f4e\u4e8e\u5730\u7403\uff1b\u7b2c\u4e8c\uff0c\u706b\u661f\u5927\u6c14\u7684\u4e3b\u8981\u6210\u5206\u662fCO<sub>2<\/sub>\uff1b\u7b2c\u4e09\uff0c\u706b\u661f\u6c14\u6e29\u4f4e\u4e8e\u5730\u7403\u6c14\uff1b\u7b2c\u56db\uff0c\uff0c\u706b\u661f\u8868\u9762\u7684\u7d2b\u5916\u7ebf\u5f3a\u5ea6\u6bd4\u5730\u7403\u9ad8\u51fa7-8\u500d\uff1b\u7b2c\u4e94\uff0c\u706b\u661f\u4e0a\u7684\u03b3\u5c04\u7ebf\u8f90\u5c04\u5f3a\u5ea6\u6bd4\u5730\u7403\u5927\u7ea6\u4e09\u4e2a\u6570\u91cf\u7ea7\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u88681\u5730\u7403\u548c\u706b\u661f\u73af\u5883\u56e0\u7d20\u7684\u5b9a\u91cf\u6bd4\u8f83<\/strong><\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-93820\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/11-6.png\" alt=\"\" width=\"680\" height=\"353\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/11-6.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/11-6-300x156.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u706b\u661f\u6a21\u62df\u6c14\u8c61\u5ba4<\/strong><\/span><\/p>\n<p>\u5efa\u7acb\u706b\u661f\u6a21\u62df\u6c14\u8c61\u5ba4\u7684\u76ee\u7684\u662f\u5728\u5408\u7406\u7684\u73af\u5883\u6761\u4ef6\u4e0b\u5206\u6790TENG\u7684\u8f93\u51fa\u6027\u80fd\u3002\u9664\u4e86\u9759\u6001\u6027\u80fd\u5916\uff0c\u8fd8\u53ef\u4ee5\u89c2\u5bdf\u5230\u52a8\u6001\u73af\u5883\u56e0\u7d20\u5bf9\u8f93\u51fa\u6027\u80fd\u9020\u6210\u7684\u5b9e\u65f6\u53d8\u5316\u3002\u5982\u56fe1A\u6240\u793a\uff0c\u8be5\u6c14\u8c61\u5ba4\u7531\u949f\u5f62\u7f50\u548c\u91d1\u5c5e\u76d6\u7ec4\u6210\uff0cTENG\u5b89\u88c5\u5728\u60ac\u6302\u7684\u4e9a\u683c\u529b\u677f\u4e0a\u3002\u56fa\u4f53CO<sub>2<\/sub>\u548c\u9664\u6e7f\u5242\u88ab\u653e\u7f6e\u5728\u6c14\u8c61\u5ba4\u5185\u4ee5\u6a21\u62df\u706b\u661f\u4e0a\u7684CO<sub>2<\/sub>\u6c1b\u56f4\u548c\u6781\u5ea6\u5e72\u71e5\u7684\u73af\u5883\u3002\u5c06\u6574\u4e2a\u6c14\u8c61\u5ba4\u653e\u7f6e\u5728\u7edd\u70ed\u5305\u88c5\u4e2d\u4ee5\u4f7f\u6e29\u5ea6\u53d1\u751f\u6574\u4f53\u6539\u53d8\u3002<\/p>\n<p>\u7531\u7535\u78c1\u632f\u52a8\u5668\u4ea7\u751f\u7684\u673a\u68b0\u80fd\u901a\u8fc7\u673a\u68b0\u9988\u901a\u4f20\u9012\u5230TENG\u3002TENG\u4e0a\u4e0b\u7535\u6781\u53d1\u751f\u6301\u7eed\u7684\u63a5\u89e6\u5206\u79bb\u8fd0\u52a8\uff0c\u8fdb\u800c\u4ea7\u751f\u8f93\u51fa\u529f\u7387\u3002TENG\u5904\u4e8e\u63a5\u89e6\u72b6\u6001\u65f6\uff0c\u4e0a\u7535\u6781\u4e0e\u4e0b\u90e8\u7684PDMS\u6469\u64e6\u8d77\u7535\u5c42\u76f8\u63a5\u89e6\uff0c\u5bfc\u81f4\u9876\u90e8\u805a\u79ef\u5927\u91cf\u7684\u6b63\u7535\u8377\u3002\u968f\u7740\u4e0a\u4e0b\u4e24\u4e2a\u7535\u6781\u7684\u5206\u79bb\uff0c\u4e0a\u7535\u6781\u7684\u6b63\u7535\u8377\u8f6c\u79fb\u5230\u4e0b\u7535\u6781\u3002\u7535\u8377\u5206\u5e03\u7684\u53d8\u5316\u5bfc\u81f4\u4e0a\u4e0b\u4e24\u7535\u6781\u4e4b\u95f4\u4ea7\u751f\u7535\u4f4d\u5dee\uff08\u5373\u7535\u538b\uff09\u548c\u7535\u8377\u6d41\uff08\u5373\u7535\u6d41\uff09\u3002\u5982\u56fe1B\u6240\u793a\uff0c\u706b\u661f\u6a21\u62df\u6c14\u8c61\u5ba4\u4e2d\u7684TENG\u7684\u8f93\u51fa\u7279\u6027\u5177\u6709\u826f\u597d\u7684\u53ef\u91cd\u590d\u6027\u3002\u5728\u6700\u9ad8\u8f93\u51fa\u6027\u80fd\u6761\u4ef6\u4e0b\uff0c\u5f00\u8def\u7535\u538b\uff08V<sub>OC<\/sub>\uff09\u7684\u5e73\u5747\u503c\u548c\u76f8\u5bf9\u6807\u51c6\u504f\u5dee\u503c\uff08RSD\uff09\u5206\u522b\u4e3a130.0 V\u548c0.9\uff05\u3002 \u5cf0\u503c\u77ed\u8def\u7535\u6d41\uff08I<sub>SC<\/sub>\uff09\u7684\u5e73\u5747\u503c\u548cRSD\u5206\u522b\u4e3a7.99 \u03bcA\u548c1.5\uff05\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u56fe<\/strong><strong>1. <\/strong><strong>\u706b\u661f\u6a21\u62df\u6c14\u8c61\u5ba4<\/strong><\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-93821\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/\u5fae\u4fe1\u622a\u56fe_20170729215405.png\" alt=\"\" width=\"707\" height=\"258\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/\u5fae\u4fe1\u622a\u56fe_20170729215405.png 707w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/\u5fae\u4fe1\u622a\u56fe_20170729215405-300x109.png 300w\" sizes=\"(max-width: 707px) 100vw, 707px\" \/><\/p>\n<p style=\"text-align: left;\">A) \u706b\u661f\u6a21\u62df\u6c14\u8c61\u5ba4\u7684\u914d\u7f6e\u56fe\u3002<\/p>\n<p style=\"text-align: left;\">(B) \u6469\u64e6\u7eb3\u7c73\u53d1\u7535\u673a\u7684\u8f93\u51fa\u5f00\u8def\u7535\u538b\u548c\u77ed\u8def\u7535\u6d41\u3002<\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u5927\u6c14\u538b\u529b\u548c\u6210\u5206\u7684\u5f71\u54cd<\/strong><\/span><\/p>\n<p>\u4e3a\u4e86\u533a\u5206\u5927\u6c14\u538b\u529b\u4e0e\u5927\u6c14\u6210\u5206\u5bf9TENG\u8f93\u51fa\u6027\u80fd\u7684\u5f71\u54cd\uff0c\u5bf9\u56db\u79cd\u73af\u5883\u60c5\u51b5\u8fdb\u884c\u4e86\u6d4b\u8bd5\uff08\u56fe2A\uff09\u3002\u4ece\u6d4b\u91cf\u7ed3\u679c\u6765\u770b\uff0cV<sub>OC<\/sub>\u5728\u8f83\u9ad8\u7684\u538b\u529b\u548cCO<sub>2<\/sub>\u6c14\u6c1b\u4e0b\u90fd\u8f83\u9ad8\u3002\u5730\u7403\u5927\u6c14\u73af\u5883\uff08\u7a7a\u6c14\uff0c760 Torr\uff09\u548c\u706b\u661f\u73af\u5883\uff08CO<sub>2<\/sub>\uff0c8 Torr\uff09\u4e2d\u7684\u7684\u5e73\u5747V<sub>OC<\/sub> \u5206\u522b\u4e3a\u5206\u522b\u4e3a44.0 V\u548c27.9 V\uff0c\u5373\u706b\u661f\u6c14\u6c1b\u4e0bV<sub>OC<\/sub>\u964d\u4f4e\u4e8637\uff05\u3002\u5982\u679c\u5c06TENG\u5c01\u88c5\u5728CO<sub>2<\/sub>\u6c1b\u56f4\u7684\u6c14\u8c61\u5ba4\u4e2d\uff0c\u4f7f\u6c14\u8c61\u5ba4\u5185\u7684\u538b\u529b\u4fdd\u6301\u5728760 Torr\uff0c\u6b64\u65f6\u7684\u8f93\u51fa\u6027\u80fd\u53ef\u63d0\u9ad8157\uff05\u3002<\/p>\n<p>\u5982\u56fe2B\uff0c2C\u6240\u793a\uff0c V<sub>OC<\/sub>\u968f\u6c14\u538b\u53d8\u5927\u800c\u589e\u52a0\uff0c\u8fd9\u79cd\u53d8\u5316\u8d8b\u52bf\u5bf9\u4e8e\u7a7a\u6c14\u548cCO<sub>2<\/sub>\u6c14\u6c1b\u662f\u4e00\u81f4\u7684\uff0c\u5e76\u4e14\u5bf9\u4e8e\u56fa\u5b9a\u7684\u538b\u529b\u503c\uff0cCO<sub>2<\/sub>\u6c14\u6c1b\u4e2d\u7684V<sub>OC<\/sub>\u90fd\u660e\u663e\u9ad8\u4e8e\u7a7a\u6c14\u6c1b\u56f4\u4e2d\u7684V<sub>OC<\/sub>\u3002\u5f53\u4e0a\u4e0b\u7535\u6781\u5206\u79bb\u65f6\uff0c\u6b63\u8d1f\u6469\u64e6\u7535\u8377\u901a\u8fc7\u5468\u56f4\u73af\u5883\u53d1\u751f\u653e\u7535\uff0c\u56e0\u6b64\u603b\u7684\u6469\u64e6\u7535\u8377\u5bc6\u5ea6\u964d\u4f4e\u3002\u7535\u8377\u5f1b\u8c6b\u540e\u5269\u4f59\u7684\u6469\u64e6\u7535\u8377\u5bc6\u5ea6\u662fPaschen\u6781\u9650\u51b3\u5b9a\u7684\u3002\u5f53\u6c14\u538b\u4f4e\u81f3\u5927\u7ea610 Torr\u65f6\uff0c\u964d\u4f4e\u7684Paschen\u6781\u9650\u4f1a\u52a0\u901f\u7535\u8377\u5f1b\u8c6b\uff0c\u4ece\u800c\u4f7f\u5269\u4f59\u7535\u8377\u5bc6\u5ea6\u8fdb\u4e00\u6b65\u964d\u4f4e\uff0c\u6700\u7ec8\u5bfc\u81f4V<sub>OC<\/sub>\u51cf\u5c11\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u56fe2 \u5927\u6c14\u6761\u4ef6\u5bf9TENG\u8f93\u51fa\u6027\u80fd\u7684\u5f71\u54cd <\/strong><\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-93822\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/12-5.jpg\" alt=\"\" width=\"700\" height=\"196\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/12-5.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/12-5-300x84.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\uff08A\uff09\u4e0d\u540c\u5927\u6c14\u6761\u4ef6\u4e0b\u7684\u8f93\u51fa\u5f00\u8def\u7535\u538b\u968f\u65f6\u95f4\u7684\u53d8\u5316\u66f2\u7ebf\u3002<\/p>\n<p>(B) \u5f53\u5927\u6c14\u7531\u7a7a\u6c14\uff08\u9ed1\u8272\uff09\u6216CO<sub>2<\/sub>\uff08\u7ea2\u8272\uff09\u7ec4\u6210\u65f6\uff0c\u5f00\u8def\u7535\u538b\u968f\u5927\u6c14\u538b\u5f3a\u7684\u53d8\u5316\u66f2\u7ebf\u3002<\/p>\n<p>(C) \u5f53\u5927\u6c14\u7531\u4e8c\u6c27\u5316\u78b3\u7ec4\u6210\u65f6\uff0c\u5f00\u8def\u7535\u538b\u589e\u52a0\u7387\u968f\u5927\u6c14\u538b\u5f3a\u7684\u53d8\u5316\u66f2\u7ebf\u3002<\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u6e29\u5ea6\u5f71\u54cd<\/strong><\/span><\/p>\n<p>\u4e0e\u5730\u7403\u73af\u5883\u76f8\u6bd4\uff0c\u706b\u661f\u6c14\u8c61\u5ba4\u672a\u5c01\u88c5\u7684\u60c5\u51b5\u65f6V<sub>OC<\/sub>\u4e0b\u964d\u4e8617\uff05\uff0c\u5c01\u88c5\u65f6V<sub>OC<\/sub>\u4e0b\u964d\u4e8611\uff05\u3002 CO<sub>2<\/sub>\u6c14\u6c1b\u4e2d\u7684\u6e29\u5ea6\u4f9d\u8d56\u6027\u4e0e\u5148\u524d\u5728\u7a7a\u6c14\u73af\u5883\u4e2d\u6d4b\u5f97\u7684\u7ed3\u679c\u5e76\u4e0d\u76f8\u540c\uff0c\u8fd9\u610f\u5473\u7740TENG\u5bf9\u6e29\u5ea6\u7684\u4f9d\u8d56\u6027\u662f\u7531\u5927\u6c14\u6210\u5206\u548c\u5927\u6c14\u538b\u5f3a\u7efc\u5408\u5f71\u54cd\u7684\u7ed3\u679c\u3002\u4ece\u706b\u661f\u63a2\u8def\u8005\u6d4b\u91cf\u7684\u65f6\u95f4-\u6e29\u5ea6\u6570\u636e\u6765\u770b\uff0c\u706b\u661f\u4e0a\u4e00\u5929\u7684\u6e29\u5ea6\u53d8\u5316\u5728197K-261K\u4e4b\u95f4\u3002\u5728\u8fd9\u79cd\u60c5\u51b5\u4e0b\uff0c\u672a\u5c01\u88c5\u7684TENG\u5728\u4e2d\u5348\u65f6\u5206\u6709\u6700\u9ad8\u7684V<sub>OC<\/sub>\uff0825.0 V\uff09\uff0c\u5348\u591c\u65f6\u5206\u8fd9\u4e00\u503c\u964d\u5230\u6700\u4f4e\uff0820.2 V\uff09\u3002 \u76f8\u6bd4\u4e4b\u4e0b\uff0c\u5bc6\u5c01\u52a0\u538b\u6761\u4ef6\u4e0b\u7684TENG\u5728\u5348\u591c\u65f6\u5206\u62e5\u6709\u6700\u9ad8\u7684V<sub>OC<\/sub>\uff08117.4 V\uff09\uff0c\u4e2d\u5348\u65f6\u6bb5V<sub>OC<\/sub>\u964d\u5230\u6700\u4f4e\uff08108.9 V\uff09\u3002 \u603b\u4f53\u6765\u770b\uff0cTENG\u7684\u8f93\u51fa\u7279\u6027\u65e5\u95f4\u53d8\u5316\u76f8\u5bf9\u8f83\u5c0f\uff0c\u6ce2\u52a8\u572820\uff05\u4ee5\u5185\u3002\u8fd9\u79cd\u5c0f\u5e45\u5ea6\u7684\u6027\u80fd\u53d8\u5316\u610f\u5473\u7740\uff0cTENG\u5177\u6709\u4e0e\u592a\u9633\u80fd\u7535\u6c60\u677f\u76f8\u9002\u5e94\u7684\u7279\u6027\uff0c\u5373\u591c\u95f4\u6027\u80fd\u9000\u5316\u4e25\u91cd\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u56fe<\/strong><strong>3 <\/strong><strong>CO<sub>2<\/sub><\/strong><strong>\u6c14\u6c1b\u4e2d\u73af\u5883\u6e29\u5ea6\u5bf9<\/strong><strong>TENG<\/strong><strong>\u7684\u8f93\u51fa\u6027\u80fd\u7684\u5f71\u54cd<\/strong>\u3002<\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-93823\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/13.png\" alt=\"\" width=\"536\" height=\"828\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/13.png 536w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/13-194x300.png 194w\" sizes=\"(max-width: 536px) 100vw, 536px\" \/><\/p>\n<p>\uff08A\uff09\u672a\u5c01\u88c5\u65f6TENG\u8f93\u51fa\u6027\u80fd\u5bf9\u73af\u5883\u6e29\u5ea6\u7684\u4f9d\u8d56\u3002<\/p>\n<p>(B) \u5c01\u88c5\u4ee5\u540eTENG\u8f93\u51fa\u6027\u80fd\u5bf9\u73af\u5883\u6e29\u5ea6\u7684\u4f9d\u8d56\u3002<\/p>\n<p>(C) \u5c01\u88c5\u548c\u672a\u5c01\u88c5\u4e24\u79cd\u60c5\u51b5\u4e0b\uff0c\u706b\u661f\u73af\u5883\u4e2d\u7684\u4e00\u5929\u6ca1\u6e29\u5ea6\u53d8\u5316\u60c5\u51b5\u53ca\u9884\u671f\u7684TENG\u8f93\u51fa\u7279\u6027\u3002<\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u7d2b\u5916\u7ebf\u8f90\u5c04\u7684\u5f71\u54cd<\/strong><\/span><\/p>\n<p>\u5982\u56fe4\u6240\u793a\uff0cTENG\u66b4\u9732\u5728\u7d2b\u5916\u7ebf\u4e2d\u540e\uff0cV<sub>OC<\/sub>\u8fc5\u901f\u589e\u52a0\u3002\u5728\u8f90\u7167\u671f\u95f4\uff0cV<sub>OC<\/sub>\u589e\u901f\u9010\u6e10\u51cf\u6162\u76f4\u81f3\u9971\u548c\uff0c\u505c\u6b62\u7167\u5c04\u540eV<sub>OC<\/sub>\u9010\u6e10\u51cf\u5c11\u3002\u706b\u661f\u4e0a\u53ea\u6709\u767d\u5929\u6709\u7d2b\u5916\u7ebf\u8f90\u5c04\uff0c\u6211\u4eec\u7814\u7a76\u4e86\u591c\u95f4\u653e\u7535\u7279\u6027\uff0c\u5e76\u5c06\u5176\u4ece\u6d4b\u91cf\u4e0a\u5206\u4e3a\u4e24\u4e2a\u9636\u6bb5\u3002\u5728\u9ed1\u6697\u6761\u4ef6\u4e0b\uff0c\u524d3000s V<sub>OC<\/sub>\u964d\u4f4e\u4e8630\uff05\uff0c\u7136\u540e\u5728\u63a5\u4e0b\u6765\u768470\u5c0f\u65f6\u9010\u6e10\u964d\u4f4e\u81f3\u521d\u59cb\u72b6\u6001\u3002\u5728\u7d2b\u5916\u7ebf\u7167\u5c04\u671f\u95f4\u4f1a\u5f62\u6210\u8fc7\u591a\u7684\u7535\u8377\uff0c\u76f4\u5230\u7535\u8377\u4ea7\u751f\u901f\u7387\u548c\u653e\u7535\u901f\u7387\u8fbe\u5230\u5e73\u8861\u4e3a\u6b62\u3002\u8fd9\u4e9b\u7ed3\u679c\u8868\u660e\uff0c\u706b\u661f\u8868\u9762\u4e30\u5bcc\u7684\u7d2b\u5916\u7ebf\u8f90\u5c04\u5bf9\u4e8e\u63d0\u9ad8TENG\u7684\u8f93\u51fa\u6027\u80fd\u975e\u5e38\u6709\u5229\u3002V<sub>OC<\/sub>\u968fUV\u5f3a\u5ea6\u548c\u66dd\u5149\u65f6\u95f4\u589e\u52a0\u7387\u7684\u9971\u548c\u70b9\u548c\u8fbe\u5230\u9971\u548c\u70b9\u6240\u9700\u7684\u65f6\u95f4\u90fd\u589e\u52a0\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u56fe4. \u7d2b\u5916\u7ebf\u8f90\u5c04\u5bf9TENG\u8f93\u51fa\u6027\u80fd\u7684\u5f71\u54cd\u3002<\/strong><\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-93824\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/14-5.jpg\" alt=\"\" width=\"700\" height=\"468\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/14-5.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/14-5-300x201.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>(A) \u7d2b\u5916\u7ebf\u8f90\u7167\u524d\u3001\u8f90\u7167\u4e2d\u3001\u8f90\u7167\u540e\u7684\u8f93\u51fa\u7279\u6027\u3002<\/p>\n<p>(B) \u5728\u6674\u6717\u7684\u5929\u6c14\u60c5\u51b5\uff08\u7ea2\u8272\uff09\u548c\u9634\u6697\u7684\u5929\u6c14\u60c5\u51b5\uff08\u84dd\u8272\uff09\u4e0b\uff0c\u901a\u8fc7\u7d2b\u5916\u7ebf\u8f90\u7167\u540e\u7684\u653e\u7535\u7279\u6027\u3002<\/p>\n<p>(C) \u53cd\u590d\u8fdb\u884c\u7d2b\u5916\u8f90\u7167\u548c\u653e\u7535\u66f2\u7ebf\u7684\u91cd\u590d\u6027\u6d4b\u8bd5\u3002<\/p>\n<p>(D) \u4e0d\u540c\u7d2b\u5916\u7ebf\u5f3a\u5ea6\u548c\u66dd\u5149\u65f6\u95f4\u4e0b\u7684\u7684\u8f93\u51fa\u6027\u80fd\u589e\u52a0\u7387\u3002<\/p>\n<p><span style=\"color: #ff0000;\"><strong>\u03b3<\/strong><strong>\u8f90\u5c04\u7684\u5f71\u54cd<\/strong><\/span><\/p>\n<p>\u5728\u03b3\u5c04\u7ebf\u8f90\u5c04\u4e0b\uff0c V<sub>OC<\/sub>\u548cI<sub>SC<\/sub>\u5206\u522b\u589e\u957f3.6\uff05\u548c1.9\uff05\u3002\u4e0e\u5176\u4ed6\u73af\u5883\u56e0\u7d20\u76f8\u6bd4\uff0c\u8fd9\u4e00\u53d8\u5316\u7387\u5e76\u4e0d\u663e\u8457\u3002\u56e0\u6b64\uff0c\u706b\u661f\u7684\u4f3d\u9a6c\u8f90\u5c04\u4e0d\u662f\u8bbe\u8ba1TENG\u6240\u9700\u8003\u8651\u7684\u91cd\u8981\u95ee\u9898\uff0c\u4e5f\u4e0d\u4f1a\u6210\u4e3a\u9650\u5236\u56e0\u7d20\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u56fe<\/strong><strong>5<\/strong><strong>. <\/strong><strong>\u73af\u5883\u56e0\u7d20\u5bf9<\/strong><strong>TENG<\/strong><strong>\u8f93\u51fa\u6027\u80fd\u7684\u5f71\u54cd\u5c0f\u7ed3\u3002<\/strong><\/span><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-93826\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/15.png\" alt=\"\" width=\"620\" height=\"698\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/15.png 620w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/15-266x300.png 266w\" sizes=\"(max-width: 620px) 100vw, 620px\" \/><\/p>\n<p>(A) \u706b\u661f\u548c\u5730\u7403\u4e0a\u7684\u9884\u671f\u7684TENG\u8f93\u51fa\u6027\u80fd\u3002<\/p>\n<p>(B) \u706b\u661f\u6c14\u8c61\u5ba4\u4e2d\u7684TENG\u76f4\u63a5\u9a71\u52a8\u7684LED\uff0c\u4e0d\u9700\u8981\u4efb\u4f55\u5b58\u50a8\u5143\u4ef6\u548c\u7535\u8def\u3002<\/p>\n<p><span style=\"color: #3366ff;\"><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/span><\/p>\n<p>\u73af\u5883\u56e0\u7d20\u5bf9TENG\u6027\u80fd\u7684\u5f71\u54cd\u5982\u4e0b\uff1a<\/p>\n<ol>\n<li>CO<sub>2<\/sub>\u6c14\u6c1b\u3001\u4f4e\u6e29\u548c\u9ad8\u5f3a\u5ea6\u8868\u9762\u7d2b\u5916\u7ebf\u8f90\u5c04\u53ef\u4ee5\u63d0\u9ad8TENG\u7684\u8f93\u51fa\u6027\u80fd\uff1b<\/li>\n<li>\u4f4e\u6c14\u538b\u964d\u4f4eTENG\u7684\u8f93\u51fa\u6027\u80fd\uff1b<\/li>\n<li>\u03b3\u5c04\u7ebf\u8f90\u5c04\u5bf9TENG\u7684\u6027\u80fd\u51e0\u4e4e\u6ca1\u6709\u5f71\u54cd\u3002<\/li>\n<\/ol>\n<p>\u57fa\u4e8e\u672c\u7814\u7a76\u7684\u6df1\u5165\u5206\u6790\uff0c\u6211\u4eec\u6709\u7406\u7531\u7545\u60f3\uff1a\u5728\u672a\u6765\u7684\u706b\u661f\u63a2\u6d4b\u4e2d\uff0c\u5728\u9633\u5149\u5145\u8db3\u7684\u767d\u5929\uff0c\u592a\u9633\u80fd\u7535\u6c60\u662f\u53d1\u7535\u7684\u4e3b\u529b\uff0c\u800cTENG\u53ef\u4ee5\u4f5c\u4e3a\u5907\u7528\u7535\u6e90\u3002\u5f53\u906d\u9047\u957f\u671f\u7684\u6c99\u5c18\u66b4\u5929\u6c14\u65f6\uff0c\u592a\u9633\u80fd\u7535\u6c60\u65e0\u6cd5\u4ea7\u751f\u8db3\u591f\u7684\u7535\u529b\uff0c\u6b64\u65f6TENG\u5c06\u53d6\u800c\u4ee3\u4e4b\u6210\u4e3a\u4e3b\u8981\u7684\u7535\u6e90\u3002\u8fd9\u79cd\u4e92\u8865\u7684\u5149\u4f0f\u00ad-TENG\u6df7\u5408\u7cfb\u7edf\u5c06\u4e3a\u706b\u661f\u63a2\u6d4b\u548c\u4eba\u7c7b\u6816\u606f\u5730\u6301\u7eed\u63d0\u4f9b\u5145\u8db3\u7684\u7535\u529b\u3002<\/p>\n<p><strong>\u3010\u6587\u732e\u4fe1\u606f\u3011<\/strong><\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong>Triboelectric nanogenerator for Mars environment (Nano Energy, 2017, DOI: 10.1016\/j.nanoen.2017.07.004 )<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u65b0\u80fd\u6e90\u5c0f\u7ec4<strong>\u6674\u96ea<\/strong>\u6574\u7406\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<\/strong><a href=\"http:\/\/www.ceshigu.com\/\">\u6d4b\u8bd5\u8c37<\/a><strong>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u63a2\u7d22\u706b\u661f\u662f\u4eba\u7c7b\u957f\u4e45\u4ee5\u6765\u7684\u68a6\u60f3\uff0c\u8fc4\u4eca\u4e3a\u6b62\u5df2\u6709\u56db\u53f0\u63a2\u6d4b\u8f66\u6210\u529f\u767b\u9646\u706b\u661f\uff0c\u5176\u4e2d\u7684\u4e24\u53f0\u4ecd\u5728\u6267\u884c\u4efb\u52a1\u3002\u7535\u529b\u7684\u751f\u4ea7\u548c\u7ba1\u7406\u5bf9\u4e8e\u706b\u661f\u8f66\u7eed\u822a\u3001\u4eea\u5668\u8fd0\u884c\u4ee5\u53ca\u4e0e\u5730\u7403\u901a\u8baf\u662f\u81f3\u5173&#8230;<\/p>\n","protected":false},"author":1132,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-93805","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/93805"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1132"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=93805"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/93805\/revisions"}],"predecessor-version":[{"id":93827,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/93805\/revisions\/93827"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=93805"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=93805"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=93805"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}