{"id":99062,"date":"2017-09-02T14:00:14","date_gmt":"2017-09-02T06:00:14","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=99062"},"modified":"2017-08-31T15:47:26","modified_gmt":"2017-08-31T07:47:26","slug":"%e6%b7%b1%e5%9c%b3%e5%85%88%e8%bf%9b%e9%99%a2%e7%ad%89%ef%bc%9a%e5%9c%a8%e7%ba%b3%e7%b1%b3%e5%b0%ba%e5%ba%a6%e7%83%ad%e5%af%bc%e6%b5%8b%e9%87%8f%e9%a2%86%e5%9f%9f%e5%8f%96%e5%be%97%e8%bf%9b%e5%b1%95","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=99062","title":{"rendered":"\u6df1\u5733\u5148\u8fdb\u9662\u7b49\uff1a\u5728\u7eb3\u7c73\u5c3a\u5ea6\u70ed\u5bfc\u6d4b\u91cf\u9886\u57df\u53d6\u5f97\u8fdb\u5c55"},"content":{"rendered":"<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u65e5\u524d\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u6df1\u5733\u5148\u8fdb\u6280\u672f\u7814\u7a76\u9662\u4e0e\u534e\u76db\u987f\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u5728\u7eb3\u7c73\u5c3a\u5ea6\u8f93\u8fd0\u6027\u8d28\u7684\u5b9a\u91cf\u6d4b\u91cf\u9886\u57df\u53d6\u5f97\u8fdb\u5c55\u3002\u7814\u7a76\u6210\u679c\u4ee5<em><i>Quantitative nanoscale mapping of three-phase thermal conductivities in filled skutterudites via scanning thermal microscopy<\/i><\/em>\u4e3a\u9898\u53d1\u8868\u5728<em><i>National Science Review<\/i><\/em>\u4e0a\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe1\u00a0SThM\u8bbe\u7f6e\u539f\u7406\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-99063\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/1-91.png\" alt=\"\" width=\"600\" height=\"316\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/1-91.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/1-91-300x158.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u5e73\u8861\u60e0\u65af\u767b\u7535\u6865\u7535\u8def\u4e2d\u7684\u7535\u963b\u52a0\u70ed\u70ed\u63a2\u5934<\/p>\n<p>\uff08b,c\uff09\u70ed\u63a2\u9488\u7528\uff08b\uff09\u8f83\u4f4e\u548c\uff08c\uff09\u8f83\u9ad8\u7684\u70ed\u5bfc\u7387\u626b\u63cf\u76f8<\/p>\n<p><strong>\u56fe2\u00a0Yb<sub>0.7<\/sub>Co<sub>4<\/sub>Sb<sub>12<\/sub>\u7684SThM\u6620\u5c04<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-99064\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/2-59.png\" alt=\"\" width=\"600\" height=\"180\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/2-59.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/08\/2-59-300x90.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a,b\uff09\u60e0\u65af\u901a\u7535\u6865\u7684\uff08a\uff09\u5f62\u8c8c\uff08b\uff09\u7535\u538b\u5206\u5e03<\/p>\n<p>\uff08c\uff09BSE\u56fe\u50cf<\/p>\n<p><strong>\u3010\u7814\u7a76\u5185\u5bb9\u3011<\/strong><\/p>\n<p>\u7eb3\u7c73\u5c3a\u5ea6\u8f93\u8fd0\u6027\u8d28\u7684\u5b9a\u91cf\u6d4b\u91cf\u662f\u56fd\u5bb6\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u7eb3\u7c73\u79d1\u6280\u91cd\u70b9\u4e13\u9879\u7684\u4e00\u4e2a\u91cd\u8981\u76ee\u6807\u3002\u5728\u8fc7\u53bb20\u4f59\u5e74\uff0c\u7eb3\u7c73\u6750\u6599\u4e0e\u7ed3\u6784\u8fc5\u731b\u53d1\u5c55\uff0c\u6781\u5927\u63d0\u5347\u4e86\u6750\u6599\u7684\u5b8f\u89c2\u6027\u80fd\uff0c\u8fd9\u5728\u70ed\u7535\u9886\u57df\u5c24\u4e3a\u663e\u8457\uff0c\u7136\u800c\u7eb3\u7c73\u7ed3\u6784\u70ed\u7535\u6750\u6599\u7684\u6027\u80fd\u63d0\u5347\u5374\u662f\u5728\u65e0\u6cd5\u5bf9\u5176\u975e\u5747\u5300\u5206\u5e03\u7684\u70ed\u7535\u6027\u80fd\u8fdb\u884c\u51c6\u786e\u6d4b\u91cf\u7684\u80cc\u666f\u4e0b\u5b9e\u73b0\u7684\u3002\u5f53\u524d\u5c1a\u65e0\u6cd5\u5728\u7eb3\u7c73\u5c3a\u5ea6\u5b9a\u91cf\u6d4b\u91cf\u6750\u6599\u7684\u5c40\u57df\u6027\u80fd\uff0c\u56e0\u6b64\u4e5f\u65e0\u6cd5\u5c06\u7eb3\u7c73\u7ed3\u6784\u4e0e\u5176\u5b8f\u89c2\u6027\u80fd\u76f4\u63a5\u5173\u8054\uff0c\u53ea\u80fd\u4f9d\u9760\u8ba1\u7b97\u6750\u6599\u5b66\u7684\u7406\u8bba\u548c\u6a21\u62df\u6307\u5f15\u3002<\/p>\n<p>\u7814\u7a76\u4e2d\uff0c\u79d1\u7814\u4eba\u5458\u8fd0\u7528\u626b\u63cf\u70ed\u6210\u50cf\u539f\u5b50\u529b\u663e\u5fae\u955c\uff08SThM\uff09\u5b9a\u91cf\u6d4b\u91cf\u4e09\u76f8\u7ed3\u6784\u7684\u65b9\u94b4\u77ff\u70ed\u7535\u6750\u6599\u7684\u5c40\u57df\u70ed\u5bfc\u7387\uff0c\u901a\u8fc7\u80cc\u6563\u5c04\u7535\u5b50\u663e\u5fae\u955c\uff08BSE\uff09\u786e\u5b9a\u6750\u6599\u7684\u5fae\u533a\u6210\u5206\uff0c\u518d\u901a\u8fc7\u70ed\u63a2\u9488\u5b9e\u73b0\u540c\u4e00\u5c40\u57df\u7684\u70ed\u6210\u50cf\uff08SThM\uff09\u3002\u4ee5\u5f80SThM\u6210\u50cf\u500d\u53d7\u5f62\u8c8c\u8d77\u4f0f\u7684\u5e72\u6270\uff0c\u4f46\u5728\u8fd9\u4e00\u5de5\u4f5c\u4e2d\uff0c\u70ed\u6210\u50cf\uff08SThM\uff09\u4e0e\u5f62\u8c8c\u50cf\uff08Topography\uff09\u6ca1\u6709\u5173\u8054\uff0c\u800c\u4e0e\u6210\u5206\u76f8\uff08BSE\uff09\u4e00\u4e00\u5bf9\u5e94\uff0c\u8fd9\u4e00\u53d1\u73b0\u524d\u6240\u672a\u6709\u3002\u501f\u52a9\u4e8e\u4e00\u7cfb\u5217\u6807\u51c6\u6837\u54c1\u7684\u6807\u5b9a\uff0c\u7ed3\u5408\u6709\u9650\u5143\u5c40\u57df\u70ed\u4f20\u5bfc\u8fc7\u7a0b\u6a21\u62df\uff0c\u7814\u7a76\u4eba\u5458\u786e\u5b9a\u51fa\u6750\u6599\u5c40\u57df\u7684\u70ed\u5bfc\u7387\u5206\u5e03\uff0c\u5e76\u51c6\u786e\u6355\u6349\u5176\u5728\u4e24\u76f8\u754c\u9762\u5904\u7684\u53d8\u5316\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u5f97\u5230\u56fd\u5bb6\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u7eb3\u7c73\u79d1\u6280\u91cd\u70b9\u4e13\u9879\u7684\u652f\u6301\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.cas.cn\/syky\/201708\/t20170825_4612263.shtml\" target=\"_blank\" rel=\"noopener\">http:\/\/www.cas.cn\/syky\/201708\/t20170825_4612263.shtml<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/doi.org\/10.1093\/nsr\/nwx074\" target=\"_blank\" rel=\"noopener\">Quantitative nanoscale mapping of three-phase thermal conductivities in filled skutterudites via scanning thermal microscopy<\/a> \uff08Natl.Sci.Rev. ,2017, DOI:10.1093\/nsr\/nwx074\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8Allen\u7f16\u8f91\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u6210\u679c\u7b80\u4ecb\u3011 \u65e5\u524d\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u6df1\u5733\u5148\u8fdb\u6280\u672f\u7814\u7a76\u9662\u4e0e\u534e\u76db\u987f\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u5728\u7eb3\u7c73\u5c3a\u5ea6\u8f93\u8fd0\u6027\u8d28\u7684\u5b9a\u91cf\u6d4b\u91cf\u9886\u57df\u53d6\u5f97\u8fdb\u5c55\u3002\u7814\u7a76\u6210\u679c\u4ee5Quantitative nanosc&#8230;<\/p>\n","protected":false},"author":349,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-99062","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/99062"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/349"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=99062"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/99062\/revisions"}],"predecessor-version":[{"id":99559,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/99062\/revisions\/99559"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=99062"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=99062"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=99062"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}