{"id":95963,"date":"2017-08-12T06:30:55","date_gmt":"2017-08-11T22:30:55","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=95963"},"modified":"2017-08-11T15:56:41","modified_gmt":"2017-08-11T07:56:41","slug":"%e6%9c%b1%e5%98%89%e8%af%be%e9%a2%98%e7%bb%84natl-sci-rev-%ef%bc%9a%e4%ba%ba%e5%b7%a5%e8%92%b8%e8%85%be%ef%bc%9a%e6%96%b0%e5%9e%8b%e9%ab%98%e6%95%88%e5%a4%aa%e9%98%b3%e8%83%bd","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=95963","title":{"rendered":"\u6731\u5609\u8bfe\u9898\u7ec4Natl. Sci. Rev.\uff1a\u201c\u4eba\u5de5\u84b8\u817e\u201d\uff1a\u65b0\u578b\u9ad8\u6548\u592a\u9633\u80fd\u6c34\u5904\u7406\u7ed3\u6784"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u9ad8\u6548\u7684\u592a\u9633\u80fd\u8f6c\u6362\u4e0e\u5229\u7528\u88ab\u89c6\u4e3a\u56fd\u5bb6\u80fd\u6e90\u7684\u91cd\u5927\u9700\u6c42\u3002\u5176\u4e2d\uff0c\u5149-\u70ed\uff08\u84b8\u6c7d\uff09\u8f6c\u5316\u5728\u6d77\u6c34\u6de1\u5316\u3001\u5206\u998f\u3001\u706d\u83cc\u7b49\u9886\u57df\u5c55\u73b0\u51fa\u5f88\u597d\u7684\u5e94\u7528\u524d\u666f\u3002\u7136\u800c\u7531\u4e8e\u5149\u5b66\u548c\u70ed\u5b66\u7684\u635f\u8017\uff0c\u4f20\u7edf\u7684\u5149-\u70ed\uff08\u84b8\u6c7d\uff09\u8f6c\u5316\u6548\u7387\u8f83\u4f4e\uff08~40%\uff09\uff0c\u5f88\u5927\u7a0b\u5ea6\u4e0a\u9650\u5236\u4e86\u5176\u5e7f\u6cdb\u5e94\u7528\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p><strong>\u5357\u4eac\u5927\u5b66\u73b0\u4ee3\u5de5\u7a0b\u4e0e\u5e94\u7528\u79d1\u5b66\u5b66\u9662<\/strong><strong>\u6731\u5609\u6559\u6388\u8bfe\u9898\u7ec4<\/strong>\u5728\u9ad8\u6548\u754c\u9762\u5149\u70ed\u8f6c\u6362\u9886\u57df\u505a\u51fa\u4e86\u4e00\u7cfb\u5217\u5de5\u4f5c\uff1a\u9996\u5148\u6210\u529f\u5730\u5b9e\u73b0\u4e86\u6700\u9ed1\u7b49\u79bb\u6fc0\u5143\u5438\u6536\u4f53\u7684\u5236\u5907\uff08Science Advances, 2, e1501227 (2016)\uff09\uff1b\u5728\u6b64\u57fa\u7840\u4e4b\u4e0a\u5b9e\u73b0\u4e86\u9996\u4e2a\u57fa\u4e8e\u7b49\u79bb\u6fc0\u5143\u589e\u5f3a\u6548\u5e94\u7684\u592a\u9633\u80fd\u6d77\u6c34\u6de1\u5316\u5668\u4ef6\uff08Nature Photonics, 10, 393-398 (2016)\uff09\uff0c\u5f88\u5927\u7a0b\u5ea6\u89e3\u51b3\u4e86\u5438\u6536\u4f53\u7684\u5149\u5b66\u635f\u8017\u95ee\u9898\uff1b\u968f\u540e\u901a\u8fc7\u4e8c\u7ef4\u6c34\u901a\u9053\u7684\u8bbe\u8ba1\u6765\u5b9e\u73b0\u5438\u6536\u4f53\u4e0e\u6c34\u4f53\u7684\u95f4\u63a5\u63a5\u89e6\uff0c\u5927\u5927\u964d\u4f4e\u4e86\u5668\u4ef6\u5411\u6c34\u4f53\u7684\u70ed\u4f20\u5bfc\u635f\u8017\uff08PNAS, 113, 13953-13958 (2016)\uff09\u3002<\/p>\n<p>\u8fd1\u671f\uff0c\u8be5\u8bfe\u9898\u7ec4\u7740\u529b\u4e8e\u6700\u5927\u9650\u5ea6\u5730\u89e3\u51b3\u5728\u5b9e\u9645\u5e94\u7528\u4e2d\u592a\u9633\u80fd\u5165\u5c04\u89d2\u4e0d\u65ad\u53d8\u5316\u5e26\u6765\u7684\u5149\u5b66\u635f\u8017\u548c\u70ed\u5b66\u635f\u8017\uff08\u70ed\u4f20\u5bfc\uff0c\u70ed\u5bf9\u6d41\u548c\u70ed\u8f90\u5c04\uff09\u95ee\u9898\u5e76\u53d6\u5f97\u4e86\u5f88\u597d\u7684\u8fdb\u5c55\u3002\u8fd9\u9879\u6700\u65b0\u7684\u7814\u7a76\u6210\u679c\u4ee5<strong>\u201c<\/strong><strong>Three-dimensional artificial transpiration for efficient solar waste water treatment<\/strong><strong>\u201d<\/strong>\u4e3a\u9898\u53d1\u8868\u4e8e<strong>\u300a\u56fd\u5bb6\u79d1\u5b66\u8bc4\u8bba\u300b\uff08<\/strong><strong>National Science Review<\/strong><strong>\uff09<\/strong>\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>1 <\/strong><strong>\u4e0d\u540c\u592a\u9633\u80fd\u84b8\u6c7d\u53d1\u751f\u5668\u539f\u7406\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-95994 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e00.jpg\" alt=\"\" width=\"600\" height=\"573\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e00.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e00-300x287.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) \u4f20\u7edf\u7684\u5149-\u70ed(\u84b8\u6c7d)\u8f6c\u5316\u5668\u4ef6\u793a\u610f\u56fe<\/p>\n<p>(b) \u4e09\u7ef4(3D)\u4eba\u5de5\u84b8\u817e\u5668\u4ef6\u793a\u610f\u56fe<\/p>\n<p>(c-e) \u5438\u6536\u4f53\u3001\u6c34\u6269\u5c55\u5c42\u548c\u4e00\u7ef4\u6c34\u8def\u5f84\u7684\u7535\u955c\u56fe<\/p>\n<p><strong>\u56fe<\/strong><strong>2 <\/strong><strong>\u4e0d\u540c\u7684\u592a\u9633\u80fd\u84b8\u6c7d\u53d1\u751f\u5668\u7684\u6e29\u5ea6\u5206\u5e03\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-95991 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e8c.jpg\" alt=\"\" width=\"600\" height=\"595\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e8c.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e8c-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e8c-300x298.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a-c) \u4e8c\u7ef4\u76f4\u63a5\u63a5\u89e6\u3001\u4e8c\u7ef4\u95f4\u63a5\u63a5\u89e6\u548c\u4e09\u7ef4\u4eba\u5de5\u84b8\u817e\u5668\u4ef6\u56fe\u7247<\/p>\n<p>(d-f) \u5149\u7167\u524d\uff0c\u6c27\u5316\u77f3\u58a8\u70ef\u5c42\u7684\u6e29\u5ea6<\/p>\n<p>(g-i) 30min\u592a\u9633\u5149\u7167\u6761\u4ef6\u540e\uff0c\u6c27\u5316\u77f3\u58a8\u70ef\u5c42\u7684\u6e29\u5ea6<\/p>\n<p><strong>\u56fe<\/strong><strong>3 <\/strong><strong>\u5149\u7167\u6761\u4ef6\u4e0b\uff0c\u592a\u9633\u80fd\u84b8\u6c7d\u53d1\u751f\u5668\u7684\u6027\u80fd<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-95992 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e09.jpg\" alt=\"\" width=\"600\" height=\"420\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e09.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u4e09-300x210.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) \u5149\u7167\u548c\u975e\u5149\u7167\u6761\u4ef6\u4e0b\uff0c\u4e8c\u7ef4\u76f4\u63a5\u63a5\u89e6\u84b8\u817e\u5668\u4ef6\u8d28\u91cf\u968f\u65f6\u95f4\u53d8\u5316\u66f2\u7ebf<\/p>\n<p>(b) \u5149\u7167\u548c\u975e\u5149\u7167\u6761\u4ef6\u4e0b\uff0c\u4e8c\u7ef4\u95f4\u63a5\u63a5\u89e6\u84b8\u817e\u5668\u4ef6\u8d28\u91cf\u968f\u65f6\u95f4\u53d8\u5316\u66f2\u7ebf<\/p>\n<p>(c) \u5149\u7167\u548c\u975e\u5149\u7167\u6761\u4ef6\u4e0b\uff0c\u4e09\u7ef4\u4eba\u5de5\u84b8\u817e\u5668\u4ef6\u8d28\u91cf\u968f\u65f6\u95f4\u53d8\u5316\u66f2\u7ebf<\/p>\n<p>(d) \u5ba4\u5916\u9633\u5149\u7167\u5c04\u6761\u4ef6\u4e0b\uff0c\u4e8c\u7ef4\u76f4\u63a5\u63a5\u89e6\u3001\u4e8c\u7ef4\u95f4\u63a5\u63a5\u89e6\u548c\u4e09\u7ef4\u4eba\u5de5\u84b8\u817e\u5668\u4ef6<\/p>\n<p><strong>\u56fe<\/strong><strong>4 <\/strong><strong>\u592a\u9633\u80fd\u5e9f\u6c34\u5904\u7406\u7684\u4e24\u79cd\u9014\u5f84<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-95993 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u56db.jpg\" alt=\"\" width=\"600\" height=\"421\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u56db.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/\u56fe\u56db-300x211.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) \u5904\u7406\u524d\u540e\u4e0d\u540c\u91d1\u5c5e\u79bb\u5b50\u6d53\u5ea6\uff0c\u84dd\u8272\u7ebf\u53c2\u8003\u4e16\u754c\u536b\u751f\u7ec4\u7ec7\u7684\u996e\u7528\u6c34\u6807\u51c6<\/p>\n<p>(b) \u4e0d\u540cpH\u6761\u4ef6\u5904\u7406\u524d\u540e\u94dc\u79bb\u5b50\u6d53\u5ea6<\/p>\n<p>(c) \u4e09\u7ef4\u4eba\u5de5\u84b8\u817e\u5668\u4ef6\u7a33\u5b9a\u7684\u5faa\u73af\u6027\u80fd\uff0c\u5904\u7406\u94c5\u79bb\u5b50\u6c61\u67d3\u6c3450\u4e2a\u5faa\u73af\uff0c\u6bcf\u4e2a\u5faa\u73af\u6301\u7eed1h<\/p>\n<p>(d) \u7167\u5c04\u65f6\u95f4\u5185\u7eaf\u5316\u6c34\u7684\u8f93\u51fa\u91cf<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u8be5\u5de5\u4f5c\u9996\u6b21\u63d0\u51fa\u5e76\u5b9e\u73b0\u4e86\u201c\u4eba\u5de5\u84b8\u817e\u201d\u7ed3\u6784\uff0c\u7a81\u7834\u4f20\u7edf\u4e8c\u7ef4\u5e73\u9762\u5668\u4ef6\u7684\u5c40\u9650\uff0c\u8bbe\u8ba1\u51fa\u4e09\u7ef4\u7684\u7a7a\u5fc3\u9525\u5f62\u7ed3\u6784\uff0c\u5927\u5927\u7f13\u89e3\u4e86\u5668\u4ef6\u5728\u771f\u5b9e\u73af\u5883\u4e2d\u5bf9\u592a\u9633\u5149\u5165\u5c04\u89d2\u7684\u4f9d\u8d56\u6027\u3002\u540c\u65f6\uff0c\u6709\u6548\u5730\u964d\u4f4e\u4e86\u5668\u4ef6\u7684\u84b8\u53d1\u6e29\u5ea6\uff0c\u8fdb\u800c\u6709\u6548\u63a7\u5236\u4e86\u70ed\u5bf9\u6d41\u548c\u70ed\u8f90\u5c04\u7684\u635f\u8017\u3002\u201c\u4eba\u5de5\u84b8\u817e\u201d\u7ed3\u6784\u7684\u53e6\u4e00\u4e2a\u4f18\u52bf\u662f\u901a\u8fc7\u4e00\u7ef4\u7684\u4f9b\u6c34\u901a\u9053\u6709\u6548\u63a7\u5236\u70ed\u4f20\u5bfc\u635f\u8017\uff0c\u4ece\u800c\u9996\u6b21\u5b9e\u73b0\u4e86\u65e0\u5916\u754c\u8f85\u52a9\u3001\u6b63\u5e38\u5149\u7167\u6761\u4ef6\u4e0b85%\u4ee5\u4e0a\u7684\u5149-\u84b8\u6c7d\u8f6c\u6362\u6548\u7387\u3002\u5728\u5e94\u7528\u5c42\u9762\uff0c\u8be5\u5de5\u4f5c\u9996\u6b21\u5c06\u754c\u9762\u5149-\u84b8\u6c7d\u8f6c\u6362\u62d3\u5c55\u5230\u91cd\u91d1\u5c5e\u6c61\u6c34\u5904\u7406\u4e0a\u3002\u5b9e\u9a8c\u7ed3\u679c\u8868\u660e\uff1a\u8be5\u6280\u672f\u4e0d\u4ec5\u53ef\u4ee5\u5f97\u5230\u7b26\u5408\u996e\u7528\u6807\u51c6\u7684\u6c34\uff0c\u540c\u65f6\u4e5f\u53ef\u6709\u6548\u7684\u56de\u6536\u91cd\u91d1\u5c5e\uff08\u5982\u91d1\uff0c\u94dc\u7b49\uff09\uff0c\u4e3a\u9ad8\u6548\u7684\u592a\u9633\u80fd\u5149-\u70ed\uff08\u84b8\u6c7d\uff09\u7684\u5229\u7528\u548c\u53d1\u5c55\u63d0\u4f9b\u65b0\u7684\u601d\u8def\u3002<\/p>\n<p><strong>\u6587\u732e\u8fde\u63a5\uff1a<\/strong><a href=\"https:\/\/doi.org\/10.1093\/nsr\/nwx051\" target=\"_blank\" rel=\"noopener\">Three-dimensional artificial transpiration for efficient solar waste water treatment<\/a> (Natl. Sci. Rev., 2017, DOI: 10.1093\/nsr\/nwx051)<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u751f\u7269\u6750\u6599\u7ec4\u5728\u6cb3\u4e4b\u821f\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6750\u6599\u4eba\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u4eba\u7f51\u5411\u5404\u5927\u56e2\u961f\u8bda\u5fc3\u7ea6\u7a3f\uff0c\u8bfe\u9898\u7ec4\u6700\u65b0\u6210\u679c\u3001\u65b9\u5411\u603b\u7ed3\u3001\u56e2\u961f\u8bbf\u8c08\u3001\u5b9e\u9a8c\u6280\u80fd\u7b49\u7686\u53ef\u6295\u7a3f\uff0c\u4f18\u79c0\u7a3f\u4ef6\u4e00\u7ecf\u5f55\u7528\uff0c\u6211\u4eec\u4f1a\u5949\u4e0a\u7a3f\u916c\uff0c\u8bf7\u8054\u7cfb\uff1a\u90ae\u7bb1tougao@cailiaoren.com \u6216 QQ\uff1a97482208\u3002<\/p>\n<p><strong>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1a<\/strong><strong>xiaofire-18<\/strong><strong>\uff0c\u5434\u73ab\uff0c\u6211\u4eec\u4f1a\u62c9\u5404\u4f4d\u8001\u5e08\u52a0\u5165\u4e13\u5bb6\u7fa4\u3002<\/strong><\/p>\n<p>\u4eea\u5668\u8bbe\u5907\u3001\u8bd5\u5242\u8017\u6750\u3001\u6750\u6599\u6d4b\u8bd5\u3001\u6570\u636e\u5206\u6790\uff0c\u627e<a href=\"http:\/\/mai.cailiaoren.com\/\" target=\"_blank\" rel=\"noopener\">\u6750\u6599\u4eba<\/a>\u3001\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u9ad8\u6548\u7684\u592a\u9633\u80fd\u8f6c\u6362\u4e0e\u5229\u7528\u88ab\u89c6\u4e3a\u56fd\u5bb6\u80fd\u6e90\u7684\u91cd\u5927\u9700\u6c42\u3002\u5176\u4e2d\uff0c\u5149-\u70ed\uff08\u84b8\u6c7d\uff09\u8f6c\u5316\u5728\u6d77\u6c34\u6de1\u5316\u3001\u5206\u998f\u3001\u706d\u83cc\u7b49\u9886\u57df\u5c55\u73b0\u51fa\u5f88\u597d\u7684\u5e94\u7528\u524d\u666f\u3002\u7136\u800c\u7531\u4e8e\u5149\u5b66\u548c\u70ed\u5b66\u7684\u635f\u8017\uff0c\u4f20&#8230;<\/p>\n","protected":false},"author":2697,"featured_media":95994,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-95963","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/95963"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2697"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=95963"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/95963\/revisions"}],"predecessor-version":[{"id":96002,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/95963\/revisions\/96002"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/95994"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=95963"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=95963"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=95963"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}